129 resultados para Energy-band theory of solids.
Resumo:
The optical band gap (E-g) of the boron (B)-doped hydrogenated nano-crystalline silicon (nc-Si:H) films fabricated using plasma enhanced chemical vapor deposition (PECVD) was investigated in this work. The transmittance of the films were measured by spectrophotometric and the E-g was evaluated utilizing three different relations for comparison, namely: alphahnu=C(hnu-E-g)(3), alphahnu=B-0(hnu-E-g)(2), alphahnu=C-0(hnu-E-g)(2). Result showed that E-g decreases with the increasing of Boron doping ratio, hydrogen concentration, and substrate's temperature (T-s), respectively. E-g raises up with rf power density (P-d) from 0.45W.cm(-2) to 0.60w.cm(-2) and then drops to the end. These can be explained for E-g decreases with disorder in the films.
Resumo:
A quantum chemistry based Green's function formulation of long-range charge transfer in deoxyribose nucleic acid (DNA) double helix is proposed. The theory takes into account the effects of DNA's electronic structure and its incoherent interaction with aqueous surroundings. In the implementation, the electronic tight-binding parameters for unsolvated DNA molecules are determined at the HF/6-31G* level, while those for individual nucleobase-water couplings are at a semiempirical level by fitting with experimental redox potentials. Numerical results include that: (i) the oxidative charge initially at the donor guanine site does hop sequentially over all guanine sites; however, the revealed rates can be of a much weaker distance dependence than that described by the ordinary Ohm's law; (ii) the aqueous surroundings-induced partial incoherences in thymine/adenine bridge bases lead them to deviate substantially from the superexchange regime; (iii) the time scale of the partially incoherent hole transport through the thymine/adenine pi stack in DNA is about 5 ps. (C) 2002 American Institute of Physics.
Resumo:
InAs self-organized quantum dots (QDs) grown on annealed low-temperature GaAs (LT-GaAs) epi-layers and on normal temperature GaAs buffer layers have been compared by transmission electron microscopy (TEM) and photoluminescence (PL) measurements. TEM evidences that self-organized QDs were formed with a smaller size and larger density than that on normal GaAs buffer layers. It is discussed that local tensile surface strain regions that are preferred sites for InAs islands nucleation are increased in the case of the LT-GaAs buffer layers due to exhibiting As precipitates. The PL spectra show a blue-shifted peak energy with narrower linewidth revealing the improvement of optical properties of the QDs grown on LT-GaAs epi-layers. It suggests us a new way to improve the uniformity and change the energy band structure of the InAs self-organized QDs by carefully controlling the surface stress states of the LT-GaAs buffers on which the QDs are formed. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
InAs self-organized quantum dots (QDs) grown on annealed low temperature GaAs (LT-GaAs) epi-layer were investigated by transmission electron microscopy (TEM) and photoluminescence (PL) measurement. TEM showed that QDs formed on annealed LT-GaAs epi-layer have a smaller size and a higher density than QDs formed on normal GaAs buffer layer. In addition, the PL spectra analysis showed that the LT-GaAs epi-layer resulted in a blue shift in peak energy, and a narrower linewidth in the PL peak. The differences were attributed to the point defects and As precipitates in annealed LT-GaAs epi-layer for the point defects and As precipitates change the strain field of the surface. The results provide a method to improve the uniformity and change the energy band structure of the QDs by controlling the defects in the LT-GaAs epi-layer.
Resumo:
A deep level transient spectroscopy technique has been used to determine the emission activation energies and capture barriers for electrons and holes in InAs self-assembled quantum dots embedded in GaAs. The ground electron and hole energies relative to their respective energy band edges of GaAs are 0.13 and 0.09 eV. Measurements show that the capture cross section of quantum dots is thermally activated. The capture barrier of quantum dots for electrons and holes are 0.30 and 0.26 eV, respectively. The results fit well with the results of photoluminescence spectroscopy measurements. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
X-ray photoelectron spectroscopy has been used to measure the valence band offset of the ZnO/BaTiO3 heterojunction grown by metal-organic chemical vapor deposition. The valence band offset (VBO) is determined to be 0.48 +/- 0.09 eV, and the conduction band offset (CBO) is deduced to be about 0.75 eV using the band gap of 3.1 eV for bulk BaTiO3. It indicates that a type-II band alignment forms at the interface, in which the valence and conduction bands of ZnO are concomitantly higher than those of BaTiO3. The accurate determination of VBO and CBO is important for use of semiconductor/ferroelectric heterojunction multifunctional devices.
Valence band offset of MgO/TiO2 (rutile) heterojunction measured by X-ray photoelectron spectroscopy
Resumo:
The valence band offset (VBO) of MgO/TiO2 (rutile) heterojunction has been directly measured by Xray photoelectron spectroscopy. The VBO of the heterojunction is determined to be 1.6 +/- 0.3 eV and the conduction band offset (CBO) is deduced to be 3.2 +/- 0.3 eV, indicating that the heterojunction exhibits a type-I band alignment. These large values are sufficient for MgO to act as tunneling barriers in TiO2 based devices. The accurate determination of the valence and conduction band offsets is important for use of MgO as a buffer layer in TiO2 based field-effect transistors and dye-sensitized solar cells.
Resumo:
N+ GaAs-n GaInP lattice-matched heterostructures, grown by metalorganic vapour phase epitaxy, have been studied by capacitance-voltage, current-voltage and current-temperature techniques. This allowed the determination of the conduction band offset in three different and independent ways. The value obtained (0.24-0.25 eV) has been verified by photoluminescence and photoluminescence excitation on a 90 angstrom thick GaAs well in GaInP grown under the same conditions.