Sm3+-doped yttrium aluminum perovskite (YAP) single crystal was grown by Czochralski (CZ) method. The absorption and fluorescence spectra along the crystallographic axis b were measured at room temperature. Judd-Ofelt theory was used to calculate the intensity parameters (Omega(t)), the spontaneous emission probability, the branching ratio and the radiative lifetime of the state (4)G(5/2). The peak emission cross-sections were also estimated at 567, 607, and 648 nm wavelengths. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Zinc oxide (ZnO) thin films were grown on the beta-Ga2O3 (100) substrate by pulsed laser deposition (PLD). X-ray diffraction (XRD) indicated that the ZnO films are c-axis oriented. The optical and electrical properties of the films were investigated. The room temperature Photoluminescence (PL) spectrum showed a near band emission at 3.28 eV with two deep level emissions. Optical absorption indicated a visible exciton absorption at room temperature. The as-grown films had good electrical properties with the resistivities as low as 0.02 Omega cm at room temperature. Thus, beta-Ga2O3 (100) substrate is shown to be a suitable substrate for fabricating ZnO film. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Beta gallium oxide (beta-Ga2O3) single crystals were grown by the floating zone technique. The absorption spectra and the luminescence of the crystals were measured. The absorption spectra showed an intrinsic short cutoff edge around 260 nm with two shoulders at 270 and 300 nm. Not only the characteristic UV (395 nm), blue (471 nm) and green (559 nm) lights, but also the red (692 nm) light can be seen in the emission spectra. The deep UV light was attributed to the existing of quantum wells above the valence band and the red light was owed to the electron-hole recombination via the vicinity donors and acceptors. (c) 2006 Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Gd2SiO5 (GSO) single crystal codoped with Yb3+ and Er3+ (Abbr. as Er:Yb:GSO) was successfully grown by the Czochralski (CZ) method for the first time and the spectral characteristics were investigated. The absorption and fluorescence spectra were measured. The emission lifetime of the I-4(13/2)-Er-level was measured to be 5.84ms and the emission cross-section at 1529nm was calculated to be 1.03 x 10(-20) cm(2). The results indicate that Er:Yb:GSO is a potential laser material at similar to 1. 55 mu m wavelength region. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

For the first time, a high optical quality 10 at.% Yb3+-doped gadolinium oxyorthosilicate laser crystal Gd2SiO5 (GSO) was grown by the Czochralski (Cz) method. The segregation coefficient of Yb3+ was studied by the inductively coupled plasma atomic emission spectrometer (ICP-AES) method. The crystal structure has monoclinic symmetry with space group P2(1)/c; this was determined by means of an x-ray diffraction analysis. The absorption spectra, fluorescence spectra and fluorescence decay curves of Yb3+ ions in a GSO crystal at room temperature were also studied. Then, the spectroscopic parameters of Yb:GSO were calculated. The advantages of the Yb:GSO crystal include high crystal quality, quasi-four-level laser operating scheme, high absorption cross-sections and particularly broad emission bandwidth (similar to 72 nm). The results indicated that the Yb:GSO crystal seemed to be a very promising laser gain medium in diode-pumped femtosecond laser and tunable solid state laser applications when LD pumped at 940 and 980 nm.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Transparent gamma-LiAlO2 single crystal has been grown by Temperature Gradient technique. The surface of the wafer annealed in O-2-atmosphere at 1100 degrees C for 70 h became opaque and Li-poor phase (LiAl5O8); while, that annealed in Li-rich atmosphere kept transparent and smooth. The full-width at half maximum value dropped to 30 arcsecs when the wafer was annealed in Li-rich atmosphere. That annealed in O-2-atmosphere increased to 78 arcsec. Compared with absorption spectra, we can conclude that the 196 nm absorption peak was caused by Li vacancies and the 736 nm peak was caused by O vacancies.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Cerium-doped lutetium pyrosilicate crystal, Ce:Lu2Si2O7 (Ce:LPS), was grown by the Czochralski method. The segregation coefficient of Ce3+ ion was studied by the ICP-AES method. X-ray diffraction analysis showed that the structure of Ce:LPS crystal was monoclinic symmetry with space group of C2/m. Perfect cleavage planes (110) and imperfect cleavage planes (001) were observed by optical microscope. The reasons why it is difficult to grow crack-free crystals were studied. After optimized growth parameters, a Ce:LPS crystal with dimension of Phi 25 x 30 mm was grown, which is colorless, high optical quality, cracking-free and no inclusions. The transmittance of Ce:LPS crystal from 380 to 800 nm is over 82% and there is no observable absorption. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A large and transparent Yb:FAP crystal with dimensions up to circle divide 30 mm x 85 mm has been grown by the Czochralski method. The preparation of the raw material has been investigated. X-ray power diffraction studies of Yb:FAP crystal confirm that the as-grown crystal is isostructural with the FAP crystal. The crystalline quality has been studied using X-ray rocking curve analysis. The segregation coefficient of Yb3+ in the Yb:FAP crystal has been also determined. Linear thermal expansion coefficients in [001] and [100] directions have been measured in the 30-800 degrees C temperature range. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

For the first time, a high optical quality Yb3+-doped lutetium pyrosilicate laser crystal Lu2Si2O7 (LPS) was grown by the Czochralski (Cz) method. The segregation coefficient of ytterbium ion in Yb:LPS crystal detected by the inductively coupled plasma atomic emission spectrometer (TCP-AES) method is equal to 0.847. X-ray powder diffraction result confirms the C2/m phase monoclinic space group of the grown crystal and the peaks corresponding to different phases were indexed. The absorption and fluorescence spectra, as well as fluorescence decay lifetime of Yb3+ ion in LPS have been investigated. The absorption and fluorescence cross-sections of the transitions F-2(7/2) <-> F-2(5/2) of Yb3+ ion in LPS crystal have been determined. The advantages of the Yb:LPS crystal including high crystal quality, quasi-four-level laser operating scheme, high absorption cross-sections (1.33 x 10(-2) cm(2)) and particularly broad emission bandwidth (similar to 62 nm) indicated that the Yb:LPS crystal seemed to be a promising candidate used as compact, efficient thin chip lasers when LD is pumped at 940 and 980 nm due to its low-symmetry monoclinic structure and single crystallographic site. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this paper, single crystal of ytterbium (Yb) doped Ca-5(PO4)(3)F (FAP) has been grown along the c-axis by using the Czochralski method. The segregation coefficients of Yb3+ in the Yb:FAP crystal has been determined by ICP-AES method. The absorption spectrum, fluorescence spectrum and fluorescence lifetime of the Yb:FAP crystal has been also measured at room temperature. In the absorption spectra, there are two absorption bands at 904 and 982 nm, respectively, which are suitable for InGaAs diode laser pumping. The absorption cross-section (sigma(abs)) is 5.117 x 10(-20) cm(2) with an FWHM of 4 nm at 982 nm. The emission cross-section is (sigma(em)) 3.678 x 10(-20) cm(2) at 1042 nm. Favorable values of the absorption cross-section at about 982 nm are promising candidates for laser diode (LD) pumping. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

ZnO crystals with dimensions of 30 x 38 x 8 turn 3 have been grown by the hydrothermal method using a mixed solution of KOH, LiOH and H2O2. The growing rates for +c(0001) and -c(000 (1) over bar) were 0.17 and 0.09 mm/day, respectively. The crystal color was very light green for +c sector and dark brown for -c sector. For the +c sector, the resistivity at room temperature was 80 0 cm, the carrier concentration was about 10(4)/cm(3), and the mobility was about 100 cm(2)/Vs. The full-width at half-maximum (FWHM) of double axis X-ray rocking curve for the polished Zn face cut from +c sector was 45 arcsec. The photoluminescence (PL) spectrum and the absorption spectrum of +c part of the crystals at room temperature were also reported and discussed in this paper. (c) 2008 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

g-LiAlO2 single crystal is a promising substrate for GaN heteroepitaxy. In this paper, we present the growth of large-sized LiAlO2 crystal by modified Czochralski method. The crystal quality was characterized by high-resolution X-ray diffraction and chemical etching. The results show that the as-grown crystal has perfect quality with the full width at half maximum (FWHM) of 17.7-22.6 arcsec and etch pits density of (0.3-2.2) x 10(4) cm(-2) throughout the crystal boule. The bottom of the crystal boule shows the best quality. The optical transmission spectra from UV to IR exhibits that the crystal is transparent from 0.2 to 5.5 mu m and becomes completely absorbing around 6.7 mu m wavelength. The optical absorption edge in near UV region is about 191 nm.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

ZnO films were fabricated on LiGaO2 (0 0 1), (10 0) and (0 10) planes by RF magnetron sputtering. The structural, morphological and optical properties of as-grown ZnO films were investigated by X-ray diffraction (XRD), atomic force microscopy (AFM), Raman spectra and photoluminescence (PL) spectra. It is found that the orientation of ZnO films is strongly dependent on the substrate plane. [0 0 0 11, [1 (1) over bar 00] and [11 (2) over bar0] oriented ZnO films are deposited on LiGaO2 (001), (100) and (010), respectively. AFM shows the (0001) ZnO film consists of well-aligned regular hexagonal grains. Raman spectra reveal a tensile stress in the (0 0 0 1) ZnO film and a compressive stress in (110 0) and (112 0) ZnO films. PL spectra of all ZnO films exhibit only a near-band-edge UV emission peak. (C) 2008 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Er3+ -doped Gd2SiO5 (Er:GSO) single crystal with dimensions of circle divide 35 x 40 mm(3) has been grown by the Czochralski method. The absorption and fluorescence spectra of the Er:GSO crystal were measured at room temperature. The spectral parameters were calculated based on Judd-Ofelt theory, and the intensity parameters Omega(2), Omega(4) and Omega 6 are obtained to be 6.168 x 10(-20), 1.878 x 10(-20), and 1.255 x 10(-20) cm(2), respectively. The emission cross-section has been calculated by Fuechtbauer-Ladenbury formula. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The YAG crystal codoped with Yb3+ and Tm3+ has been grown by Czochralski (Cz) method. The crystal structure of the crystal has been determined by X-ray diffraction analysis. The absorption and emission spectra of Yb,Tm:YAG crystal at room temperature have also been studied. The emission cross-sections have been calculated by Fuechtbauer-Ladenburg formula and reciprocity method. (C) 2007 Elsevier B.V. All rights reserved.