959 resultados para Single crystal substrates
Resumo:
LiAlO2 single crystals doped with Ti at concentration 0.2 at.% are grown by the Czochralskl technique with dimensions Phi 42 x 55 mm. Ti ions in the crystal are quadrivalence proven by comparing the absorption and fluorescence spectra of pure LiAlO2 and Ti: LiAlO2. After air and Li-rich atmosphere annealing, the absorption peaks in the range of 600-800nm disappear. We conclude that 682 and 756nm absorption peaks are attributed to the V-Li and V-O absorptions, respectively. The peaks at 716nm and 798nm may stem from the V-Li(+) and F+ absorptions. The colour-centre model can be applied to explain the experimental phenomena. Ti4+-doping produces more lithium vacancies in the LiAlO2 crystal. The intensities of [LiO4] and the associated bonds remain unchanged, which improves the anti-hydrolyzation and thermal stability of LiAlO2 crystals.
Resumo:
Absorption and emission spectral properties of GdVO4 single crystal doped with Ho3+ ions were investigated at room temperature. Polarized absorption cross section is calculated in the range of 400-2200nm. Results were analyzed and parameters were calculated based on Judd-Ofelt theory, the emission spectrum shows that the emission intensity around the wavelength of 546 nm associated with transition S-5(2) -> I-5(8) is much stronger than other bands in the observed range and potentially enable the green light output around this emission band in this crystal. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
For the first time, a high optical quality Yb3+-doped lutetium pyrosilicate laser crystal Lu2Si2O7 (LPS) was grown by the Czochralski (Cz) method. The segregation coefficient of ytterbium ion in Yb:LPS crystal detected by the inductively coupled plasma atomic emission spectrometer (TCP-AES) method is equal to 0.847. X-ray powder diffraction result confirms the C2/m phase monoclinic space group of the grown crystal and the peaks corresponding to different phases were indexed. The absorption and fluorescence spectra, as well as fluorescence decay lifetime of Yb3+ ion in LPS have been investigated. The absorption and fluorescence cross-sections of the transitions F-2(7/2) <-> F-2(5/2) of Yb3+ ion in LPS crystal have been determined. The advantages of the Yb:LPS crystal including high crystal quality, quasi-four-level laser operating scheme, high absorption cross-sections (1.33 x 10(-2) cm(2)) and particularly broad emission bandwidth (similar to 62 nm) indicated that the Yb:LPS crystal seemed to be a promising candidate used as compact, efficient thin chip lasers when LD is pumped at 940 and 980 nm due to its low-symmetry monoclinic structure and single crystallographic site. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
Absorption spectrum from 400 to 2000 run and upconversion fluorescence spectra under 940 nm pumping of YAG single crystal codoped with 5 at.% Yb3+ and 4 at.% Tm3+ were studied at room temperature. The blue upconversion emission centered at 483 nm corresponds to the transition (1)G(4) -> H-3(6), the emission band around 646 nm corresponds to the transition (1)G(4) -> F-3(4) of Tm3+. Energy transfer from Yb3+ to Tm3+ is mainly nonradiative and the transfer efficiency was experimentally assessed. The line strengths, transition probabilities and radiative lifetimes of (1)G(4) level were calculated by using Judd-Ofelt theory. Gain coefficient calculated from spectra shows that the upconversion corresponding with transitions (1)G(4) -> H-3(6) in YAG doped with Yb3+ and Tm3+ is potentially useful for blue light Output. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
In this paper, single crystal of ytterbium (Yb) doped Ca-5(PO4)(3)F (FAP) has been grown along the c-axis by using the Czochralski method. The segregation coefficients of Yb3+ in the Yb:FAP crystal has been determined by ICP-AES method. The absorption spectrum, fluorescence spectrum and fluorescence lifetime of the Yb:FAP crystal has been also measured at room temperature. In the absorption spectra, there are two absorption bands at 904 and 982 nm, respectively, which are suitable for InGaAs diode laser pumping. The absorption cross-section (sigma(abs)) is 5.117 x 10(-20) cm(2) with an FWHM of 4 nm at 982 nm. The emission cross-section is (sigma(em)) 3.678 x 10(-20) cm(2) at 1042 nm. Favorable values of the absorption cross-section at about 982 nm are promising candidates for laser diode (LD) pumping. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
beta-Ga2O3: Cr single crystals were grown by floating zone technique. Absorption spectra and fluorescence spectra were measured at room temperature. The values of field splitting parameter Dq and Racah parameter B were obtained by the peak values of absorption spectra. The value 10Dq/B=23.14 manifests that in beta-Ga2O3 crystals Cr3+ ions are influenced by low energy crystal field. After high temperature annealing in air, the Cr3+ intrinsic emission was enhanced and the green luminescence disappeared. The strong and broad 691 nm emission was obtained at 420 nm excitation due to the electron transition occurred from T-4(2) to (4)A(2). The studies manifest that the beta-Ga2O3 crystals have the potential application for tunable laser.
Resumo:
The growth and fabrication of GaN/InGaN multiple quantum well (MQW) light emitting diodes ( LEDs) on ( 100) beta-Ga2O3 single crystal substrates by metal-organic chemical vapour deposition (MOCVD) technique are reported. x-ray diffraction (XRD) theta-2 theta. scan spectroscopy is carried out on the GaN buffer layer grown on a ( 100) beta-Ga2O3 substrate. The spectrum presents several sharp peaks corresponding to the ( 100) beta-Ga2O3 and ( 004) GaN. High-quality ( 0002) GaN material is obtained. The emission characteristics of the GaN/InGaN MQW LED are measurement. The first green LED on beta-Ga2O3 with vertical current injection is demonstrated.
Resumo:
The effects of gamma-irradiation on the air-annealed 10 at.% Yb:Y3Al5O12 (YAG) and air annealing on the gamma-irradiated 10at.% Yb:YAG have been studied by the difference absorption spectra before and after treatment. The gamma-irradiation and air annealing led to opposite changes of the absorption properties of the Yb:YAG crystal. After air annealing, the gamma-irradiation induced centers were totally removed and the concentration of Fe3+ and Yb3+ were lightly increased. For the first time, the gamma-irradiation induced valence changes between Yb3+ and Yb2+ ions in Yb:YAG crystals have been observed. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
g-LiAlO2 single crystal is a promising substrate for GaN heteroepitaxy. In this paper, we present the growth of large-sized LiAlO2 crystal by modified Czochralski method. The crystal quality was characterized by high-resolution X-ray diffraction and chemical etching. The results show that the as-grown crystal has perfect quality with the full width at half maximum (FWHM) of 17.7-22.6 arcsec and etch pits density of (0.3-2.2) x 10(4) cm(-2) throughout the crystal boule. The bottom of the crystal boule shows the best quality. The optical transmission spectra from UV to IR exhibits that the crystal is transparent from 0.2 to 5.5 mu m and becomes completely absorbing around 6.7 mu m wavelength. The optical absorption edge in near UV region is about 191 nm.
Resumo:
National Nature Science Foundation of China (Grant No. 60607015)