524 resultados para MULTIPLE QUANTUM-WELLS
Resumo:
The Rashba spin-orbit splitting of a hydrogenic donor impurity in GaAs/GaAlAs quantum wells is investigated theoretically in the framework of effective-mass envelope function theory. The Rashba effect near the interface between GaAs and GaAlAs is assumed to be a linear relation with the distance from the quantum well side. We find that the splitting energy of the excited state is larger and less dependent on the position of the impurity than that of the ground state. Our results are useful for the application of Rashba spin-orbit coupling to photoelectric devices.
Resumo:
We have investigated spin polarization-related localized exciton photoluminescence (PL) dynamics in GaInNAs quantum wells by time-resolved PL spectroscopy. The emission energy dependence of PL polarization decay time as well as polarization-independent PL decay time suggests that the acoustic phonon scattering in the process of localized exciton transfer from the high-energy localized states to the low-energy ones dominates the PL polarization relaxation. By increasing the excitation power from 1 to 10 mW, the PL polarization decay time is changed from 0.17 to more than 1 ns, which indicates the significant effect of the trapping of localized electrons by nonradiative recombination centers. These experimental findings indicate that the spin-related PL polarization in diluted nitride semiconductors can be manipulated through carrier scattering and recombination process. (C) 2009 The Japan Society of Applied Physics
Resumo:
We investigate theoretically the Dyakonov-Perel spin relaxation time by solving the eight-band Kane model and Poisson equation self-consistently. Our results show distinct behavior with the single-band model due to the anomalous spin-orbit interactions in narrow band-gap semiconductors, and agree well with the experiment values reported in recent experiment [K. L. Litvinenko et al., New J. Phys. 8, 49 (2006)]. We find a strong resonant enhancement of the spin relaxation time appears for spin align along [1 (1) over bar0] at a certain electron density at 4 K. This resonant peak is smeared out with increasing the temperature.
Resumo:
We investigate the temperature dependence of photoluminescence (PL) and time-resolved PL on the metamorphic InGaAs quantum wells (QWs) with an emission wavelength of 1.55 mu m at room temperature. Time-resolved PL measurements reveal that the optical properties can be partly improved by introducing antimony (Sb) as a surfactant during the sample growth. The temperature dependence of the radiative lifetime is measured, showing that for QWs grown with Sb assistance, the intrinsic exciton emission is dominated when the temperature is below 60 K, while the nonradiative process becomes activated with further increases in temperature. However, without Sb assistance, the nonradiative centers are activated when the temperature is higher than 20 K.
Resumo:
High-indium-content InxGa1-xAs/GaAs single/multi-quantum well (SQW/MQW) structures have been systematically investigated. By optimizing the molecular-beam epitaxy growth conditions, the critical thickness of the strained In0.475Ga0.525As/GaAs QWs is raised to 7 nm, which is much higher than the value given by the Matthews and Blakeslee model. The good crystalline quality of the strained InGaAs/GaAs MQWs is proved by x-ray rocking curves. Photoluminescence measurements show that an emission wavelength of 1.25 mum at room temperatures with narrower full width at half maximum less than 30 meV can be obtained. The strain relaxation mechanism is discussed using the Matthews-Blakeslee model. (C) 2004 American Institute of Physics.
Resumo:
The effects of pre-TMIn flow prior to QW growth and TMIn flow rates during QW growth on the interface and optical properties of InGaN/GaN MQWs were investigated. Pre-depositing indium prior to QW growth and an appropriate TMIn flow rate can improve the interface abruptness and increase the EL intensity. InGaN/GaN MQWs with improved interface abruptness have increasing emission intensity and wavelength. We attribute the interface improvement and the increase of EL intensity to the improvement of the indium compositional profiles. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Photoluminescence (PL) spectra of the GaInNAs/GaAs single quantum well (SQW) with different N compositions are carefully studied in a range of temperatures and excitation power densities. The anomalous S-shape temperature dependence of the PL peak is analysed based on the competition and switching-over between the peaks related to N-induced localized states and the peak related to interband excitonic recombination. It is found that with increasing N composition, the localized energy increases and the turning point of the S-shape temperature dependence occurs at higher temperature, where the localized carriers in the bandtail states obtain enough thermal activation energy to be dissociated and delocalized. The rapid thermal annealing (RTA) effectively reduces the localized energy and causes a decrease of the switching-over temperature.
Resumo:
Suppression of the exciton recombination in GaAs0.7Sb0.3/GaAs/GaAs0.7P0.3 coupled quantum well (CQW) induced by an external magnetic field is investigated theoretically. Unlike the usual electro-Stark effect, the exciton energy dispersion of an exciton is modified by an external in-plane magnetic field, the ground state of the magnetoexciton shifts from a zero in-plane center of mass (CM) momentum to a finite CM momentum, and the Lorentz force induces the spatial separation of electron and hole. Consequently, this effect renders the ground state of magnetoexciton stable against radiative recombination due to momentum conservation. This effect depends sensitively on the thickness and height of GaAs0.7Sb0.3 layer, therefore it could provide us useful infometion about the band alignment of CQW. (C) 2004 American Institute of Physics.
Resumo:
High structural and optical quality 1.3 mu m GaInNAs/GaAs quantum well (QW) samples with higher (42.5%) indium content were successfully grown by molecular-beam epitaxy. The cross-sectional transmission electron microscopy measurements reveal that there are no structural defects in such high indium content QWs. The room-temperature photoluminescence peak intensity of the GaIn0.425NAs/GaAs (6 nm/20 nm) 3QW is higher than, and the full width at half maximum is comparable to, that of In0.425GaAs/GaAs 3QW, indicating improved optical quality caused by strain compensation effect of introducing N to the high indium content InGaAs epilayer. (C) 2005 American Institute of Physics.
Resumo:
High-quality GaNAs/GaAs quantum wells with high substitutional N concentrations, grown by molecular-beam epitaxy, are demonstrated using a reduced growth rate in a range of 0.125-1 mu m/h. No phase separation is observed and the GaNAs well thickness is limited by the critical thickness. Strong room-temperature photoluminescence with a record long wavelength of 1.44 mu m is obtained from an 18-nm-thick GaN0.06As0.94/GaAs quantum well. (C) 2005 American Institute of Physics.
Resumo:
Optical properties of highly strained GaInAs/GaAs quantum wells (QWs) grown by molecular beam epitaxy with Sb assistance are investigated. The samples grown by Sb incorporation and Sb pre-deposition methods display high room-temperature photoluminescence (PL) intensity at extended long wavelength. This result is explained by the surfactant effects of Sb during the growth of GaInAs/GaAs QW systems. An abnormal S-shaped temperature dependence of the PL peak position is found in the In0.42Ga0.58As/GaAs triple QWs sample grown with Sb pre-deposition. By investigating the transmission electron microscope images and time-resolved PL spectra, it is found that the S-shaped temperature dependence of the PL peak position originates from the exciton localization effect brought by the Sb-rich clusters on the QW interface.
Resumo:
Molecular beam epitaxy (MBE) growth of (InyGa1-yAs/GaAs1-xSbx)/GaAs bilayer quantum well (BQW) structures has been investigated. It is evidenced by photo luminescence (PL) that a strong blue shift of the PL peak energy of 47 meV with increasing PL excitation power from 0.63 to 20 mW was observed, indicating type II band alignment of the BQW. The emission wavelength at room temperature from (InyGa1-yAs/GaAs1-xSbx)/GaAs BQW is longer (above 1.2 μ m) than that from InGaAs/GaAs and GaAsSb/GaAs SQW structures (1.1 μ m range), while the emission efficiency from the BQW structures is comparable to that of the SQW. Through optimizing growth conditions, we have obtained room temperature 1.31 μ m wavelength emission from the (InyGa1-yAs/GaAs1-xSbx)/GaAs BQW. Our results have proved experimentally that the GaAs-based bilayer (InyGa1-yAs/GaAs1-xSbx)/GaAs quantum well is a useful structure for the fabrication of near-infrared wavelength optoelectronic devices. © 2005 Elsevier B.V. All rights reserved.
Resumo:
Long-wavelength high indium content InxGa1-xAs/GaAs single/multi quantum wells (QWs) structures have been successfully grown by molecular beam epitaxy. It is evidenced by X-ray measurements that the critical thickness of the well width of InxGa1-xAs/GaAs QWs with an indium content x of 47.5% can be raised up to 7nm without strain relation. 1.25μ m photoluminescence (PL) emission is obtained from the QWs with narrower full-width at half maximum (FWHM) less than 30meV. Our results are important basements which are useful for further fabricating GaAs-based long-wavelength devices. © 2005 Elsevier B.V. All rights reserved.
Resumo:
Coherent tunnelling is studied in framework of the effective mass approximation for an asymmetric coupled quantum well. The Hartree potential due to the electron-electron interaction is considered in our calculation. The effects of the longitudinal and transverse magnetic field on coherent tunnelling characteristics are discussed. It has been found that the external field plays an important role in modulating the electron states.
Resumo:
The InGaNAs(Sb)/(GaNAs)/GaAs quantum wells (QWs) emitting at 1.3-1.55 mu m have been grown by molecular beam epitaxy (MBE). The parameters of the radio frequency (RF) such as RF power and flow rate are optimized to reduce the damages from the ions or energetic species. The growth temperature is carefully controlled to prevent the phase segregation and strain relaxation. The effects of Sb on the wavelength and quality are investigated. The GaNAs barrier is used to extend the wavelength and reduce the strain. A 1.5865 mu m InGaNAs(Sb)/GaNAs SQW edge emitting laser lasing at room temperature at continuous wave operation mode is demonstrated. (c) 2006 Elsevier B.V. All rights reserved.