1000 resultados para CE3 -DOPED CA2AL2SIO7
Resumo:
Terbium ions were successfully incorporated in nano-sized zinc oxide particles with a doping concentration up to 3% by using a wet chemical route. Four narrow emission peaks of Tb3+ ions and a broad emission band of the surface states on ZnO nano-hosts were observed for all Tb-doped nanoparticles. Relaxation of carriers from excited states of ZnO hosts to rare earth (RE) dopants is disclosed by the fact that the emission intensity of Tb3+ centers increases with increased Tb content at the expense of the emission from surface defect states in ZnO matrix. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
We observed the decrease of the hysteresis effect and the transition from the stable to the dynamic domain regime in doped superlattices with increasing temperature. The current-voltage characteristics and the behaviours of the domain boundary are dominated by the temperature-dependent lineshape of the electric field dependence of the drift velocity (V(F)), As the peak-valley ratio in the V(F) curve decreases with increasing temperature, the hysteresis will diminish and temporal current self-oscillations will occur. The simulated calculation, which takes the difference in V(F) curves into consideration, gives a good agreement with the experimental results.
Resumo:
We report on a detailed investigation on the temperature-dependent behavior of photoluminescence from molecular beam epitaxy (MBE)-grown chlorine-doped ZnSe epilayers. The overwhelming neutral donor bound exciton ((ClX)-X-0) emission at 2.797 eV near the band edge with a full-width at half-maximum (FWHM) of similar to 13 meV reveals the high crystalline quality of the samples used. In our experiments, the quick quenching of the (ClX)-X-0 line above 200 K is mainly due to the presence of a nonradiative center with a thermal activation energy of similar to 90 meV, The same activation energy and similar quenching tendency of the (ClX)-X-0 line and the I-3 line at 2.713 eV indicate that they originate from the same physical mechanism. We demonstrate for the first time that the dominant decrease of the integrated intensity of the I, line is due to the thermal excitation of the "I-3 center"-bound excitons to its free exciton states, leaving the "I-3 centers" as efficient nonradiative centers. The optical performance of ZnSe materials is expected to be greatly improved if the density of the "I-3 center" can be controlled. The decrease in the luminescence intensity at moderately low temperature (30-200 K) of the (ClX)-X-0 line is due to the thermal activation of neutral-donor-bound excitons ((ClX)-X-0) to free excitons. (C) 2000 Published by Elsevier Science B.V.
Resumo:
The hydrogenated amorphous SiOx films (a-SiOx:H) with various oxygen contents have been prepared using plasma enhanced chemical vapor deposition technique. The films were implanted with erbium and annealed by rapid thermal annealing. An intense photoluminescence (PL) of Er at 1.54 mum has been observed at 77 K and at room temperature. The PL intensity depends strongly on both the oxygen content of the film and the rapid thermal annealing temperature and reaches its maximum if the ratio of O/Si in the film is approximately equal to 1.0 at 77 K and to 1.76 at room temperature. The microstructure of the film also has strong influences on the PL intensity. The PL intensity at 250 K is slightly more than a half of that at 15 K. It means that the temperature quenching effect of the PL intensity is very weak.
Resumo:
Photoluminescence (PL) measurements were performed on several series of single-side Si-doped pseudomorphic high electron mobility transistors (p-HEMTs) quantum well (QW) samples, with different spacer layer widths, well widths and Si delta -doped concentrations , under different temperatures and excitation power densities. The dynamic competitive luminescence mechanism between the radiations of e2-hh1 and e1-hh1 was discussed in detail. The confining potential, subband energies, corresponding envelope functions, subband occupations and transferring efficiency etc., were calculated by self-consistent finite differential method at different temperatures in comparison with the present experiment results. The relative variation of the integrated luminescence intensity of the two transitions (e1-hh1 and e2-hh1) was found to be dependent on the temperature and the structure's properties, e. g. spacer layer width, dopant concentration and well width.
Resumo:
In this work we report the photoluminescence (PL) and interband absorption study of Si-modulation-doped multilayer InAs/GaAs quantum dots grown by molecular beam epitaxy (MBE) on (100) oriented GaAs substrates. Low-temperature PL shows a distinctive double-peak feature. Power-dependent PL and transmission electron microscopy (TEM) confirm that they stem from the ground states emission of islands of bimodal size distribution. Temperature-dependent PL study indicates that the family of small dots is ensemble effect dominated while the family of large dots is likely to be dominated by the intrinsic property of single quantum dots (QDs). The temperature-dependent PL and interband absorption measurements are discussed in terms of thermalized redistribution of the carriers among groups of QDs of different sizes in the ensemble. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Hydrogenated amorphous silicon films co-doped with oxygen (O), boron (B) and phosphorus (P) were fabricated using PECVD technique. The erbium (Er) implanted samples were annealed in a N-2 ambient by rapid thermal annealing. Strong photoluminescence (PL) spectra of these samples were observed at room temperature. The incorporation of O, B and P could not only enhance the PL intensity but also the thermal annealing temperature of the strongest PL intensity. It seems that the incorporation of B or P can decrease the grain boundary potential barriers thus leading to an easier movement of carriers and a stronger PL intensity. Temperature dependence of PL indicated the thermal quenching of Er-doped hydrogenated amorphous silicon is very weak.
Resumo:
Eu2+ doped ZnS nanocrystals exhibit new luminescence properties because of the enlarged energy gap of nanocrystalline ZnS host due to quantum confinement effects. Photoluminescence emission at about 520 nm from Eu2+ doped ZnS nanocrystals at room temperature is investigated by using photoluminescence emission and excitation spectroscopy. Such green emission with long lifetime (ms) is proposed to be a result of excitation, ionization, carriers recapture and recombination via Eu2+ centers in nanocrystalline ZnS host.
Resumo:
Manganese doped CdS nanoparticles were synthesized in basic aqueous solution by using mercapto acetate as capping reagents. The nanoparticles were characterized by HRTEM, EPR, photoluminescence and optical absorption measurements. Out of our expectation, doping of Mn2+ ions altered the recombination paths in CdS nanoparticles markedly. The surface stares facilitated PL from Mn2+ doped CdS nanoparticles is reported. A complete suppression of the emission from surface states at room temperature when doping with Mn2+ ions has been observed for the first time. (C) 2000 Elsevier Science Ltd. All rights reserved.
Resumo:
We have observed the transition from static to dynamic electric field domain formation induced by a transverse magnetic field and the sample temperature in a doped GaAs/AlAs superlattice. The observations can be very well explained by a general analysis of instabilities and oscillations of the sequential tunnelling current in superlattices based solely on the magnitude of the negative differential resistance region in the tunnelling characteristic of a single barrier. Both increasing magnetic field and sample temperature change the negative differential resistance and cause the transition between static and dynamic electric field domain formation. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Al-related DX-like centers were observed in n-type Al-doped ZnS1-xTex epilayers grown by molecular-beam epitaxy on GaAs substrates. The capacitance-voltage measurement, deep-level transient spectroscopy, and photoconductivity spectroscopy revealed that the behaviors of Al donors in ZnS1-xTex were similar to the so-called DX centers in AlxGa1-xAs. The optical ionization energies (E-i) and emission barriers (E-e) for the observed two Al-related DX-like centers were determined as E-i similar to 1.0 and 2.0cV and E-e similar to 0.21 and 0.39 eV, respectively. It was also shown that the formation of Al-related DX-like centers resulted in a significantly large lattice relaxation in ZnS1-xTex. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Hydrogenated amorphous SiOx films are fabricated via plasma enhanced chemical vapor deposition technique. After erbium implantation and rapid thermal annealing, photoluminescence (PL) are measured at 77 K and room temperature (RT), respectively. We observed the strong PL at 1.54 mu m at RT. The 1.54 mu m PL intensity changes with the variation of concentration of oxygen. The most intense PL at 77 K in a-SiOx:H (Er) corresponds to O/Si = 1.0 and at RT to O/Si = 1.76. Based on our results, we propose that Er ions contributed to PL come from O-rich region in the film. Er ions in Si-rich region have no relation with FL. Temperature dependence of the intensity of the 1.54 mu m line of the Er3+ transition displays a very weak temperature quenching in Er-doped hydrogenated amorphous Si. The PL intensity at 250 K is a little more one half of that at 15 K.
Resumo:
Tb3+-doped zinc oxide nanocrystals with a hexagonal wurzite structure were successfully prepared by reaction between Zn-O-Tb precursors and LiOH in ethanol. Good incorporation of Tb3+ in ZnO nanocrystals is proved by XRD, FTIR, PL and PLE measurements. The presence of acetate complexes to zinc atoms on particle surfaces is disclosed by FTIR results. Emission from both Tb3+ ions and surface states in ZnO matrix, as well as their correlation were observed. The luminescence mechanism is discussed. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
In this paper, we reported on the fabrication of 980 nm InGaAs/InGaAsP strained quantum-well (QW) lasers with broad waveguide. The laser structure was grown by low-pressure metalorganic chemical vapor deposition on a n(+)- GaAs substrate. For 3 mu m stripe ridge waveguide lasers, the threshold current is 30 mA and the maximum output power and the output power operating in fundamental mode are 350 mW and 200 mW, respectively. The output power from the single mode fiber is up to 100 mW, the coupling efficiency is 50%. We also fabricated 100 mu m broad stripe coated lasers with cavity length of 800 mu m, a threshold current density of 170 A/cm(2), a high slope efficiency of 1.03 W/A and a far-field pattern of 40 x 6 degrees are obtained. The maximum output power of 3.5 W is also obtained for 100 mu m wide coated lasers. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Exciton-mediated energy transfer model in Er-doped silicon was presented. The emission intensity is related to optically active Er concentration, lifetime of excited Er3+ ion and spontaneous emission. The thermal quenching of the Er luminescence in Si is caused by thermal ionization of Er-bound exciton complex and nonradiative energy back-transfer processes, which correspond to the activation energy of 6.6 and 47.4 meV, respectively. Er doping in silicon introduces donor states, a large enhancement in the electrical activation of Er (up to two orders of magnitude) is obtained by co-implanting Er with O. It appears that the donor states are the gateway to the optically active Er. (C) 2000 Elsevier Science B.V. All rights reserved.