521 resultados para chemical vapor deposition processes


Relevância:

100.00% 100.00%

Publicador:

Resumo:

As reported by other authors, we have also observed that the Si growth rate decreases with increasing phosphine (PH3) flow rate in gas source-Si molecular beam epitaxy using phosphorous (P) as a n-type dopant. Why small quantity PH3 can affect Si growth rate? Up to now, the quantitative characterization of PH3 flow influence on Si growth rate is little known. In this letter, the PH, influence will be analyzed in detail and a model considering strong P surface segregation and its absorption of hydrogen will be proposed to characterize the effect. (C) 2000 Elsevier Science B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A novel semiconductor laser structure is put forward to resolve the major difficulties of high power laser diodes. In this structure, several active regions are cascaded by tunnel junctions to form a large optical cavity and to achieve super high efficiency. This structure can solve the problems of catastrophic optical damage of facet, thermal damage and poor light beam quality effectively. Low-pressure metalorganic chemical vapor deposition method is adopted to grow the novel semiconductor laser structures, which are composed of Si:GaAs/C:GaAs tunnel junctions, GaAs/InGaAs strain quantum well active regions. External differential quantum efficiency as high as 2.2 and light power output of 2.5 W per facet (under 2A drive current) are achieved from an uncoated novel laser device with three active regions.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Phosphor-doped nano-crystalline silicon ((n))nc-Si:H) films are successfully grown on the p-type (100) oriented crystal silicon ((p) c-Si) substrate by conventional plasma-enhanced chemical vapor deposition method. The films are obtained using high H-2 diluted SiH4 as a reaction gas source and using PH3 as the doping gas source of phosphor atoms. Futhermore, the heterojunction diodes are also fabricated by using (n)nc-Si:H films and (p)c-Si substrate. I-V properties are investigated in the temperature range of 230-420K. The experimental results domenstrate that (n)nc-Si:H/(p) c-Si heterojunction is a typical abrupt heterojunction having good rectifing and temperature properties. Carrier transport mechanisms are tunneling - recombination model at forward bias voltages. In the range of low bias voltages ( V-F< 0.8 V), the current is determined by recombination at the (n)nc-Si:H side of the space charge region, while the current becomes tunneing at higher bias voltages( V-F>1.0 V). The present heterojunction has high reverse breakdown voltage ( > - 75 V) and low reverse current (approximate to nA).

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this paper, we conduct a theoretical analysis of the design, fabrication, and performance measurement of high-power and high-brightness strained quantum-well lasers emitting at 0.98 mum, The material system of interest consists of an Al-free InGaAs-InGaAsP active region and AlGaAs cladding layers. Some key parameters of the laser structure are theoretically analyzed, and their effects on the laser performance are discussed. The laser material is grown by metal-organic chemical vapor deposition and demonstrates high quality with low-threshold current density, high internal quantum efficiency, and extremely low internal loss. High-performance broad-area multimode and ridge-waveguide single-mode laser devices are fabricated. For 100-mum-wide stripe lasers having a cavity length of 800 mum, a high slope efficiency of 1.08 W-A, a low vertical beam divergence of 34 degrees, a high output power of over 4.45 W, and a very high characteristic temperature coefficient of 250 K were achieved. Lifetime tests performed at 1.2-1.3 W (12-13 mW/mum) demonstrates reliable performance. For 4-mum-wide ridge waveguide single-mode laser devices, a maximum output power of 394 mW and fundamental mode power up to 200 mW with slope efficiency of 0.91 mW/mum are obtained.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The hydrogenated amorphous SiOx films (a-SiOx:H) with various oxygen contents have been prepared using plasma enhanced chemical vapor deposition technique. The films were implanted with erbium and annealed by rapid thermal annealing. An intense photoluminescence (PL) of Er at 1.54 mum has been observed at 77 K and at room temperature. The PL intensity depends strongly on both the oxygen content of the film and the rapid thermal annealing temperature and reaches its maximum if the ratio of O/Si in the film is approximately equal to 1.0 at 77 K and to 1.76 at room temperature. The microstructure of the film also has strong influences on the PL intensity. The PL intensity at 250 K is slightly more than a half of that at 15 K. It means that the temperature quenching effect of the PL intensity is very weak.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

By mass-selected low energy ion beam deposition, amorphous carbon film was obtained. X-ray diffraction, Raman and Auger electron spectroscopy depth line shape measurements showed that such carbon films contained diamond particles. The main growth mechanism is subsurface implantation. Furthermore, it was indicated in a different way that ion bombardment played a decisive role in bias enhanced nucleation of chemical vapor deposition diamond.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The surface reaction mechanism of Si1-xGex/Si growth using SiH4 and GeH4 in UHV/CVD system was studied. The saturated adsorption and desorption of SiH4 from Si(1 0 0) surface was investigated with the help of TPD and RHEED, and it was found that all the 4 hydrogen atoms of one SiH4 molecule were adsorbed to the Si surface, which meant that the dissociated adsorption ratio was proportional to 4 power of surface vacancies. The analysis of the reaction of GeH4 was also done. A new surface reaction kinetic model on Si1-xGex/Si epitaxial growth under UHV conditions by SiH4/GeH4 was proposed based on these studies. The predictions of the model were verified by the experimental results. (C) 2000 Elsevier Science B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Three-dimensional GaN pyramids have been successfully obtained on submicron dot-patterned (0001) sapphire substrates by using the selective metalorganic vapor phase epitaxy (MOVPE) technique. The dot-pattern is a hexagon arranged with a 0.5-mu m width and 1.0-mu m spacing. The GaN structure comprises a hexagonal pyramid covered with six {1 (1) over bar 01} pyramidal facets on the side of a hexagonal pyramid having a (0001) facet on the top. Cathodoluminescence (CL) measurement was carried our. on the hexagonal pyramid at low temperature. Two distinct spectra were observed to occur at about 359 and 329 nm. The higher energy is thought to be related to GaN dot, and the lower one is due to GaN dot band edge emission. The intensities of the two spectra were investigated as a function of temperature in the range of 135-150 K. (C) 2000 Published by Elsevier Science B.V.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We have studied the effect of rapid thermal annealing (RTA) on GaInNAs/GaAs quantum wells (QWs) grown by molecular-beam epitaxy using a dc plasma as the N source. It was found that RTA at low temperature (LT, 650 degrees C) and high temperature (HT, 900 degrees C) could both improve the QW quality significantly. To clarify the mechanism of quality improvement by RTA, a magnetic field perpendicular to the path of the N plasma flux was applied during the growth of the GaInNAs layers for the sake of comparison. It was found that LT-RTA mainly removed dislocations at interfaces related to the ion bombardment, whereas, HT-RTA further removed dislocations originating from the growth. LT-RTA caused only a slight blueshift of photoluminescence peak wavelength, probably due to defect-assisted interdiffusion of In-Ga at the QW interfaces. The blueshift caused by HT-RTA, on the other hand, was much larger. It is suggested that this is due to the fast defect-assisted diffusion of N-As at the QW interfaces. As defects are removed by annealing, the diffusion of In-Ga at interfaces would be predominant. (C) 2000 American Institute of Physics. [S0003- 6951(00)01535-7].

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A constant amount of Ge was deposited on strained GexSi1-x layers of approximately the same thickness but with different alloy compositions, ranging from x = 0.06 to x = 0.19. From their atomic-force-microscopy images, we found that both the size and density of Ge islands increased with the Ge composition of the strained layer. By conservation of mass, this implies that these islands must incorporate material from the underlying strained layer. (C) 2000 American Institute of Physics. [S0003-6951(00)03529-4].

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Hydrogenated amorphous SiOx films are fabricated via plasma enhanced chemical vapor deposition technique. After erbium implantation and rapid thermal annealing, photoluminescence (PL) are measured at 77 K and room temperature (RT), respectively. We observed the strong PL at 1.54 mu m at RT. The 1.54 mu m PL intensity changes with the variation of concentration of oxygen. The most intense PL at 77 K in a-SiOx:H (Er) corresponds to O/Si = 1.0 and at RT to O/Si = 1.76. Based on our results, we propose that Er ions contributed to PL come from O-rich region in the film. Er ions in Si-rich region have no relation with FL. Temperature dependence of the intensity of the 1.54 mu m line of the Er3+ transition displays a very weak temperature quenching in Er-doped hydrogenated amorphous Si. The PL intensity at 250 K is a little more one half of that at 15 K.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We have studied the growth of GaInNAs by a plasma-assisted molecular-beam epitaxy (MBE). It was found that the N-radicals were incorporated into the epitaxial layer like dopant atoms. In the range of 400-500 degrees C, the growth temperature (T-g) mainly affected the crystal quality of GaInNAs rather than the N concentration. The N concentration dropped rapidly when T-g exceeded 500 degrees C. Considering N desorption alone is insufficient to account for the strong falloff of the N concentration with T-g over 500 degrees C, the effect of thermally-activated N surface segregation must be taken into account. The N concentration was independent of the arsenic pressure and the In concentration in GaInNAs layers, but inversely proportional to the growth rate. Based on the experimental results, a kinetic model including N desorption and surface segregation was developed to analyze quantitatively the N incorporation in MBE growth. (C) 2000 American Institute of Physics. [S0003-6951(00)00928-1].

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We report on the strong blue-violet photoluminescence (PL) at room temperature from the large-scale highly aligned boron carbonitride (BCN) nanofibers synthesized by bias-assisted hot filament chemical vapor deposition. The photoluminescence peak wavelength shifts in the range of 470-390 nm by changing the chemical composition of the BCN nanofibers, which shows an interesting blue and violet-light-emitting material with adjustable optical properties. The mechanism for the shift of the PL peaks at room temperature is also discussed. (C) 2000 American Institute of Physics. [S0003-6951(00)04427-2].

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Raman scattering measurement has been used to study the residual strains in the thin 3C-SiC/Si(001) epilayers with a variation of film thickness from 0.1 to 1.2 mu m. which were prepared by chemical vapor deposition (CVD)growth. Two methods have been exploited to figure our the residual strains and the exact LO bands. The final analyzing results show that residual strains exist in the 3C-SiC epilayers. The average stress is 1.3010 GPa, and the relative change of the lattice constant is 1.36 parts per thousand. Our measurements also show that 3C-SiC phonons are detectable even for the samples with film thickness in the range of 0.1 to 0.2 mu m. (C) 2000 Published by Elsevier Science S.A. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this paper, we reported on the fabrication of 980 nm InGaAs/InGaAsP strained quantum-well (QW) lasers with broad waveguide. The laser structure was grown by low-pressure metalorganic chemical vapor deposition on a n(+)- GaAs substrate. For 3 mu m stripe ridge waveguide lasers, the threshold current is 30 mA and the maximum output power and the output power operating in fundamental mode are 350 mW and 200 mW, respectively. The output power from the single mode fiber is up to 100 mW, the coupling efficiency is 50%. We also fabricated 100 mu m broad stripe coated lasers with cavity length of 800 mu m, a threshold current density of 170 A/cm(2), a high slope efficiency of 1.03 W/A and a far-field pattern of 40 x 6 degrees are obtained. The maximum output power of 3.5 W is also obtained for 100 mu m wide coated lasers. (C) 2000 Elsevier Science B.V. All rights reserved.