991 resultados para KERATEINE BLEND FILMS
Resumo:
The optical constants of two cyanine dye films that we prepared were measured with a RAP-1-type (RAP is rotating analyzer and polarizer) spectroscopic ellipsometer. Toward making a simplified model for the wafers of a recordable compact disk (CD-R), we give their optimization designs developed with the cyanine dye films. in addition, the dynamic storage performances of two sample disks were tested by our dynamic storage testing system. Measurement results of the sample disks were obtained to test and verify our film designs. (C) 2000 Optical Society of America. OCIS codes: 160.4890, 160.4760, 210.4810.
Resumo:
The time response of optical switching properties of Sb thin films under focused laser pulses is investigated. The results show that the response course can be divided into onset, opening, and closing stages. Formulas for their lengths are given. The onset and opening times decrease with increasing pumping light power density. The closing time is about 150 ns. For optical memory, if the power density of the readout and recording lasers changes from 5 x 10(9) to 15 x 10(9) W/m(2), the onset time changes from 2.5 to 0.30 mus, and the opening time is on the nanosecond scale. (C) 2003 Society of Photo-Optical Instrumentation Engineers.
Resumo:
SrBi2Ta2O9 (SBT) thin films on quartz substrates were prepared by use of the pulsed-laser deposition technique. The nonlinear refractive indices, n(2), Of the SBT films were measured by use of z-scan techniques with picosecond pulses. Large negative nonlinear refractive indices of 3.84 and 3.58 cm(2)/GW were obtained for the wavelengths 532 nm and 1.064 mum, respectively. The two-photon absorption coefficient was determined to be 7.3 cm/GW for 532 nm. The limiting behavior of SBT thin film on a quartz substrate was investigated in an f/5 defocusing geometry by use of 38-ps-duration, 532-nm, 1.064-mum. laser excitation. (C) 2001 Optical Society of America.
Resumo:
In this paper, GdFeCo/DyFeCo exchange-coupled double-layer films used for center aperture type magnetically induced super resolution were investigated through experiments and theoretical calculation. The samples were prepared by magnetron sputtering method. The polar Kerr effect was measured to prove the spin reorientation of the readout layer. Theoretical study of magnetization profiles was performed on the basis of the mean-field theory and the continuum model. The theoretical results showed that the magnetization orientation of the readout layer changed gradually from in-plane to out-of-plane with the rise of the temperature. Theoretical analysis explained the experimental results successfully. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Crystallization is achieved in amorphous Ge2Sb2Te5 films upon irradiation with a single femtosecond laser pulse. Transmission electron microscopy images evidence the morphology of the crystallized spot which depends on the fluence of the ferntosecond laser pulse. Fine crystalline grains are induced at low fluence, and the coarse crystalline grains are obtained at high fluence. At the damage fluence, ablation of the films occurs. (C) 2004 Elsevier Ltd. All rights reserved.
Resumo:
The single-layer and multilayer Sb-rich AgInSbTe films were irradiated by a single femtosecond laser pulse with the duration of 120 fs. The morphological feature resulting from the laser irradiation have been investigated by scanning electron microscopy and atom force microscopy. For the single-layer film, the center of the irradiated spot is a dark depression and the border is a bright protrusion; however, for the multilayer film, the center morphology changes from a depression to a protrusion as the energy increases. The crystallization threshold fluence of the single-layer and the multilayer films is 46.36 mJ/cm(2), 63.74 mJ/cm(2), respectively.
Resumo:
Crystallization in amorphous Ge2Sb2Te5 films by irradiation with femtosecond laser was investigated. The reflectivity and X-ray diffraction measurements confirmed that the crystalline state has been achieved in amorphous Ge2Sb2Te5 films under the irradiation of fermosecond laser with an average power of 65 mW at a frequency of 1000 Hz and a pulsed width of 120 fs. The surface morphology before and after femtosecond laser irradiation was studied by scanning electron microscope; results showed that the surface of films with irradiation of femtosecond laser was composed of some the crystallized micro-region. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
A new composition content quaternary-alloy-based phase change thin film, Sb-rich AgInSbTe, has been prepared by DC-magnetron sputtering on a K9 glass substrate. After the film has been subsequently annealed at 200degreesC for 30 min, it becomes a crystalline thin film. The diffraction peak of antimony (Sb) are observed by shallow (0.5 degree) x-ray diffraction in the quaternary alloy thin film. The analyses of the measurement from differential scanning calorimetry (DSC) show that the crystallization temperature of the phase change thin film is about 190degreesC and increases with the heating rate. By Kissinger plot, the activation energy for crystallization is determined to be 3.05eV. The reflectivity, refractive index and extinction coefficient of the crystalline and amorphous phase change thin films are presented. The optical absorption coefficient of the phase change thin films as a function of photon energy is obtained from the extinction coefficient. The optical band gaps of the amorphous and crystallization phase change thin films are 0.265eV and 1.127eV, respectively.
Resumo:
The morphology of materials resulting from laser irradiation of the single-layer and the multilayer amorphous Ge2Sb2Te5 films using 120 fs pulses at 800 nm was observed using scanning electron microscopy and atomic force microscopy. For the single-layer film, the center of the irradiated spot is depression and the border is protrusion, however, for the multilayer film, the center morphology changes from a depression to a protrusion as the increase of the energy. The crystallization threshold fluence of the single-layer and the multilayer film is 22 and 23 mJ/cm(2), respectively. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Optical transmission through flat media should be smaller than 1. However, we have observed optical transmission up to T=1.18. The samples were ZnS-SiO2/AgOx/ZnS-SiO2 sandwiched thin films on glass substrate. The supertransmission could only be observed in the near field. We attribute the supertransmission to the lateral propagation relayed by the laser activated and decomposed Ag nanoparticles. (c) 2006 American Institute of Physics.
Resumo:
With light illumination from an Ar ion laser, the photoinduced changes in vacuum evaporated amorphous GeSe2 films; were investigated with the X-ray diffraction (XRD), infrared absorption (IR), scanning electron microscope (SEM), transmitting electron microscope (TEM) and transmittance spectra analysis. It was observed that the optical transmittance edges of films shifted to shorter wavelength according to annealing and light illumination and the shift in well-annealed films could be recovered by annealing at 200 degrees C for 1 h in Ar air. The magnitude of shift increased with the increase of the intensity of illumination light and the illumination time. By sides, photoinduced crystallization was also observed in the exposed regions of GeSe2 films and more of it was observed with stronger intensity of illumination light.
Resumo:
Three kinds of new nickel(II) complexes of alpha-isoxazolylazo-beta-diketones with blue-violet light absorption were synthesized. Their structures were postulated based on elemental analysis, MS and FT-IR spectra. Smooth films on K9 glass substrates were prepared using the spin-coating method. The absorption properties and thermal stability of these complexes were discussed. The static optical recording test for high density digital versatile disc-recordable (HD-DVD-R) system was also studied. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
The NiOx thin films were deposited by reactive dc-magnetron sputtering from a nickel metal target in Ar + O-2 with the relative O-2 content 5%. The as-deposited NiOx, thin films could represent a two-component system comprising crystalline NiO particles dispersed in an amorphous Ni2O3. Decomposition temperature of the as-deposited NiO, thin films was at about 263 degrees C. After annealed at 400 degrees C for 30 min in air, the surface morphology of the films became very rough due to the decomposition of the Ni2O3, leading to the changes of the optical properties of the NiO, thin films. The reflectivity of the films annealed at 400 degrees C was lower than that of the as-deposited one and the optical contrast was 52% at 405 nm. (c) 2006 Elsevier B.V. All rights reserved.