297 resultados para TEMPERATURE PHOTOLUMINESCENCE

em Chinese Academy of Sciences Institutional Repositories Grid Portal


Relevância:

100.00% 100.00%

Publicador:

Resumo:

We report a room temperature study of the direct band gap photoluminescence of tensile-strained Ge/Si0.13Ge0.87 multiple quantum wells grown on Si-based germanium virtual substrates by ultrahigh vacuum chemical vapor deposition. Blueshifts of the luminescence peak energy from the Ge quantum wells in comparison with the Ge virtual substrate are in good agreement with the theoretical prediction when we attribute the luminescence from the quantum well to the c Gamma 1-HH1 direct band transition. The reduction in direct band gap in the tensile strained Ge epilayer and the quantum confinement effect in the Ge/Si0.13Ge0.87 quantum wells are directly demonstrated by room temperature photoluminescence.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Novel room temperature photoluminescence (PL) of the Ge/Si islands in multilayer structure grown on silicon-on-insulator substrates is investigated. The cavity formed by the mirrors at the surface and the buried SiO2 interface has a strong effect on the PL emission. The peak position is consistent with the theoretical calculation and independent of the exciting power, which is the evidence of cavity effect on the room temperature photoluminescence. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Wurtzite ZnO/MgO superlattices were successfully grown on Si (001) substrates at 750 degrees C using radio-frequency reactive magnetron sputtering method. X-ray reflection and diffraction, electronic probe and photoluminescence analysis were used to characterize the multiple quantum wells (MQWs). The results showed the periodic layer thickness of the MQWs to be 1.85 to 22.3 nm. The blueshift induced by quantum confinement was observed. Least square fitting method was used to deduce the zero phonon energy of the exciton from the room-temperature photoluminescence. It was found that the MgO barrier layers has a much larger offset than ZnMgO. The fluctuation of periodic layer thickness of the MQWs was suggested to be a possible reason causing the photoluminescence spectrum broadening.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The influences of the cavity on the low-temperature photoluminescence of Si0.59Ge0.41/Si multiquantum wells grown on silicon-on-insulator substrates are discussed. The positions of the modulated photoluminescence (PL) peaks not only relate to the nature of SiGe/Si multiquantum wells, but also relate to the characteristic of the cavity. With increasing temperature, a redshift of the modulated PL peak originating from the thermo-optical effect of the cavity is observed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Photoluminescence measurements have been performed in Si-rich a-SiNx:H (x less than or equal to 1.3) alloys prepared by glow discharge. It is observed that the blue shift of the peak of room temperature luminescence spectrum with increasing N content parallels increasing intensity. Two distinct luminescence mechanisms are proposed in a-SiNx:H with the threshold near x = 0.8. For low x, the samples show typical luminescence properties of a-Si:H, while for high x, the normalized luminescence bands are independent of temperature. Combining percolation theory, the luminescence origins are discussed on the basis of Brodsky's quantum well model. (C) 2000 Elsevier Science B.V. All rights reserved.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

A series of metamorphic high electron mobility transistors (MMHEMTs) with different V/III flux ratios are grown on GaAs (001) substrates by molecular beam epitaxy (XIBE). The samples are analysed by using atomic force microscopy (AFM), Hall measurement, and low temperature photoluminescence (PL). The optimum V/III ratio in a range from 15 to 60 for the growth of MMHEMTs is found to be around 40. At this ratio, the root mean square (RMS) roughness of the material is only 2.02 nm; a room-temperature mobility and a sheet electron density are obtained to be 10610.0cm(2)/(V.s) and 3.26 x 10(12)cm(-2) respectively. These results are equivalent to those obtained for the same structure grown on InP substrate. There are two peaks in the PL spectrum of the structure, corresponding to two sub-energy levels of the In0.53Ga0.47 As quantum well. It is found that the photoluminescence intensities of the two peaks vary with the V/III ratio, for which the reasons are discussed.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

The effect of thermal annealing on the luminescence properties of neon implanted GaN thin films was studied. Low temperature photoluminescence (PL) measurements were carried out on the samples implanted with different doses ranging from 10(14) to 9 x 10(15) cm(-2) and annealed isochronally at 800 and 900 degrees C. We observed a new peak appearing at 3.44 eV in the low temperative PL spectra of all the implanted samples after annealing at 900 degrees C. This peak has not been observed in the PL spectra of implanted samples annealed at 800 degrees C except for the samples implanted with the highest dose. The intensity of the yellow luminescence (YL) band noticed in the PL spectra measured after annealing was observed to decrease with the increase in dose until it was completely suppressed at a dose of 5 x 10(15) cm(-2). The appearance of a new peak at 3.44 eV and dose dependent suppression of the YL band are attributed to the dissociation of VGaON complexes caused by high energy ion implantation.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Wurtzite stalactite-like quasi-one-dimensional ZnS nanoarrays with ZnO protuberances were synthesized through a thermal evaporation route. The structure and morphology of the samples are studied and the growth mechanism is discussed. X-ray diffraction (XRD) results show both the ZnS stem and the ZnO protuberances have wurtzite structure and show preferred [001] oriented growth. The photoluminescence and field emission properties have also been investigated. Room temperature photoluminescence result shows it has a strong green light emission, which has potential application for green light emitter. Experimental results also show that the stalactite arrays have a good field emission property, with turn-on field of 11.4 V/mu m, and threshold field of 16 V/mu m. The ZnO protuberances on the ZnS stem might enhance the field emission notably.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

This letter reports on the Raman, optical and magnetic properties of FeNi co-doped ZnO nanowires prepared via a soft chemical solution method. The microstructural investigations show that the NiFe co-dopants are substituted into wurtzite ZnO nanostructure without forming any secondary phase. The co-doped nanowires show a remarkable reduction of 34 nm (267.9 meV) in the optical band gap, while suppression in the deep-level defect transition in visible luminescence. Furthermore, these nanowires exhibit ferromagnetism and an interesting low-temperature spin glass behavior, which may arise due to the presence of disorder and strong interactions of frustrated spin moments of Ni and Fe co-dopants on the ZnO lattice sites. Copyright (C) EPLA, 2009

Relevância:

70.00% 70.00%

Publicador:

Resumo:

A two-step approach of preparation for SiGe/Si heterogeneous nanostructures, which combined with ultra-high vacuum chemical deposition and electrochemical anodization techniques, is demonstrated. Uniformly distributed nanostructures with a quite uniform distribution of size and morphology are obtained. A strong room-temperature photoluminescence from the nanostructures was observed with a narrow full-width at half-maximum of around 110 meV. The possible origins of the two main peaks at around 1.6 and 1.8 eV have been discussed in detail. The two-step approach is proved to be a promising method to fabricate new Si-based optoelectronic materials. (C) 2009 Elsevier B.V. All rights reserved.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Two emission peaks were observed in the low temperature photoluminescence (LTPL) spectra of an InGaN/GaN multiple quantum well (MQW) structure before and after nanopillar fabrication. After nanopillar fabrication it is found that among the two peaks the longer wavelength peak exhibits a clear blue shift and has a much stronger enhancement in LTPL intensity than the shorter one. Combined with x-ray diffraction and spatially resolved cathodoluminescence analyses, the difference induced by nanopillar fabrication is ascribed to different strain relaxation states in the lower and upper quantum well layers. It is found that the lower QW layers of the as-grown MQW which causes the longer wavelength PL peak are more strained, while the upper ones are almost fully strain-relaxed. Therefore, the nanopillar fabrication induces much less strain relaxation in the upper part of the MQW than in the lower one.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Sharp and strong room-temperature photoluminescence (PL) of the Si0.59Ge0.41/Si multiquantum wells grown on the silicon-on-insulator substrate is investigated. The cavity formed by the mirrors at the surface and the buried SiO2 interface enhances the PL emission and has a wavelength-selective effect on the luminescence. The peak position is consistent with the simulation result and independent of the exciting power, which indicates a strong cavity effect on the room-temperature PL. (C) 2004 American Institute of Physics.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Low-temperature photoluminescence measurement is performed on an undoped AlxGa1-xN/GaN heterostructure. Temperature-dependent Hall mobility confirms the formation of two-dimensional electron gas (2DEG) near the heterointerface. A weak photoluminescence (PL) peak with the energy of similar to 79meV lower than the free exciton (FE) emission of bulk GaN is related to the radiative recombination between electrons confined in the triangular well and the holes near the flat-band region of GaN. Its identification is supported by the solution of coupled one-dimensional Poisson and Schrodinger equations. When the temperature increases, the red shift of the 2DEG related emission peak is slower than that of the FE peak. The enhanced screening effect coming from the increasing 2DEG concentration and the varying electron distribution at two lowest subbands as a function of temperature account for such behaviour.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Mn-doped ZnS nanocrystals of about 3 nm diameter were synthesized by a wet chemical method. X-ray diffraction (XRD) measurements showed that the nanocrystals have the structure of cubic zinc blende. The broadening of the XRD lines is indicative of nanomaterials. Room temperature photoluminescence (PL) spectrum of the undoped sample only exhibited a defected-related blue emission band. But for the doped samples, an orange emission from the Mn2+ T-4(1)-(6)A(1) transition was also observed, apart from the blue emission. The peak position (600 nm) of the Mn2+ emission was shifted to longer wavelength compared to that (584 nm) of bulk ZnS:Mn. With the increase of the Mn2+ concentration, the PL of ZnS:Mn was significantly enhanced. The concentration quenching effect was not observed in our experiments. Such PL phenomena were attributed to the absence of Mn2+ pairs in a single ZnS:Mn nanocrystal, considering the nonradiative energy transfer between Mn2+ ions based on the Poisson approximation. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

The room-temperature photoluminescence (PL) of copper doped zinc sulfide (ZnS:Cu) nanoparticles were investigated. These ZnS:Cu nanoparticles were synthesized by a facile wet chemical method, with the copper concentration varying from 0 to 2 mol%. By Gaussian fitting, the PL spectrum of the undoped ZnS nanoparticles was deconvoluted into two blue luminescence peaks (centered at 411 nm and 455 nm, respectively), which both can be attributed to the recombination of the defect sates of ZnS. But for the doped samples, a third peak at about 500 nm was also identified. This green luminescence originates from the recombination between the shallow donor level (sulfur vacancy) and the t(2) level of Cu2+. With the increase of the CU2+ concentration, the green emission peak is systematically shifted to longer wavelength. In addition, it was found that the overall photoluminescence intensity is decreased at the Cu2+ concentration of 2%. The concentration quenching of the luminescence may be caused by the formation of CuS compound. (c) 2005 Elsevier B.V. All rights reserved.