940 resultados para Ag addition


Relevância:

100.00% 100.00%

Publicador:

Resumo:

It is important that long superconducting tape must have desired strain tolerance (less reduction of Jc with applied strains) and stress tolerance (less reduction of JC in applied stresses) for its use as coils and magnets. Ag addition to the BPSCCO system has many advantages with its physical and chemical inertness to the system, reduces the processing temperature, and promotes the grain growth, grain alignment and connectivity. All these not only enhance the critical current density of the tapes but also improve the mechanical properties. But the published results show very much scattering on the type of Ag additive to be selected, method of addition and its optimum percentage. Also there are some negative reports in this regard. The present work has been undertaken to study the effect of silver addition in different forms (Ag powder, Ag2O, AgNO3) on the superconducting and mechanical properties of (Bi,Pb)-2223/Ag tapes and to find out a suitable form of Ag additive and its optimum percentage to have better superconducting and mechanical properties. Also it is the aim of the present work is to optimise the process parameters needed to prepare (Bi,Pb)-2223/Ag multifilamentary tapes of length ~ 12 m in solenoid and pancake coil forms with good critical current density and homogeneity of J C along the length of the tapes.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The effect of 4 mass% Ag addition on the thermal behavior of the Cu-9 mass% Al alloy was studied using differential scanning calorimetry (DSC), optical microscopy (OM), scanning electron microscopy (SEM), energy dispersive X-ray analysis (EDX) and X-ray diffractometry (XRD). The results showed that the presence of silver causes (Cu)-alpha+(alpha+gamma1)-->(Cu)-alpha+beta transformation to occur in two stages. In the first one, part of the produced beta phase combines with the precipitated Ag to give a silver-rich phase and in the second one the transformation is completed. The formation of this silver-rich phase seems to be enhanced at very low cooling rates.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Thermal analysis and compression tests at room temperature have been carried out for Cu-10 wt.% Al and Cu-10 wt.% Al-10 wt.% Ag alloys samples. The results indicate that the decomposition reaction of the (beta(1)) parent phase is decreased suppressed and a martensite stabilization effect can be induced by Ag addition. The Cu-Al-Ag alloy shows some degree of shape memory capacity. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this work the influence of Ag additions on the thermal behavior of the Cu-11 mass% Al alloy was studied using differential scanning calorimetry, in situ X-ray diffractometry and scanning electron microscopy. The results indicated that changes in the heating rate shift the peak attributed to alpha phase formation to higher temperatures, evidencing the diffusive character of this reaction. The activation energy value for the alpha phase formation reaction, obtained from a non-isotherm kinetic model, is close to that corresponding to Cu atoms self diffusion, thus confirming that this reaction is dominated by Cu atoms diffusion through the martensite matrix.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The effect of Ag addition on the phase transformations that occur in the Cu-10% Al alloy was studied using differential thermal analysis, scanning electron and optical microscopies and energy dispersive X-ray analysis. The results indicated that Ag addition is responsible for the separation of the reverse martensitic transformation in two stages, and for the refinement of the α-phase grains. The relative amount of the β1 martensitic phase, retained on slow cooling (above 2 K min-1 of cooling rate), and the relative fraction of phase α2 are increased. The solubility limit of Ag in the matrix is close to 6 mass% and at this concentration the maximum stability of the β-phase is reached. © 2005 Akadémiai Kiadó, Budapest.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The phase transitions that occur in the Cu-22.26 at.%Al-9.93 at.%Mn and Cu-22.49 at.%Al-10.01 at.%Mn-1.53 at.%Ag alloys after slow cooling were studied using differential scanning calorimetry at different heating rates, microhardness changes with temperature, magnetization changes with temperature, scanning electron microscopy and energy dispersion X-ray spectroscopy. The results indicated that the presence of Ag does not modify the transition sequence of Cu-Al-Mn alloy, introduces a new transition due to the (Ag-Cu)-rich precipitates dissolution at about 800 K, and changes the mechanism of DO 3 phase dissolution. This mechanistic change was analyzed and a sequence of phase transitions was proposed for the reaction. © 2013 Elsevier B.V.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

The influence of 4 wt.%Ag addition on the isothermal decomposition kinetics of the beta' phase in the Cu-9wt.%Al alloy was studied by microhardness measurements, optical and scanning electron microscopy (SEM), energy dispersive X-ray (EDX) analysis, and X-ray diffractometry. The results showed that the presence of Ag decreases the beta' --> (alpha + gamma(1)) decomposition reaction rate in the Cu-9%Al-4%Ag alloy, an effect that may be associated to the gamma(1) phase which catalyses the Ag precipitation, making it faster than the decomposition reaction, and thus, stabilizing the martensitic phase. (C) 2003 Elsevier B.V. All rights reserved.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

The reverse martensitic transformation in the Cu-10 wt%Al-6 wt%Ag alloy was studied by classical differential thermal analysis (IDTA), scanning electron microscopy (SEM), energy dispersive X-ray analysis (EDX) and X-ray diffractometry (XRD). The results indicated that the presence of Ag in the Cu-10%Al alloy is responsible for the separation of the competitive reactions that occur during the reverse martensitic transformation and is also associated to an increase in the disordering degree at high temperatures, when compared with alloys without Ag addition. (c) 2005 Springer Science + Business Media, Inc.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

In this work the effect of Ag concentration on the thermal behavior of the Cu-10 mass% Al and Cu-11 mass% Al alloys with additions of 4, 6, 8 and 10 mass% Ag was studied using differential scanning calorimetry (DSC), in situ X-ray diffractometry (XRD) and scanning electron microscopy (SEM). The results showed that for the Cu-10 mass% Al alloy Ag addition induce the beta'(1) phase formation and for the Cu-11 mass% Al alloy these additions increase the amount of martensite formed on quenching and decrease the stability range of this phase on heating.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The electrochemical response of chalcopyrite was studied using electrochemical noise analysis (ENA). The assay was carried out under constant aeration using 30 mL in two electrochemical cells containing iron-free mineral salts solution. These cells were initially monitored for 56 hours, After 72 hours, 7.25x 10(10) cells mL(-1) of A, ferrooxidans strain LR were added in both cells and monitored until 128 h. Subsequent to this period, 0.927 mmol L-1 of silver ions and 400 mmol L-1 of chloride ions were added each one separately. Both conditions were monitored until 168 hours. According to results obtained, it was observed that Cl- ions addition induced an accelerated corrosion process. However, there is a tendency of the system to reach the stationary state due to repassivation of the electrodic surface. In the other side, the Ag+ addition contributed for the maintenance of the oxidant atmosphere, in spite of controversial effect caused by considerable variations in the R-n values, resulting in a instability in the chalcopyrite reactivity.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The Bi-Sr-Ca-Cu-O system has been one of the most studied superconducting ceramic materials for industry applications. The most of the studies with this aim are on silver/ceramic composites, due to the benefits and great compatibility of this metal with the oxide. Tapes made by the powder in tube (PIT) method have been successfully tested in pilot power plants in many countries but in Brazil. In this paper, 5, 10, and 20-wt% silver powders are introduced to compose the core of the tape along with the Bi:2212 ceramic powder. The results of electrical experiments are compared with those made with no silver addition Ag tapes. The best current density, at 60 K and no applied magnetic field, was found for the 10-wt% silver proportion, doubling the value obtained for the tape with no silver in the core.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Nucleic Acid Testing (NAT) as a tool for primary screening of blood donors became a reality in the end of the 1990 decade. We report here the development of an "in-house" RT-PCR method that allows the simultaneous (multiplex) detection of HCV and HIV-RNA in addition to an artificial RNA employed as an external control. This method detects all HIV group M subtypes, plus group N and O, with a detection threshold of 500 IU/mL. After validation, the method replaced p24 Ag testing, in use for blood donation screening since 1996 at our services. From July 2001 to February 2006, 102,469 donations were tested and 41 (0.04%) were found HIV-RNA reactive. One NAT-only reactive donation (antibody non-reactive) was observed, with subsequent seroconversion of the implied donor, giving a yield of 1:102,469. This rate is in contrast to the international experience that reports a detection of approximately 1:600,000 - 1:3,100,000 of isolated HIV-RNA donations.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Tese de Doutoramento (Programa doutoral em Engenharia de Materiais)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

PhD in Sciences Specialty in Physics