63 resultados para Uniformity coefficient
Resumo:
Compositional influences on the spectroscopic properties of Yb3+ and the structural variations with the introduction of YbF3 were studied in fluorophosphate glasses. Emission cross-section (sigma(emi)) and gain coefficient (sigma(emi) x tau(f)) were calculated which exhibit maximum at RF2 = 33 mol%. YbF3 has an important effect on the glass forming ability of fluorophosphate glasses when RF2 is over 36 mol%. The study of Raman spectra showed big differences on the glass structure between non-Yb3+ and Yb3+ -doped glasses. The main building units in Yb3+-doped samples are metaphosphate groups, pyrophosphate groups (P-2(O,F)(7), PO3F), Al[F-6] +Al[O,F](6) and F3Al-O-AlF3 while those of the non-Yb3+-doped glasses are monophosphate group P(O,F)(4), little pyrophosphate group, Al[F-4] + Al[F-6] + Al[O,F](4) + Al[O,F](6) and F3Al-O-AlF3, which means Yb3+ ions contribute to a better glass polymerization and network uniformity. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Some results of an investigation on the layer thickness uniformity of glancing angle deposition are presented. A zirconia monolayer has been deposited by glancing angle deposition to analyze the layer thickness uniformity. The experimental results indicate that the thickness variation over the substrate is less than 0. 1%, which is considered as good uniformity. It is found that the non-uniformity of experimental results is larger than that of the theoretical results. (c) 2005 Elsevier Ltd. All rights reserved.
Resumo:
Three groups of gynogenetic diploid bighead carp were successfully obtained by means of artificial gynogenesis. The activation rates of gynogenesis varied from 75.9% to 98.8%, and the frequency of spontaneous diploidization was around 0.4%. Over 2000 normally gynogenetic diploid fry were obtained in three gynogenetic groups. The haploid karyotype consisted of nine metacentric, 12 submetacentric, three subtelocentric chromosomes and 45 arms. The chromosome number was 48 from gynogenetic diploid. The results showed that the genetic material of offspring was maternal. The aneuploid hybrid embryos of bighead carp and Xingguo red common carp with chromosome numbers ranging from 28 to 73 did not survive post hatch, likely the result of incompatibility between the nucleus and the cytoplasm of two parents. Sixty RAPD primers from three groups were used for total DNA amplification of gynogenetic offspring, maternal and 'paternal' fish. A total of 451 bands were amplified from three kinds of samples above. From maternal bighead carp, 256 bands were amplified; however, there were 251 shared bands between maternal and gynogenetic bighead carp. From artificial gynogenetic offspring, two 'paternal' DNA segments without an expression function were found. An UPGMA tree showed that gynogenetic offspring were closely clustered and the genetic identity among them was very high (0.956).
Resumo:
For a second-order DFB-LD, the presence of a metal contact layer can reduce I-st-order radiation. Part of the reflected power is redistributed into guided modes and results in a variation of the effective coupling coefficient kappa(eff). In this paper, we study the effect of the Au top contact's reflection on the kappa(eff) of 2(nd)-order DFB lasers. (C) 2004 Wiley Periodicals, Inc.
Resumo:
The hydrogen dilution profiling (HDP) technique has been developed to improve the quality and the crystalline uniformity in the growth direction of mu c-Si:H thin films prepared by hot-wire chemical-vapor deposition. The high H dilution in the initial growth stage reduces the amorphous transition layer from 30-50 to less than 10 nm. The uniformity of crystalline content X-c in the growth direction was much improved by the proper design of hydrogen dilution profiling which effectively controls the nonuniform transition region of Xc from 300 to less than 30 nm. Furthermore, the HDP approach restrains the formation of microvoids in mu c-Si: H thin films with a high Xc and enhances the compactness of the film. As a result the stability of mu c-Si: H thin films by HDP against the oxygen diffusion, as well as the electrical property, is much improved. (c) 2005 American Institute of Physics.
Resumo:
The electronic structures of InSb1-xNx nanowires are investigated using the ten-band k center dot p method. It is found that nitrogen increases the Rashba coefficient of the nanowires dramatically. For thick nanowires, the Rashba coefficient may increase by more than 20 times. The semiconductor-metal transition occurs more easily in InSb1-xNx nanowires than in InSb nanowires. The electronic structure of InSb1-xNx nanowires is very different from that of the bulk material. For fixed x the bulk material is a semimetal, while the nanowires are metal-like. In InSb1-xNx bulk material and thick nanowires, an interesting decrease of electron effective mass is observed near k=0 which is induced by the nitrogen, but this phenomenon disappears in thin nanowires.
Resumo:
The morphological defects and uniformity of 4H-SiC epilayers grown by hot wall CVD at 1500 degrees C on off-oriented (0001) Si faces are characterized by atomic force microscope, Nomarski optical microscopy, and Micro-Raman spectroscopy. Typical morphological defects including triangular defects, wavy steps, round pits, and groove defects are observed in mirror-like SiC epilayers. The preparation of the substrate surface is necessary for the growth of high-quality 4H-SiC epitaxial layers with low-surface defect density under optimized growth conditions. (c) 2006 Elsevier Ltd. All rights reserved.
High uniformity of self-organized InAs quantum wires on InAlAs buffers grown on misoriented InP(001)
Resumo:
Highly uniform InAs quantum wires (QWRs) have been obtained on the In0.5Al0.5As buffer layer grown on the InP substrate 8 degrees off (001) towards (111) by molecular-beam epitaxy. The quasi-periodic composition modulation was spontaneously formed in the In0.5Al0.5As buffer layer on this misoriented InP (001). The width and period of the In-rich bands are about 10 and 40 nm, respectively. The periodic In-rich bands play a major role in the sequent InAs QWRs growth and the InAs QWRs are well positioned atop In-rich bands. The photoluminescence (PL) measurements showed a significant reduction in full width at half maximum and enhanced PL efficiency for InAs QWRs on misoriented InP(001) as compared to that on normal InP(001). (c) 2006 American Institute of Physics.
Resumo:
Microdefects originating from impurity-dislocation interactions in undoped InP that had been annealed in phosphorus and iron phosphide ambiances have been studied using optical microscopy. The electrical uniformity of the annealed wafer is improved by removing impurity aggregation around dislocations and by eliminating impurity striations in the annealing process. Compared to as-grown Fe-doped semi-insulating (SI) material, SI wafers obtained by annealing undoped InP in iron phosphide ambiances have better uniformity. This is attributed to the avoidance of Fe aggregation around dislocations and dislocation clusters, Fe precipitation and impurity striations, and is related to the use of a low concentration of Fe in the annealed material. The influence of Fe diffusion on the migration of dislocations in the annealing process has been studied and reviewed. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
Tensile-strained InAlAs layers have been grown by solid-source molecular beam epitaxy on as-grown Fe-doped semi-insulating (SI) InP substrates and undoped SI InP substrates obtained by annealing undoped conductive InP wafers (wafer-annealed InP). The effect of the two substrates on InAlAs epilayers and InAlAs/InP type II heterostructures has been studied by using a variety of characterization techniques. Our calculation data proved that the out-diffusion of Fe atoms in InP substrate may not take place due to their low diffusion, coefficient. Double-crystal X-ray diffraction measurements show that the lattice mismatch between the InAlAs layers and the two substrates is different, which is originated from their different Fe concentrations. Furthermore, photoluminescence results indicate that the type II heterostructure grown on the wafer-annealed InP substrate exhibits better optical and interface properties than that grown on the as-grown Fe-doped substrate. We have also given a physically coherent explanation on the basis of these investigations. (C) 2003 Elsevier Science B.V. All rights reserved.
Resumo:
Growth interruption was introduced after the deposition of GaAs cap layer, which is thinner than the mean height of Quantum dots. Uniformity of quantum dots has been enhanced because the full width of half maximum of photoluminescence decrease from 80meV to 27meV in these samples as the interruption time increasing from 0 to 120 second. Meanwhile, we have observed that the peak position of photoluminescence is a function of interruption time. This effect can be used to control the energy level of quantum dots. The phenomena mentioned above can be attributed to the diffusion of In atoms from the top of InAs islands to the top of GaAs cap layer caused by the difference of surface energies between InAs and GaAs.
Resumo:
Semi-insulating (SI) InP wafers of 2 and 3 in. diameters have been prepared by annealing undoped LEC InP at 930 degreesC for 80 h under pure phosphorus ambient (PP) and iron phosphide ambient (IP). The electrical uniformity of annealed undoped SI wafers, along with a Fe-doped as-grown SI LEC InP wafer, has been characterized by whole wafer PL mapping and radial Hall measurements. Defects in these wafers have been detected by photo-induced current transient spectroscopy (PICTS). The results indicated that the uniformity of IP wafer is much better than that of PP wafer and as-grown Fe-doped Si InP wafer. There are fewer traps in undoped SI InP IP wafer than in as grown Fe-doped and undoped SI InP PP wafer, as evidenced by PICTS. The good uniformity of the IP wafer is related to the nonexistence of high concentration of thermally induced defects. The mechanism for this phenomenon is discussed based on the results. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
High-quality and high-resistivity GaN films were grown on (0001) sapphire face by metal-organic vapour phase epitaxy. To measure the surface acoustic wave properties accurately, we deposited metallized interdigital transducers on the GaN surface. The acoustic surface wave velocity and electromechanical coupling coefficient were measured, respectively, to be 5667 m/s and 1.9% by the pulse method.