985 resultados para Luminescence.
Resumo:
beta-Ga2O3: Cr single crystals were grown by floating zone technique. Absorption spectra and fluorescence spectra were measured at room temperature. The values of field splitting parameter Dq and Racah parameter B were obtained by the peak values of absorption spectra. The value 10Dq/B=23.14 manifests that in beta-Ga2O3 crystals Cr3+ ions are influenced by low energy crystal field. After high temperature annealing in air, the Cr3+ intrinsic emission was enhanced and the green luminescence disappeared. The strong and broad 691 nm emission was obtained at 420 nm excitation due to the electron transition occurred from T-4(2) to (4)A(2). The studies manifest that the beta-Ga2O3 crystals have the potential application for tunable laser.
Resumo:
本文研究了红外飞秒激光照射下Ce^3+ 掺杂的YAP和LSO两种闪烁晶体的上转换发光现象.实验发现在飞秒激光泵浦下,这两种晶体的荧光均来自于Ce^3+离子的5d-4f跃迁.荧光强度与泵浦光功率之间的依赖关系揭示了Ce^3+:YAP和Ce^3+:LSO晶体的上转换过程皆由三光子吸收过程所主导.分析表明,Ce^3+:YAP和Ce^3+:LSO晶体中的三光子吸收是三光子同时吸收.
Resumo:
通过冷却熔融法制备出铋掺杂的硅酸盐玻璃,这些玻璃具有覆盖1000—1600nm波段的超宽带红外发光,荧光的半高宽(FWHM)超过200nm;荧光寿命超过400μs;荧光强度随着玻璃碱性的增加而减弱。荧光峰随碱性氧化物的种类不同而移动。除了红外发光,还观察到了发光峰在640m左右的可见发光。640m的可见发光和红外发光有可能来源于同一种发光离子。认为红外发光源于低价态铋离子。铋掺杂的硅酸盐玻璃由于它们的超宽带特性,有可能成为超宽带光纤放大器的增益介质。
Resumo:
基于975nm激发的室温下荧光光谱测量,系统地研究了在新型钠、镱共掺的氟化钙晶体中钠离子的作用机理,分析了掺钠离子浓度与激光阈值的关系,获得了具有最低激光阈值的掺杂浓度优化配比.激光实验表明对于2%Yb^3+离子浓度的氟化钙,掺入3%的钠离子能够获得最低阈值的激光运转,这与理论和荧光分析完全一致.
Resumo:
利用激光脉冲沉积(PLD)技术在(302)γ-LiAIO2衬底上成功生长了非极性的a面(112^-0)γZnO薄膜.衬底温度为350℃时,薄膜是混合取向(a向和C向),以c面ZnO为主,且晶粒尺寸分布很宽;提高温度达500℃,薄膜变为单一的(1120)取向,摇摆曲线半高宽O.65^o,晶粒尺寸分布趋窄,利用偏振透射谱可以明显看出其面内的各向异性.衬底温度650℃下制备的样品晶粒继续长大,虽然摇摆曲线半高宽变大,但光致发光谱(PL)带边发射峰半高宽仅为105meV,比在350℃,500℃下制备的样品小1/5
Resumo:
In this work, alpha-Al2O3:C, a highly sensitive thermoluminescence dosimetry crystal, was grown by the EFG method in which a graphite heating unit and shield acted as the carbon source during the growth process. The optical, luminescent properties and dosimetric characteristics of the crystal were investigated. The as-grown crystal shows a single glow peak at 536 K, which is associated with Cr3+ ions. After annealing in H-2 at 1673 K for 80 h, the crystal shows a single glow peak at 460 K and a blue emission band at 415 nm. The thermoluminescent response of the annealed crystal shows linear-sublinear-saturation characteristics in the dose range from 5 x 10(-6) to 100 Gy.
Resumo:
High optical quality Lu2SiO5 (LSO) and (Lu0.5Gd0.5)(2)SiO5 (LGSO) laser crystals codoped with Er3+ and Yb3+ have been fabricated by the Czochralski method. Intense upconversion (UC) and infrared emission (1543 nm) are observed under excitation of 975 nm. The luminescence processes are explained and the emission efficiencies are quantitatively obtained by measuring the UC efficiency and calculating the emission cross section. The temperature-dependent optical properties of the crystals are also investigated. Our study indicates that Er3+-Yb3+ : LSO and Er3+-Yb3+: LGSO crystals are promising gain media for developing the solid-state 1.5 mu m optical amplifiers and tunable UC lasers. (c) 2008 American Institute of Physics.
Resumo:
Ytterbium-doped calcium pyroniobate single crystal has been grown for the first time. Spectral properties of Yb: Ca2Nb2O7 were investigated by emission and absorption spectra. Its cooperative luminescence and fluorescence lifetime were also studied. Yb ions in Ca2Nb2O7 showed very broad absorption and emission bandwidth and relatively large absorption and emission cross-sections. Along with other optical properties, this Yb-doped crystal would be a potential self-frequency doubling femtosecond laser gain material. (C) 2007 Published by Elsevier B.V.
Resumo:
以高纯α-Al2O3和石墨为原料,采用温梯法生长了α-Al2O3:C晶体,使用RisΦTL/OSL-DA-15型热释光和光释光仪研究了其热释光和光释光特性.α-Al2O3:C晶体在462K附近有单一热释光峰,发射波长位于410nm.随着辐照剂量的增加,热释光强度逐渐增强,462K的热释光特征峰位置保持不变.α-Al2O3:C晶体的光释光衰减曲线由快衰减和慢衰减两个部分组成,随着辐照剂量的增加,快衰减部分衰减速率变化不大,而慢衰减部分衰减速率加快.在5×10-6—10Gy剂量范围内,α-Al2O3:C晶体的热释光剂量响应呈现良好的线性关系,30Gy时达到饱和;光释光剂量响应在5×10-6—60Gy剂量范围内呈现良好的线性关系,100Gy时达到饱和.与热释光相比,光释光剂量响应具有更高的灵敏度和更宽的线性剂量响应范围.
Resumo:
The electronic structures and absorption spectra for the perfect PbMoO4 crystal and the crystal containing lead vacancy V-Pb(2-) with lattice structure optimized are calculated using density functional theory code CASTEP. The calculated absorption spectra of the PbMoO4 crystal containing V-Pb(2-) exhibit three absorption bands peaking at 2.0 eV (620 nm), 3.0 eV (413 run) and 3.3 eV (375 nm), which are in good agreement with experimental values. The theory predicts that the 390 nm, 430 nm and 580 run absorption bands are related to the existence of V-Pb(2-) in the PbMoO4 crystal.
Resumo:
CO2 laser irradiation experiments on ZnO thin films are reported. The structural, optical, luminescent and vibrational properties of the samples were investigated by X-ray diffraction (XRD), transmittance, photoluminescence (PL) and Raman measurements. XRD results show that the crystalline of the irradiated films was improved. The (002) peaks of irradiated ZnO films shift to. higher 20 angles due to the stress relaxation in the case of laser beam irradiation. From optical transmittance spectra, all films exhibit high transmittance in the visible range, the optical band edge of irradiated films showed a redshift compared with that of as-grown films. Compared with the as-grown films, the photoluminescence emission (in particular the relative intensities of visible emissions) intensities of irradiated samples enhanced. In the Raman scattering spectral both the A I. and E modes exhibited slight Raman blueshift. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
The optical absorption edge and ultraviolet (UV) emission energy of ZnO films deposited by direct current (DC) reactive magnetron sputtering at room temperature have been investigated. With the oxygen ratio increasing, the structure of films changes from zinc and zinc oxide coexisting phase to single-phase ZnO and finally to the highly (002) orientation. Both the grain size and the stress of ZnO film vary with the oxygen partial pressure. Upon increasing the oxygen partial pressure in the growing ambient, the visible emission in the room-temperature photoluminescence spectra was suppressed without sacrificing the band-edge emission intensity in the ultraviolet region. The peaks of photoluminescence spectra were located at 3.06---3.15 eV. From optical transmittance spectra of ZnO films, the optical band gap edge was observed to shift towards shorter wavelength with the increase of oxygen partial pressure.
Resumo:
O objetivo deste trabalho foi investigar amostras do tipo MgSiO dopadas com 1,0% e 5,0% de Mn2+, obtidas em temperatura ambiente que luminesceram na faixa do vermelho. As amostras foram produzidas por reação de estado sólido sob alta temperatura e caracterizadas e pelo método de difração de raios X. Para análise das características físicas presentes na amostra após a dopagem, usamos a espectroscopia de fotoluminescência. Através da teoria do campo cristalino, dos espectros de luminescência e excitação e com a ajuda do diagrama e das matrizes de Tanabe-Sugano, foi possível identificar as luminescências, os níveis de energia excitados, os parâmetros de energia do campo cristalino, os parâmetros de Racah e a simetria do sítio ocupado por Mn2+.
Resumo:
23rd Congress of the International Comission for Optics (ICO 23)