171 resultados para time-resolved Kerr rotation


Relevância:

100.00% 100.00%

Publicador:

Resumo:

利用800nm抽运和400nm探针技术,测量了CaF2和MgO的时间分辨反射率,研究了材料的电子激发和弛豫超快动力学过程。采用耦合动力学模型,探讨了飞秒激光对透明介质材料的激发,以及材料的激发对抽运激光在材料中的传输、分布和反射特性的影响。根据这个理论模型计算了时间分辨反射率的演化,计算结果和实验结果相吻合。研究表明,多光子电离(MPI)和碰撞电离(II)在介质材料的导带电子激发中起着重要的作用。

Relevância:

100.00% 100.00%

Publicador:

Resumo:

详细论述了时间分辨X射线衍射探测原子动态过程和生物大分子瞬态结构的各种方法。介绍了多种超快X射线脉冲光源及其在材料和生化领域中的研究进展状况。材料方面:在皮秒时间尺度探测到了晶格间距毫埃的微小变化;在亚皮秒的时间尺度直接观测到晶体的超快熔化过程和晶体内的相干声子散射;生物化学方面:采用时间分辨X射线劳厄衍射方法探测了蛋白质大分子结构的变化和功能之间的关系;精确描述了有机分子在光作用下形态发生改变时分子键角的扭转角度,从结构上揭示了其动态机理。

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We report on the conversion of near-ultraviolet radiation of 250-350 nm into near-infrared emission of 970-1100 nm in Yb3+-doped transparent glass ceramics containing Ba2TiSi2O8 nanocrystals due to the energy transfer from the silicon-oxygen-related defects to Yb3+ ions. Efficient Yb3+ emission (F-2(5/2)-> F-2(7/2)) was detected under the excitation of defects absorption at 314 nm. The occurrence of energy transfer is proven by both steady state and time-resolved emission spectra, respectively, at 15 K. The Yb2O3 concentration dependent energy transfer efficiency has also been evaluated, and the maximum value is 65% for 8 mol % Yb2O3 doped glass ceramic. These materials are promising for the enhancement of photovoltaic conversion efficiency of silicon solar cells via spectra modification.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The damage morphologies, threshold fluences in ZnO films were studied with femtosecond laser pulses. Time-resolved reflectivity and transmissivity have been measured by the pump-probe technique at different pump fluences and wavelengths. The results indicate that two-phase transition is the dominant damage mechanism, which is similar to that in narrow band gap semiconductors. The estimated energy loss rate of conduction electrons is 1.5 eV/ps. (c) 2005 Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A pump and probe system is developed, where the probe pulse duration tau is less than 60 fs while the pump pulse is stretched up to 150-670 fs. The time-resolved excitation processes and damage mechanisms in the omnidirectional reflectors SiO2/TiO2 and ZnS/MgF2 are studied. It is found that as the pump pulse energy is higher than the threshold value, the reflectivity of the probe pulse decreases rapidly during the former half, rather than around the peak of the pump pulse. A coupled dynamic model based on the avalanche ionization (AI) theory is used to study the excitation processes in the sample and its inverse influences on the pump pulse. The results indicate that as pulse duration is longer than 150 fs, photoionization (PI) and AI both play important roles in the generation of conduction band electrons (CBEs); the CBE density generated via AI is higher than that via PI by a factor of 10(2)-10(4). The theory explains well the experimental results about the ultrafast excitation processes and the threshold fluences. (c) 2006 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We report the single-shot damage thresholds of MgF2/ZnS onmidirectional reflector for laser pulse durations from 50 A to 900 fs. A coupled dynamic model is applied to study the damage mechanisms, in which we consider not only the electronic excitation of the material, but also the influence of this excitation-induced changes in the complex refractive index of material on the laser pulse itself. The results indicate that this feedback effect plays a very important role during the damage of material. Based on this model, we calculate the threshold fluences and the time-resolved excitation process of the multiplayer. The theoretical calculations agree well with our experimental results. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We studied the single-shot damage in magnesium fluoride irradiated by 800 nm femtosecond (fs) laser. The dependence of damage thresholds on the laser pulse durations from 60 to 750 fs was measured. The pump-probe measurements were carried out to investigate the time-resolved electronic excitation processes. A coupled dynamic model was applied to study the microprocesses in the interaction between fs laser and magnesium fluoride. The results indicate that both multiphoton ionization and avalanche ionization play important roles in the femtosecond laser-induced damage in MgF2. (C) 2006 Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The conventional TbFeCo magneto-optical (MO) medium has a relatively smaller Kerr rotation angle in the blue region than in the red. With the recording wavelength gradually moving to the short wavelength, if TbFeCo is still used as recording medium, the conventional MO disk structure must be optimized to get a larger carrier to noise ratio (CNR). Sabi et al. have found that adding a metal layer attached to the TbFeCo film as thermal control layer is a useful way to get a high CNR. In this paper, we proved this through calculation, and carried out optimization of the new type of disk. Calculation results showed that the new structure is useful in preventing an excessive temperature increase, and has a better thermal response. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

用磁控溅射法制备了GdFeCo/TbFeCo交换耦合两层薄膜,利用不同温度的克尔磁滞回线和VSM磁滞回线研究了读出层(GdFeCo)变温磁化方向变化过程.结果表明,随温度升高读出层从平面磁化转变为垂直磁化,交换耦合两层薄膜具有中心孔探测磁超分辨的基本性能.转变过程主要受饱和磁化强度(Ms)的影响,在GdFeCo的补偿温度附近,读出层的磁化强度较小,退磁场能也较小,在交换耦合的作用下,使读出层(GdFeCo)的磁化方向发生转变.磁化方向的转变在75℃~125℃的温度范围内变化较快.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The emission intensity of Ni2+ at 1200 nm in transparent ZnO-Al2O3-SiO2 glass ceramics containing ZnAl2O4 nanocrystals is improved approximately 8 times by Cr3+ codoping with 532 nm excitation. This enhanced emission could be attributed to an efficient energy transfer from Cr3+ to Ni2+, which is confirmed by time-resolved emission spectra. The energy transfer efficiency is estimated to be 57% and the energy transfer mechanism is also discussed. (C) 2008 Optical Society of America.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Transparent Li2O-Ga2O3-SiO2 glass ceramics containing Cr3+/Ni2+ codoped LiGa5O8 nanocrystals were synthesized. The steady state emission spectra indicated that the near-infrared emission intensity of Ni2+ at 1300 nm in Cr3+/Ni2+ codoped glass ceramics was enhanced up to about 7.3 times compared with that in Ni2+ single-doped glass ceramics with 532 nm excitation. This enhancement in emission intensity was due to efficient energy transfer from Cr3+ to Ni2+, which was confirmed by time-resolved emission spectra. The energy transfer efficiency was estimated to be 85% and the energy transfer mechanism was discussed. (C) 2008 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

细胞色素b6f蛋白复合体(Cytochrome b6f complex, Cyt b6f)是光合膜上参与光合作用原初反应过程的主要膜蛋白超分子复合体之一。莱茵衣藻和嗜热蓝细菌的Cyt b6f三维晶体结构均显示,每Cyt b6f单体分子含有1分子Chlorophyll a (Chl a ),充分肯定了Chl a 是Cyt b6f天然成分的观点(Kurisu et al,2003;Stroebel et al,2003)。研究表明不同来源的Cyt b6f中Chla单线激发态寿命(或荧光寿命)并不一样,多数的研究结果认为Cyt b6f中Chla单线激发态寿命只有200ps左右,但是也有Cyt b6f中Chla单线激发态寿命为~600ps的报道;而甲醇中游离Chl a 的单线激发态寿命为4ns左右。针对Cyt b6f中Chla单线激发态寿命快速淬灭的现象,Dashdorj 等(2005)根据晶体结构推测Cyt b6f中Chla单线激发态和邻近的Cyt b6亚基上Tyr105残基发生电子交换传递,从而快速淬灭Chla单线激发态,减少了三线态Chl a和单线态氧的产生,并且认为这是Cyt b6f保护自身不受单线态氧破坏的一种机制,但是这一推测缺乏有力的证据。另外,Cyt b6f中Chla的功能仍然未知。本文以菠菜Cyt b6f为对象,结合多种实验手段,测定了菠菜Cyt b6f中Chl a单线激发态寿命,并对复合体中Chl a 单线激发态淬灭的机理进行了深入研究。此外,我们还对复合体中Chl a 可能的功能进行了初步地探讨。获得了如下的结果: 1.针对不同来源的Cyt b6f中Chla单线激发态寿命(或荧光寿命)测定结果不同的报道,仔细分析了其中的原因,发现除了样品来源的差异外,使用不同的去垢剂可能是一个不可忽视的因素。在实验中,不同的研究者分别采用了十二烷基麦芽糖苷(n-Dodecyl β-D-maltoside,DDM,)和八烷基葡萄糖苷(n-Octyl β-D-glucopyranoside,β-OG)作为溶解样品的去垢剂。因此,本文借助稳态吸收和稳态荧光光谱、瞬态光散射技术,CD光谱和亚皮秒时间分辨吸收光谱等技术,分别研究了这两种去垢剂对Cyt b6f结构和功能的不同影响。结果表明,DDM去垢剂能使Cyt b6f处于较好的分散体系中,其中血红素和Chl a分子处于特定的蛋白环境中,不会导致Cyt b6f变性;而β-OG去垢剂会使Cyt b6f产生聚合现象,其中的血红素和Chl a与蛋白环境的相互作用减弱,和DDM相比其电子传递活性显著降低,Chl a单线激发态寿命延长,Chl a更容易被光破坏。通过这一工作,我们优化和确定了Cyt b6f的溶解条件,为下面的研究工作打下了良好的基础。 2.利用Tyr的特异性修饰剂p-Nitrobenzenesulfonyl Fluoride(NBSF)对Cyt b6f样品进行特性修饰,经原子吸收谱、荧光谱、CD谱、质谱等方法对修饰后的样品进行鉴定,并结合时间分辨飞秒吸收光谱技术,测得修饰后的样品在660nm激发下Chl a 单线激发态寿命延长,从而在实验上提供了Tyr与淬灭Chla单线激发态有关的证据。但是对Cyt b6f 中Chl a瞬态吸收图谱仔细研究表明,菠菜Cyt b6f 中Chl a单线激发态快速淬灭过程中并没有发现Tyr与Chl a 之间发生电子传递时所形成的Chla•¯。以上结果表明,Cyt b6f 中Chl a单线激发态快速的淬灭确实和邻近的Tyr105有关,但是与Dashdorj 等提出的Chla单线激发态和Tyr105残基发生了电子交换传递从而淬灭Chla单线激发态这一想法不符,关于这一问题值得进一步深入研究。 3.红光和绿光对Cyt b6f 照射,Cyt f可以被还原,并且红光比绿光更容易使Cyt f 还原,暗示Cyt f 的还原与Chl a 的关系密切,有可能是Chl a 被激发后,其被激发的电子传给Cyt f。对这一现象的进一步研究表明,Cyt b6f在光照条件下,Cyt f 的还原与体系内C10-PQ库的氧化还原状况相关,氧化型的C10-PQ可能介导电子从Chla传向Cyt f。由于在体内质体醌库的氧化还原状态往往决定Cyt b6f 的氧化还原状态,而通过对Cyt b6f不同氧化和还原状态的吸收谱和荧光谱的研究表明,氧化态和还原态的Cyt b6f 中,Chl a 与蛋白的结合状态是有差异的。这些差异可能暗示着Chl a 分子在行使其功能时与复合体的氧化还原状态是有关系的。通过以上的结果,对Cyt b6f中Chl a 可能的功能进行了假设。 4.此外,我们还发现Cyt b6f具有明显的过氧化物酶活性。在0.1 mmol/L乙酸钠缓冲液,pH3.6,25℃,[H2O2] <40mmol/L的条件下,其催化反应的速度常数为kobs=26±1.2M•s-1;对H2O2的Km 值为50mmol/L,对guaiacol的Km 值为2mmol/L;反应的最适pH为3.6,最适离子强度为0.1,最适温度为35℃。推测Cyt b6f的这种过氧化物酶活性可能是在胁迫环境下使Cyt b6f中的血红素和Chl a 分子免受H2O2的破坏。

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The influence of well thickness on the electroluminescence (EL) of InGaN/GaN multiple quantum wells (MQWs) grown by metalorganic chemical vapor deposition is investigated. It is found that the peak wavelength of EL increases with the increase of well thickness when the latter is located in the range of 3.0-5.1 nm. The redshift is mainly attributed to the quantum confined Stark effect (QCSE). As a contrast, it is found that the EL intensity of InGaN/GaN MQWs increases with the increase of well thickness in spite of QCSE. The result of X-ray diffraction demonstrates that the interface become smoother with the increase of well thickness and suggests that the reduced interface roughness can be an important factor leading to the increase of EL intensity of InGaN/GaN MQWs. (C) 2009 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

By using photoluminescence (PL) and time-resolved PL spectra, the optical properties of single InAs quantum dot (QD) embedded in the p-1-n structure have been studied under an applied electric field With the increasing of electric field, the exciton lifetime increases due to the Stark effect. We noticed that the decrease or quenching of PL intensity with increasing the electric field is mainly due to the decrease of the carriers captured by QD.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

An improved peak power method for measuring frequency responses of photodetectors in a self-heterodyne system consisting of a distributed Bragg reflector laser is proposed. The time-resolved spectrum technique is used to measure the peak power of the beat signal and the intrinsic linewidth of heat signal for calibration. The experimental results show that the impact of the thermal-induced frequency drift, which is the main reason for producing an error in measurement by conventional peak power method and spectrum power method, can be removed.