183 resultados para leaf thickness
Resumo:
In order to examine the role of environmental factors affecting foliar morphology, we performed a case study of leaf morphological variation of Ranunculus natans found in the arid zone of northwest China. We found that foliar phenotypic variation differed significantly between populations. We described substantial positive correlations between altitude and leaf area (LA) as well as leaf perimeter (LP), and also between longitude and number of teeth, along with dissection index (DI). The pH, conductivity, and salinity of the environment caused a significant decrease in both LA and LP. Ranked in terms of their impacts on leaf morphology, the six selected factors were: altitude > pH > conductivity > salinity > longitude > latitude. We found that foliar morphological variations are functional responses to water-quantity factors (e.g., altitude and longitude at regional scales) and water-availability relation factors (e.g., pH, conductivity, and salinity at local scales), rather than to temperature-relation factors (latitude). Therefore, altitude and longitude, along with pH, conductivity, and salinity, are the main factors that significantly influence foliar morphology in the arid zone of China. We found that main factors played major roles in plant phenotypic plasticity in a complex ecosystem, although different combinations and interactions of environmental and geographical factors in each local environment may obscure the general trends in trait changes along environmental gradients.
Resumo:
Photosynthetic responses to irradiance and temperature of "leaves" and receptacles were compared in February ( vegetative stage) and May ( reproductive stage) in the seaweed, Hizikia fusiforme ( Harvey) Okamura (Sargassaceae, Phaeophyta) from Nanao Island, Shantou, China. Irradiance-saturated photosynthesis (P-max) was significantly higher in receptacles than in "leaves" on a fresh weight basis, and that of "leaves" was greater in May than in February at ambient seawater temperatures. The optimum temperature for P-max was 30 degrees C for both "leaves" and receptacles, being 5 - 10 degrees C higher than the ambient seawater temperature. The apparent photosynthetic efficiencies were greater in receptacles than in "leaves" within the tested temperature range of 10 - 40 degrees C. The irradiance for saturating photosynthesis for both "leaves" and receptacles was temperature-dependent, with the highest values ( about 200 mu mol photons m(-2) s(-1)) at 30 degrees C.
Resumo:
The influence of well thickness on the electroluminescence (EL) of InGaN/GaN multiple quantum wells (MQWs) grown by metalorganic chemical vapor deposition is investigated. It is found that the peak wavelength of EL increases with the increase of well thickness when the latter is located in the range of 3.0-5.1 nm. The redshift is mainly attributed to the quantum confined Stark effect (QCSE). As a contrast, it is found that the EL intensity of InGaN/GaN MQWs increases with the increase of well thickness in spite of QCSE. The result of X-ray diffraction demonstrates that the interface become smoother with the increase of well thickness and suggests that the reduced interface roughness can be an important factor leading to the increase of EL intensity of InGaN/GaN MQWs. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
We present the growth of GaN epilayer on Si (111) substrate with a single AlGaN interlayer sandwiched between the GaN epilayer and AlN buffer layer by using the metalorganic chemical vapour deposition. The influence of the AlN buffer layer thickness on structural properties of the GaN epilayer has been investigated by scanning electron microscopy, atomic force microscopy, optical microscopy and high-resolution x-ray diffraction. It is found that an AlN buffer layer with the appropriate thickness plays an important role in increasing compressive strain and improving crystal quality during the growth of AlGaN interlayer, which can introduce a more compressive strain into the subsequent grown GaN layer, and reduce the crack density and threading dislocation density in GaN film.
Resumo:
We studied the impact of the thickness of GaN buffer layer on the properties of distributed Bragg reflector (DBR) grown by metalorganic chemical vapor deposition (MOCVD). The samples were characterized by using metallographic microscope, transmission electron microscope (TEM), atomic force microscopy (AFM), X-ray diffractometer (XRD) and spectrophotometer. The results show that the thickness of the GaN buffer layer can significantly affect the properties of the DBR structure and there is an optimal thickness of the GaN buffer layer. This work would be helpful for the growth of high quality DBR structures.
Resumo:
Hexagonal GaN is grown on a Si(111) substrate with AlN as a buffer layer by gas source molecular beam epitaxy (GSMBE) with ammonia. The thickness of AlN buffer is changed from 9 to 72 nm. When the thickness of AlN buffer is 36 nm, the surface morphology and crystal quality of GaN is optimal. The in-situ reflection high energy electron diffraction (RHEED) reveals that the transition to a two-dimensional growth mode of AlN is the key to the quality of GaN. However, the thickness of AlN buffer is not so critical to the residual in-plane tensile stress in GaN grown on Si(111) by GSMBE for AlN thickness between 9 to 72 nm.
Effect of p-GaN layer thickness on the performance of p-i-n structure GaN ultraviolet photodetectors
Resumo:
We investigated the influence of thickness of p-GaN layer on the performance of p-i-n structure GaN ultraviolet photodetector. Through the simulation calculation, it was found that both the quantum efficiency and dark current of device decrease when employing thicker p-GaN layer, while both the quantum efficiency and dark current increase with decreasing thickness of p-GaN layer. It is suggested that the Schottky contact junction between the metal and p-GaN may be responsible for the incompatible effect. We has to make a suitable choice of the thickness of p-GaN in the device design according to the application requirement.
Resumo:
This paper investigates the dependence of current-voltage characteristics of AlAs/In0.53Ga0.47As/InAs resonant tunnelling diodes (RTDs) on spacer layer thickness. It finds that the peak and the valley current density J in the negative differential resistance (NDR) region depends strongly on the thickness of the spacer layer. The measured peak to valley current ratio of RTDs studied here is shown to improve while the current density through RTDs decreases with increasing spacer layer thickness below a critical value.
Resumo:
InN thin films with different thicknesses are grown by metal organic chemical vapor deposition, and the dislocations, electrical and optical properties are investigated. Based on the model of mosaic crystal, by means of X-ray diffraction skew geometry scan, the edge dislocation densities of 4.2 x 10(10) cm(-2) and 6.3 x 10(10) cm(-2) are fitted, and the decrease of twist angle and dislocation density in thicker films are observed. The carrier concentrations of 9 x 10(18) cm(-3) and 1.2 x 10(18) cm(-3) are obtained by room temperature Hall effect measurement. V-N is shown to be the origin of background carriers, and the dependence of concentration and mobility on film thickness is explained. By the analysis of S-shape temperature dependence of photoluminescence peak, the defects induced carrier localization is suggested be involved in the photoluminescence. Taking both the localization and energy band shrinkage effect into account, the localization energies of 5.05 meV and 5.58 meV for samples of different thicknesses are calculated, and the decrease of the carrier localization effect in the thicker sample can be attributed to the reduction of defects.
Resumo:
The effect of thickness of the high-temperature (HT) AlN buffer layer on the properties of GaN grown on Si(111) has been investigated. Optical microscopy (OM), atomic force microscopy (AFM) and X-ray diffraction (XRD) are employed to characterize these samples grown by metal-organic chemical vapor deposition (MOCVD). The results demonstrate that the morphology and crystalline properties of the GaN epilayer strongly depend on the thickness of HT AlN buffer layer, and the optimized thickness of the HT AlN buffer layer is about 110 nm. Together with the low-temperature (LT) AlN interlayer, high-quality GaN epilayer with low crack density can be obtained. (C) 2008 Elsevier Ltd. All rights reserved.
Resumo:
The influence of low-temperature AlN buffer layer thickness on GaN epilayer was investigated by triple-axis X-ray diffraction (XRD) and photoluminescence measurements. A method was proposed to measure the screw and edge dislocation densities by XRD. It was found that the buffer layer thickness was a key parameter to affect the quality of GaN epilayer and an appropriate thickness resulted in the best structural and optical properties except the lateral grain size. After the thickness exceeding the appropriate value, the compressive stress in the epilayer decreased as the thickness increased, which led to the redshift of the near-band edge luminescence. The experimental results showed the buffer layer thickness had more influence on edge dislocation than screw type and the former was perhaps the main source of the yellow band. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
InGaN/GaN multiquantum-well (MQW) structures grown by metalorganic chemical-vapor deposition on n-type GaN and capped by p-type GaN were investigated by cross-sectional transmission electron microscopy, double crystal x-ray diffraction, and temperature-dependent photoluminescence. For the sample with strained-layer thicknesses greater than the critical thicknesses, a high density of pure edge type threading dislocations generated from MQW layers and extended to the cap layer was observed. These dislocations result from a relaxation of the strained layers when their thicknesses are beyond the critical thicknesses. Because of indium outdiffusion from the well layers due to the anneal effect of Mg-doped cap layer growth and defects generated from strain relaxation, the PL emission peak was almost depressed by the broad yellow band with an intensity maximum at 2.28 eV. But for the sample with strained-layer thicknesses less than the critical thicknesses, it has no such phenomenon. The measured critical thicknesses are consistent with the calculated values using the model proposed by Fischer, Kuhne, and Richter. (C) 2004 American Institute of Physics.
Resumo:
We have studied the effect of the post-growth rapid thermal annealing on optical and electrical properties of InAs/InAlAs/InP quantum wires with various InAs deposited thickness. Quite different annealing behaviors in photoluminescence and dark resistance are observed, which can be attributed to dislocations in samples. After annealing at 800 degrees C, quantum wires still exist in the sample with two monolayer InAs deposited thickness, but the temperature-dependent PL properties are changed greatly due to the intermixing of In/Al atoms. (c) 2005 Elsevier B.V. All rights reserved.