Effect of polymerization methods and thermal cycling on color stability of acrylic resin denture teeth
Contribuinte(s) |
Universidade Estadual Paulista (UNESP) |
---|---|
Data(s) |
30/09/2013
20/05/2014
30/09/2013
20/05/2014
01/12/2009
|
Resumo |
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP) Processo FAPESP: 2006/60850-4 Statement of problem: Acrylic resin denture teeth are widely used due to the chemical bond to the acrylic resin of the denture base. However, discoloration of acrylic resin denture teeth can be a problem. Purpose: The purpose of this study was to investigate the effect of polymerization methods and thermal cycling on the color change of acrylic resin denture teeth. Material and methods: Ten different brands of acrylic resin denture teeth were evaluated: Art Plus (AP), Biolux (BX), Biotone IPN (BI), Magister (MG), Mondial 6 (MD), Premium 6 (PR), SR Vivodent PE (SR), Trilux (TR), Trubyte Biotone (TB), and Vipi Dent Plus (VP). Each brand was divided into 2 groups (n=12); each group was subjected to 1 of 2 polymerization methods (microwave, 500 W for 3 minutes, or water bath, 74°C for 9 hours). After polymerization, all of the specimens were thermal cycled between 5°C and 55°C with 30-second dwell times for 5000 cycles. The specimen colors were measured with a spectrophotometer, using the CIE L*a*b* system, at baseline (B), after polymerization (P), and after thermal cycling (T). Color differences (ΔE) were calculated for periods between P and B (PB), T and B (TB), and T and P (TP). A ΔE of ≤3.3 was considered clinically acceptable. The data were evaluated by 3-way repeated-measures ANOVA and the Tukey HSD test (α=.05). Results: The highest ΔE values were obtained for BI and SR teeth; these were significantly higher than the values obtained for the other brands (P<.05). There was no significant difference between the 2 polymerization methods. There was no significant difference between TB and PB for either polymerization method. Conclusions: The ΔE values are within acceptable clinical limits for all brands, for both polymerization methods and different measurement periods. © 2009 The Editorial Council of the Journal of Prosthetic Dentistry. |
Formato |
385-392 |
Identificador |
http://dx.doi.org/10.1016/S0022-3913(09)60200-6 Journal of Prosthetic Dentistry, v. 102, n. 6, p. 385-392, 2009. 0022-3913 http://hdl.handle.net/11449/130511 10.1016/S0022-3913(09)60200-6 WOS:000275762800010 2-s2.0-72049090374 |
Idioma(s) |
eng |
Publicador |
Mosby-elsevier |
Relação |
Journal of Prosthetic Dentistry |
Direitos |
closedAccess |
Palavras-Chave | #Acrylic acid resin #Water #Color #Colorimetry #Dental care #Hardness #Heat #Materials testing #Microwave radiation #Phase transition #Prosthesis #Tooth prosthesis #Acrylic Resins #Color #Colorimetry #Dental Stress Analysis #Hardness #Hot Temperature #Materials Testing #Microwaves #Phase Transition #Prosthesis Coloring #Tooth, Artificial #Water |
Tipo |
info:eu-repo/semantics/article |