980nm InGaAs/InGaAsP/AlGaAs strained quantum well lasers,vitta novel large optical cavity and asymmetrical claddings was fabricated bg MOCVD. Very high differential quantum efficiency elf 90% (1.15W/A) and low vertical divergence angle of 24 degrees at long cavity length were obtained for 100 mu m stripe lasers. The differential quantum efficiency is up to 94% (1.20) at cavity length of 500 mu m.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We investigate the nanoscale periodic corrugation (NPC) structures on the dynamic fracture surface of a typical tough bulk metallic glass, submitted to high-velocity plate impact and scanned by atomic force microscopy (AFM). The detrended fluctuation analysis (DFA) of the recorded AFM profiles reveals that the valley landscapes of the NPC are nearly memoryless, characterized by Hurst parameter of 0.52 and exhibiting a self-similar fractal character with the dimension of about 1.48. Our findings confirm the existence of the “quasi-cleavage” fracture underpinned by tension transformation zones (TTZs) in metallic glasses.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A theoretical model about the size-dependent interface energy between two thin films with different materials is developed by considering the chemical bonding contribution based on the thermodynamic expressions and the structure strain contribution based on the mechanical characteristics. The interface energy decreases with reducing thickness of thin films, and is determined by such available thermodynamic and mechanical parameters as the melting entropy, the melting enthalpy, the shear modulus of two materials, etc. The predicted interface energies of some metal/MgO and metal/Al2O3 interfaces based on the model are consistent with the results based on the molecular mechanics calculation. Furthermore, the interface fracture properties of Ag/MgO and Ni/Al2O3 based on the atomistic simulation are further compared with each other. The fracture strength and the toughness of the interface with the smaller structure interface energy are both found to be lower. The intrinsic relations among the interface energy, the interface strength, and the fracture toughness are discussed by introducing the related interface potential and the interface stress. The microscopic interface fracture toughness is found to equal the structure interface energy in nanoscale, and the microscopic fracture strength is proportional to the fracture toughness. (C) 2010 American Institute of Physics. [doi:10.1063/1.3501090]

Relevância:

20.00% 20.00%

Publicador:

Resumo:

For the cube-corner indenter, an approximate linear relationship between the ratio of hardness (H) to reduced modulus (E-r) and the ratio of unloading work (W-u) to total loading work (W-t) is confirmed by finite-element calculations and by experiments. Based on this relationship a convenient method to determine the fracture toughness (K-IC) of brittle materials, especially for those at small scale, using cube-corner indentations is proposed. Finally, the method is calibrated by indentation experiments on a set of brittle materials. (C) 2009 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An analytical model about size-dependent interface energy of metal/ceramic interfaces in nanoscale is developed by introducing both the chemical energy and the structure stain energy contributions. The dependence of interface energy on the interface thickness is determined by the melting enthalpy, the molar volume, and the shear modulus of two materials composing the interfaces, etc. The analytic prediction of the interface energy and the atomic scale simulation of the interface fracture strength are compared with each other for Ag/MgO and Ni/Al2O3 interfaces, the fracture strength of the interface with the lower chemical interface energy is found to be larger. The potential of Ag/MgO interface related to the interface energy is calculated, and the interface stress and the interface fracture strength are estimated further. The effect of the interface energy on the interface strength and the behind mechanism are discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Dynamic planar compressive experiments on a typical tough Zr-BMG (Bulk Metallic Glass) were carried out under impact velocity of 500-600 m/sec and strain rate of 10(6)/s. The fracture surface of samples exhibits different fracture patterns at different parts of the sample. At a corner close to the front loading boundary, fracture patterns from the free edge toward the centre changed from equiaxial veins in microscale to periodic corrugations in nanoscale; in the middle of the sample, the fracture surface contains glazed zones laid out orderly along the same boundary. FEM simulation was performed to investigate the stress distributions in the impacted sample under a short duration impact loading. It has revealed that the fracture patterns changing from the free edge toward the centre were resulted from the fracture modes' changing from the tensile dominant fracture to the shear dominant fracture. Whereas at the middle part of the sample, fracture initiated from several parallel shear bands propagating close to the same boundary is due to a large strain or much higher shear stress in this area.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Controlled vertical drying deposition method was used to make high-quality single crystal close-packed colloidal films formed of different radii polystyrene latex spheres on glass substrates coming from a low concentration water suspension (0.1% volume fraction). Regardless of the spheres radii the film thickness was about 6.3 microns. However, cracks destroyed the crystalline film structure during the colloidal film growth. The effect of particle radius (85-215 nm range) on film cracking was systematically studied using in situ optical fracture monitoring. Primary parallel cracks run along the vertical growth direction, later followed by secondary branched cracks in-between the primary cracks due to residual water evaporation. Quantitative theoretical relationship between the cracks spacing and particles radius was derived and shows good agreement with experimental observations. Normalized cracks spacing is related to a reciprocal ratio of the dimensionless particle radius.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The hydraulic conductivity function of fractures is a key scientific question to describe and reveal the process and the role of water seepage reasonably. In this paper, the generation technology of random fracture network and the latest numerical computation method for equivalent permeability tensor of fracture network are applied to analyze the landslide located at Wangjiayuanzi in Wanzhou District of Chongqing by simulating the changes of the seepage field caused by the running of the Three Gorges Reservoir. The influences of the fracture seepage on the seepage field and stability of the landslide were discussed with emphasis. The results show that the fractures existing in the soil increase the permeability coefficient of the landslide body and reduce the delay time of the underground water level in the landslide which fluctuates relative to the water level of reservoir,that causes the safe coefficient of the slope changes more gently than that of the same slope without fractures. It means, if only water level fluctuating condition is concerned, the fractures existing in the soil plays a positive role to the stability of slopes.