272 resultados para P-TYPE GAN
Resumo:
The optical, electrical and photoelectric properties of rare earth monophosphides (LnP, Ln = La, Nd, Sm, Y, Dy and Yb) have been studied in thin films. The films exhibit semiconducting behaviour with energy gaps of 1.0-1.46 eV and n-type electrical conduction. Their resistivities are 10(-2) OMEGA-cm with corresponding Hall mobilities of 8.5-400 cm2 V-1 s-1. The films are deposited on a p-type silicon substrate in vacuum. Voltage-current characteristic measurements show that a p-n junction has been formed between LnP and silicon. Spectral sensitivity and a photovoltaic effect have been observed in LnP-Si junctions. They may be useful photoelectric materials.
Resumo:
The catalytic performances of Mn-based catalysts have been investigated for the oxidative dehydrogenation of both ethane (ODE) and propane (ODP). The results show that a LiCl/MnOx/PC (Portland cement) catalyst has an excellent catalytic performance for oxidative dehydrogenation of both ethane and propane to ethylene and propylene, more than 60% alkanes conversion and more than 80% olefins selectivity could be achieved at 650 degrees C. In addition, the results indicate that Mn-based catalysts belong to p-type semiconductors, the electrical conductivity of which is the main factor in influencing the olefins selectivity. Lithium, chlorine and PC in the LiCl/MnOx/PC catalyst are all necessary components to keep the excellent catalytic performance at a low temperature.
Resumo:
To search for compounds with superior anti-human immunodeficiency virus type 1 (HIV-1) activity, ten 5,5'-(p-phenylenebisazo)-8-hydroxyquinoline sulfonates (4a-j) were synthesized and preliminarily evaluated as HIV-1 inhibitors in vitro for the first time. Some compounds demonstrated anti-HIV-1 activity, especially 5,5'-(p-phenylenebisazo)-8-hydroxyquinoline p-ethylbenzenesulfonate (4g) and 5,5'-(p-phenylenebisazo)-8-hydroxyquinoline p-chlorobenzenesulfonate (41) showed the more potent anti-HIV-1 activity with 50% effective concentration (EC50) values of 2.59 and 4.01 mu g/ml, and therapeutic index (TI) values of 31.77 and 24.51, respectively.
Resumo:
Submitted by zhangdi (zhangdi@red.semi.ac.cn) on 2009-04-13T11:45:31Z
Resumo:
Submitted by zhangdi (zhangdi@red.semi.ac.cn) on 2009-06-04T08:36:34Z No. of bitstreams: 1 dspace.cfg: 33388 bytes, checksum: ac9630d3fdb36a155287a049e8b34eb7 (MD5)
Resumo:
p-GaN surfaces are nano-roughened by plasma etching to improve the optical performance of GaN-based light emitting diodes (LEDs). The nano-roughened GaN present a relaxation of stress. The light extraction of the LEDs with nano-roughened surfaces is greatly improved when compared with that of the conventional LEDs without nano-roughening. PL-mapping intensities of the nano-roughened LED epi-wafers for different roughening times present two to ten orders of enhancement. The light output powers are also higher for the nano-roughened LED devices. This improvement is attributed to that nano-roughened surfaces can provide photons multiple chances to escape from the LED surfaces.
Effect of p-GaN layer thickness on the performance of p-i-n structure GaN ultraviolet photodetectors
Resumo:
We investigated the influence of thickness of p-GaN layer on the performance of p-i-n structure GaN ultraviolet photodetector. Through the simulation calculation, it was found that both the quantum efficiency and dark current of device decrease when employing thicker p-GaN layer, while both the quantum efficiency and dark current increase with decreasing thickness of p-GaN layer. It is suggested that the Schottky contact junction between the metal and p-GaN may be responsible for the incompatible effect. We has to make a suitable choice of the thickness of p-GaN in the device design according to the application requirement.
Resumo:
Visible-blind p-i-n avalanche photodiodes (APDs) were fabricated with high-quality GaN epilayers deposited on c-plane sapphire substrates by metal-organic chemical vapour deposition. Due to low dislocation density and a sophisticated device fabrication process, the dark current was as small as similar to 0.05 nA under reverse bias up to 20V for devices with a large diameter of 200 mu m, which was among the largest device area for GaN-based p-i-n APDs yet reported. When the reverse bias exceeded 38V the dark current increased sharply, exhibiting a bulk avalanche field-dominated stable breakdown without microplasma formation or sidewall breakdown. With ultraviolet illumination (360 nm) an avalanche multiplication gain of 57 was achieved.
Resumo:
The leakage mechanism of GaN-based p-i-n (p-AlGaN/i-GaN/n-GaN) UV detector has been investigated. With the same dislocation density, devices made from material with higher density of V-pits on surface produce larger leakage current. SEM images show that some V-pits penetrate into i-GaN layer, sometimes even the n-GaN layer. If p-ohmic contact metal (Ni/Au) deposits in the V-pits, Schottky contact would be formed at the interface of metal and i-GaN, or form ohmic contact at the interface of metal and n-GaN. The existence of parallel Schottky junction and ohmic contact resistance enhances the leakage current greatly.
Resumo:
In this paper frequency dependence of small-signal capacitance of p-i-n UV detectors, which were fabricated on GaN grown on sapphire substrate by metalorganic chemical vapor deposition, has been studied. The Schibli-Milnes model was used to analyze the capacitance-frequency characteristics. According to high frequency C-V measurements, the deep level mean concentration is about 2.98 x 10(20) cm(-3). The deep level is caused by the un-ionised Mg dopant. The calculated Mg activation energy is 260 meV and the hole thermal capture cross section of the deep level is about 2.73 x 10(-22) cm(2). The applicability of the Schibli-Milnes model is also discussed when the concentration of deep levels exceeds that of the heavily doped n-side. It is concluded that the analytic expression of the Schibli-Milnes model can still be used to describe the capacitance-frequency characteristics of GaN p-i-n UV detectors in good agreement with experiment. (c) 2005 Elsevier Ltd. All rights reserved.
Resumo:
Thick GaN films with high quality have been grown on (0001) sapphire substrate in a home-made vertical HVPE reactor. Micron-size hexagonal pits with inverted pyramid shape appear on the film surface, which have six triangular {10-11} facets. These I {10-11} facets show strong luminescence emission and are characteristic of doped n-type materials. Broad red emission is suppressed in {10-11} facets and is only found at the flat region out of the pit, which is related with the decreasing defects on {10-11} facets. Low CL emission intensity is observed at the apex of V-shape pits due to the enhanced nonradiative recombination. Raman spectra show that there are higher carrier concentration and low strain in the pit in comparison to the flat region out of the pit. The strain relaxation may be the main mechanism of the V-shape pits formation on the GaN film surface. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Properties of the Ag/Ni/p-GaN structure at different temperatures are studied by Auger electron spectroscopy, scanning electron microscopy and high resolution x-ray diffraction. The effect of Ag in ohmic contact on the crystalline quality is investigated and the optimized value of annealing temperature is reported. The lowest specific contact resistance of 2.5 x 10(-4) Omega cm(2) is obtained at annealing temperature of 550 degrees C.
Resumo:
AlGaN/GaN npn heterojunction bipolar transistor structures were grown by low-pressure MOCVD. Secondary ion mass spectroscopy (SIMS) measurements were carried out to study the Mg memory effect and redistribution in the emitter-base junction. The results indicated that there is a Mg-rich film formed in the ongrowing layer after the Cp2Mg source is switched off. The Mg-rich film can be confined in the base section by switching off the Cp2Mg source for appropriate time before the end of base growth. Low temperature growth of the undoped GaN spacer suppresses the Mg redistribution from Mg rich film. The delay rate of the Mg profile in sample C with spacer growing in low temperature is about 56 nm/decade, which becomes sharper than 80 nm/decade of the samples A and B without low temperature spacer. (C) 2005 Elsevier Ltd. All rights reserved.
Resumo:
n-ZnO/p-GaN heterojunction light-emitting diodes with and without a sandwiched AlN layer were fabricated. The electroluminescence (EL) spectrum acquired from the n-ZnO/p-GaN displays broad emission at 650 nm originating from ZnO and weak emission at 440 nm from GaN, whereas the n-ZnO/AlN/p-GaN exhibits strong violet emission at 405 nm from ZnO without GaN emission. The EL intensity is greatly enhanced by inserting a thin AlN intermediate layer and it can be attributed to the suppressed formation of the GaOx interfacial layer and confinement effect rendered by the AlN potential barrier layer.