831 resultados para Biodegradable


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The concept behind a biodegradable ligament device is to temporarily replace the biomechanical functions of the ruptured ligament, while it progressively regenerates its capacities. However, there is a lack of methods to predict the mechanical behaviour evolution of the biodegradable devices during degradation, which is an important aspect of the project. In this work, a hyper elastic constitutive model will be used to predict the mechanical behaviour of a biodegradable rope made of aliphatic polyesters. A numerical approach using ABAQUS is presented, where the material parameters of the model proposal are automatically updated in correspondence to the degradation time, by means of a script in PYTHON. In this method we also use a User Material subroutine (UMAT) to apply a failure criterion base on the strength that decreases according to a first order differential equation. The parameterization of the material model proposal for different degradation times were achieved by fitting the theoretical curves with the experimental data of tensile tests on fibres. To model all the rope behaviour we had considered one step of homogenisation considering the fibres architectures in an elementary volume. (C) 2012 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The influence of glycerol concentration (C-g), process temperature (T-p), drying temperature (T-s), and relative humidity (RH) on the properties of achira flour films was initially assessed. The optimized process conditions were C-g of 17g glycerol/100g flour, T-p of 90 degrees C, T-s of 44.8 degrees C, and RH of 36.4%. The films produced under these conditions displayed high mechanical strength (7.0 MPa), low solubility (38.3%). and satisfactory elongation values (14.6%). This study showed that achira flour is a promising source for the development of biodegradable films with good mechanical properties, low water vapor permeability, and solubility compared to films based on other tubers. (c) 2011 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this this study, glycerol content and its incorporation method on tensile and barrier properties of biodegradable films (BF) based on cassava starch were analyzed. ANOVA showed that the glycerol incorporation method did not influence the results (P > 0.05), however the glycerol content influenced significantly the tensile and barrier properties of the films (P < 0.05). Films prepared with lower glycerol content presented better tensile and barrier properties than films with higher content. Films were then prepared with addition of clay nanoparticles and their tensile and barrier properties and glass transition temperature were measured. ANOVA indicated that both glycerol and clay nanoparticles influenced significantly the tensile and barrier properties (P < 0.05), diminishing film permeability when clay nanoparticles were present, while the glass transition temperature was not influenced (P > 0.05). (C) 2011 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Aims: The long-term clinical performance of drug-eluting stents (DES) coated with biodegradable polymers is poorly known. Methods and results: A total of 274 coronary patients were randomly allocated to paclitaxel-eluting stents, sirolimus-eluting stents, or bare metal stems (2:2:1 ratio). The two DES used the same biodegradable polymers and were identical except for the drug. At three years, the pooled DES population had similar rates of cardiac death or myocardial infarction (9.0% vs. 7.1; p=0.6), but lower risk of repeat interventions (10.0% vs. 29.9%; p<0.01) than controls with bare stents. The cumulative 3-year incidence of definite or probable stent thrombosis in the pooled DES group was 2.3% (first year: 1.8%; second year: 0.4%; third year: zero). There were no significant differences in outcomes between paclitaxel- and sirolimus-eluting stents. Conclusions: The biodegradable-polymer coated DES releasing either paclitaxel or sirolimus were effective in reducing the 3-year rate of re-interventions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This PhD work was aimed to design, develop, and characterize gelatin-based scaffolds, for the repair of defects in the muscle-skeletal system. Gelatin is a biopolymer widely used for pharmaceutical and medical applications, thanks to its biodegradability and biocompatibility. It is obtained from collagen via thermal denaturation or chemical-physical degradation. Despite its high potential as biomaterial, gelatin exhibits poor mechanical properties and a low resistance in aqueous environment. Crosslinking treatment and enrichment with reinforcement materials are thus required for biomedical applications. In this work, gelatin based scaffolds were prepared following three different strategies: films were prepared through the solvent casting method, electrospinning technique was applied for the preparation of porous mats, and 3D porous scaffolds were prepared through freeze-drying. The results obtained on films put into evidence the influence of pH, crosslinking and reinforcement with montmorillonite (MMT), on the structure, stability and mechanical properties of gelatin and MMT/gelatin composites. The information acquired on the effect of crosslinking in different conditions was utilized to optimize the preparation procedure of electrospun and freeze-dried scaffolds. A successful method was developed to prepare gelatin nanofibrous scaffolds electrospun from acetic acid/water solution and stabilized with a non-toxic crosslinking agent, genipin, able to preserve their original morphology after exposure to water. Moreover, the co-electrospinning technique was used to prepare nanofibrous scaffolds at variable content of gelatin and polylactic acid. Preliminary in vitro tests indicated that the scaffolds are suitable for cartilage tissue engineering, and that their potential applications can be extended to cartilage-bone interface tissue engineering. Finally, 3D porous gelatin scaffolds, enriched with calcium phosphate, were prepared with the freeze-drying method. The results indicated that the crystallinity of the inorganic phase influences porosity, interconnectivity and mechanical properties. Preliminary in vitro tests show good osteoblast response in terms of proliferation and adhesion on all the scaffolds.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Incomplete endothelialization has been found to be associated with late stent thrombosis, a rare but devastating phenomenon, more frequent after drug-eluting stent implantation. Optical coherence tomography (OCT) has 10 times greater resolution than intravascular ultrasound and thus appears to be a valuable modality for the assessment of stent strut coverage. The LEADERS trial was a multi-centre, randomized comparison of a biolimus-eluting stent (BES) with biodegradable polymer with a sirolimus-eluting stent (SES) using a durable polymer. This study sought to evaluate tissue coverage and apposition of stents using OCT in a group of patients from the randomized LEADERS trial.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This study reports the 12-month clinical outcomes of the LEADERS clinical trial which compared a biolimus eluting stent with a biodegradable polymer (BES) to a sirolimus eluting stent with a durable polymer (SES).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Background The effectiveness of durable polymer drug-eluting stents comes at the expense of delayed arterial healing and subsequent late adverse events such as stent thrombosis (ST). We report the 4 year follow-up of an assessment of biodegradable polymer-based drug-eluting stents, which aim to improve safety by avoiding the persistent inflammatory stimulus of durable polymers. Methods We did a multicentre, assessor-masked, non-inferiority trial. Between Nov 27, 2006, and May 18, 2007, patients aged 18 years or older with coronary artery disease were randomly allocated with a computer-generated sequence to receive either biodegradable polymer biolimus-eluting stents (BES) or durable polymer sirolimus-eluting stents (SES; 1:1 ratio). The primary endpoint was a composite of cardiac death, myocardial infarction, or clinically-indicated target vessel revascularisation (TVR); patients were followed-up for 4 years. Analysis was by intention to treat. This trial is registered with ClinicalTrials.gov, number NCT00389220. Findings 1707 patients with 2472 lesions were randomly allocated to receive either biodegradable polymer BES (857 patients, 1257 lesions) or durable polymer SES (850 patients, 1215 lesions). At 4 years, biodegradable polymer BES were non-inferior to durable polymer SES for the primary endpoint: 160 (18·7%) patients versus 192 (22·6%) patients (rate ratios [RR] 0·81, 95% CI 0·66–1·00, p for non-inferiority <0·0001, p for superiority=0·050). The RR of definite ST was 0·62 (0·35–1·08, p=0·09), which was largely attributable to a lower risk of very late definite ST between years 1 and 4 in the BES group than in the SES group (RR 0·20, 95% CI 0·06–0·67, p=0·004). Conversely, the RR of definite ST during the first year was 0·99 (0·51–1·95; p=0·98) and the test for interaction between RR of definite ST and time was positive (pinteraction=0·017). We recorded an interaction with time for events associated with ST but not for other events. For primary endpoint events associated with ST, the RR was 0·86 (0·41–1·80) during the first year and 0·17 (0·04–0·78) during subsequent years (pinteraction=0·049). Interpretation Biodegradable polymer BES are non-inferior to durable polymer SES and, by reducing the risk of cardiac events associated with very late ST, might improve long-term clinical outcomes for up to 4 years compared with durable polymer SES. Funding Biosensors Europe SA, Switzerland.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Biolimus-eluting stents (BESs) with a biodegradable polymer in abluminal coating achieve more complete coverage at 9 months compared with sirolimus-eluting stents (SESs) with a durable polymer, as assessed by optical coherence tomography (OCT). Whether this advantage persists or augments after complete resorption of the polymer (>12 months) is unknown.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Aims: The current study reports clinical outcomes at three year follow-up of the LEADERS clinical trial which was the first all-comers trial comparing a new generation biodegradable polymer biolimus drug-eluting stent (BES) with the first generation permanent polymer sirolimus-eluting stent (SES). Methods and results: One thousand seven hundred and seven patients were randomised to unrestricted use of BES (n=857) or SES (n=850) in an all-comers population. Three year follow-up was available in 95% of the patients, 812 treated with BES and 809 treated with SES. At three years, BES remains non-inferior to SES for the primary endpoint of major adverse cardiac events (composite of cardiac death, myocardial infarction (MI), or clinically-indicated target vessel revascularisation (CI-TVR) (BES 15.7% versus SES 19%; HR 0.82 CI 0.65-1.03; p=0.09). The MACE Kaplan Meier event curves increasingly diverge with the difference in events increasing from 1.4% to 2.4% and 3.3% at 1, 2 and 3 years, respectively in favour of BES. The rate of cardiac death was non-significantly lower 4.2% versus 5.2% (HR=0.81 CI 0.52-1.26; p=0.34) and the rate of myocardial infarction was equivalent 7.2% versus 7.1% (HR 1.01 CI 0.70-1.44; p=0.97) for BES versus SES, respectively. Thus BES was non-inferior to SES in all the safety endpoints. Clinically-indicated TVR occurred in 9.4% of BES treated patients versus 11.1% of SES treated patients (HR 0.84 CI 0.62-1.13; p=0.25). Rates of definite stent thrombosis were 2.2% for BES and 2.9% for SES (HR 0.78 CI 0.43-1.43; p=0.43), with the event rate increase of 0.2% from one to three years for BES and 0.9% for SES. For patients presenting with ST-elevation myocardial infarction BES was superior to SES in reducing MACE. Conclusions: The findings of the three year follow-up support the claim that the biodegradable polymer biolimus-eluting stent has equivalent safety and efficacy to permanent polymer sirolimus-eluting stent in an all-comers patient population. Its performance is superior in some subpopulations such as in ST-elevation MI patients and event rates for BES are overall lower than for SES with a trend toward increasing divergence of outcomes over three years. - See more at: http://www.pcronline.com/eurointervention/42nd_issue/125/#sthash.E5HhMQ4a.dpuf

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Background: The SYNTAX score (SXscore) has been shown to be an effective predictor of clinical outcomes in patients undergoing percutaneous coronary intervention (PCI). Methods and results: The SXscore was prospectively collected in 1,397 of the 1,707 patients enrolled in the “all-comers” LEADERS trial (patients post-surgical revascularisation were excluded). Post hoc analysis was performed by stratifying clinical outcomes at two-year follow-up, according to one of three SXscore tertiles: SXlow ≤8 (n=464), 816 (n=461). At two-year follow-up the rate of major adverse cardiovascular events was 18.4%, 12.0% and 9.4% in the SXhigh, SXmid, and SXlow tertile, respectively (HR 1.45; CI 1.21-1.74; p<0.01). There was a significantly higher rate of cardiac death in patients in the highest SXscore tertile (7% SXhigh versus 2.4% SXmid versus 1.8% SXlow; HR 2.22; CI 1.5-3.27; p<0.001). Within the SXhigh tertile the rate of cardiac death was significantly lower in patients treated with the biolimus-eluting stent compared with the sirolimus-eluting stent (4.7% versus 9.6%, HR 0.48; CI 0.23-0.99; p=0.046). Conclusions: The SXscore when applied to an “all-comers” patient population allows for prospective risk stratification of patients undergoing PCI up to two years follow-up. In addition, the SXscore appears to separate the performance of devices in high risk patient groups.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objectives This study sought to investigate safety and efficacy of biolimus-eluting stents (BES) with biodegradable polymer as compared with sirolimus-eluting stents (SES) with durable polymer through 2 years of follow-up. Background BES with a biodegradable polymer provide similar efficacy and safety as SES with a durable polymer at 9 months. Clinical outcomes beyond the period of biodegradation of the polymer used for drug release and after discontinuation of dual antiplatelet therapy are of particular interest. Methods A total of 1,707 patients were randomized to unrestricted use of BES (n = 857) or SES (n = 850) in an all-comers patient population. Results At 2 years, BES remained noninferior compared with SES for the primary endpoint, which was a composite of cardiac death, myocardial infarction, or clinically indicated target vessel revascularization (BES 12.8% vs. SES 15.2%, hazard ratio [HR]: 0.84, 95% confidence interval [CI]: 0.65 to 1.08, pnoninferiority < 0.0001, psuperiority = 0.18). Rates of cardiac death (3.2% vs. 3.9%, HR: 0.81, 95% CI: 0.49 to 1.35, p = 0.42), myocardial infarction (6.3% vs. 5.6%, HR: 1.12, 95% CI: 0.76 to 1.65, p = 0.56), and clinically indicated target vessel revascularization (7.5% vs. 8.6%, HR: 0.86, 95% CI: 0.62 to 1.20, p = 0.38) were similar for BES and SES. The rate of definite stent thrombosis through 2 years was 2.2% for BES and 2.5% for SES (p = 0.73). For the period between 1 and 2 years, event rates for definite stent thrombosis were 0.2% for BES and 0.5% for SES (p = 0.42). After discontinuation of dual antiplatelet therapy, no very late definite stent thrombosis occurred in the BES group. Conclusions At 2 years of follow-up, the unrestricted use of BES with a biodegradable polymer maintained a similar safety and efficacy profile as SES with a durable polymer. (Limus Eluted From a Durable Versus Erodable Stent Coating [LEADERS]; NCT00389220)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The efficacy of durable polymer drug-eluting stents (DES) is delivered at the expense of delayed healing of the stented vessel. Biodegradable polymer DES aim to avoid this shortcoming and may potentially improve long-term clinical outcomes, with benefit expected to accrue over time. We sought to compare long-term outcomes in patients treated with biodegradable polymer DES vs. durable polymer sirolimus-eluting stents (SES).