Cylindrical vector beams were produced from laser diode end-pumped Nd:YAG ceramic microchip laser by use of two types of subwavelength multilayer gratings as the axisymmetric-polarization output couplers respectively. The grating mirrors are composed of high- and low-refractive-index (Nb2O5/SiO2) layers alternately while each layer is shaped into triangle and concentric corrugations. For radially polarized laser output, the beam power reached 610mW with a polarization extinction ratio ( PER) of 61: 1 and a slope efficiency of 68.2%; for azimuthally polarized laser output, the beam power reached 626mW with a PER of 58: 1 and a slope efficiency of 47.6%. In both cases, the laser beams had near-diffraction limited quality. Small differences of beam power, PER and slope efficiency between radially and azimuthally polarized laser outputs were not critical, and could be minimized by further optimized adjustment to laser cavity and the reflectances of respective grating mirrors. The results manifested, by use of the photonic crystal gratings mirrors and end-pumped microchip laser configuration, CVBs can be generated efficiently with high modal symmetry and polarization purity. (C) 2008 Optical Society of America.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this work, microwave dielectric properties of A-site substitution by La3+ in (Pb0.45Ca0.55) (Fe0.5Nb0.5) 03 system were investigated. Microwave dielectric properties of A-site charge unbalance substitution of [(Pb0.45Ca0.55)(1-x) La-x] (Fe0.5Nb0.5)O-3(+) (P45CLFN) were improved because the solid solution of small amount of surplus La3+ with (Pb, Ca)(2+) could eliminate oxygen vacancies, and the formation of secondary phase (pyrochlore) was also caused by surplus La3+. The decreasing of dielectric constant with the increase of La3+ content is due to the formation of pyrochlore. The grain size is changed slightly and Q(f) values (7000 similar to 7300 GHz) are almost unchanged at x = 0.02 similar to 0.10, but the temperature coefficient of resonant frequency (TCF) are increased and changed from negative to positive. TCF is zero at x 0.075 with Q(f) = 7267 GHz and K = 89. TCF of all specimens are within +/- 5 x 10(-6)degrees C-1.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The laser-induced damage threshold (LIDT) and damage morphology of antireflection (AR) coatings on quartz and sapphire are investigated. A very interesting phenomena is found in the measurement. In the case of a single pulse laser, the LIDT of the AIR coatings on quartz is higher than that of sapphire. On the contrary, for a free-pulse laser, the LIDT of AIR coatings on sapphire is higher than that of quartz. (C) 2004 Society of Photo-Optical Instrumentation Engineers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Coatings with layer structures of Ag/glass, Ag/Cr/glass, and Ag/Cr-Ag/Cr/glass deposited with magnetron sputtering are investigated. The results indicate that the performance for reflectance, hardness, adherence, and humidity durability of the silver coatings with Ag/Cr/glass and Ag/Cr-Ag/Cr/glass structures are better than pure silver film. In addition, the silver coatings with an Ag/Cr-Ag/glass structure present more advantages than that of the Ag/Cr/glass. Reasons are analyzed accordingly. (C) 2004 Society of Photo-Optical Instrumentation Engineers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Laser conditioning effects of the HfO2/SiO2 antireflective (AR) coatings at 1064 nm and the accumulation effects of multishot laser radiation were investigated. The HfO2/SiO2 AR coatings were prepared by E-beam evaporation (EBE). The singleshot and multi-shot laser induced damage threshold was detected following ISO standard 11254-1.2, and the laser conditioning was conducted by three-step raster scanning method. It was found that the single-shot LIDT and multi-shot LIDT was almost the same. The damage mostly > 80% occurred in the first shot under multi-shot laser radiation, and after that the damage occurring probability plummeted to < 5%. There was no obvious enhancement of the laser damage resistance for both the single-shot and multi-shot laser radiation of the AR coatings after laser conditioning. A Nomarski microscope was employed to map the damage morphology, and it found that the damage behavior is defect-initiated for both unconditioned and conditioned samples. © 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Y2O3/SiO2 coatings were deposited on fused silica by electron beam evaporation. A continuous wave CO2 laser was used to condition parts of the prepared samples at different scanning speeds in the air. LAMBDA 900 spectrometer was used to investigate the changes of the transmittance and residual reflection spectrum. A Nomarski microscope under dark field was used to examine the changes of the micro defect density. The changes of the surface roughness and the microstructure of the film before and after conditioning were investigated by AFM and X-ray diffraction, respectively. We found that laser-induced damage threshold (LIDT) of the films conditioning at 30 mm/s scanning speed was increased by more than a factor of 3 over the thresholds of the as-deposited films. The conditioning effect was correlated with an irradiation-induced decrease of the defect density and absorption of the films. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

There are two different effects to generate group delay dispersion by multilayer thin film mirrors: chirper effect and Gires-Tournois effect. Both effects are employed to introduce desired dispersion in the designed mirror. Thus the designed mirror provides large dispersion throughout broad waveband. Such mirror can be used for dispersion compensation in Ti:sapphire femtosecond lasers. Most group delay dispersion of a 5-mm Ti:sapphire crystal can be compensated perfectly with only four bounces of the designed mirror.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

ZrO2 coatings were deposited on different substrates of Yb:YAG and fused silica by electron beam evaporation. After annealed for 12 h at 673 and 1073 K, respectively, weak absorption of coatings was measured by surface thermal lensing (STL) technique, and then laser-induced damage threshold (LIDT) was determined also. The crystalline phase of ZrO2 coatings and the size of the crystal grain were investigated by X-ray diffraction. It was found that microstructure of ZrO2 coatings was dependent on both annealing temperature and substrate structure, and coatings containing monoclinic phases had higher damage threshold than others. Due to the strong absorption of Yb:YAG, damage threshold of coatings on Yb:YAG was much less than that on fused silica. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

By analysis of impurity elements in HfO2 coating material, the influence of main impurity elements on the characteristic of coatings were studied. The results indicate that the metal elements and absorptive dielectric elements damage the HfO2 coatings. The more the Zr element content is, the more the absorption is for the coatings in ultraviolet wave. The negative ion element will become the gas source center and form an ejection in the process of evaporation of coating material, so decrease the damage threshold of the coatings.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

渐变折射率薄膜,又称为非均匀膜。利用德鲁德理论分析了混合介质膜的介电常量与各个膜料的介电常量之间的关系,介绍了共蒸法制备非均匀膜的制备机理。对混合膜的沉积速率为两种膜料的沉积速率之和的情况,分别从两种膜料的单分子体积是否相等和总的沉积速率是否为常数两个方面,探讨了双源共蒸法制备的非均匀膜的折射率分布规律与膜料的沉积速率之间的关系,并给出了几种常见的折射率分布如线性变化、正弦变化、指数变化和双曲变化规律的膜料沉积速率表达式。最后以混合介质膜的总沉积速率为常数、折射率按照线性变化为例进行了说明。

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Used in chirped-pulse amplification system and based on multi-layer thin film stack, pulse compressor gratings (PCG) are etched by ion-beam and holographic techniques. Diffraction efficiency and laser-induced damage threshold rely on the structural parameters of gratings. On the other hand, they depend greatly on the design of multi-layer. A theoretic design is given for dielectric multi-layer, which is exposed at 413.1 nm and used at 1053 nm. The influences of coating design on optical characters are described in detail. The analysis shows that a coating stack of H3L (H2L) (boolean AND) 9H0.5L2.01H meets the specifications of PCG well. And there is good agreement of transmission between experimental and the theoretic design. (c) 2005 Elsevier GmbH. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

利用德鲁德理论和洛伦兹一洛伦茨理论,从介电常数分析人手,探讨了混合介质膜的折射率表达式,给出利用双源共蒸法镀制的渐变折射率薄膜在混合介质膜的总沉积速率恒定、两种膜料的单分子大小近似相等和沉积速率均为线性变化时的折射率表达式;从正变和负变、单周期和多周期、不同的周期数和不同的单周期厚度几个方面对渐变折射率薄膜的光学特性进行了模拟分析和讨论;对渐变折射率薄膜的实现、应用以及实验制备中有待进一步解决和处理的问题进行了讨论。

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Laser induced damage threshold (LIDT) of multi-layer dielectric used in pulse compressor gratings (PCG) was investigated. The sample was prepared by e-beam evaporation (EBE). LIDT was detected following ISO standard 11254-1.2. It was found that LIDTs of normal and 51.2 deg. incidence (transverse electric (TE) mode) were 14.14 and 9.31 J/cm2, respectively. A Nomarski microscope was employed to map the damage morphology, and it was found that the damage behavior was pit-concave-plat structure for normal incidence, while it was pit structure for 51.2 deg. incidence with TE mode. The electric field distribution was calculated to illuminate the difference of LIDT between the two incident cases.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Two different kinds of 1064 nm high-reflective (HR) coatings, with and without SiO2 protective layer, were prepared by electron beam evaporation. Three-dimensional damage morphology, caused by a Nd:YAG pulsed laser, was investigated for these HR coatings. Development of laser-induced damage on HR coatings was revealed by both temperature field calculation and discrete meso-element simulation. Theoretical results met experimental very well. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

TiO2 coatings were prepared on fused silica with conventional electron beam evaporation deposition. After TiO2 thin films were annealed at different temperatures for 4 h, several properties were investigated by X-ray diffraction (XRD), spectrometer.. photoelectron spectroscopy (XPS) and AFM. It was found that with the annealing temperature increasing, the transmittance of TiO2 coatings decreased, and the cutoff wavelength shifted to long wavelength in near ultraviolet band. Especially, when coatings were annealed at high temperature, the optical loss is very serious, which can be attributed to the scattering and the absorption of TiO2 coatings. XRD patterns revealed that only anatase phase was observed in TiO2 coatings regardless of the different annealing temperatures. XPS results indicated that the fine chemical shift of TiO2 2p(1/2) should be attributed to existence of oxygen vacancies around Ti+4 ion. The investigation on surface morphology by AFM showed that the RMS of titania thin films gradually increases from less than 0.40 nm to 5.03 nm and it should be ascribed to the growth of titanium dioxide grain size with the increase of annealing temperature. (C) 2005 Elsevier B.V. All rights reserved.