969 resultados para vinyl bromide
Resumo:
A poly(vinyl chloride)(PVC)-based membrane of 15-crown-5 exhibits a good response for lead(II) ions over a wide concentration range. The response time of the sensor is 30 s and the membrane can be used for more than four months without observing any divergence. The selectivity of the sensor is comparable with those reported for other such electrodes. It was possible to determine lead in polluted waters using this electrode assembly.
Resumo:
A series of full interpenetrating polymer network (full-IPN) films of poly(acrylic acid) (PAA)/poly (vinyl alcohol) (PVA) were prepared by radical solution polymerization and sequential IPN technology. Attenuated total reflectance-Fourier transform infrared spectroscopy, swelling properties, mechanical properties, morphology, and glass transition temperature of the films were investigated. FTIR spectra analysis showed that new interaction hydrogen bonds between PVA and PAA were formed. Swelling property of the films in distilled water and different pH buffer solution was studied. Swelling ratio increased with increasing PAA content of IPN films in all media, and swelling ratio decreased with increasing PVA crosslink degree. Tensile strength and elongation at break related not only to the constitution of IPNs but also to the swelling ratio of IPNs.
Resumo:
Self-assembly of binary blends of two triblock copolymers of poly(4-vinyl pyridine)-b-polystyrene-b-poly(4-vinyl pyridine), i.e., P4VP(43)-b-PS260-b-P4VP(43) (P1) and P4VP(43)-b-PS366-b-P4VP(43) (P2), in dioxane/water solution was studied. These two triblock copolymers individually tend to form vesicles (P2) and cylindrical micelles (P1) in dilute solution. It was found that copolymer components in the blend, sample preparation method, and annealing time had significant effect on hybridization aggregate morphology. By increasing P1 content in the copolymer blends, fraction of looped and stretched cylinders increased, while fraction of bilayers decreased. Nearly no bilayer was observed when P1 content was above 85 wt%.
Resumo:
The stability of the complex of cationic lipid with nucleic acid, especially when facing serum, is crucial for the efficiency of gene delivery. Here, we demonstrated that the stability of the complex of didodecyldimethylammonium bromide (DDAB, a cationic lipid) with DNA in the presence of serum dramatically increased after coating DDAB onto the surface of the gold nanoparticles. The stability of the complex was demonstrated with dye intercalation assay, and agarose gel electrophoresis.
Resumo:
Submicrometer zinc oxide (ZnO) with different morphologies including spindle-like, pencil-like, branch rod-like and frizzy flower-like shapes, have been hydrothermally synthesized in mixed solvents of ethanol and water at 140 degrees C. It was found that the volumes of added ammonia, surfactant (cetyltrimethylammonium bromide, CTAB), and mixed solvent play crucial roles in morphological control of ZnO nanostructures. Increasing the volume of ammonia added to the reaction system, the shape of ZnO evolves from spindle into branch rod-like. Synergetic influence between CTAB and ammonia can only be observed at high concentration of ammonia.
Resumo:
Single-crystal Au nanosheets and fcc gold nanocrystals of uniform size were synthesized by a novel and simple route. The results of field-emission scanning electron microscopy (SEM), transmission electron microscopy (TEM) and X-ray diffraction (XRD) indicated the formation of the single-crystal structure of gold nanosheets and fcc nanocrystals. Energy-dispersive analysis of X-ray (EDAX) showed absorbance of cetyltrimethylammonium bromide (CTAB) molecules onto the surface of gold nanostructures.
Resumo:
Branched polystyrenes with abundant pendant vinyl functional groups were prepared via radical polymerization of an asymmetric divinyl monomer, which possesses a higher reactive styryl and a lower reactive butenyl. Employing a fast reversible addition fragmentation chain transfer (RAFT) equilibrium, the concentration of active propagation chains remained at a low value and thus crosslinking did not occur until a high level of monomer conversion. The combination of a higher reaction temperature (120 degrees C) and RAFT agent cumyl dithiobenzoate was demonstrated to be optimal for providing both a more highly branched architecture and a higher polymer yield.
Resumo:
Liquid polybutadiene with desirable 1,2-units content was synthesized by Co(naph)(2)-Al-2(C2H5)(3)Cl-3-P(OPh)(3) catalyst system. It was shown that liquid polybutadiene having adequate 1,2-unit content (vinvl =35%-40%) molecular weight(M-n = 700-3500), and acceptabele conversion(>= 55%) can synthesized after optimizing polymerization conditions.
Resumo:
Super-hydrophobic films with vinyl-modified silica nanoparticles (V-SiOx-NPs) were successfully prepared. The rough surface, which was composed of microstructures of disordered V-SiOx-NPs and nanostructures on the surface of V-SiOx-NPs, rather than the chemical composition devoted to the super-hydrophobicity of film. The relationship between contact angle and diameter of V-SiOx-NPs was then investigated. The sessile contact angles (CA) of films with 150-1600nm V-SiOx-NPs were around 166 regardless the diameter, while the film with 85 nm V-SiOx-NPs had the lowest CA of about 158. The packing manner of V-SiOx-NPs determined the air fraction on the surface and then the CA.
Resumo:
Hyperbranched vinyl polymers were prepared by reversible addition-fragmentation chain transfer ( RAFT) polymerization of a styrenic asymmetric divinyl monomer. This was achieved by using cumyl dithiobenzoate or S-dodecyl-S'-(alpha,alpha'-dimethyl-alpha ''-acetic acid) trithiocarbonate as the chain transfer agent, 1,1'-azobis(cyclohexanecarbonitrile) or thermal initiation as a source of radicals. Cross-linking was inhibited by a rapid RAFT-based equilibrium between active propagation chains and dormant species, and thus a hyperbranched polymer with a monomer conversion as high as 80% was obtained. The hyperbranched structure and properties of the resultant polymers were characterized by a combination of H-1-NMR spectroscopy and a triple detection size exclusion chromatography (TRI-SEC). The hyperbranched vinyl polymer has a broad molecular weight distributions and a low Mark-Houwink exponent alpha value compared with the linear counterpart.
Resumo:
The effect of template phase on the structures of as-synthesized silica nanoparticles with fragile DDAB vesicles as templates is reported. It is found that the template phase plays a critical role in the growth process of silica: the unstable DDAB vesicles in liquid-crystalline phase often lead to the formation of mesostructured solid spheres, and the rather stable DDAB vesicles in gel phase lead to the formation of hollow spheres with less mesostructures.
Resumo:
The morphological development and crystallization behavior of poly(epsilon-caprolactone) (PCL) in miscible mixtures of PCL and poly(vinyl methyl ether) (PVME) were investigated by optical microscopy as a function of the mixture composition and crystallization temperature. The results indicated that the degree of crystallinity of PCL was independent of the mixture composition upon melt crystallization because the glass-transition temperatures of the mixtures were much lower than the crystallization temperature of PCL. The radii of the PCL spherulites increased linearly with time at crystallization temperatures ranging from 42 to 49 degrees C. The isothermal growth rates of PCL spherulites decreased with the amount of the amorphous PVME components in the mixtures. Accounting for the miscibility of PCL/PVME mixtures, the radial growth rates of PCL spherulites were well described by a kinetic equation involving the Flory-Huggins interaction parameter and the free energy for the nuclei formation in such a way that the theoretical calculations were in good agreement with the experimental data. From the analysis of the equilibrium melting point depression, the interaction energy density of the PVME/PCL system was calculated to be -3.95 J/cm(3).