Resumo:
Undoped GaN epilayer on c-face (0 0 0 1) sapphire substrate has been grown by metalorganic vapor-phase epitaxy (MOVPE) in a horizontal-type low-pressure two-channel reactor. Photoluminescence (PL) as a function of temperature and excitation intensity have been systematically studied, and the competition between near band gap ultraviolet (UV) and defect-related yellow luminescence (YL) has been extensively investigated, It is revealed that the ratio of the UV-to-YL peak intensities depends strongly on the excitation intensity and the measurement temperature. The obtained results have been analyzed in comparison with the theoretical predications based on a bimolecular model. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
GaN epilayers on sapphire substrate grown by metalorganic vapor-phase epitaxy (MOVPE) in a horizontal-type low-pressure two-channel reactor were investigated. Samples were characterized by X-ray diffraction (XRD), Raman scattering, atomic force microscopy (AFM) and photoluminescence (PL) measurements. The influence of the temperature changes between low temperature (LT) deposited GaN buffer and high temperature (WT) grown GaN epilayer on crystal quality of epilayer was extensively studied. The effect of in situ thermal annealing during the growth on improving the GaN layer crystal quality was demonstrated and the possible mechanism involved in such a growth process was discussed. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
Three-dimensional GaN pyramids have been successfully obtained on submicron dot-patterned (0001) sapphire substrates by using the selective metalorganic vapor phase epitaxy (MOVPE) technique. The dot-pattern is a hexagon arranged with a 0.5-mu m width and 1.0-mu m spacing. The GaN structure comprises a hexagonal pyramid covered with six {1 (1) over bar 01} pyramidal facets on the side of a hexagonal pyramid having a (0001) facet on the top. Cathodoluminescence (CL) measurement was carried our. on the hexagonal pyramid at low temperature. Two distinct spectra were observed to occur at about 359 and 329 nm. The higher energy is thought to be related to GaN dot, and the lower one is due to GaN dot band edge emission. The intensities of the two spectra were investigated as a function of temperature in the range of 135-150 K. (C) 2000 Published by Elsevier Science B.V.
Resumo:
We measured the depth profiling of photoluminescence (PL) in cubic GaN films. The depth-resolved PL of normal grown GaN layers showed that the near-band-edge luminescence intensities of both cubic and wurtzite domains remained constant only until an etching depth of up to 2.7 mu m, but their ratio remained unchanged at all etching depths. Moreover, when a thin In0.1Ga0.9N layer was sandwiched between two GaN layers, the content of the wurtzite domains increased, and its distribution showed a dependence on thickness. As the reactive ion etching depth increased, the PL intensity ratio of cubic GaN to wurtzite domains increased. Based on the distribution, the strain relaxation, instead of the instability of cubic GaN at high temperature, was attributed to the origin of wurtzite domains. (C) 2000 Elsevier Science S.A. All rights reserved.
Resumo:
We observe "ghost" islands formed on terraces during homoepitaxial nucleation of GaN. We attribute the ghost islands to intermediate nucleation states, which can be driven into "normal" islands by scanning tunneling microscopy. The formation of ghost islands is related to excess Ga atoms on the surface. The excess Ga also affect island number density: by increasing Ga coverage, the island density first decreases, reaching a minimum at about 1 monolayer (ML) Ga and then increases rapidly for coverages above 1 ML. This nonmonotonic behavior points to a surfactant effect of the Ga atoms.
Resumo:
Interdigital metal-semiconductor-metal (MSM) ultraviolet photoconductive detectors have been fabricated on undoped GaN films grown by molecular beam epitaxy (MBE), Response dependence on wavelength, applied current, excitation powers and chopper frequency has been extensively investigated. It is shown that the photodetector's spectral response remained nearly constant for wavelengths above the band gap and dropped sharply by almost three orders of magnitude for wavelengths longer than the band gap. It increases linearly with the applied constant current, but very nonlinearly with illuminating power. The photodetectors showed high photoconductor gains resulting from trapping of minority carriers (holes) at acceptor impurities or defects. The results demonstrated the high quality of the GaN crystal used to fabricate these devices. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Strains in cubic GaN films grown on GaAs (001) were measured by a triple-axis x-ray diffraction method. Residual strains in the as-grown epitaxial films were in compression, contrary to the predicted tensile strains caused by large lattice mismatch between epilayers and GaAs substrates (20%). It was also found that the relief of strains in the GaN films has a complicated dependence on the growth conditions. We interpreted this as the interaction between the lattice mismatch and thermal mismatch stresses. The fully relaxed lattice constants of cubic GaN are determined to be 4.5038 +/- 0.0009 Angstrom, which is in excellent agreement with the theoretical prediction of 4.503 Angstrom. (C) 2000 American Institute of Physics. [S0021-8979(00)07918-4].
Resumo:
Photoluminescence measurements have been performed on cubic GaN films with carrier concentration as low as 3 x 10(13) cm(-3). From the temperature and excitation intensity dependence, the emission lines at 3.268, 3.150 and 3.081 eV were assigned to the excitonic, donor-acceptor pair, and free-to-acceptor transitions, respectively Additionally, we observed two additional emission lines at 2.926 and 2.821 eV, and suggested that they belong to donor-acceptor pair transitions. Furthermore, from the temperature dependence of integral intensities, we confirmed that three donor-acceptor pair transitions (3.150, 2.926, and 2.821 eV) are from a common shallow donor to three different accepters. The excitonic emission at 3.216 eV has a full-width-at-half-maximum value of 41 meV at room temperature, which indicates a good optical quality of our sample.
Resumo:
Deep levels in undoped GaN materials grown by modified molecular beam epitaxy (MBE) are investigated by photoluminescence (PL) and optical quenching of photoconductivity measurements. A broad band which extends from 2.1 to 3.0 eV with a maximum at about 2.7 eV is observed, and four prominent quenching bands were found located at 2.18, 2.40, 2.71, and 2.78 eV above the valence band, respectively. These levels are attributed to four holes trap levels existence in the material. The defects cannot be firmly identified at present. (C) 2000 Elsevier Science B.V, All rights reserved.
Resumo:
Using Raman spectroscopy we have analysed the strain status of GaN films grown on sapphire substrates by NH3 source molecular beam epitaxy (MBE). In addition to the expected compressive biaxial strain, in some cases GaN films grown on c-face sapphire substrates suffer from serious tensile biaxial strain. This anomalous behaviour has been well interpreted in terms of interstitial hydrogen-dependent lattice dilation. The hydrogen concentration in the films is measured by nuclear reaction analysis (NRA). With increasing hydrogen incorporation, the residual compressive biaxial strain is first further relaxed, and then turns into tensile strain when the hydrogen contaminant exceeds a critical concentration. The hydrogen incorporation during the growth process is found to be growth-rate dependent, and is supposed to be strain driven. We believe that the strain-induced interstitial incorporation is another way for strain relaxation during heteroepitaxy, besides the two currently well known mechanisms: formation of dislocations and growth front roughening.
Resumo:
Cubic GaN(c-GaN) films are grown on GaAs(001) substrates by metalorganic chemical vapor deposition (MOCVD). Two GaN samples were grown with different buffer layer, the deposition time of each was 1 and 3 min, respectively. 4-circle X-ray double crystal diffraction (XRDCD) was used to study the secondary crystallographic phases presented in the c-GaN films. The phase composition of the epilayers was determined by X-ray reciprocal space mapping. The intensities of the c-GaN(002) and h-GaN(10 (1) over bar 1) planes detected in the mapping were investigated by omega scans. The content of the hexagonal phase inclusions in the c-GaN films was calculated to about 1.6 and 7.9%, respectively. The thicker buffer layer is not preferable for growing high quality pure c-GaN films. (C) 2000 Elsevier Science S.A. All rights reserved.
Resumo:
We present some results on the effect of initial buffer layer on the crystalline quality of Cubic GaN epitaxial layers grown on GaAs(100) substrates by metalorganic chemical vapor deposition. Photoluminescence and Hall measurements were performed to characterize the electrical and optical properties of cubic GaN. The crystalline quality subsequently grown high-temperature (HT) cubic GaN layers strongly depended on thermal effects during the temperature ramping process after low temperature (LT) growth of the buffer layers. Atomic force microscope (AFM) and reflection high-energy electron diffraction (RHEED) were employed to investigate this temperature ramping process. Furthermore, the role of thermal treatment during the temperature ramping process was identified. Using the optimum buffer layer, the full width at half maxim (FWHM) at room temperature photoluminescence 5.6 nm was achieved. To our knowledge, this is the best FWHM value for cubic GaN to date. The background carrier concentration was as low as 3 x 10(13) cm(-3). (C) 2000 Published by Elsevier Science S.A. All rights reserved.
Resumo:
The hole effective-mass Hamiltonian for the semiconductors of wurtzite structure is established, and the effective-mass parameters of GaN and AlxGa1-xN are given. Besides the asymmetry in the z and x, y directions, the linear term of the momentum operator in the Hamiltonian is essential in determining the valence band structure, which is different from that of the zinc-blende structure. The binding energies of acceptor states are calculated by solving strictly the effective-mass equations. The binding energies of donor and acceptor for wurtzite GaN are 20 and 131, 97 meV, respectively, which are inconsistent with the recent experimental results. It is proposed that there are two kinds of acceptors in wurtzite GaN. One kind is the general acceptor such as C, substituting N, which satisfies the effective-mass theory, and the other includes Mg, Zn, Cd etc., the binding energy of which deviates from that given by the effective-mass theory. Experimentally, wurtzite GaN was grown by the MBE method, and the PL spectra were measured. Three main peaks are assigned to the DA transitions from the two kinds of acceptor. Some of the transitions were identified as coming from the cubic phase of GaN, which appears randomly within the predominantly hexagonal material. The binding energy of acceptor in ALN is about 239, 158 meV, that in AlxGa1-xN alloys (x approximate to 0.2) is 147, 111 meV, close to that in GaN. (C) 2000 Published by Elsevier Science S.A. All rights reserved.
Resumo:
GaN epilayers grown on pre-nitridated (0001) sapphire substrates by metallorganic vapor phase epitaxy were investigated by wavelength dispersive X-ray spectroscopy and energy dispersive S-ray spectroscopy. Precipitates were observed to mainly consist of O impurity whose strengths were weaker than surrounding matrix. The precipitates were larger in size and distributed more sparsely and inhomogeneously in < 11-20 > directions of the epilayers grown on substrates pre-nitridated for longer periods. The larger precipitates often joined to cracks in the TEM specimens. The crack formation seems to be attributed to the compressive stress concentration at edge angles of the larger precipitates. Yellow luminescence of the epilayers was imaged by cathodoluminescence. The distribution similarity between the cathodoluminescence and the precipitates suggested that the precipitates were responsible for the yellow luminescence band. (C) 2000 Elsevier Science S.A, All rights reserved.
Resumo:
The optical properties of cubic GaN films have been investigated in the temperature range of 10-300 K. Five peaks were observed at 10 K. From the dependence of photoluminescence emissions on the temperature and excitation intensity, we have assigned two of the five peaks (2.926 and 2.821 eV) to donor-acceptor pair (DAP) transitions. Furthermore, these two peaks were found to be related to a common shallow donor involved in the peak position previously reported at 3.150 eV. The intensities of DAP transitions were much weaker than that of excitonic emission even at low temperature, indicating a relatively high purity of our samples. (C) 2000 American Institute of Physics. [S0003-6951(00)00921-9].