In this paper, GdFeCo/DyFeCo exchange-coupled double-layer films used for center aperture type magnetically induced super resolution were investigated through experiments and theoretical calculation. The samples were prepared by magnetron sputtering method. The polar Kerr effect was measured to prove the spin reorientation of the readout layer. Theoretical study of magnetization profiles was performed on the basis of the mean-field theory and the continuum model. The theoretical results showed that the magnetization orientation of the readout layer changed gradually from in-plane to out-of-plane with the rise of the temperature. Theoretical analysis explained the experimental results successfully. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Weak epitaxy growth (WEG) can afford high-mobility thin films of disk-like organic semiconductor of which mobility is up to the level of the corresponding single crystals. We investigated the WEG behavior and mechanism of planar phthalocyanine in the model system of metal-free phthalocyanine (H2Pc) grown on p-sexiphenyl (p-6P) ultrathin films (monolayers and double layers). Highly oriented H2Pc films with molecules standing up exhibited two kinds of different in-plane orientations, i.e., three sets of in-plane orientations and only one set of in-plane orientation, on p-6P monolayer and double-layer films, respectively.
Resumo:
Copper phthalocyanine doped polymethacrylate Langmuir-Blodgett films were transferred to align a nematic liquid crystal 5CB, It is found that the pre-tilt angle of the liquid crystal can be controlled with the variation of the doped copper phthalocyanine molecular ratio and is correlated with the dichroic ratio of the aligning layer. The polarity of the aligning layer is regarded as the most likely underlying factor that causes the different LC alignment configurations. (C) 1997 Elsevier Science B.V.
Resumo:
The effects of in situ annealing treatment in the initial growth stage and In-doping during growth of the GaN on the material properties were investigated. GaN was grown by LP-MOVPE. In situ annealing reduced the full-width at half-maximum (FWHM) of X-ray rocking curves and reduced etch pit density of GaN films. It improved the optical properties of the epilayer. Undoped and In-doped GaN films of initial growth stage were investigated. It was found that morphology and optical properties were improved in In-doped samples. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
The effects of in situ annealing treatment in the initial growth stage and In-doping during growth of the GaN on the material properties were investigated. GaN was grown by LP-MOVPE. In situ annealing reduced the full-width at half-maximum (FWHM) of X-ray rocking curves and reduced etch pit density of GaN films. It improved the optical properties of the epilayer. Undoped and In-doped GaN films of initial growth stage were investigated. It was found that morphology and optical properties were improved in In-doped samples. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
The electrochemical and electrogenerated chemiluminescence of Ru(bpy)(3)(2+) immobilized in {clay/Ru(bpy)(3)(2+)}(n) multilayer films by layer-by-layer assembly were investigated. The stable multilayer films of clay and Ru(bpy)(3)(2+) were assembled by alternate adsorption of negatively charged clay platelets and positively charged Ru(bpy)(3)(2+) from their aqueous dispersions. UV-vis spectroscopy, quartz crystal microbalance (QCM), cyclic voltammetry, and electrogenerated chemiluminescence (ECL) were used to monitor the immobilization of Ru( bpy)(3)(2+) and the regular growth of the {clay/Ru( bpy)(3)(2+)}(n) multilayer films. The multilayer films modified electrode was used for the ECL detection of tripropylamine ( TPA) and oxalate. The proposed novel immobilized method exhibited good stability, reproducibility and high sensitivity for the determination of TPA and oxalate, which mainly resulted from the contributing of clay nanoparticles with appreciable surface area, special structural features and unusual intercalation properties.
Resumo:
Ce3+ and/or Tb3+-doped LaPO4 nanocrystalline thin films and their patterning were fabricated by a sol-gel process combined with soft lithography on silicon and quartz glass substrates. The results of XRD indicated that the films began to crystallize at 700 degreesC. The 1000 degreesC annealed single layer films are transparent by eyes, uniform and crack-free with a thickness of about 200 nm and an average grain size of 100 nm. Patterned thin film with different band widths (5-50 mum) were obtained by micro-molding in capillaries technique. The luminescence and energy transfer properties of Ce3+ and Tb3+ were studied in LaPO4 films.
Resumo:
Based on the Fresnel-Kirchkoff diffraction theory, we build up a Gaussian diffraction model of metal-oxide-type super-resolution near field structure (super-RENS), which can describe far field optical properties. The spectral contrast induced by refractive index and the structural changes in AgOx, PtOx and PdOx thin films, which are the key functional layers in super-RENS, are studied by using this model. Comparison results indicate that the spectral contrast intensively on laser-induced distribution and change of the refractive index in the metal-oxide films. The readout mechanism of the metal-oxide-type super-RENS optical disc is further clarified. This Gaussian diffraction model can be used as a simple and effective method for choosing proper active materials in super-RENS.
Resumo:
用离子束溅射法制备了锆单层薄膜.用设计新型夹具和预置种子方法,对薄膜中结瘤微缺陷的生长过程进行了研究.在高分辨率光学显微镜和扫描电子显微镜下观察发现,结瘤在其生长初期呈现出分形的特征.用分子动力学和薄膜生长的扩散限制聚集模型,薄膜中结瘤微缺陷成核时的分形现象得到了很好的解释.
Resumo:
用电子束热蒸发方法在熔融石英基底上沉积了Al2O3和MgF2两种材料的单层膜,研究了两种材料的光学特性,采用光度法计算并给出了薄膜材料在180~230nm的折射率n/和消光系数k的色散曲线。以两种材料作为高低折射率材料组合,采用1/4波长规整膜系设计并镀制了193nm的高反射膜,反射膜在退火后的反射率在193nm达到96%以上。结果表明在一定工艺条件下Al2O3和MgF2两种材料能够在193nm获得较好的光学性能,适用于高反射膜的制备。
Resumo:
用电子束蒸发制备了用于掺钛蓝宝石啁啾脉冲放大激光系统的TiO2/HfO2/SiO2高反膜,其带宽约为176nm(R>98%, λ0=800nm),激光损伤阈值(LIDT)为2.4 J/cm2。通过TiO2和HfO2单层膜的透过光谱计算了这两种材料的折射率和消光系数。高反膜的性能主要由高折射率材料决定:折射率越高,反射带越宽;消光系数越小,薄膜吸收越小,LIDT越高。最后,讨论了高反膜的激光损伤机制。
Resumo:
Three minutes' growth was carried out to investigate the indium-doping effect on initially grown GaN. Indium-doped and undoped samples were grown by low-pressure metalorganic vapor phase epitaxy. Atomic force microscope observation revealed that In-doping modified the morphology of the nuclei. Indium-doping also enhanced wetting between the buffer and nuclei layers, which was also supported by optical transmission. Photoluminescence suggested that indium-doping obviously enhanced band-edge related emission even in the nucleation stage. X-ray diffraction performed on samples grown for 20 minutes indicated improvement of the crystalline quality through indium-doping. The mechanism of the indium-doping effect was discussed.
Resumo:
用辉光放电质谱法和二次离子质谱仪测定了两种HfO2材料及它们相应的单层膜中的杂质含量,结果发现,无论是在体材料中还是在用电子束蒸发技术沉积的材料单层薄膜中,ZrO2都是这两种HfO2材料中最主要的杂质。而且,这两种HfO2材料中Zr含量的差别远远大于Ti、Fe含量的差别,这说明Zr含量的差别正是引起两种HfO2膜层光学性能差别的原因。用这两种不同纯度的HfO2材料与同一纯度的SiO2材料组合,沉积形成266nm的紫外反射镜,实验结果表明这两种反射镜的反射率分别在99.85% 和 99.15%左右。这个结果与依据单层膜得出的光学常数所设计的结果符合的很好。
Resumo:
The growth of InAsxSb1-x films on (100) GaSb substrates by liquid-phase epitaxy (LPE) has been investigated and epitaxial InAs0.3Sb0.7 films with InAs0.9Sb0.09 buffer layers have been successfully obtained. The low X-ray rocking curve FHWM values of InAs0.3Sb0.7 layer shows the high quality of crystal-orientation structure. Hall measurements show that the highest electron mobility in the samples obtained is 2.9 x 10(4) cm(2) V-1 s(-1) and the carrier density is 2.78 x 10(16)cm(-3) at room temperature (RT). The In As0.3Sb0.7 films grown on (10 0) GaSb substrates exhibit excellent optical performance with a cut-off wavelength of 12 mu m. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
ZnO/MgF2/ZnO sandwich structure films were fabricated. The effects of a buffer layer on structure and optical properties of ZnO films were investigated by X-ray diffraction, photoluminescence, optical transmittance and absorption measurements. Measurement results showed that the buffer layer had the effects of improving the quality of ZnO films and releasing the residual stresses in the films. The near-band edge emissions of ZnO films deposited on the MgF2 buffer layer were significantly enhanced compared with those deposited on bare substrate due to the smaller lattice mismatch between MgF2 and ZnO than that between fused silica and ZnO. (c) 2006 Elsevier B.V. All rights reserved.