Resumo:

Deposition of 1000 eV pure carbon ions onto Si(001) held at 800 degrees C led to direct nucleation of diamond crystallites, as proven by high-resolution transmission electron microscopy and electron energy loss spectroscopy. Molecular dynamic simulations show that diamond nucleation in the absence of hydrogen can occur by precipitation of diamond clusters in a dense amorphous carbon matrix generated by subplantation. Once the diamond clusters are formed, they can grow by thermal annealing consuming carbon atoms from the amorphous matrix. The results are applicable to other materials as well.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

ZnO vertical well-aligned nanorods were grown on A1N/sapphire by using metal-organic chemical vapor deposition. We first observed the ZnO net-like structures under the nanorods. The different strain was determined in these two layers by using double crystal X-ray diffraction, Raman spectra, which revealed that the nanorods were relaxed and the net-like structures were strained. The optical properties of two layers were measured by using the cathodoluminescence and photo luminescence and the shift of UV peaks was observed. Moreover, the growth mechanism of the ZnO nanorods and the net-like structures is discussed. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The Raman spectra of GaP nanorods grown in carbon nanotube templates have been reported. The red shifts of the TO and LO modes were observed due to phonon confinement effect in GaP nanorods. The measured red shifts range from 2 to 10cm(-1) depending on the size of the measured nanorods. It has been found that the polarization properties, which cannot be well explained by the selection rules of single nanorod, result from the direction disorder of nanorods in the measured area. The more the disorder is, the weaker the directionality of polarization properties is. The decrease of the Raman frequency of the TO and LO mode of the nanorods with the increasing power of the exciting laser suggests that the heating effect of the nanorods is far stronger than the bulk material. In addition, the saturation and then decrease of the Raman intensity with the increasing laser power indicate the rapid increase of the defects in the nanorods exposed to a strong exciting laser.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

GaN nanorods with vertebra-like morphology were synthesized by nitriding Ga2O3/ZnO films at 1000 degrees C for 20min. Ga2O3 thin films and ZnO middle layers were pre-deposited in turn on Si(111) substrates by r.f. magnetron sputtering system. In the flowing ammonia ambient, ZnO was reducted to Zn and Zu sublimated at 1000 degrees C. Ga2O3 was reducted to Ga2O and Ga2O reacted with NH3 to synthesize GaN nanorods in the help of the sublimation of Zn. The structure and morphology of the nanorods were studied by X-ray diffraction (XRD) and scanning electron microscopy (SEM), The composition of GaN nanorods was studied by energy dispersive spectroscopy (EDS) and fourier transform infrared (FTIR) system.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Medium energy (5-25 keV) C-13(+) ion implantation into diamond (100) to a fluence ranging from 10(16) cm(-2) to 10(18) cm(-2) was performed for the study of diamond growth via the approach of ion beam implantation. The samples were characterized with Rutherford backscattering/channelling spectroscopy, Raman spectroscopy, X-ray photoemission spectroscopy and Auger electron spectroscopy. Extended defects are formed in the cascade collision volume during bombardment at high temperatures. Carbon incorporation indeed induces a volume growth but the diamond (100) samples receiving a fluence of 4 x 10(17) to 2 x 10(18) at. cm(-2) (with a dose rate of 5 x 10(15) at. cm(-2) s(-1) at 5 to 25 keV and 800 degrees C) showed no He-ion channelling. Common to these samples is that the top surface layer of a few nanometers has a substantial amount of graphite which can be removed by chemical etching. The rest of the grown layer is polycrystalline diamond with a very high density of extended defects.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Well-defined 3D Fe3S4 flower-like microspheres were synthesized via a simple biomolecule-assisted hydrothermal process for the first time. On the basis of a series of contrast experiments, the probable growth mechanism and fabrication process of the products were proposed. The electrical conductivity property of the as-synthesized Fe3S4 sample exhibited a rectifying characteristic when a forward bias was applied for the bottom-contacted device. The magnetic properties of the products were studied as well and the results demonstrated that the products presented ferromagnetic properties related to the corresponding microstructure. In addition, we first verified that the Fe3S4 flower-like microspheres could store hydrogen electrochemically, and a discharge capacity of 214 mA h g(-1) was measured without any activation under normal atmospheric conditions at room temperature.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

For their biocompatibility and potential bionanoelectronic applications, integration of carbon nanotubes (CNTs) with biomolecules such as redox enzyme is highly anticipated. Therein, CNTs are expected to act not only as an electron transfer promoter, but also as immobilizing substrate for biomolecules. In this report, a novel method for immobilization of biomolecules on CNTs was proposed based on ionic interaction, which is of universality and widespread use in biological system. As illustrated, glucose oxidase (GOD) and single-walled carbon nanotubes (SWNTs) were integrated into a unitary bionanocomposite by means of ionic liquid-like unit on functionalized SWNTs. The resulted bionanocomposite illustrated better redox response of immobilized GOD in comparison of that prepared by weak physical absorption without ionic interaction. As a potential application of concept, the electrochemical detection of glucose was exemplified based on this novel bionanocomposite.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Stable lipid film was made by casting dipalmitoylphosphatidylcholine (DPPC) and rutin onto the surface of a glassy carbon (GC) electrode. The electrochemical behavior of rutin in the DPPC film was studied. The modified electrode coated with rutin gave quasi-reversible reduction-oxidation peak on cyclic voltammogram in the phosphate buffer (pH 7.4). The peak current did not decrease apparently after stored at 4 degreesC for 8 hours in refrigerator. This model of biological membrane was used to investigate the oxidation of dihydronicotinamide adenine dinucleotide (NADH) by rutin. Rutin in the film acts as a mediator. The modified electrode shows a great enhancement and the anodic peak potential was reduced by about 220 mV in the oxidation of 5 X 10(-3) mol L-1 NADN compared with that obtained at a bare glassy carbon electrode. (C) 2000 Elsevier Science S.A. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

It has been reported recently that single carbon nanotubes were attached to AFM tips to act as nanotweezers. In order to investigate its stability, a vertical single-walled carbon nanotube (SWCNT) under its own weight is studied in this paper. The lower end of the carbon nanotube is clamped. Firstly the governing dimensionless numbers are derived by dimensional analysis. Then the theoretical analysis based on an elastic column model is carried out. Two ratios, I.e., the ratio of half wall thickness to radius (t=R) and the ratio of gravity to elastic resilience ($\rho$gR=E), and their influences on the ratio of critical length to radius are discussed. It is found that the relationship between the critical ratio of altitude to radius and ratio of half thickness to radius is approximately linear. As the dimensionless number $\rho$gR=E increases, the compressive force per unit length (weight) becomes larger, thus critical ratio of altitude to radius must become smaller to maintain stability. At last the critical length of SWCNT is calculated. The results of this paper will be helpful for the stability design of nanotweezers-like nanostructures.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

We report the synthesis and characterization of Zn-doped InN nanorods by metal-organic chemical vapor deposition. Electron microscopy images show that the InN nanorods are single-crystalline structures and vertically well-aligned. Energy-dispersive X-ray spectroscopy analyses suggest that Zn ions are distributed nonhomogenously in InN nanorods. Simulations based on diffusion model show that the doping concentration along the radial direction of InN nanorod is bowl-like from the exterior to the interior, the doping concentration decreases, and Such dopant distribution result in a bimodal EDXS spectrum of Zn across the nanorod. The study of the mechanism of doping effect is useful for the design of InN-based nanometer devices. Also, high-quality Zn-doped InN nanorods will be very attractive as building blocks for nano-optoelectronic devices.'

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Well-aligned Zn1-xMgxO nanorods and film with Mg-content x from 0 to 0.051 have been successfully synthesized by metal organic chemical vapor deposition (MOCVD) without any catalysts. The characterization results showed that the diameters and lengths of the nanorods were in the range of 20-80 nm and 330-360 nm, which possessed wurtzite structure with a c-axis growth direction. As the increase of Mg precursor flows into the growth chamber, the morphology of Zn1-xMgxO evolves from nanorods to a film with scale-like surface and the height of the nanorods and the film was almost identical, it is suggested that the growth rate along the c-axis was hardly changed while the growth of six equivalent facets of the type {1 0 (1) over bar 0} of the Zn1-xMgxO has been improved. Photoluminescence and Raman spectra show that the products have a good crystal quality with few oxygen vacancies. With the Mg incorporation, multiple-phonon scattering become weak and broad, and the intensities of all observed vibrational modes decrease. And the ultraviolet near-band-edge emission shows a clear blueshift (x=0.051, as much as 90 meV) and slightly broadening compared with that of pure ZnO nanorods. (C) 2008 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The Hamiltonian in the framework of eight-band effective-mass approximation of the zinc-blende nanowires and nanorods in the presence of external homogeneous magnetic field is given in the cylindrical coordinate. The electronic structure, optical properties, magnetic energy levels, and g factors of the nanowires and nanorods are calculated. It is found that the electron states consist of many hole-state components, due to the coupling of the conduction band and valence band. For the normal bands which are monotone functions of |k(z)|, long nanorods can be modeled by the nanowires, the energy levels of the nanorods approximately equal the values of the energy band E(k(z)) of the nanowires with the same radius at a special k(z), where k(z) is the wave vector in the wire direction. Due to the coupling of the states, some of the hole energy bands of the nanowires have their highest points at k(z)=0. Especially, the highest hole state of the InSb nanowires is not at the k(z)=0 point. It is an indirect band gap. For these abnormal bands, nanorods can not be modeled by the nanowires. The energy levels of the nanorods show an interesting plait-like pattern. The linear polarization factor is zero, when the aspect ratio L/2R is smaller than 1, and increases as the length increases. The g(z) and g(x) factors as functions of the k(z), radius R and length L are calculated for the wires and rods, respectively. For the wires, the g(z) of the electron ground state increases, and the g(z) of the hole ground state decreases first, then increases with the k(z) increasing. For the rods, the g(z) and g(x) of the electron ground state decrease as the R or the L increases. The g(x) of the hole ground state decreases, the g(z) of the hole ground state increases with the L increasing. The variation of the g(z) of the wires with the k(z) is in agreement with the variation of the g(z) of the rods with the L.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Nanocrystalline diamond films were grown by a two-step process on Si(1 0 0) substrate, which was first pretreated by pure carbon ions bombardment. The bombarded Si substrate was then transformed into a hot-filament chemical vapor deposition (HFCVD) system for further growth. Using the usual CH4/H-3 feed gas ratio for micro crystalline diamond growth, nanodiamond crystallites were obtained. The diamond nucleation density is comparable to that obtained by biasing the substrate. The uniformly distributed lattice damage is proposed to be responsible for the formation of the nanodiamond. (C) 2002 Elsevier Science B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Si1-xCx alloys of carbon (C) concentration between 0.6%-1.0% were grown in Si by ion implantation and high temperature annealing. The formation of Si1-xCx alloys under different ion doses and their stability during annealing were studied. If the implanted dose was less than that for amorphizing Si crystals, the implanted C atoms would like to combine with defects produced during implantation and it was difficult to form Si1-xCx alloys after being annealed at 850 degreesC. With the increment of implanted C ion doses, the lattice damage increased and it was easier to form Si1-xCx alloys. But the lattice strain would become saturate and only part of implanted carbon atoms would occupy the substitutional positions to form Si1-xCx alloys as the implanted carbon dose increased to a certain degree. Once Si1-xCx alloys were formed, they were stable at 950 degreesC, but part of their strain would release as the annealing temperature increased to 1 000 degreesC. Stability of the alloys became worse with the increment of carbon concentration in the alloys.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

It is believed that during the initial stage of diamond film growth by chemical-vapor deposition (CVD), ion bombardment is the main mechanism in the bias-enhanced-nucleation (BEN) process. To verify such a statement, experiments by using mass-separated ion-beam deposition were carried out, in which a pure carbon ion beam, with precisely defined low energy, was selected for investigating the ion-bombardment effect on a Si substrate. The results are similar to those of the BEN process, which supports the ion-bombardment-enhanced-nucleation mechanism. The formation of sp(3) bonding is based on the presumption that the time of stress generation is much shorter than the duration of the relaxation process. The ion-bombarded Si is expected to enhance the CVD diamond nucleation density because the film contains amorphous carbon embedded with nanocrystalline diamond and defective graphite. (C) 2001 American Institute of Physics.