944 resultados para Tool wear
Resumo:
We measured the wear resistances of alumina, alumina/silicon carbide composite and alumina/mullite composite by abrasive wear. And we studied the influence of fracture mode and worn surface pullout on wear resistance. The results are as follows: the main wear mechanisms of alumina and alumina/silicon carbide were fracture wear and plastic wear respectively, and for alumina/mullite composite, fracture wear and plastic wear mechanisms worked together. The wear resistance of the alumina/silicon carbide composite and the alumina/mullite composite was better by a factor of 1 similar to 3 than that of the monolithic alumina. There were two main reasons for the better wear resistance, i.e., the improved mechanical properties and the more smooth worn surfaces. However, The primary reason was the reduction of area fraction of pullout on the worn surfaces induced by fracture mode transition. (C) 2007 Published by Elsevier B.V.
Resumo:
Alumina and alumina/mullite composites with mullite content of 0.96-8.72 vol.% were subjected to an abrasive wear test under loads of 0.1-2.0 N with a ball-on-disc apparatus. The wear rate and area fraction of pullout f(po) on the worn surfaces were measured. The wear resistances of the alumina/mullite composites were better by a factor of 1-2 than that of pure alumina. The main wear mechanism of alumina is fracture wear, and for alumina/mullite composites, fracture wear and plastic wear mechanisms work together. The influence of mechanical properties on wear resistance was estimated by Evans' method. It was found that the wear rate depends on f(po), and the primary reason for the better wear resistance of alumina/mullite composites is the reduction off, induced by fracture mode transition. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
A multi-mode logic cell architecture in a tile-based heterogeneous FPGA is proposed, and a logic synthesis tool, called Vsyn, based on this architecture is presented. The logic cell architecture design and its synthesis tool development are strongly influencing each other. Any feature or parameter from one needs to be fully exercised and verified on the other. In this paper, we presented experimental results based MCNC benchmarks to show that the integration of the synthesis tool and the FPGA architecture can achieve high performance in the targeted FPGA applications. In addition, Vsyn can also target embedded special-purpose macros for the heterogeneous FPGA.
Resumo:
Combinatorial testing is an important testing method. It requires the test cases to cover various combinations of parameters of the system under test. The test generation problem for combinatorial testing can be modeled as constructing a matrix which has certain properties. This paper first discusses two combinatorial testing criteria: covering array and orthogonal array, and then proposes a backtracking search algorithm to construct matrices satisfying them. Several search heuristics and symmetry breaking techniques are used to reduce the search time. This paper also introduces some techniques to generate large covering array instances from smaller ones. All the techniques have been implemented in a tool called EXACT (EXhaustive seArch of Combinatorial Test suites). A new optimal covering array is found by this tool.
Resumo:
Coupling with bionic principles, an attempt to improve the wear resistance of ball bearing steel (GCr15) with biomimetic units on the surface was made using a pulsed Nd: YAG laser. Air and water film was employed as processing medium, respectively. The microstructures of biomimeitc units were examined by scanning electron microscope and X-ray diffraction was used to describe the microstructure and identify the phases as functions of different mediums as well as water film with different thicknesses. The results indicated that the microstructure zones in the biomimetic specimens processed with water film were more refined and had better wear resistance increased by 55.8% in comparison with that processed in air; a significant improvement in microhardness was achieved by laser surface melting. The application of water film provided considerable microstructural changes and much more regular grain shape in biomimetic units, which played a key role in improving the wear resistance of ball bearing steel. (c) 2010 Elsevier B.V. All rights reserved.
Resumo:
Dry sliding tests were performed on as-cast magnesium alloys Mg97Zn1Y2 and AZ91 using a pin-on-disc configuration. Coefficients of friction and wear rates were measured within a load range of 20-380 and 20-240 N at a sliding velocity of 0.785 m/s. X-ray differactometer, scanning electron microscopy, tensile testing machine were used to characterize the microstructures and mechanical properties of Mg97Zn1Y2 alloy and AZ91 alloy. Worn surface morphologies of Mg97Zn1Y2 and AZ91 were examined using scanning electron microscopy.
Resumo:
A promising method for assembling carbon nanotubes (CNTs) and poly(diallyldimethylammonium chloride) protected Prussian blue nanoparticles (P-PB) to form three-dimensional (3D) nanostructured films is proposed. The electrostatic interaction, combined with layer-by-layer self-assembly (LBL), between negatively charged CNTs and positively charged P-PB is strong enough to drive the formation of the 3D nanostructured films. Thus, prepared multilayer films were characterized by ultraviolet-visible-near-infrared spectroscopy (UV-vis-NIR), scanning electron microscopy (SEM) and cyclic voltammetry (CV).
Resumo:
A wear mechanism map of uncoated high-speed steel (HSS) tools was constructed under the conditions of dry-drilling die-cast magnesium alloys. Three wear mechanisms appear in the map based on the microanalysis of drilled HSS tools by SEM, including adhesive wear, abrasive wear and diffusion wear. In the map, there exists a minor wear region which is called "safety zone". This wear mechanism map will be a good reference for choosing suitable drilling parameters when drilling die-cast magnesium alloys.
Resumo:
Nanometer-scale plowing friction and wear of a polycarbonate thin film were directly measured using an atomic force microscope (AFM) with nanoscratching capabilities. During the nanoscratch tests, lateral forces caused discrepancies between the maximum forces for the initial loadings prior to the scratch and the unloading after the scratch. In the case of a nanoscratch test performed parallel to the cantilever probe axis, the plowing friction added another component to the moment acting at the cantilevered end compared to the case of nanoindentation, resulting in an increased deflection of the cantilever. Using free-body diagrams for the cases of nanoindentation and nanoscratch testing, the AFM force curves were analyzed to determine the plowing friction during nanoscratch testing. From the results of this analysis, the plowing friction was found to be proportional to the applied contact force, and the coefficient of plowing friction was measured to be 0.56 +/- 0.02. Also, by the combination of nanoscratch and nanoindentation testing, the energetic wear rate of the polycarbonate thin film was measured to be 0.94 +/- 0.05 mm(3)/(N m).
Resumo:
The main characteristics of structural relaxation and the associated Tool-Narayanaswamy-Moynihan (TNM) model are thoroughly introduced, The structural relaxation of an inorganic glass (Li2O . 2SiO(2)) at different aging temperatures and aging times is found to be well modeled by the TNM model.
Resumo:
A FeNiSiBV amorphous composite coating was developed by laser cladding of metallic powders on AISI 1020 low carbon steel substrate. The coatings were studied using X-ray diffraction, transmission electron microscopy and scanning electron microscopy. The coating reveals different microstructures along the depth of the coating. The transition zone exhibits good metallurgical bonding between the substrate and the coating. The layer consists of amorphous phase in majority and nanocrystalline phase/crystalline phase in minority. Accompanied with the nanocrystalline phase, the amorphous phase is concentrated in the middle of the coating. The crystalline phase in the coating is identified as Fe2B. A gradient distribution of the microhardness ranges from 1208 HV0.2 to 891 HV0.2 in the coating along the depth. The coating shows higher microhardness and better wear property than the substrate.
Resumo:
The effect of Cl- on the corrosive wear behaviour of AISI 321 stainless steel in H2SO4 solution was studied via the corrosive wear rate, the load bearing capacity of passive film and the relationship between pitting and corrosive wear. There is a critical load at natural potential, below which the corrosive wear rate is slightly lowered by Cl-, while above which is increased. At natural potential there are more pits at low load than that at a higher one in the wear tracks and the pits are also deeper. The load bearing capacity is lowered by Cl- at passive region and then the corrosive wear rate increased.
Resumo:
The method for the measurement of the pure mechanical wear loss for 321 stainless steel, 1045 steel and pure iron in the study of the synergy between corrosion and wear was studied, The methods studied included the measurement in distilled water, by cathodic protection and by adding inhibitor KI, and all were compared with the wear loss in air. The experiment showed that the pure mechanical wear losses and friction coefficients obtained by the three methods were close to each other and can be used to calculate the various wear components in the study of the interaction of corrosion and wear, but the measurements in distilled water for pure iron and 1045 steel are not recommended due to their corrosion.