998 resultados para ferroelectric thin films
Resumo:
Pure and Nb doped PbZr0.4Ti0.603 thin films was prepared by the polymeric precursor method and deposited by spin coating on Pt/Ti/SiO2/Si (100) substrates and annealed at 700 degreesC. The films are oriented in (1 1 0) and (1 0 0) direction. The electric properties of PZT thin films show strong dependence of the crystallographic orientation. The P-E hysteresis loops for the thin film with composition PbZr0.39Ti0.6Nb0.103 showed good saturation, with values for coercive field (E-c) equal to 60 KV cm(-1) and for remanent polarization (P-r) equal to 20 muC cm(-2). The measured dielectric constant (epsilon) is 1084 for this film. These results show good potential for application in FERAM. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
The (1 1 7) and (0 0 1 0)-oriented Bi4Ti3O12 thin films were fabricated on Pt/Ti/SiO2/Si substrates by using a polymeric precursor solution under appropriate crystallization conditions. Atomic force microscopy and scanning electron microscopy showed relatively large grains, which is typical for this system. The capacitance dependence on voltage is strongly non-linear, confirming the ferroelectric properties of the films resulting from the domain switching. The (1 1 7)-oriented films exhibited a higher remanent polarization (23.7 μ C cm(-2)) than the (0 0 1 0)-oriented films (11.8 μ C cm(-2)). Fatigue tests revealed that the temperature of thermal treatment and degree of orientation affect the performance of the device. © 2005 Elsevier B.V. All rights reserved.
Resumo:
Calcium modified lead titanate sol was synthesized using a soft solution processing, the so-called polymeric precursor method. In soft chemistry method, soluble precursors such as lead acetate trihydrate, calcium carbonate and titanium isopropoxide, as starting materials, were mixed in aqueous solution. Pb0.7Ca0.3TiO3 thin films were deposited on platinum-coated silicon and quartz substrates by means of the spinning technique. The surface morphology and crystal structure, dielectric and optical properties of the thin films were investigated. The electrical measurements were conducted on metal-ferroelectric-metal (MFM) capacitors. The typical measured small signal dielectric constant and dissipation factor at a frequency of 100 kHz were 299 and 0.065, respectively, for a thin film with 230 nm thickness annealed at 600degreesC for 2 h. The remanent polarization (2P(r)) and coercive field (E-c) were 32 muC/cm(2) and 100 kV/cm, respectively. Transmission spectra were recorded and from them, refractive index, extinction coefficient, and band gap energy were calculated. Thin films exhibited good optical transmissivity, and had optical direct transitions. The present study confirms the validity of the DiDomenico model for the interband transition, with a single electronic oscillator at 6.858 eV. The optical dispersion behavior of PCT thin film was found to fit well the Sellmeir dispersion equation. The band gap energy of the thin film, annealed at 600degreesC, was 3.56 eV. The results confirmed that soft solution processing provides an inexpensive and environmentally friendly route for the preparation of PCT thin films.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Ferroelectric barium titanate thin films were produced by the polymeric precursor method. In this technique, the desired metal cations are chelated in a solution using a hydroxycarboxylic acid as the chelating agent. Barium carbonate and titanium IV isopropoxide were used as precursors for the citrate solution. Ethylene glycol and citric acid were used as polymerization/complexation agents for the process. The crystalline structure of the film annealed at 700 °C had a single perovskite phase with a tetragonal structure. The BaTiO3 film showed good P-E hysteresis loops and C-V characteristics due to the switched ferroelectric domains.
Resumo:
Ferroelectric SrBi2Nb2O9 (SBN) thin films were prepared by pulsed laser deposition (PLD) on Pt/Ti/SiO2/Si(100) using a sequential deposition process from two SBN and Bi2O3 targets. This route allows for bismuth enrichment of the film composition in order to improve the ferroelectric characteristics. Structural and microstructural characterizations were performed by X-ray diffraction (XRD) and scanning electron microscopy (SEM). The composition of films and targets was determined by energy dispersive X-ray spectrometry (EDX). The deposition temperature, which provided well-crystallized layered perovskite SBN phase films in situ, was found to be 700°C. The results were compared with those obtained for SBN films deposited at 400°C and then crystallized ex situ. For an ex situ annealing temperature of 750°C, a remanent polarization value (Pr) of 23.2 μc/cm2 and a coercive field (Ec) of 112 kV/cm were measured. © 2001 Elsevier Science Ltd. All rights reserved.
Resumo:
Lead zirconate titanate (PZT) solutions were prepared using a polymeric precursor method, Zr n-propoxide and Ti i-propoxide were used as starting materials with ethylene glycol and water as solvents. The PZT solution was spin-coated on Pt/Ti/SiO2/Si substrates, baked on a hot plate, and finally heat-treated in a tube furnace between 400 and 800°C. The surface morphology and grain size of the films were characterized by atomic force microscopy (AFM), using a tapping mode with amplitude modulation. The films, thermal annealed at temperatures higher than 500°C, exhibited a dense microstructure, without noticeable cracks or voids. Electrical properties were investigated as a function of composition and annealing temperature.
Resumo:
It is very important for the building of the SAW devices to study dielectric and ferroelectrics properties because every SAW device is based in piezoelectric effect that it is made up to transform an electric sign in the mechanical or acoustic sign and a mechanical or acoustic sign in an electric sign. Thus, the purpose of the present work is to prepare PbZr 0,53Ti0.47O3 (PZT) and PbTiO3 (PT) thin films on the Si (100) substrates across spin-coating using a chemical method based in polymeric precursors. After conventional treatment in the furnace, the films were characterized by impedance spectroscopy and hysteresis loops to know its dielectric and ferroelectric properties.
Resumo:
Structural, microstructural and ferroelectric properties of Pb0.90Ca0.10TiO3 (PCT10) thin films deposited using La0.50Sr0.50CoO3 (LSCO) thin films which serve only as a buffer layer were compared with properties of the thin films grown using a platinum-coated silicon substrate. LSCO and PCT10 thin films were grown using the chemical solution deposition method and heat-treated in an oxygen atmosphere at 700 °C and 650 °C in a tube oven, respectively. X-ray diffraction (XRD) and Raman spectroscopy results showed that PCT10 thin films deposited directly on a platinum-coated silicon substrate exhibit a strong tetragonal character while thin films with the LSCO buffer layer displayed a smaller tetragonal character. Surface morphology observations by atomic force microscopy (AFM) revealed that PCT10 thin films with a LSCO buffer layer had a smoother surface and smaller grain size compared with thin films grown on a platinum-coated silicon substrate. Additionally, the capacitance versus voltage curves and hysteresis loop measurement indicated that the degree of polarization decreased for PCT10 thin films on a LSCO buffer layer compared with PCT10 thin films deposited directly on a platinum-coated silicon substrate. This phenomenon can be described as the smaller shift off-center of Ti atoms along the c-direction 〈001〉 inside the TiO6 octahedron unit due to the reduction of lattice parameters. Remnant polarization (P r ) values are about 30 μC/cm2 and 12 μC/cm2 for PCT10/Pt and PCT10/LSCO thin films, respectively. Results showed that the LSCO buffer layer strongly influenced the structural, microstructural and ferroelectric properties of PCT10 thin films. © 2013 Elsevier Ltd and Techna Group S.r.l.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
The ferroelectric properties and leakage current mechanisms of preferred oriented Bi3.25La0.75 Ti3O12 (BLT) thin films deposited on La0.5Sr0.5CoO3 (LSCO) by the polymeric precursor method were investigated. Atomic force microscopy indicates that the deposited films exhibit a dense microstructure with a rather smooth surface morphology. The improved ferroelectric and leakage current characteristics can be ascribed to the plate-like grains of the BLT films. © 2006 Trans Tech Publications, Switzerland.
Resumo:
Single-phase multiferroic materials are of considerable interest for future memory and sensing applications. Thin films of Aurivillius phase Bi 7Ti3Fe3O21 and Bi6Ti 2.8Fe1.52Mn0.68O18 (possessing six and five perovskite units per half-cell, respectively) have been prepared by chemical solution deposition on c-plane sapphire. Superconducting quantum interference device magnetometry reveal Bi7Ti3Fe 3O21 to be antiferromagnetic (TN = 190 K) and weakly ferromagnetic below 35 K, however, Bi6Ti2.8Fe 1.52Mn0.68O18 gives a distinct room-temperature in-plane ferromagnetic signature (Ms = 0.74 emu/g, μ0Hc =7 mT). Microstructural analysis, coupled with the use of a statistical analysis of the data, allows us to conclude that ferromagnetism does not originate from second phase inclusions, with a confidence level of 99.5%. Piezoresponse force microscopy (PFM) demonstrates room-temperature ferroelectricity in both films, whereas PFM observations on Bi6Ti2.8Fe1.52Mn0.68O18 show Aurivillius grains undergo ferroelectric domain polarization switching induced by an applied magnetic field. Here, we show for the first time that Bi6Ti2.8Fe1.52Mn0.68O18 thin films are both ferroelectric and ferromagnetic and, demonstrate magnetic field-induced switching of ferroelectric polarization in individual Aurivillius phase grains at room temperature.
Resumo:
Polycrystalline films of SrBi2Nb2O9 were grown using pulsed-laser ablation. The ferroelectric properties were achieved by low-temperature deposition followed by a subsequent annealing process. The lower switching voltage was obtained by lowering the thickness, which did not affect the insulating nature of the films. The hysteresis results showed an excellent square-shaped loop with results (P-r=6 mu C/cm(2), E-c=100 kV/cm) in good agreement with earlier reports. The films also exhibited a dielectric constant of 250 and a dissipation factor of 0.02. The transport studies indicated an ohmic behavior, while higher voltages induced a bulk space charge.