990 resultados para Er:Yb:glass


Relevância:

20.00% 20.00%

Publicador:

Resumo:

ZnO films are prepared on glass substrates by pulsed laser deposition (PLD) at different oxygen pressures, and the effects of oxygen pressure on the structure and optoelectrical properties of as-grown ZnO films are investigated. The results show that the crystallite size and surface roughness of the films increase, but the carrier concentration and optical energy gap E-g decrease with increasing oxygen pressure. Only UV emission is found in the photoluminescence (PL) spectra of all the samples, and its intensity increases with oxygen pressure. Furthermore, there are marked differences in structure and properties between the films grown at low oxygen pressures (0.003 and 0.2 Pa) and the films grown at high oxygen pressures (24 and 150 Pa), which is confirmed by the fact that the crystallite size and UV emission intensity markedly increase, but the carrier concentration markedly decreases as oxygen pressure increases from 0.2 to 24 Pa. These results show that the crystal quality, including the microstructural quality and stoichiometry proportion, of the prepared ZnO films improves as oxygen pressure increases, particularly from 0.2 to 24 Pa.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This letter reports on the Raman, optical and magnetic properties of FeNi co-doped ZnO nanowires prepared via a soft chemical solution method. The microstructural investigations show that the NiFe co-dopants are substituted into wurtzite ZnO nanostructure without forming any secondary phase. The co-doped nanowires show a remarkable reduction of 34 nm (267.9 meV) in the optical band gap, while suppression in the deep-level defect transition in visible luminescence. Furthermore, these nanowires exhibit ferromagnetism and an interesting low-temperature spin glass behavior, which may arise due to the presence of disorder and strong interactions of frustrated spin moments of Ni and Fe co-dopants on the ZnO lattice sites. Copyright (C) EPLA, 2009

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Raman measurements and photoluminescence (PL) were performed on the metal-organic chemical-vapor deposition epitaxially grown GaN before and after the implantation with Er and Er+O. Several Raman defect modes have emerged from the implantation-damaged samples. The structures around 300 and 595 cm(-1) modes are attributed to the disorder-activated Raman scattering, whereas the 670 cm(-1) peak is assigned to nitrogen-vacancy-related defect scattering. One additional peak at 360 cm(-1) arises after Er+O coimplantation. This Raman peak is attributed to the O-implantation-induced defect complex. The appearance of the 360 cm(-1) mode results in the decrease of the Er3+ -related infrared PL intensity for the GaN:Er+O samples. (C) 2004 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this study, we report the dependences of infrared luminescence properties of Er-implanted GaN thin films (GaN:Er) on the kinds of substrates used to grow GaN, the growth techniques of GaN, the implantation parameters and annealing procedures. The experimental results showed that the photoluminescence (PL) intensity at 1.54 mum was severely influenced by different kinds of substrates. The integrated PL peak intensity from GaN:Er /Al2O3 (00001) was three and five times stronger than that from GaN:Er /Si (111) grown by molecular beam epitaxy (MBE) and by metalorganic chemical vapor deposition (MOCVD), respectively. The PL spectra observed from GaN:Er/Al2O3 (0001) grown by MOCVD and by MBE displayed a similar feature, but those samples grown by MOCVD exhibited a stronger 1.54 mum PL. It was also found that there was a strong correlation between the PL intensity with ion implantation parameters and annealing procedures. Ion implantation induced damage in host material could be only partly recovered by an appropriate annealing temperature procedure. The thermal quenching of PL from 15 to 300 K was also estimated. In comparison with the integrated PL intensity at 15 K, it is reduced by only about 30 % when going up to 300 K for GaN:Er/Al2O3 sample grown by MOCVD. Our results also show that the strongest PL intensity comes from GaN:Er grown on Al2O3 substrate by MOCVD. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report the technique of the ion-implanted semi-insulating GaAs wafer used for passive Q-switched mode locking in double-cladding Yb:fiber laser. The wafer was implanted with 400-keV energy, 10(16)/cm(2) dose As+ ions, and was annealed at 600degreesC for 20 min. At the pump power of 5W, we achieved output power of 200mW. The repetition rate of envelope of Q-switched mode locking is 50-kHz with a FWHM envelope of 4mus. The repetition rate of mode locked pulse train was found to be 15-MHz. This is the first report of such a kind of laser to the best of our knowledge.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report on recent experimental results of the spontaneous antiphase dynamics that occurs in a laser-diode-pumped multimode passively Q-switched microchip Yb:YAG (where YAG is yttrium aluminum garnet) lasers with a saturable absorber GaAs. We observe that the pulse sequence of the first mode characterized by one, two, and three pulses as a group and all the modes display an antiphase state as the pumping ratio rises. We modify the multimode rate equations to account for nonlinear absorption due to GaAs in the presence of spatial hole burning. We perform numerical simulations based on the proposed rate equations and reproduce the observed antiphase state of two and three active modes.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Erbium was implanted with energies 200 or 400 keV into epitaxial (0 0 0 1) GaN grown on (0 0 0 1) Al2O3 substrate at room temperature (RT) and 400degreesC. Both random (10degrees tilt from c-axis) and channeled (along c-axis) implantations were studied. RBS/Channeling technique was used to study the dependences of the radiation damage with ion implantation energy, direction and temperature. It was found that the channeling implantation or elevating temperature implantation both resulted in the decrease of the damage. Moreover, the Photoluminscence (PL) properties of Er-implanted GaN thin filius were also studied. The experimental results indicate that the PL intensity can be enhanced by raising implantation energy or implanting along channeling direction. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Er photoluminescence (Er PL) and dangling bonds (DBs) of annealed Er-doped hydrogenated amorphous silicon nitride (a-SiN:H(Er)) with various concentrations of nitrogen are studied in the temperature range 62-300 K. Post-annealing process is employed to change the DBs density of a-SiN:H(Er). PL spectra, DBs density and H, N concentrations are measured. The intensity of Er PL displays complicated relation with Si DBs density within the annealing temperature range 200-500 degreesC. The intensity of Er PL first increases with decreasing density of Si dangling bonds owing to the structural relaxation up to 250 degreesC, and continues to increase up to 350 degreesC even though the density of Si DBs increases due to the improvement of symmetry environment of Er3+. (C) 2003 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this work, The TBS glass microspheres doped with Er3+ for morphology-dependent resonances of upconversion emission were designed. The glass sample components are 25TiO(2)-27BaCO(3)-8Ba(NO3)(2)-6ZnO(2)-9CaCO(3)-5H(3)BO(3)-10SiO(2)-7water glass-3Er(2)O(3) (wt%), and the emission spectra of TBS glass and a TBS glass microsphere (about 48 mum in diameter) were measured under 633 nm excitation and discussed. The strong morphology-dependent resonances of upconversion luminescences in the microsphere were observed. The observed resonances could be assigned by using the well-known Lorenz-Mie Formalism. (C) 2003 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Antiphase dynamics has been observed experimentally for the laser modes operation in a laser-diode-pumped Q-switched microchip Yb:YAG laser with GaAs as a saturable absorber in the presence of spatial hole-burning. The Q-switched pulses sequences of two modes at different pump power have been obtained. The experimental results have shown that the pulses sequences displayed classic antiphase dynamics. (C) 2003 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Diode-pumped passively mode-locked laser operation of Yb3+,Na+:CaF2 single crystal has been demonstrated for the first time. By using a SESAM ( semiconductor saturable mirror), simultaneous transform-limited 1-ps passively mode-locked pulses, with the repetition rate of 183MHz, were obtained under the self-Q-switched envelope induced by the laser medium. The average output power of 360mW was attained at 1047nm for 3.34W of absorbed power at 976nm, and the corresponding pulse peak power arrived at 27kW, indicating the promising application of Yb3+,Na+-codoped CaF2 crystals in achieving ultra-short pulses and high pulse peak power. (c) 2005 Optical Society of America.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Hall, current-voltage, and deep-level transient spectroscopy measurements were used to characterize the electrical properties of metalorganic chemical vapor deposition grown undoped, Er- and Pr-implanted GaN films. Only one deep level located at 0.270 eV below the conduction band was found in the as-grown GaN films. However, four defect levels located at 0.300, 0.188, 0.600, and 0.410 eV below the conduction band were found in the Er-implanted GaN films after annealing at 900 degrees C for 30 min, and four defect levels located at 0.280, 0.190, 0.610, and 0.390 eV below the conduction band were found in the Pr-implanted GaN films after annealing at 1050 degrees C for 30 min. The origins of the deep defect levels are discussed. (C) 2005 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The structure and magnetic properties of the RCo5Ga7 (R = Y, Tb, Dy, Ho and Er) compounds with the ScFe6Ga6-type structure have been studied. The stability of RCo5Ga7 is closely related with the ratio of the metal radii R-RE/R-(Co,R-Ga). With R-RE/R-(Co,R-Ga) less than or equal to 1.36, the compounds can be stabilized in the ScFe6Ga6-type structure. The lattice of RCo5Ga7 shrinks as the atomic order of R increases, and it is consistent with the lanthanide contraction. The structure analysis based on X-ray diffraction patterns reveals that in the orthorhombic RCo5Ga7 (Immm), R occupies the 2a site, and Co enters into the 8k and the 4h sites, and Ga is at the 4e, 4f, 4g, 4h and 8k sites. The interatomic distances and the coordination numbers of RCo5Ga7 are provided from the refinement results. The short interatomic distance (less than 2.480 Angstrom) between the Co ions results in the negative magnetic interaction, which does not favor ferromagnetic ordering. The magnetic moment of YCo5Ga7 is absent, and RCo5Ga7 (R = Tb, Dy, Ho and Er) may have long-range magnetic ordering with the paramagnetic Curie temperature lower than 5 K. (C) 2004 Elsevier Inc. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

C-axis-orientated ZnO thin films were prepared on glass substrates by pulsed-laser deposition (PLD) technique in an oxygen-reactive atmosphere, using a metallic Zn target. The effects of growth condition such as laser energy and substrate temperature on the structural and optical properties of ZnO films had been investigated by X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission spectra and room-temperature (RT) photoluminescence (PL) measurements. The results showed that the thickness, crystallite size, and compactness of ZnO films increased with the laser energy and substrate temperature. Both the absorption edges and the UV emission peaks of the films exhibited redshift, and UV emission intensity gradually increased as the laser energy and substrate temperature increased. From these results, it was concluded that crystalline quality of ZnO films was improved with increasing laser energy and substrate temperature. (c) 2007 Elsevier B.N. All rights reserved.