302 resultados para Diagramma E-R redattore ER modello relazionale SharpER

em Chinese Academy of Sciences Institutional Repositories Grid Portal


Relevância:

100.00% 100.00%

Publicador:

Resumo:

General equations of the electrocatalytic reaction at an ultramicroelectrode modified with redox species have been described according to the Andrieux Saveant model. The electrocatalytic kinetic process has been discussed for the whole set of cases, ie (R), (R + S), (SR) (SR + E), (E), (R + E), (ER), (S), (ER + S) and (S + E) limiting situations. The effect of gamma on the catalytic steady state current shows that the higher the value of gamma, the lower the catalytic current. The kinetic process shifts rapidly from R to E with increasing values of gamma. It is favorable for catalysis only when gamma is very low. Therefore, the redox species modified ultramicroelectrode with thin film is utilized for electrocatalysis, and the larger the radius of ultramicroelectrode, the higher the catalytic efficiency.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The structure and magnetic properties of the RCo5Ga7 (R = Y, Tb, Dy, Ho and Er) compounds with the ScFe6Ga6-type structure have been studied. The stability of RCo5Ga7 is closely related with the ratio of the metal radii R-RE/R-(Co,R-Ga). With R-RE/R-(Co,R-Ga) less than or equal to 1.36, the compounds can be stabilized in the ScFe6Ga6-type structure. The lattice of RCo5Ga7 shrinks as the atomic order of R increases, and it is consistent with the lanthanide contraction. The structure analysis based on X-ray diffraction patterns reveals that in the orthorhombic RCo5Ga7 (Immm), R occupies the 2a site, and Co enters into the 8k and the 4h sites, and Ga is at the 4e, 4f, 4g, 4h and 8k sites. The interatomic distances and the coordination numbers of RCo5Ga7 are provided from the refinement results. The short interatomic distance (less than 2.480 Angstrom) between the Co ions results in the negative magnetic interaction, which does not favor ferromagnetic ordering. The magnetic moment of YCo5Ga7 is absent, and RCo5Ga7 (R = Tb, Dy, Ho and Er) may have long-range magnetic ordering with the paramagnetic Curie temperature lower than 5 K. (C) 2004 Elsevier Inc. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

对于稀土与非稀土所组成的二元复合氧化物的研究国外已有较多的报导。但是,对于稀土和锑的复合氧化物只是近年来才开始有些研究工作。含锑与稀土的多元复合氧化物的报导就更少。本文在我们实验室张静筠等人三元复合氧化物研究的基础上,开展Mo—Sb_2O_5—R_2O_3—R'_2O_3—Bi_2O_3多元体系的研究工作,这对于我国丰产元素稀土和锑的应用以及利用Bi~(3+)的激活与敏化将是有益的。本文按Thornton等人的方法合成了Ba_2BiSbO_6,Ba_2GdSbO_6,按EγΦECEHKO等人的方法合成了M_2RSbO_6 (M = Ba、Sr、Ca, R = La Y)。并以M_2RSbO_6为基质,掺Sm~(3+)、Eu~(3+)、Dy~(3+)、Ho~(3+)、Er~(3+)、Tm~(3+)和Bi~(3+),研究它们的化学组成,晶体结构与发光性能的关系及规律,Bi~(3+)的荧光和敏作用。同时研究了它们的磁学和热学性能。化学组成的分析结果表明,计算的含量与实验测得的含量符合较好,说明化学反应是按化学计量比进行的。通过X-射线粉沫物相分析和晶胞参数的理论计算确定M_2RSbO_6(M = Ba、Sr、R = La、Y、Gd、Bi)复合氧化物是属于立方钙钛太型化合物。空间群为Fm3m,点群为Oh。用计算机计算了Ca_2YSbO_6的晶胞参数并结合荧光光谱分析确定它属于畸变的单斜钙钛矿,空间群为P_(21)。用磁天平测量了样品M_2RSbO_6 (M = Ba、Sr、Ca; R = Gd、Y、Bi)的磁化率。除Ba_2GdSbO_6是顺磁性物质外共余的都是反磁性的物质。按所用原料Sb_2O_5计算的磁化率与测量值符合较好,表明在所研究的M_2RSbO_6化合物中锑是正五价的。用热重热差分析仪测量了样品在反应中的热性能,观察到在化合物形成的过程中所用原料Sb_2O_3大约在520 ℃左右氧化变为Sb_2O_5。除所用原料碳酸盐分解外没有挥发性的物质,这就进一步证明化学组成分析和磁化率测量的结果是正确的。光学测量的结果表明,所有的磷光体随着激活离子浓度的不同其光谱都发生规律性的变化。对于不同Eu~(3+)浓度的Ba_2YSbO_6:Eu~(3+)和Br_2YSbO_6:Eu~(3+), Bi~(3+)体系用254nm激发时均能观察到Eu~(3+)于595nm的尖峰发射。用基质和Bi~(3+)的激发峰325nm激发时,明显地看到敏化剂Bi~(3+)到Eu~(3+)的能量传递,使Eu~(3+)于595nm的发射大大增强,我们认为Bi~(3+)对Eu~(3+)的敏化作用是由于基质和Bi~(3+)的~1S。→ 3P_1的跃迁吸收了激发的能量,然后无辐射弛豫到Eu~(3+)的激发态~5D_0,产生~5D_0 → 7F_1的磁偶极跃迁。对于不同Eu~(3+)浓度的Sr_2YSbO_6:Eu~(3+)和Sr_2YSbO_6:Eu~(3+), Bi~(3+)体系用245nm激发时均能观察到Eu~(3+)于595nm的尖峰发射。用基质和Bi~(3+)的激发峰335nm激发时,观察到基质和Bi~(3+)对Eu~(3+)具有某种能量传递。敏化作用机理与上述的Ba_2YSbO_6:Eu~(3+)和Ba_2YSbO_6:Eu~(3+), Bi~(3+)体系相同。对于不同Eu~(3+)浓度的Ca_2YSbO_6:Eu~(3+)和Ca_2YSbO_6:Eu~(3+), Bi~(3+)体系用396nm激发时,均能观察到Eu~(3+)于613nm很强的尖峰发射。用基质和Bi~(3+)的激发峰313nm激发时,见到Bi~(3+)和基质对Eu~(3+)具有某种能量传递,这种敏化作用主要是由于基质和Bi~(3+)的3P_1 → ~1S_0的400nm的宽带发射和Eu~(3+)的~7F_0 → ~5L_6的396nm的吸收相匹配产生~5L_6→~5D_0→~7F_2的跃迁。通过对激发光谱和荧光光谱的分析给出了Ca_2Y_(0.96)Eu_(0.04)SbO_6的能级图,从实验上可见,Eu~(3+)的发光强烈地依赖于钙钛矿的结构,当Eu~(3+)在空间群为Fm3m 的Ba_2YSbO_6和Sr_2YSbO_6中处于Oh点对称性时,主要是~5D_0 → ~7F_1的磁偶极跃迁。当Eu~(3+)在空间群为P_(21)的单斜钙钛矿中时,主要是~5D_0 → ~7F_2的电偶极跃迁。对于不同掺杂浓度M_2YSbO_6:R~(13+)(M = Ba、Ca; R' = Sm、Dy、Ho、Er、Tm)体系,通过激发和荧光光谱的研究,合理地确定了谱项。发现基质对Sm~(3+)、Dy~(3+)、Ho~(3+)具有敏化作用。对不同Bi~(3+)浓度的Ca_2YSbO_6:Bi~(3+),由激发和荧光光谱可见Bi~(3+)具有二个激发带,第一激发带位于240nm处相当于~1S_0 → ~1P_1的跃迁,第二激发带位于315nm处相当于~1S_0 → ~3P_1的跃迁。有一个很强的兰紫色发射位于400nm处相当于~3P_1 →~1S_0的跃迁。

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Chemical bond parameters in RBa2Cu4O8(R = Dy, Ho, Er, Tm, Yb) and Y2Ba4Cu7O14.3 were calculated by using complex chemical bond theory. The results indicated that the bond covalency in CuO chain was larger than that in CuO2 plane. For metal atoms, the bond covalency of five coordinated case was larger than that of six coordinated case.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

使用复杂晶体上化学键理论计算了 RBa2 Cu4 O8(R=Dy,Ho,Er,Tm ,Yb)和 Y2 Ba4 Cu7O14 .3 的化学键参数 .结果表明 ,Cu O链上的 Cu O键共价性大于它们在 Cu O2 面的共价性 .当金属元素与氧形成五配位时 ,其共价性的数值大于这些元素在六配位时的情形

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Bond covalencies in R2BaCuO5 (R = Sm, Gd, Dy, Ho, Y, Er, Tm, Yb, Lu) were calculated by means of a semiempirical method. This method is the generalization of the dielectric description theory of Phillips-Van Vechten-Levine-Tanaka scheme. The present paper presents the formula concerning the decomposing of complex crystals which are usually anisotropic systems into the sum of binary crystals which are isotropic systems. It can be seen that although the bond covalency is related to many physical quantities, it is mainly influenced by bond valence or bond charge, and a higher bond valence will produce higher bond covalency.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

RBa2Cu3O7 (R = Pr, Sm, Eu, Gd, Dy, Y, Ho, Er, Tm) has been studied using complex chemical bond theory. The results indicated that with the decreasing of R radius, the ionicities for all considered types of bond decrease. This is in good agreement with the experimental fact that T-c decreases with the decreasing of R radius. PrBa2Cu3O7 with no Ba-site Pr in this calculation is also predicted to be a superconductor. This supports the conclusion obtained by Blackstead et al. The ionicity for each bond obeys the following order: Ba-O > R-O > Cu(2)-O(1) > Cu(2)-O(2,3) > Cu(1)-O(4) similar to Cu(1)-O(1).

Relevância:

30.00% 30.00%

Publicador:

Resumo:

用提拉法成功地生长了6mol%的高浓度掺铒铌酸锂晶体。测量了晶体的两个非偏振方向(X和Z)以及两个偏振方向(π和δ)的吸收光谱。高浓度掺铒铌酸锂晶体的吸收系数高,有利于提高泵浦效率。根据所测的吸收光谱用Judd-Ofelt理论拟合出了Er^3+离子的强度参数Ωλ。所得的均方差结果显示偏振拟合的误差要小于非偏振拟合。利用偏振吸收数据计算了各能级跃迁的自发辐射跃迁几率(AJJ’)、辐射寿命(τ)、荧光分支比(β)和积分发射截面(σp)等参数,对计算结果进行了讨论并与其他文献的报道结果进行了比较。

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The contamination and distribution of polychlorinated dibeinizo-p-dioxins and dibenzofurans (PCDD/Fs) from two agricultural fields of a heavily polluted lake area in China (Ya-Er Lake) are presented. The vertical distribution pattern of total PCDD/Fs in soil cores reveals that the maximum concentration was in the layer of 20-30 cm. The concentrations in the top layer of soil at the two sites were similar (17.48 ng/kg at Site 1 and 18.10 ng/kg at Site 2), but the maximum concentration of Site 1 (120.8 ng/kg) was two times higher than that of Site 2 (64.39 ng/kg). The maximum concentration of PCDD/Fs in mud cores in rice fields (0-50 cm) at Sites 1 and 2 was in the layer of 0-10 cm. The maximum PCDD/F concentration in the top layer in mud at Site 1 (203.1 ng/kg) was higher than that at Site 2: (143.3 ng/kg). Significant correlations were found between the mind PCDD/Fs and the organic carbon content (R = 0.9743, P< 0,05 at Site 1; R = 0.9821, P< 0.05 at Site 2), the two variables being highly correlated (R = 0.9049, P< 0.05, at Site 1; R = 0.9916, P< 0.05 at Site 2). All correlation coefficients were significant at the 95% level. Concentrations were highly correlated with organic carbon, indicating that sorption to organic carbon was the dominant mechanism. Using principal component analysis, the homologue profiles of soil, mud, and plants (rice and radish) were compared. The PCDD/F patterns in plants were found not to be correlated to those in soil and mud. This suggests that atmospheric deposition may be the main source of PCDD/Fs in rice grain. However, mixed exposure involving uptake mechanisms and atmospheric deposition is considered main the source of PCDD/F pollution in radishes. (C) 2002 Elsevier Science (USA).

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Photoluminescence from Er3+-implanted Si-in-SiN, films emitting efficiently visible light were investigated. A Stark structure in the Er3+ photoluminescence spectrum was observed at room temperature, which reveals more than one site symmetry for the Er3+-centers in the Si-in-SiN, matrix. The correlation between the visible photoluminescence from the silicon nanoparticles and the 1.54 mu m emission from the Er3+-centers was discussed. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

本论文合成了R_1Ba_2Cu_3O_(2-x) (R = La、Nd、Sm、Eu、Gd、Dr、Ho、Er、Tm、Yb)、Y_2Ba_2Cu_3O_(2-x) (x = 0.10~1.17)和Y_1Ba_2Cu_3O_(7-x)S_x (x = 0~2),并对磁性和超导电性进行了较为系统的研究。R_1Ba_2Cu_3O_(2-x)的磁化率在T > Tc的很宽的温度范围内服从Curic-Weiss定律,求得的有效磁矩略大于理论值,差值与Y_1Ba_2Cu_3O_(2-x)中Cu~(2+)磁矩相近,说明Cu~(2+)的磁矩对体系磁性有额外贡献,这贡献随R~(3+)离子中自旋平行的电子权的增多而增大。其高温下的磁化率CT > 700K)相对Curic-Weiss定律发生较大偏离,这偏离可能的来源有三个:高温下稀土离子发生较大的能级反转效应,高温下结构相变对磁性的影响,高温下氧含量减少造成Cu~(2+)磁矩增大。R_1Ba_2Cu_3O_(2-x)磁化率在T < Tc时也服从Curic-Weiss定律,R~(3+)磁矩是定域的,表明超导与磁性相互独立。互不相关,稀土磁矩与传导电子间无相互作用。用Sr取代R_1Ba_2Cu_3O_(2-x)中的Ba,没能使体系产生磁有序的变化,但却使有效磁矩增大,并完全破坏了样品的超导电性。Sm~(3+)磁化率不服从Curic-Weiss定律,在Sm_1Ba_2Cu_3O_(2-x)中Sm~(3+)显示了典型Van VlccK离子的特性。Y_1Ba_2Cu_3O_(2-x)随氧含量减少发生超导体一半导体一绝缘体的转化,当氧含量由6.90减小至6.49时发生由正交到四方的结构相变。当(7-x) = 5.83时有较多杂质相出现,123相开始分解。样品磁化率均服从Curic-Weiss定律,并随氧含量增大磁化率-温度曲线越来越趋于平缓(直线),当(7-x) = 6.90时磁化率基本不随温度变化,这时Pauli顺磁性占主导地位,这说明氧含量增加定域磁矩减少,求得的有效磁矩Peff随氧含量增大总趋势减小。提出了电子“巡游”的观点,较好地解释了上述现象,并推测出Cu(2)的d电子是离域的,对样品磁矩没有贡献,样品Peff来源于部分Cu(1)的定域Cu~(2+)的磁矩,上述推测被EPR结果证实。正交相Y_1Ba_2Cu_3O_(2-x)的EPR谱显示了中心对称成准立方晶场中Cu~(2+)(d~9, S = 1/2, I = 3/2)的EPR物性。而四方相样品的EPR谱却出现了明显的各向异性,说明观察到的为Cu(1)的EPR信号,由Cu(1)~(2+)的写域磁矩产生。Y_1Ba_2Cu_3O_(2-x)的EPR信号束源于本体相,而非Y_2Cu_2O_5、BaCuO_2、Y_2BaCuO_5等杂质相。各样品EPR信号的自旋浓度远小于1spin/cu,并随氧含量减小而增大,当(7-x) = 6.49、6.40时自旋浓度出现陡增,这时伴随由正交到四方的转化,证明了电子“巡游”观点的正确。用硫部分取代Y_1Ba_2Cu_3O_2g中的氧,当Y_1Ba_2Cu_3O_(2-x)Sx中x = 0.11时Tc = 92.6K,比Y_1Ba_2Cu_3O_(7-x)升高2K,但由于杂质相的存在,ΔTc加宽。其他样品多为半导体和绝缘体。硫取代0,当x = 0.04,0.06,0.11和1.20时磁化率服从Curic-Weiss定律,并且x = 0.87,1.2时分别在230K、240K出现反铁磁有序。其他样品由于Cu被还原为+1价而变成抗磁性。x = 0.11 (Tc = 92.6K),EPR谱为正交场中Cu~(2+)的信号。自旋浓度与温度无关。当所有Cu均为Cu~(1+)时,测问的是-s-的EPR信号,而Cu为混合价态(+1和+2时)测问是上述两种信号的叠加。

Relevância:

30.00% 30.00%

Publicador:

Resumo:

SiOx films with oxygen concentrations ranging 13-46 at.% were deposited by plasma enhanced chemical vapor deposition (PECVD) technique using: pure SiH4 and N2O mixture. Erbium was then implanted at an energy of 500 KeV with dose of 2x10(15) ions/cm(2). The samples were subsequently annealed in N-2 for 20 sec at temperatures of (300-950 degrees C). Room temperature (RT) photo-luminescence (PL) data were collected by Fourier Transform Infrared Spectroscopy (FTIS) with an argon laser at a wavelength of 514.5 nm and an output power from 5 to 2500 mw. The intense room-temperature luminescence was observed around 1.54 mu m. The luminescence intensity increases by 2 orders of magnitude as compared with that of Er-doped Czochralski (CZ) Si. We found that the Er3+ luminescence depends strongly on the SiOx microstructure. Our experiment also showed that the silicon grain radius decreased with increasing oxygen content and finally formed micro-crystalline silicon or nano-crystalline silicon. As a result, these silicon small particles could facilitate the energy transfer to Er3+ and thus enhanced the photoluminescence intensity.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In this study, we report the dependences of infrared luminescence properties of Er-implanted GaN thin films (GaN:Er) on the kinds of substrates used to grow GaN, the growth techniques of GaN, the implantation parameters and annealing procedures. The experimental results showed that the photoluminescence (PL) intensity at 1.54 mum was severely influenced by different kinds of substrates. The integrated PL peak intensity from GaN:Er /Al2O3 (00001) was three and five times stronger than that from GaN:Er /Si (111) grown by molecular beam epitaxy (MBE) and by metalorganic chemical vapor deposition (MOCVD), respectively. The PL spectra observed from GaN:Er/Al2O3 (0001) grown by MOCVD and by MBE displayed a similar feature, but those samples grown by MOCVD exhibited a stronger 1.54 mum PL. It was also found that there was a strong correlation between the PL intensity with ion implantation parameters and annealing procedures. Ion implantation induced damage in host material could be only partly recovered by an appropriate annealing temperature procedure. The thermal quenching of PL from 15 to 300 K was also estimated. In comparison with the integrated PL intensity at 15 K, it is reduced by only about 30 % when going up to 300 K for GaN:Er/Al2O3 sample grown by MOCVD. Our results also show that the strongest PL intensity comes from GaN:Er grown on Al2O3 substrate by MOCVD. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Photoluminescence (PL) from Er-implanted hydrogenated amorphous silicon suboxide (a-SiOX:H<Er>(x<2.0)) films was measured. Two luminescence bands with maxima at lambda congruent to 750 nm and lambda congruent to 1.54mum, ascribed to the a-SiOX:H intrinsic emission and Er3+ emission, were observed. Peak intensities of the two bands follow the same trend as a function of annealing temperature from 300 to 1000degreesC. Micro-Raman results indicate that the a-SiOX:H<Er> films are a mixture of two phases, an amorphous SiOX matrix and amorphous silicon (a-Si) domains embedded there in. FTIR spectra confirm that hydrogen effusion from a-SiOX:H<Er> films occurs during annealing. Hydrogen effusion leads to a reconstruction of the microstructure of a-Si domains, thus having a strong influence on Er3+ emission. Our study emphasizes the role of a-Si domains on Er3+ emission in a-SiOX:H<Er> films.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Theoretical researches are performed on the alpha-R2MoO6 (R = Y, Gd, Tb Dy, Ho, Er, Tm and Yb) and pyrochlore-type R2Mo2O7 (R = Y, Nd, Sm, Gd, Tb and Dy) rare earth molybdates by using chemical bond theory of dielectric description. The chemical bonding characteristics and their relationship with thermal expansion property and compressibility are explored. The calculated values of linear thermal expansion coefficient (LTEC) and bulk modulus agree well with the available experimental values. The calculations reveal that the LTECs and the bulk moduli do have linear relationship with the ionic radii of the lanthanides: the LTEC decreases from 6.80 to 6.62 10(-6)/K and the bulk modulus increases from 141 to 154 GPa when R goes in the order Gd, Tb Dy, Ho, Er, Tm, and Yb in the alpha-R2MoO6 series; while in the R2Mo2O7 series, the LTEC ranges from 6.80 to 6.61 10(-6)/K and the bulk modulus ranges from 147 to 163 GPa when R varies in the order Nd, Sm, Gd, Tb and Dy.