Resumo:
Laser conditioning effects of the HfO2/SiO2 antireflective (AR) coatings at 1064 nm and the accumulation effects of multishot laser radiation were investigated. The HfO2/SiO2 AR coatings were prepared by E-beam evaporation (EBE). The singleshot and multi-shot laser induced damage threshold was detected following ISO standard 11254-1.2, and the laser conditioning was conducted by three-step raster scanning method. It was found that the single-shot LIDT and multi-shot LIDT was almost the same. The damage mostly > 80% occurred in the first shot under multi-shot laser radiation, and after that the damage occurring probability plummeted to < 5%. There was no obvious enhancement of the laser damage resistance for both the single-shot and multi-shot laser radiation of the AR coatings after laser conditioning. A Nomarski microscope was employed to map the damage morphology, and it found that the damage behavior is defect-initiated for both unconditioned and conditioned samples. © 2004 Elsevier B.V. All rights reserved.
Resumo:
Adhesion between the interface of pure silver thin film and three kinds of low refractive index coatings MgF2, Al2O3, SiO2 were compared in this article. The results indicated that the adhesion of Al2O3 and Ag was evidently superior to that of MgF2 and Ag, and the adhesion of MgF2 and Ag was evidently superior to that Of SiO2 and Ag. Reasons were analyzed accordingly. On the other hand, we compared the effect on the optical characteristic of Ag film when these three kinds of films were used as protective coatings and enhanced coatings. Considering the difference of the adhesion between Ag and MgF2, Al2O3, SiO2, suited uses are given for each other. © 2004 Elsevier B.V. All rights reserved.
Resumo:
ZrO2 coatings were deposited on different substrates of Yb:YAG and fused silica by electron beam evaporation. After annealed for 12 h at 673 and 1073 K, respectively, weak absorption of coatings was measured by surface thermal lensing (STL) technique, and then laser-induced damage threshold (LIDT) was determined also. The crystalline phase of ZrO2 coatings and the size of the crystal grain were investigated by X-ray diffraction. It was found that microstructure of ZrO2 coatings was dependent on both annealing temperature and substrate structure, and coatings containing monoclinic phases had higher damage threshold than others. Due to the strong absorption of Yb:YAG, damage threshold of coatings on Yb:YAG was much less than that on fused silica. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
A series of ZnO thin films were deposited on ZnO buffer layers by DC reactive magnetron sputtering. The buffer layer thickness determination of microstructure and optical properties of ZnO films was investigated by X-ray diffraction (XRD), photoluminescence (PL), optical transmittance and absorption measurements. XRD results revealed that the stress of ZnO thin films varied with the buffer layer thickness. With the increase of buffer layer thickness, the band gap edge shifted toward longer wavelength. The near-band-edge (NBE) emission intensity of ZnO films deposited on ZnO buffer layer also varied with the increase of thickness due to the spatial confinement increasing the Coulomb interaction between electrons and holes. The PL measurement showed that the optimum thickness of the ZnO buffer layer was around 12 nm. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Two different kinds of 1064 nm high-reflective (HR) coatings, with and without SiO2 protective layer, were prepared by electron beam evaporation. Three-dimensional damage morphology, caused by a Nd:YAG pulsed laser, was investigated for these HR coatings. Development of laser-induced damage on HR coatings was revealed by both temperature field calculation and discrete meso-element simulation. Theoretical results met experimental very well. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Optical properties and microstructure of Ag film on glass substrate with Cr intermediate layer were studied by using spectrophotometer and XRD. The spectra results showed that introducing Cr intermediate layer reduced the surface roughness and promoted the reflectivity of Ag film. The XRD analysis showed that the crystalline grains increased and the stress decreased. The adhesion was also improved by using the tape test method. (c) 2006 Published by Elsevier B.V.
Resumo:
Negative ion element impurities breakdown model in HfO2 thin film was reported in this paper. The content of negative ion elements were detected by glow discharge mass spectrum analysis (GDMS); HfO2 thin films were deposited by the electron-beam evaporation method. The weak absorption and laser induced damage threshold (LIDT) of HfO2 thin films were measured to testify the negative ion element impurity breakdown model. It was found that the LIDT would decrease and the absorption would increase with increasing the content of negative ion element. These results indicated that negative ion elements were harmful impurities and would speed up the damage of thin film. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Laser conditioning effects of the dielectric mirror coatings with different designs were investigated. Simple quarter-wave ZrO2:Y2O3/SiO2 mirrors and half-wave SiO2 over-coated ZrO2:Y2O3/SiO2 mirror coatings were fabricated by E-beam evaporation (EBE). The absorbance of the samples before and after laser conditioning was measured by surface thermal lensing (STL) technology and the defects density was detected under Nomarski microscope. The enhancement of the laser damage resistance was found after laser conditioning. The dependence of the laser conditioning on the coating design was also observed and the over-coated sample obtained greatest enhancement, whereas the absorbance of the samples did not change obviously. During the sub-threshold fluence raster scanning, the minor damage about defects size was found and the assumption of pre-damage mechanism, based on the functional damage concept, was put forward. The improvement of the laser induced damage threshold (LIDT) was attributed to the benign damage of the defects and the dependence on the coating design owed to the damage growth behavior of different coating designs. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
A series of HR coatings, with and without overcoat, were prepared by electron beam evaporation using the same deposition process. The laser-induced damage threshold (LIDT) was measured by a 355 nm Nd:YAG laser with a pulse width of 8 ns. Damage morphologies of samples were observed by Leica-DMRXE Microscope. The stress was measured by viewing the substrate deformation before and after coatings deposition using an optical interferometer. Reflectance of the samples was measured by Lambda 900 Spectrometer. The theoretical results of electric field distributions of the samples were calculate by thin film design software (TFCalc). It was found that SiO2 overcoat had improved the LIDT greatly, while MgF2 overcoat had little effect on the LIDT because of its high stress in the HR coatings. The damage morphologies were different among HR coatings with and without overcoats. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
The glancing angle deposition (GLAD) technique was used to deposit ZnS films by electron beam evaporation method. The cross sectional scanning electron microscopy (SEM) image illustrated a highly orientated microstructure composed of slanted column. The atomic force microscopy (APM) analysis indicated that incident flux angle had significant effects on the nodule size and surface roughness. Under identical nominal thickness, the actual thickness of the GLAD films is related to the incident flux angle. The refractive index and in-plane birefringence of the GLAD ZnS films were discussed, and the maximum bireffingence Delta n = 0.036 was obtained at incident flux angle of alpha = 80 degrees. Therefore, the glancing angle deposition technique is a promising way to create a columnar structure with enhanced birefringent property. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
ZrO2 thin films were prepared on BK7 glass substrates by electron beam evaporation deposition method. The influence of deposition rate varying from 1.2 to 6.3 nm s(-1) on surface morphology and other properties of ZrO2 films were examined. With increasing deposition rate, the surface defect density increased. The decrease in half width at full maximum in X-ray diffraction pattern with deposition rate indicates an increase in crystal dimension with increasing deposition rate. Electron beam deposited ZrO2 films are known to be inhomogeneous. From the change of the peak transmittance value, it can be deduced that the inhomogeneity of ZrO2 films strengthened gradually with increasing deposition rate. The type of surface defects changed from nodules to craters when the deposition rate was high enough.
Resumo:
A model for refractive index of stratified dielectric substrate was put forward according to theories of inhomogeneous coatings. The substrate was divided into surface layer, subsurface layer and bulk layer along the normal direction of its surface. Both the surface layer (separated into N-1 sublayers of uniform thickness) and subsurface layer (separated into N-2 sublayers of uniform thickness), whose refractive indices have different statistical distributions, are equivalent to inhomogeneous coatings, respectively. And theoretical deduction was carried Out by employing characteristic matrix method of optical coatings. An example of mathematical calculation for optical properties of dielectric coatings had been presented. The computing results indicate that substrate subsurface defects can bring about additional bulk scattering and change propagation characteristic in thin film and Substrate. Therefore, reflectance, reflective phase shift and phase difference of an assembly of coatings and substrate deviate from ideal conditions. The model will provide some beneficial theory directions for improving optical properties of dielectric coatings via substrate surface modification. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Four kinds of Y2O3 stabilized ZrO2 (YSZ) thin films with different Y2O3 content have been prepared on BK7 substrates by electron-beam evaporation method. Structural properties and surface morphology of thin films were investigated by X-ray diffraction (XRD) spectra and scanning probe microscope. Laser induced damage threshold (LIDT) was determined. It was found that crystalline phase and microstructure of YSZ thin films was dependent on Y2O3 molar content. YSZ thin films changed from monoclinic phase to high temperature phase (tetragonal and cubic) with the increase of Y2O3 content. The LIDT of stabilized thin film is more than that of unstabilized thin films. The reason is that ZrO2 material undergoes phase transition during the course of e-beam evaporation resulting in more numbers of defects compared to that of YSZ thin films. These defects act as absorptive center and the original breakdown points. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Zinc oxide (ZnO) films with c-oriented were grown on fused quartz glass substrates at room temperature using dc reactive magnetron sputtering. The as-grown films were annealed at 700 degrees C in air and bombarded by ion beam, respectively. The effects of post-treatments on the structural and optical properties of the ZnO films were investigated by X-ray diffraction (XRD), photoluminescence (PL), optical transmittance and absorption measurements. The XRD spectra indicate that the crystal quality of ZnO films has been improved by both the post-treatments. Compared with the as-grown sample, both annealed and bombarded samples exhibited blueshift in the UV emission peaks, and a strong green emission was found in the annealed ZnO film. In both optical transmittance and absorption spectra, a blueshift of the band-gap edge was observed in the bombarded film, while a redshift was observed in the annealed film. (c) 2004 Elsevier B.V. All rights reserved.
Resumo:
Thin-film single layers of Al2O3 and MgF2 were deposited upon super polished fused-silica by electron-beam evaporation. The subsequent optical constants n and k were reported for the spectral range of 180-230 nm. High-reflectance dense multilayer coatings for 193 nm were designed on the basis of the evaluated optical constants and produced. The spectra of the reflectance of HR coatings were compared to the theoretical calculations. HR mirrors of 27 layers with a reflectance of more than 98% were reported. (c) 2004 Elsevier B.V. All rights reserved.