989 resultados para Ferroelectric polarization
Resumo:
This article reports systematic results of corona poling measurements obtained on biaxially stretched polyvinylidene fluoride films charged in dry air. Charging was performed using the constant current corona triode. The dependence of the poling process on the sample thickness, charging current, and successive charging processes was investigated. Phase transitions from alpha to delta and to beta phases were observed when virgin samples were corona charged. The thermal pulse technique showed that the polarization profiles during charging can be made consistently almost uniform and that the ferroelectric reorientation can be associated with the rising plateau region displayed on potential buildup curves. (C) 1995 American Institute of Physics.
Resumo:
The pattern of availability of free DNA phosphates, and the kind of DNA-protein complex arrangement, both induced by nuclear basic proteins, and the richness in arginine residues in these proteins were investigated cytochemically and cytophysically in spermatozoa of the South-American Hylidae species, Hyla fuscovaria and Hyla biobeba. The aim was to demonstrate differences at the level of sperm histones in two species of Hyla until recently considered to be congeneric. The results indicated differences in the spermatozoal nuclear basic proteins and DNA-protein complexes when the two species were compared. The spermatozoa of Hyla biobeba were assumed to be likely to contain a Bloch's ''type 3'' protein type (intermediate sperm basic protein), similarly to Hyla species of North and Central America. on the other hand, the data obtained for the spermatozoa of Hyla fuscovaria indicated that they contain a protamine or protamine-like protein, differing from Hyla biobeba and Hyla species of North and Central America. It is suggested that the differences reported here may be genus-specific, since Hyla fuscovaria has recently been reclassified as Scinax fuscovaria based on parameters other than sperm histone types. These findings are in agreement with the general view of a wide variability in sperm nuclear proteins in the Anura group.
Resumo:
Ferroelectric SrBi2Nb2O9 (SBN) thin films were prepared by the polymeric precursors method and deposited by spin coating onto Pt/Ti/SiO2/Si substrate and crystallized using a domestic microwave oven. It was studied the influence of the heat flux direction and the duration of the thermal treatment on the films crystallization. An element with high dielectric loss, a SiC susceptor, was used to absorb the microwave energy and transfers the heat to the film. Influence of the susceptor position to the sample crystallization was verified, the susceptor was, placed or below the substrate or above the film. The SBN perovskite phase was observed after a thermal treatment at 700 degreesC for 10 min when the susceptor was placed below the substrate and for 30 min when the susceptor was placed above the film. Electrical measurements revealed that the film crystallized at 700 degreesC for 10 min, with the susceptor placed below the film, presented dielectric constant, dielectric loss, remanent polarization and coercive field of, 67, 0.011, 4.2 muC/cm(2) and 27.5 kV/cm, respectively. When the films were crystallized at 700 degreesC for 30 min, with the susceptor placed above the film, the dielectric constant was 115 and the dissipation factor was around of 0.033, remanent polarization and coercive field were 10.8 muC/cm(2) and 170 kV/cm, respectively. (C) 2003 Elsevier B.V. All rights reserved.
SrBi2Ta2O9 ferroelectric thick films prepared by electrophoretic deposition using aqueous suspension
Resumo:
SrBi2Ta2O9 ferroelectric thick films were prepared by electrophoretic deposition (EPD). For that, ceramic powders were prepared by chemical method in order to obtain compounds with chemical homogeneity. The polymeric precursor method was used for the synthesis of the SrBi2Ta2O9 powder. The crystallographic structure of the powder was examined by X-ray diffraction, and the surface area was determined by single point BET adsorption. The 0.03 vol.% suspension was formed by dispersing the powder in water using two different polymers as dispersants: an ester polyphosphate (C213) and an ammonium polyacrilate (Darvan 821-A). It was investigated the influence of the different dispersants in the surface properties of the powder by zeta potential measurements. The films were deposited on platinum-coated alumina and Pt/Ti/SiO2/Si substrates by a 4 mA constant current, for 10 min, using two parallel electrodes placed at a separation distance of 3 min in the suspension. Several cycles of deposition-drying of the deposit were carried out until reaching the desired thickness. After thermal treatment at temperatures ranging from 700 to 1000 degreesC, the films were characterized by X-ray diffraction and scanning electron microscopy for the microstructure observation. (C) 2003 Elsevier Ltd. All rights reserved.
Resumo:
In this study, the effect of bismuth content on the crystal structure, morphology and electric properties of barium-bismuth-tantalate (BBT) ceramics was explored with the aid of X-ray diffraction (XRD), scanning electron microcopy (SEM), dielectric properties and ferroelectric hysteresis loops. BaBi2Ta2O9 (BBT) ceramics have been successfully prepared by the solid-state reaction. The BBT phase was crystallized at 900 degreesC for 2 h. The excess of bismuth controls the grain size, affecting the density of the material. Measurements of dieletric constant and dieletric losses confirm that the material is a ferroeletric with a Curie temperature around 77 degreesC. The dieletric constant measured at room temperature was 400, with a dielectric loss of 0.03. Both the phase-transition behaviour and ferroelectric properties, such as spontaneous polarization (P-s), showed a dependence on Bi content. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
PbZr0.3Ti0.7O3 (PZT) films were produced by polymeric precursor route and deposited by spin-coater technique on Pt(111)/Ti/SiO2/Si(100) substrates. The films were heat-treated using different furnaces: (a) a conventional furnace, at 700 degrees C; and (b) a domestic microwave oven, at 600 degrees C. The X-ray patterns revealed that both films are single phase and reflections were identified as belongs to the PZT phase. The intensity of these reflections showed a (111), (001) and (100) preferred orientation. Morphological and electrical characterizations showed that all samples present a rather different microstructure and both with high spontaneous polarization.
Resumo:
Bismuth titanate (Bi4Ti3O12-BIT) films were evaluated for use as lead-free piezoelectric thin-films in micro-electromechanical systems. The films were grown by the polymeric precursor method on Pt/Ti/SiO2/Si (1 0 0) (Pt) bottom electrodes at 700 degrees C for 2 h in static air and oxygen atmospheres. The domain structure was investigated by piezoresponse force microscopy (PFM). Annealing in static air leads to better ferroelectric properties, higher remanent polarization, lower drive voltages and higher piezoelectric coefficient. on the other hand, oxygen atmosphere favors the imprint phenomenon and reduces the piezoelectric coefficient dramatically. Impedance data, represented by means of Nyquist diagrams, show a dramatic increase in the resistivity for the films annealed in static air atmopshere. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
Lanthanum doped bismuth titanate thin films (Bi3.25La0.75Ti3O12-BLT) were produced by the polymeric precursor method and crystallized in a domestic microwave oven and in conventional furnace. Using platinum coated silicon substrates configuration, ferroelectric properties of the films were determined with remanent polarization P-r and a coercive field E-c of 3.9 mu C/cm(2) and 70 kV/cm for the film annealed in the microwave oven and 20 mu C/cm(2) and 52 kV/cm for the film annealed in conventional furnace, respectively. The films annealed in conventional furnace exhibited excellent retention-free characteristics at low infant periods indicating that BLT thin films can be a promise material for use in nonvolatile memories. on the other hand, the pinning of domains wall causes a strong decay at low infant periods for the films annealed in the microwave furnace which makes undesireable the application for future FeRAMS memories. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
In this brief article we discuss spin-polarization operators and spin-polarization states of 2 + 1 massive Dirac fermions and find a convenient representation by the help of 4-spinors for their description. We stress that in particular the use of such a representation allows us to introduce the conserved covariant spin operator in the 2 + 1 field theory. Another advantage of this representation is related to the pseudoclassical limit of the theory. Indeed, quantization of the pseudoclassical model of a spinning particle in 2 + 1 dimensions leads to the 4-spinor representation as the adequate realization of the operator algebra, where the corresponding operator of a first-class constraint, which cannot be gauged out by imposing the gauge condition, is just the covariant operator previously introduced in the quantum theory.
Resumo:
Ferroelectric Bi3.25La0.75Ti3O12 (BLT) thin films were deposited on Pt/Ti/SiO2/Si substrates by the polymeric precursor method. The films present c-axis preferred orientation after annealing at 700 degrees C for 2 h in conventional furnace. All the capacitors showed good polarization fatigue characteristics at least up to 1x10(10) bipolar pulse cycles and excellent retention properties up to 1x10(4) s. We found that the polarization loss is insignificant with five write/read voltages at a waiting time of 10 000 S. Independently of the applied electric field the retained switchable polarization approached a nearly steady-state value after a retention time of 10 s. (C) 2005 American Institute of Physics.
Resumo:
We have studied the phase transition behavior of Pb0.76Ca0.24TiO3 thin films using Raman scattering and dielectric measurement techniques. We also have studied the leakage current conduction mechanism as a function of temperature for these thin films on platinized silicon substrates. A Pb0.76Ca0.24TiO3 thin film was prepared using a soft chemical process, called the polymeric precursor method. The results showed that the dependence of the dielectric constant upon the frequency does not reveal any relaxor behavior. However, a diffuse character-type phase transition was observed upon transformation from a cubic paraelectric phase to a tetragonal ferroelectric phase. The temperature dependency of Raman scattering spectra was investigated through the ferroelectric phase transition. The soft mode showed a marked dependence on temperature and its disappearance at about 598 K. on the other hand, Raman modes persist above the tetragonal to cubic phase transition temperature, although all optical modes should be Raman inactive above the phase transition temperature. The origin of these modes must be interpreted in terms of a local breakdown of cubic symmetry by some kind of disorder. The lack of a well-defined transition temperature suggested a diffuse-type phase transition. This result corroborate the dielectric constant versus temperature data, which showed a broad ferroelectric phase transition in the thin film. The leakage current density of the PCT24 thin film was studied at elevated temperatures, and the data were well fitted by the Schottky emission model. The Schottky barrier height of the PCT24 thin film was estimated to be 1.49 eV. (C) 2003 American Institute of Physics.
Resumo:
SrBi2Ta2O9 thin films, produced by the polymeric precursor method, were crystallized at low temperature using a domestic microwave oven. A SiC susceptor were used to absorb the microwave energy and rapidly transfer the heat to the film. Low microwave power and short time have been used. The films thus obtained are crack-free, well-adhered, and fully crystallized, even when treated at 600 degreesC for 10 min. The microstructure displayed a polycrystalline nature with an elongate grain size comparable to the films obtained by the conventional treatment. The dielectric constant values are 240, 159 and 67, for the films treated at 600 degreesC, 650 degreesC and 700 degreesC, respectively, when the films are placed directly on the SiC susceptor. Electrical measurements revealed that the increase of the temperature treatment to 700 degreesC causes a complete loss of ferroelectricity due to degradation of the bottom interface. A 4 nun-ceramic wool put between the susceptor and the substrate minimizes the interface degradation leading to a dielectric constant, a dielectric loss, and a remnant polarization (2P(r)) of 181 muC/cm(2), 0.032 muC/cm(2), and 12.8 muC/cm(2), respectively, for a film treated at 750 degreesC for 20 min. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
High-quality ABO(3)/LaNiO3 (A = Ph, Ca, Ba; B = Ti, Zr) hetero structures have been grown on LaAlO3 (1 0 0) substrate by the chemical solution deposition method and crystallized by a microwave oven technique. The structural, morphological and electric properties were characterized by means of X-ray diffraction (XRD), atomic force microscope (AFM), and dielectric and ferroelectric measurements. XRD patterns revealed single-phase polycrystalline and oriented thin films whose feature depends on the composition of the films. The AFM surface morphologies showed a smooth and crack-free surface with the average grain size ranging from 116 to 300 nm for both LaNiO3 electrode and the ferroelectric films. Dielectric measurements on these samples revealed dielectric constants as high as 1800 at frequency of 100 KHz. Such results showed that the combination of the chemical solution method with the microwave process provides a promising technique to grow high-quality thin films with good dielectric and ferroelectric properties. (c) 2005 Elsevier Ltd. All rights reserved.
Resumo:
Barium titanate ceramics were prepared through mechanochemical synthesis starting from fresh prepared barium oxide and titanium oxide in rutile form. Mixture of oxides was milled in zirconia oxide jar in the planetary ball-mill during 30, 60, 120 and 240 min. Extended time of milling directed to formation of higher amount of barium titanate perovskite phase. Barium titanate with good crystallinity was formed after 240 min. Sintering without pre-calcinations step was performed at 1330 degrees C for 2 hours with heating rate of 10 degrees C/min. The XRD, DSC, IR and TEM analyses were performed. Electric and ferroelectric properties were studied. Very well defined hysteresis loop was obtained.
Microwave synthesis of calcium bismuth niobate thin films obtained by the polymeric precursor method
Resumo:
The crystal structure, surface morphology and electrical properties of layered perovskite calcium bismuth niobate thin films (CaBi2Nb2O9-CBN) deposited on platinum coated silicon substrates by the polymeric precursor method have been investigated. The films were crystallized in a domestic microwave and in a conventional furnace. X-ray diffraction and atomic force microscopy analysis confirms that the crystallinity and morphology of the films are affected by the different annealing routes. Ferroelectric properties of the films were determined with remanent polarization P-r and a drive voltage V-c of 4.2 mu C/cm(2) and 1.7 V for the film annealed in the conventional furnace and 1.0 mu C/cm(2) and 4.0 V for the film annealed in microwave furnace, respectively. A slight decay after 10(8) polarization cycles was observed for the films annealed in the microwave furnace indicating a reduction of the domain wall mobility after interaction of the microwave energy with the bottom electrode. (C) 2006 Elsevier Ltd. All rights reserved.