991 resultados para QC 20 (denture base resin)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Candida biofilms on denture surfaces are substantially reduced after a single immersion in denture cleanser. However, whether this effect is maintained when dentures are immersed in cleanser daily is unclear. The purpose of this study was to evaluate the effect of the daily use of enzymatic cleanser on Candida albicans biofilms on denture base materials. The surfaces of polyamide and poly(methyl methacrylate) resin specimens (n=54) were standardized and divided into 12 groups (n=9 per group), according to study factors (material type, treatment type, and periods of treatment). Candida albicans biofilms were allowed to form over 72 hours, after which the specimens were treated with enzymatic cleanser once daily for 1, 4, or 7 days. Thereafter, residual biofilm was ultrasonically removed and analyzed for viable cells (colony forming units/mm(2)) and enzymatic activity (phospholipase, aspartyl-protease, and hemolysin). Factors that interfered with the response variables were analyzed by 3-way ANOVA with the Holm-Sidak multiple comparison method (α=.05). Polyamide resin presented more viable cells of Candida albicans (P<.001) for both the evaluated treatment types and periods. Although enzymatic cleansing significantly (P<.001) reduced viable cells, daily use did not maintain this reduction (P<.001). Phospholipase activity significantly increased with time (P<.001) for both materials and treatments. However, poly(methyl methacrylate) based resin (P<.001) and enzymatic cleansing treatment (P<.001) contributed to lower phospholipase activity. Aspartyl-protease and hemolysin activities were not influenced by study factors (P>.05). Although daily use of an enzymatic cleanser reduced the number of viable cells and phospholipase activity, this treatment was not effective against residual biofilm over time.
Resumo:
The association between a toothbrush and a dentifrice is the most used denture cleaning method. The purpose of this study was to evaluate the abrasiveness of specific and non-specific denture cleaning dentifrices on different heat-polymerized acrylic resins. Sixteen specimens (90x30x3mm) of each acrylic resin (QC-20, Lucitone 550, Clássico, Vipi-Cril) were prepared and randomly assigned to 4 groups: 1: control (distilled water), 2: Colgate, 3: Bonyplus and 4: Dentu-Creme. The specimens were subjected to simulated toothbrushing in an automatic brushing machine using 35,600 brush strokes for each specimen. Brushing abrasion run at a 200-g load with the specimens immersed in 2:1 dentifrice/water slurry. Specimens were reconditioned to constant mass and the mass loss (mg) was evaluated. Data were analyzed by 2-way ANOVA and Tukey's test (a=0.05). Analysis of dentifrices' abrasive particles was made by scanning electron microscopy. Colgate produced the greatest mass reduction (42.44 mg, p<0.05), followed by Dentu-Creme (33.60 mg). Bonyplus was the less abrasive (19.91 mg), similar to the control group (19.69 mg) (p>0.05). The mass loss values indicated that QC-20 (33.13 mg) and Lucitone 550 (33.05 mg) resins were less (p<0.05) resistant to abrasion than Clássico (26.04 mg) and Vipi-Cril (23.43 mg). In conclusion, Colgate produced the greatest abrasion. Specific dentifrices for dentures tend to cause less damage to acrylic resins.
Resumo:
The aim of this study was to evaluate the following acrylic resins: Clássico®, QC-20® and Lucitone®, recommended specifically for thermal polymerization, and Acron MC® and VIPI-WAVE®, made for polymerization by microwave energy. The resins were evaluated regarding their surface nanohardness and modulus of elasticity, while varying the polymerization time recommended by the manufacturer. They were also compared as to the presence of water absorbed by the samples. The technique used was nanoindentation, using the Nano Indenter XP®, MTS. According to an intra-group analysis, when using the polymerization time recommended by the manufacturer, a variation of 0.14 to 0.23 GPa for nanohardness and 2.61 to 3.73 GPa for modulus of elasticity was observed for the thermally polymerized resins. The variation for the resins made for polymerization by microwave energy was 0.15 to 0.22 GPa for nanohardness and 2.94 to 3.73 GPa for modulus of elasticity. The conclusion was that the Classico® resin presented higher nanohardness and higher modulus of elasticity values when compared to those of the same group, while Acron MC® presented the highest values for the same characteristics when compared to those of the same group. The water absorption evaluation showed that all the thermal polymerization resins, except for Lucitone®, presented significant nanohardness differences when submitted to dehydration or rehydration, while only Acron MC® presented no significant differences when submitted to a double polymerization time. Regarding the modulus of elasticity, it was observed that all the tested materials and products, except for Lucitone®, showed a significant increase in modulus of elasticity when submitted to a lack of hydration.
Resumo:
Purpose: The aim of this study was to evaluate the influence of artificial accelerated aging on dimensional stability of two types of acrylic resins (thermally and chemically activated) submitted to different protocols of storage. Materials and Methods: One hundred specimens were made using a Teflon matrix (1.5cmx0.5mm) with four imprint marks, following the lost-wax casting method. The specimens were divided into ten groups, according to the type of acrylic resin, aging procedure, and storage protocol (30 days). GI: acrylic resins thermally activated, aging, storage in artificial saliva for 16 hours, distilled water for 8 hours; GII: thermal, aging, artificial saliva for 16 hours, dry for 8 hours; GIII: thermal, no aging, artificial saliva for 16 hours, distilled water for 8 hours, GIV: thermal, no aging, artificial saliva for 16 hours, dry for 8 hours; GV: acrylic resins chemically activated, aging, artificial saliva for 16 hours, distilled water for 8 hours; GVI: chemical, aging, artificial saliva for 16 hours, dry for 8 hours; GVII: chemical, no aging, artificial saliva for 16 hours, distilled water for 8 hours; GVIII: chemical, no aging, artificial saliva for 16 hours, dry for 8 hours GIX: thermal, dry for 24 hours; and GX: chemical, dry for 24 hours. All specimens were photographed before and after treatment, and the images were evaluated by software (UTHSCSA-Image Tool) that made distance measurements between the marks in the specimens (mm), calculating the dimensional stability. Data were submitted to statistical analysis (two-way ANOVA, Tukey test, p = 0.05). Results: Statistical analysis showed that the specimens submitted to storage in water presented the largest distance between both axes (major and minor), statistically different (p < 0.05) from control groups. Conclusions: All acrylic resins presented dimensional changes, and the artificial accelerated aging and storage period influenced these alterations.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
AIMS: There is no standard test to determine the fatigue resistance of denture teeth. With the increasing number of patients with implant-retained dentures the mechanical strength of the denture teeth requires more attention and valid laboratory test set-ups. The purpose of the present study was to determine the fatigue resistance of various denture teeth using a dynamic load testing machine. METHODS: Four denture teeth were used: Bonartic II (Candulor), Physiodens (Vita), SR Phonares II (Ivoclar Vivadent) and Trubyte (Dentsply). For dynamic load testing, first upper molars with a similar shape and cusp inclination were selected. The molar teeth were embedded in cylindrical steel molds with denture base material (ProBase, Ivoclar Vivadent). Dynamic fatigue loading was carried out on the mesio-buccal cusp at a 45° angle using dynamic testing machines and 2,000,000 cycles at 2Hz in water (37°C). Three specimens per group and load were submitted to decreasing load levels (at least 4) until all the three specimens no longer showed any failures. All the specimens were evaluated under a stereo microscope (20× magnification). The number of cycles reached before observing a failure, and its dependence on the load and on the material, has been modeled using a parametric survival regression model with a lognormal distribution. This allowed to estimate the fatigue resistance for a given material as the maximal load for which one would observe less than 1% failure after 2,000,000 cycles. RESULTS: The failure pattern was similar for all denture teeth, showing a large chipping of the loaded mesio-buccal cusp. In our regression model, there were statistically significant differences among the different materials, with SR Phonares II and Bonartic II showing a higher resistance than Physiodens and Trubyte, the fatigue resistance being estimated at around 110N for the former two, and at about 60N for the latter two materials. CONCLUSION: The fatigue resistance may be a useful parameter to assess and to compare the clinical risk of chipping and fracture of denture tooth materials.
Resumo:
Objective: The purpose of this in vitro study was to evaluate the antimicrobial activity of acrylic resins containing different percentages of silver and zinc zeolite, and to assess whether the addition of zeolite alters the flexural and impact strength of the resins. Background: The characteristics of acrylic resins support microorganism development that can threaten the health of the dentures user. Material and methods: A microwave-polymerised (Onda-Cryl) and two heat-polymerised (QC20 and Lucitone 550) acrylic resins were used. The materials were handled according to the manufacturers` instructions. Fifty rectangular-shaped specimens (8 x 10 x 4mm) were fabricated from each resin and assigned to 5 groups (n = 10) according to their percentage of Irgaguard B5000 silver-zinc zeolite (0%- control, 2.5%, 5.0%, 7.5% and 10%). Flexural strength and Izod impact strength were evaluated. The antimicrobial activity against two strains of Candida albicans and two strains of Streptococcus mutans was assessed by agar diffusion method. Data were analysed statistically by one-way ANOVA and Tukey`s test at 5% significance level. Results: The addition of 2.5% of Irgaguard B5000 to the materials resulted in antimicrobial activity against all strains. Flexural strength decreased significantly with the addition of 2.5% (QC20 and Lucitone 550) and 5.0% (Onda-Cryl) of Irgaguard B5000. The impact strength decreased significantly with the addition of 2.5% (Lucitone 550) and 5.0% (QC20 and Onda-Cryl) of zeolite. Conclusion: The addition of silver-zinc zeolite to acrylic resins yields antimicrobial activity, but may affect negatively the mechanical properties, depending on the percentage of zeolite.
Resumo:
Objective: The purpose of this study was to compare the dental movement that occurs during the processing of maxillary complete dentures with 3 different base thicknesses, using 2 investment methods, and microwave polymerization.Methods: A sample of 42 denture models was randomly divided into 6 groups (n = 7), with base thicknesses of 1.25, 2.50, and 3.75 mm and gypsum or silicone flask investment. Points were demarcated on the distal surface of the second molars and on the back of the gypsum cast at the alveolar ridge level to allow linear and angular measurement using AutoCAD software. The data were subjected to analysis of variance with double factor, Tukey test and Fisher (post hoc).Results: Angular analysis of the varying methods and their interactions generated a statistical difference (P = 0.023) when the magnitudes of molar inclination were compared. Tooth movement was greater for thin-based prostheses, 1.25 mm (-0.234), versus thick 3.75 mm (0.2395), with antagonistic behavior. Prosthesis investment with silicone (0.053) showed greater vertical change compared with the gypsum investment (0.032). There was a difference between the point of analysis, demonstrating that the changes were not symmetric.Conclusions: All groups evaluated showed change in the position of artificial teeth after processing. The complete denture with a thin base (1.25 mm) and silicone investment showed the worst results, whereas intermediate thickness (2.50 mm) was demonstrated to be ideal for the denture base.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Statement of problem. Denture bases may become increasingly weaker as a result of thermal stress and flexural cyclic loading. Information regarding this potential problem and its relationship to the denture base reline is limited.Purpose. This study evaluated the influence of thermal and mechanical stresses on the strength of intact and relined denture bases.Material and methods. Twenty-eight microwave-polymerized (Acron MC) intact denture bases were prepared in the shape of a 3-mm-thick maxillary denture. Additionally, fifty-six 2-mm-thick denture bases were relined with 1 mm of autopolymerizing resin (Tokuyama Rebase Fast II or New Truliner) (n = 28). Intact and relined specimens were divided into 4 groups (n = 7) as follows: without stress (control); a mechanical stress at 0.8 Hz for 10,000 cycles; 5000 thermal cycles between 5 degrees C and 55 degrees C; or a combination thermo-mechanical stress. The specimens were vertically loaded in compression with a rounded rod at 5 mm/min until failure, using a universal testing machine. Data on maximum fracture load (N), deflection at fracture (%), and fracture energy (N-mm) were analyzed by 2-way analysis of variance and Student-Newman-Keuls tests (alpha = .05).Results. The strength of the denture bases relined with New Truliner was not significantly affected by any of the experimental conditions, but comparing the control groups, New Truliner exhibited the lowest maximum fracture load values. The maximum fracture load of intact denture bases (P = .002) and those relined with Tokuyama Rebase Fast II (P = .01) showed a significant decrease after thermal stress. Additionally, cyclic loading significantly decreased the maximum fracture load (P < .001), deflection at fracture (P = .025), and fracture energy (P < .001) of intact denture bases and those relined with Tokuyama Rebase (P values of .002, .039, and .001, respectively).Conclusion. Thermal and mechanical stresses exert deleterious effects on the strength of intact and/or relined denture bases, which vary according to the relining material used.