571 resultados para infrared luminescence
Resumo:
The photoluminescence (PL) properties of nitrogen-doped ZnSe epilayers grown on semi-insulating GaAs(100) substrates by MBE using a rf-plasma source for N doping were investigated. The PL peak which can be related to N acceptor was observed in the PL spectra of ZnSe:N smaples. At 10K, as the excitation power density increases, the energy of donor-acceptor pair(DAP) emission shows a blue-shift and its intensity tends to saturate. As the temperature increases over a range from 10K to 300K, the relative PL intensity of donor bound exciton to that of the acceptor bound exciton increases due to the transfer between two bound excitons.
Resumo:
A novel method, based on an infrared absorption and neutron irradiation technique, has been developed for the determination of interstitial oxygen in heavily boron-doped silicon. The new procedure utilizes fast neutron irradiated silicon wafer specimens. On fast neutron irradiation, the free carriers of high concentration in silicon can be trapped by the irradiated defects and the resistivity increased. The resulting calibration curve for the measurement of interstitial oxygen in boron-doped silicon has been established on the basis of the annealing behaviour of irradiated boron-doped CZ silicon.
Resumo:
30-period InGaAs/GaAs quantum dot superlattice was fabricated by MBE. Using cross sectional transmission electron microscopy, the InGaAs quantum dots were found to be perfectly vertically aligned in the growth direction (100). Under normally incident radiation, a distinct absorption in the 8.5 similar to 10.4 mu m range peaked at 9.9 mu m was observed. The normally incident infrared absorption in vertically aligned quantum dot superlattice in the 8 similar to 12 mu m range was realized for the first time. This result indicates the potential application of the quantum dot superlattice structure without grating as normally incident infrared detector focal plane arrays.
Resumo:
A pronounced photoluminescence enhancement on chemically oxidized porous silicon was induced by a series of organic cyano compounds including 1,2-dicyanoethylene (CE), 1,3-dicyanobenzene (1,3-CB), 1,4-dicyanobenzene (1,4-CB), 1-cyanonaphthalene (1-CN), and 9-cyanoanthracene (9-CA). Photoluminescence enhancement effects were reversible for all compounds studies in this work. A dependence of photoluminescence enhancement on the steric effect and the electronic characteristics of these compounds and the structure of the porous silicon substrates were analyzed in terms of the photoluminescence enhancing factors. Surface chemical composition examined by Fourier transform infrared (FTIR) spectra demonstrated that the surface Si-H bonds were not changed and no new luminescent compounds were formed on porous silicon surface during adsorption of cyano compounds. A mechanism based on induced surface states acting as radiative recombination centers by cyano compounds adsorption was suggested.
Resumo:
We report the device performance of normal-incidence (In, Ga)As/GaAs quantum dot intersubband infrared photodetectors. A primary intersubband transition peak is observed at the wavelength of 13 mu m (E-0 --> E-1) and a secondary peak at 11 mu m (E-0 --> E-2). The measured energy spacing in the conduction band of the quantum dots is in good agreement with low temperature photoluminescence measurement and calculations. A peak detectivity of 1 x 10(10) cm Hz(1/2)/W at 13 mu m was achieved at 40 K for these devices. (C) 1998 American Institute of Physics. [S0003-6951(98)01440-5].
Resumo:
We have observed an extremely narrow absorption spectrum due to bound-to-continuum transition in GaAs/AlxGa1-xAs multiple quantum wells (MQWs). Its linewidth is only about one tenth of the values reported previously. Our calculation indicates that the broadening of the excited state in the continuum has little contribution to the absorption linewidth. We have grown a sample whose MQW region contains two kinds of wells with a minor thickness inhomogeneity. Its resultant absorption linewidth is six times as large as that of homogeneous well sample, which is in good agreement with our theoretical analysis. Thus we can suggest that the wider absorption spectra reported by many authors may be due to the well width inhomogeneity. (C) 1998 American Institute of Physics. [S0003-6951(98)03430-5]
Resumo:
The strong photoluminescence (PL) of SiOx:H prepared by plasma enhanced chemical vapor deposition has been systematically studied in conjunction with infrared and micro-Raman spectra. We have found that each PL spectrum is comprised of two Gaussian components, a main band and a shoulder. The main band might originate from amorphous silicon clusters embedded in die SiOx network, and its redshift with annealing temperature is due to expansion of the silicon clusters. The shoulder remains at about 835 nm in spite of the annealing temperature and possibly comes from luminescent defect centers. The enhanced PL spectra after 1170 degrees C annealing are attributed to the quantum confinement effects of nanocrystalline silicon embedded in the SiO2 matrix. (C) 1998 American Institute of Physics.
Resumo:
The microstructure, hydrogen bonding configurations and hydrogen content of high quality and stable hydrogenated amorphous silicon (a-Si:H) films prepared by a simple ''uninterrupted growth/annealing" plasma enhanced chemical vapor deposition technique have been investigated by Raman scattering and infrared absorption spectroscopy. The high stability a-Si:H films contain small amounts of a microcrystalline phase and not less hydrogen (10-16 at. %), particularly, the clustered phase hydrogen, Besides, the hydrogen distribution is very inhomogeneous. Some of these results are substantially distinct from those of conventional device-quality n-Si:H film or stable cr-Si:H films prepared by the other techniques examined to date. The stability of n-Si:H films appears to have no direct correlation with the hydrogen content or the clustered phase hydrogen concentration. The ideal n-Si:H network with high stability and low defect density is perhaps not homogeneous. (C) 1998 American Institute of Physics.
Resumo:
We analyze low-temperature Raman and photoluminescence spectra of MBE-grown GaN layers on sapphire. Strong and sharp Raman peaks are observed in the low frequency region. These peaks, which are enhanced by excitation in resonance with yellow luminescence transitions, are attributed to electronic transitions related to shallow donor levels in hexagonal GaN. It is proposed that a low frequency Raman peak at 11.7 meV is caused by a pseudo-local vibration mode related to defects involved in yellow luminescence transitions. The dependence of the photoluminescence spectra on temperature gives additional information about the residual impurities in these GaN layers.
Resumo:
AgI clusters in zeolite-Y (AgI/Y) were prepared by Ag+ exchange followed by reaction with NaI in solution. The formation of the clusters was determined by transmission electron microscopy and Auger electron spectroscopy. The clusters were uniform and even in size, 1.0-2.0 nm. The fluorescence spectrum of the clusters consists of two emission bands, which are attributed to AgI and Ag clusters, respectively. Photostimulated luminescence (PSL) is observed by stimulation at 675 or at 840 nm. The PSL spectrum of AgI/Y is consistent with the emission spectrum of Ag clusters and thus the PSL is considered to be caused by the charge transfer or carrier migration from the zeolite framework or from the AgI clusters to the Ag clusters. The appearance of PSL indicates that these materials may find application as a medium for erasable optical memory. (C) 1998 American Institute of Physics. [S0021-8979(98)02407-4].
Resumo:
Three new absorption bands, appearing around 670, 865 and 980 nm, are observed in BaFCl:Eu2+ phosphors. They are ascribed to F aggregates formed by association of F centers or by trapping of electrons to the primary F-n(+) (n = 2,3,4) centers. The growth curves of F and F-aggregated centers are similar and may be divided into three stages. The photostimulated luminescence (PSL) decays by stimulation into the absorption bands of F centers and of F aggregates are different; the former decay logarithmically and the latter decay hyperbolically. Some non-radiative processes related to F aggregates, such as electron migration, occur accompanying the PSL process, which may reduce the PSL efficiency and sensitivity of the phosphors. (C) 1997 Published by Elsevier Science Ltd. All rights reserved.
Resumo:
A novel process of room temperature ion beam sputtering deposition of vanadium oxide films and low temperature post annealing for uncooled infrared detectors was proposed in this work. VOx thin films with relatively low square resistance (70 K Omega / square) and large temperature coefficient of resistance (more than 3%/K) at room temperature were fabricated using this low temperature process which was very compatible with the process of uncooled infrared detectors based on micromachined technology. Furthermore, chemical composition and film surface have been characterized using X-ray photoelectron spectroscopy (XPS) and scanning electron microscopy (SEM) respectively. The results showed that the main composition of the processed thin films was V2O5 and the thin films were in the process of crystallization.
Resumo:
ZnO nanoparticles were synthesized in ethanolic solution using a sol-gel method. The structural and optical properties were investigated by X-ray diffraction, transmission electron microscopy, UV absorption, and photoluminescence. After annealing at 200 degrees C, the particle size is increased and the peak of defect luminescence in the visible region is changed. A yellow emission was observed in the as-prepared sample and a green emission in the annealed sample. The change of the visible emission is related to oxygen defects. Annealing in the absence of oxygen would increase oxygen vacancies. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
Wafers with normal light-emitting diode structure were grown by metal organic chemical vapor deposition system. The pressure and temperature were varied during growth of buffer layer in order to grow different types of epilayers. The cathodoluminescence results show that the interface distortion of quantum well plays an important role in radiant efficiency. The electroluminescence detections indicate that the dislocations also influence the external quantum efficiency by lowering the electron injection efficiency. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
We have investigated the evolution of exciton state filling in InAs/GaAs quantum dot (QD) structures as a function of the excitation power density by using rnicro-photoluminescence spectroscopy at different temperatures. In addition to the emission bands of exciton recombination corresponding to the atom-like S, P and D, etc. shells of QDs, it was observed that some extra states V between the S and P shells, and D' between the P and D shells appear in the spectra with increasing number of excitons occupying the QDs at a certain temperature. The emergence of these inter-shell excitonic levels is power density and temperature dependent, which is an experimental demonstration of strong exciton-exciton exchange interaction, state hybridization, and coupling of a multi-exciton system in QDs. (c) 2006 Elsevier B.V. All rights reserved.