997 resultados para metallic post


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Introduction: The objective of the study was to evaluate the ability of large-volume cone-beam computed tomography (CBCT) to detect horizontal root fracture and to test the influence of a metallic post. Methods: Through the examination of 40 teeth by large-volume CBCT (20-cm height and 15-cm diameter cylinder) at 0.2-mm voxel resolution, 2 observers analyzed the samples for the presence and localization of horizontal root fracture. Results: The values of accuracy in the groups that had no metallic post ranged from 33%-68%, whereas for the samples with the metallic post, values showed a wide variation (38%-83%). Intraobserver agreement showed no statistically significant difference between the groups with/without metallic post; both ranged from very weak to weak (kappa, 0.09-0.369). Conclusions: The low accuracy and low intraobserver and interobserver agreement reflect the difficulty in performing an adequate diagnosis of horizontal root fractures through a large-volume CBCT by using a small voxel reconstruction. (J Endod 2012;38:856-859)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The theoretical method to design negative refractive index metamaterials by single negative permittivity metamaterials is presented. By designing the electric and magnetic response metamaterials separately, the complexity of the design work can be simplified a lot. For the magnetic response metamaterials, the metallic post structure is adopted. Varying the height of the post, the response wavelength can be adjusted linearly. For electric metamaterials, wire-mesh structure is adopted. The effective material parameters, including refractive index, impedance, permittivity and permeability are given. Such a structure has negative refractive index during a broad frequency band and easy to design.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

This study evaluated the fracture resistance of teeth submitted to internal bleaching and restored with different non-metallic post. Eighty mandibular incisors were endodontically treated and randomly divided in 10 groups (n = 8): G1- restored with composite resin (CR), G2- CR + fiber-reinforced composite post (FRC, Everstick post, Sticktech) cemented with resin cement self-etch adhesive (RCS, Panavia F 2.0, Kuraray), G3- CR + FRC + self-adhesive resin cement (SRC, Breeze, Pentral Clinical), G4- CR+ glass fiber post (GF, Exacto Post, Angelus) + RCS, G5- CR + GF + SRC. The G6 to G10 were bleached with hydrogen peroxide (HP) and restored with the same restorative procedures used for G1 to G5, respectively. After 7 days storage in artificial saliva, the specimens were submitted to the compressive strength test (N) at 0.5 mm/min cross-head speed and the failure pattern was identified as either reparable (failure showed until 2 mm below the cement-enamel junction) or irreparable (the failure showed <2 mm or more below the cement-enamel). Data were analyzed by ANOVA and Tukey test (α = 0.05). No significant difference (p < 0.05) was found among G1 to G10. The results suggest that intracoronal bleaching did not significantly weaken the teeth and the failure patterns were predominately reparable for all groups. The non-metallic posts in these teeth did not improve fracture resistance.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Aim To evaluate, using an experimental immature tooth model, the fracture resistance of bovine incisors submitted to different reinforcement treatments with mineral trioxide aggregate (MTA).Methodology An immature tooth model was created by sectioning the coronal and apical portions of 40 bovine incisors 8 mm above and 12 mm below the cementoenamel junction. The root canals were irrigated with 1.0% sodium hypochlorite. They were enlarged both coronally and apically using number 703 carbide burs (ISO: 500-104-168-007-021) and their internal diameter was standardized to 2.1 mm. The specimens were assigned to four groups (n = 10): GI-control (without filling); GII-apical MTA plug + filling with gutta-percha and endodontic sealer; GIII-filling with MTA; GIV-apical MTA plug + filling with MTA + metallic post (Reforpost I). A polyether impression material was used to simulate the periodontal ligament. The specimens were submitted to a compressive load at a crosshead speed of 0.5 mm min(-1) in a servo-hydraulic universal testing machine (MTS 810) applied at 45 degrees to the long axis of the tooth until failure. Data were submitted to statistical analysis by the Kruskal-Wallis test at 5% significance level.Results GIV presented the highest fracture resistance (32.7N) and differed significantly from the other groups (P < 0.05). No statistically difference was found between GII (16.6N) and GIII (23.4N) (P > 0.05). GIII had a significantly higher fracture resistance than GI (P < 0.05).Conclusions the use of MTA + metallic post as an intra-radicular reinforcement treatment increased the resistance to fracture of weakened bovine teeth in an experimental immature tooth model.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The photospheres of stars hosting planets have larger metallicity than stars lacking planets. This could be the result of a metallic star contamination produced by the bombarding of hydrogen-deficient solid bodies. In the present work we study the possibility of an earlier metal enrichment of the photospheres by means of impacting planetesimals during the first 20-30 Myr. Here we explore this contamination process by simulating the interactions of an inward migrating planet with a disc of planetesimal interior to its orbit. The results show the percentage of planetesimals that fall on the star. We identified the dependence of the planet's eccentricity (e(p)) and time-scale of migration (tau) on the rate of infalling planetesimals. For very fast migrations (tau= 10(2) and 10(3) yr) there is no capture in mean motion resonances, independently of the value of e(p). Then, due to the planet's migration the planetesimals suffer close approaches with the planet and more than 80 per cent of them are ejected from the system. For slow migrations (tau= 10(5)and 10(6) yr) the percentage of collisions with the planet decreases with the increase of the planet's eccentricity. For e(p) = 0 and 0.1 most of the planetesimals were captured in the 2:1 resonance and more than 65 per cent of them collided with the star. Whereas migration of a Jupiter mass planet to very short pericentric distances requires unrealistic high disc masses, these requirements are much smaller for smaller migrating planets. Our simulations for a slowly migrating 0.1 M-Jupiter planet, even demanding a possible primitive disc three times more massive than a primitive solar nebula, produces maximum [Fe/H] enrichments of the order of 0.18 dex. These calculations open possibilities to explain hot Jupiter exoplanet metallicities.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The purpose of this work is to study the dynamic behavior of a pedestrian bridge in Alicante, Spain. It is a very slender footbridge with vertical and horizontal vibration problems during the passage of pedestrians. Accelerations have been recorded by accelerometers installed at various locations of the bridge. Two scenarios, in free vibration (after the passage of a certain number of pedestrians on the bridge) and forced vibration produced by a fixed number of pedestrians walking on the bridge at a certain speed and frequency. In each test, the effect on the comfort of the pedestrians, the natural frequencies of vibration, the mode shapes and damping factors have been estimated. It has been found that the acceleration levels are much higher than the allowable by the Spanish standards and this should be considered in the restoration of the footbridge.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The deformation and fracture response of a bulk metallic glass (BMG) post-annealing above the glass transition temperature is examined. The toughness of the glass-matrix composite exhibits a sharp transition beyond a critical volume fraction of crystallization to values as low as that of brittle silicate glass. Instrumented indentation tests supplemented by impact tests were used to study this ductile to brittle transition exhibited by the partially crystallized samples. Indentation on the anneal-embrittled specimens shows lateral cracks in addition to cracks along the corners. The applicability of the Poisson's ratio-toughness correlation with respect to partially crystallized samples is also investigated.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Nanoindentation experiments were conducted on a Ni+ ion-irradiated Zr-based bulk metallic glass (BMG). The irradiation was carried out using 2.5, 5, 10 and 15 MeV ions and a flux of similar to 10(16) ions/cm(2). Post mortem imaging of the indents reveals a transition in the deformation mechanism of the irradiated regions from heterogeneous shear banding to homogeneous flow. Additionally, the load-displacement curves exhibit a transition from serrated to continuous flow with increasing severity of irradiation damage. The stress-strain response obtained from micro-pillar compression experiments complements the indentation response exhibiting a decrease in the flow stress and an `apparent' strain hardening at the lowest irradiation damage investigated, which is not observed in the as-cast alloy. (C) 2011 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The impact response of laminated composites consisting of alternate layers of AI ahoy foam and Al2O3 was studied experimentally in low and intermediate velocity regimes. Low velocity impacts (1.2-2.8 m s(-1)) were conducted using an instrumented falling weight apparatus and were compared with static indentation tests (0.2 x 10(-4) m s(-1)). Intermediate velocity impacts were carried out by means of both Hopkinson bar (60 m s(-1)) and gas gun (200 m s(-1)) tests, Post-impact damage was assessed using X-ray radiography and microscopy, It was found that there is good correlation between low velocity impact and quasi-static responses. In both cases, penetration of the layered targets resulted in the formation of a distinctive plug. Increasing impact velocity (intermediate velocity range) snitched the penetration mode from plugging to fragmentation, giving rise to an increase in the absorbed energy. In this range, impacts led to localisation of damage in the region under the projectile, Furthermore, a comparison has been made between the penetration response of foam laminates and dense metal laminates of equivalent areal density. Preliminary results suggest that the dense metal laminates are superseded by the foam laminates on an energy absorption basis.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Introduction : La force d’adhésion à l'interface métal-céramique avec les résines auto-polymérisantes destinées au collage indirect des boîtiers orthodontiques n'a pas été évaluée à ce jour et un protocole clinique basé sur la littérature scientifique est inexistant. Objectifs : 1) Comparer la force de cisaillement maximale entre des boîtiers métalliques et des surfaces en porcelaine préparées selon différentes méthodes; 2) Suggérer un protocole clinique efficace et prévisible. Matériel et méthodes : Quatre-vingt-dix disques en leucite (6 groupes; n = 15/groupe) ont été préparés selon 6 combinaisons de traitements de surface : mécaniques (+ / - fraisage pour créer les rugosités) et chimiques (acide fluorhydrique, apprêt, silane). Des bases en résine composite Transbond XT (3M Unitek, Monrovia, California) faites sur mesure ont été collées avec le système de résine adhésive auto-polymérisante Sondhi A + B Rapid Set (3M Unitek, Monrovia, California). Les échantillons ont été préservés (H2O/24hrs), thermocyclés (500 cycles) et testés en cisaillement (Instron, Norwood, Massachusetts). Des mesures d’Index d’adhésif résiduel (IAR) ont été compilées. Des tests ANOVAs ont été réalisés sur les rangs étant donné que les données suivaient une distribution anormale et ont été ajustés selon Tukey. Un Kruskall-Wallis, U-Mann Whitney par comparaison pairée et une analyse de Weibull ont aussi été réalisés. Résultats : Les médianes des groupes varient entre 17.0 MPa (- fraisage + acide fluorhydrique) à 26.7 MPa (- fraisage + acide fluorhydrique + silane). Le fraisage en surface ne semble pas affecter l’adhésion. La combinaison chimique (- fraisage + silane + apprêt) a démontré des forces de cisaillement significativement plus élevées que le traitement avec (- fraisage + acide fluorhydrique), p<0,05, tout en possédant des forces similaires au protocole typiquement suggéré à l’acide fluorhydrique suivi d’une application de silane, l’équivalence de (- fraisage + acide fluorhydrique + silane). Les mesures d’IAR sont significativement plus basses dans le groupe (- fraisage + acide fluorhydrique) en comparaison avec celles des 5 autres groupes, avec p<0,05. Malheureusement, ces 5 groupes ont des taux de fracture élévés de 80 à 100% suite à la décimentation des boîtiers. Conclusion : Toutes les combinaisons de traitement de surface testées offrent une force d’adhésion cliniquement suffisante pour accomplir les mouvements dentaires en orthodontie. Une application de silane suivie d’un apprêt est forte intéressante, car elle est simple à appliquer cliniquement tout en permettant une excellente adhésion. Il faut cependant avertir les patients qu’il y a un risque de fracture des restorations en céramique lorsque vient le moment d’enlever les broches. Si la priorité est de diminuer le risque d’endommager la porcelaine, un mordançage seul à l’acide hydrofluorique sera suffisant.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)