Hydrothermal growth and characterization of ZnO crystals
Data(s) |
2008
|
---|---|
Resumo |
ZnO crystals with dimensions of 30 x 38 x 8 turn 3 have been grown by the hydrothermal method using a mixed solution of KOH, LiOH and H2O2. The growing rates for +c(0001) and -c(000 (1) over bar) were 0.17 and 0.09 mm/day, respectively. The crystal color was very light green for +c sector and dark brown for -c sector. For the +c sector, the resistivity at room temperature was 80 0 cm, the carrier concentration was about 10(4)/cm(3), and the mobility was about 100 cm(2)/Vs. The full-width at half-maximum (FWHM) of double axis X-ray rocking curve for the polished Zn face cut from +c sector was 45 arcsec. The photoluminescence (PL) spectrum and the absorption spectrum of +c part of the crystals at room temperature were also reported and discussed in this paper. (c) 2008 Elsevier B.V. All rights reserved. |
Identificador | |
Idioma(s) |
英语 |
Fonte |
Zhang Chang-Long;Zhou Wei-Ning;Hang Ying;LZhi;Hou Hang-De;Zuo Yan-Bin;Qin Shi-Jie;Lu Fu-Hua;Gu Shu-Lin .,J. Cryst. Growth,2008,310(7~9):1819-1822 |
Palavras-Chave | #光学材料;晶体 #characterization #substrates #hydrothermal crystal growth #oxides #zinc compounds #semiconducting II-V materials |
Tipo |
期刊论文 |