Resumo:
Previously, an inverted phase (the minority blocks comprising the continuum phase) was found in solution-cast block copolymer thin films. In this study, the effect of casting solvents on the formation of inverted phase has been studied. Two block copolymers, poly(styrene-b-butadiene) (SB) (M-w = 73 930 Da) and poly(styrene-b-butadiene-b-styrene) (SBS) (M-w = 140 000 Da), with comparable block lengths and equal polystyrene (PS) weight fraction (similar to30 wt %) were used. The copolymer thin films were cast from different solvents, toluene, benzene, cyclohexane, and binary mixtures of benzene and cyclohexane. Toluene and benzene are good solvents for both PS and PB, but have a preferential affinity for PS, while cyclohexane is a good solvent for PB but a Theta solvent for PS (T-Theta = 34.5 degreesC). The differential solvent affinity for PS and PB was estimated in terms of a difference between the polymer-solvent interaction parameter, chi, for each block. Under an extremely slow solvent evaporation rate, the time-dependent phase behavior during such a solution-to-film process was examined by freeze-drying the samples at different stages, corresponding to different copolymer concentrations, rho.
Microwave-assisted synthesis of high-molecular-weight poly(ether imide)s by phase-transfer catalysis
Resumo:
A facile and rapid polycondensation reaction of disodium bisphenol A with bis(chlorophthalimide)s was preformed with a domestic microwave oven in o-dichlorobenzene by phase-transfer catalysis. The polymerization reactions, in comparison with conventional heating polycondensation, proceeded rapidly and were completed within 25 min. The polymerizations gave the corresponding poly(ether imide)s with inherent viscosities of 0.55-0.92 dL g(-1). The effects of various factors on the polymerization, such as the amount of the catalyst, the reaction time, and the microwave power were studied. The properties of the polymers were briefly characterized.
Resumo:
Y2(1-x) Gd2xSiWO8 : A ( 0 <= x <= 1; A= Eu3+, Dy3+, Sm3+, Er3+) phosphor films have been prepared on silica glass substrates through the sol - gel dip-coating process. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), thermogravimetric and differential thermal analysis (TG-DTA), atomic force microscope (AFM), scanning electron microscopy (SEM) and photoluminescence spectra as well as lifetimes were used to characterize the resulting films. The results of the XRD indicated that the films began to crystallize at 800 degrees C and crystallized completely at 1000 degrees C. The AFM and SEM study revealed that the phosphor films, which mainly consisted of closely packed grains with an average size of 90 - 120 nm with a thickness of 660 nm, were uniform and crack free. Owing to an efficient energy transfer from the WO42- groups to the activators, the doped lanthanide ion ( A) showed its characteristic f - f transition emissions in crystalline Y2(1-x) Gd2xSiWO8 (0 <= x <= 1) films. The optimum concentrations for Eu3+, Dy3+, Sm3+, Er3+ were determined to be 21, 5, 3 and 7 mol% of Y3+ in Y2SiWO8 films, respectively.
Resumo:
Ordered hexagonal mesoporous silica material (JLU-30) has been successfully synthesized in alkaline media at high temperature (> 160 degreesC, using cationic (1,3-dimethyl-2-imidazolidin-2-ylidene)hexadecylmethyl-ammonium bromide (DIHAB) as a template, and characterized with X-ray diffraction (XRD), transmission electron microscopy (TEM), nitrogen adsorption-desorption isotherms, differential thermal analysis (DTA), and thermogravimetric analysis (TG), as well as Al-27 and Si-29 nuclear magnetic resonance (NMR) spectroscopy. Mesoporous JLU-30 shows much higher hydrothermal stability than MCM-41. Si-29 NMR spectra indicate that the pore walls of JLU-30 samples synthesized at high temperature (160 degreesC) are fully condensed, giving a Q(4)/Q(3) ratio as high as 6.2. In contrast, MCM-41 synthesized at relatively low temperature (100 degreesC) shows the Q(4)/Q(3) + Q(2) ratio at 1.1. Such unique structural feature might be responsible for the observed highly hydrothermal stability of the mesoporous silica materials (JLU-30).
Resumo:
A novel room temperature ionic liquid (RTIL) has been prepared containing a cyclic hexaalkylguanidinium cation. The selective oxidation of a series of substituted benzyl alcohols has been carried out in it, with sodium hypochlorite as the oxidant. The RTIL acts as both phase transfer catalyst (PTC) and solvent. The ionic liquid could be recycled after extraction of the benzaldehyde product with ether.
Resumo:
A new high-performance material, poly(sulfone-imide) was prepared by Ni(0)-catalyzed coupling of aromatic dichlorides containing imide structure and 4,4'-dichlorodiphenylsulfone. The copolymers were produced with high yield and moderate to high inherent viscosities of 0.52-1.13 dL/g. Wide-angle X-ray diffractograms revealed that the polymers were amorphous. Most of the polymers exhibited good solubility and could be readily dissolved in various solvents such as N-methyl-2-pyrrolidinone(NMP) and N,N-dimethylacetamide (DMAc). These polysulfone-imides had glass-transition temperatures between 317 and 345 degreesC and 10% weight loss temperatures in the range of 450476 degreesC in nitrogen atmosphere. The tough polymer films, obtained by casting from cresol solution, had a tensile strength range of 21 158 MPa and a tensile modulus range of 2.1-3.3 GPa.
Resumo:
The nucleophilic displacement reaction of n-bromooctane and potassium iodide in ionic liquid based on cyclic guanidinium cation(2) was investigated. The kinetic reasult shows that the rate of the reaction is enhanced in ionic liquid (2). The same reaction in [bmim][PF6](1)(where bmim = 1-butyl-3-methylimidazolium) was also studied. It was found that as a reaction medium ionic liquid (2) is better than (1) for nucelophilic displacement reactions.
Resumo:
Hexaalkylguanidinium halides exhibit an efficient catalytic activity in the synthesis of cyclic carbonates from, epoxides and carbon dioxide. By this method cyclic carbonates can be obtained in a high yield and a high selectivity at a low temperature and atmospheric pressure. This procedure is easy for the product isolation and recycling of the catalyst.
Resumo:
Photoluminescent multilayers were fabricated by layer-by-layer deposition between europium-substituted heteropolytungstate K-13 [Eu(SiW11O39)(2)].28H(2)O (denoted ESW) and a cationic polymer of quaternized poly(4-vinylpyridine) partially complexed with osmium bis(2,2'-bipyridine) (denoted as QPVP-Os) on glassy carbon and quartz substrates. The resulting photoluminescent organic-inorganic hybrid multilayers were characterized by electrochemical impedance spectroscopy, UV-Vis absorption spectrometry, cyclic voltammetry and photoluminescence spectra. Electrochemical impedance spectroscopy, UV-Vis absorption spectrometry and cyclic voltammetry results demonstrated that the multilayers were regular growth each layer adsorption. The photoluminescent properties of the films at room temperature were investigated to show the characteristic Eu3+ emission pattern of D-5(0) --> (7) F-j.
Resumo:
Bronsted acid-base ionic liquids (GILs) based on guanidine and acetic acid are efficient reaction media for palladium-catalyzed Heck reactions. They offer the advantages of high activity and reusability. GIL2 plays multiple roles in the reaction: it could act as solvent, as a strong base to facilitate beta-hydride elimination, and as a ligand to stabilize activated Pd species.
Resumo:
We observed that the SrMg2(PO4)(2):Eu phosphor could emit long life phosphorescence with the excitation light whose wavelength was shorter than 420 nm, however, when La, Ce, or Gd was codoped, the wavelength of the excitation light to cause the phosphorescence had a redshift of 40 nm. A possible mechanism and related discussion for this redshift phenomenon of the excitation light was given. It was suggested that the threshold between the trap and valence band was decreased with the addition of the codopants.
Resumo:
A novel sulfonated aromatic dichloride monomer was successfully prepared by the reaction of 2, 5-dichlorobenzophenone with fuming sulfuric acid. Copolymerization of this monomer in the form of sodium salt (1) with N-(4-chloro-2-trifluoromethylphenyl)-5-chloro-1,8-naphthalimide (2) or bis(N-(4-chloro-2-trifluoromethylphenyl)1,4,5,8-naphthalimide (3) generated two series of novel poly(arylene-co-naphthalimide) s I-x and II-x where x represents the content of the sulfonated monomer. The synthesized copolymers with the -SO3H group in the side chains possessed high molecular weights revealed by their high viscosity and the formation of tough and flexible membranes. The copolymers exhibited excellent stability toward water and oxidation due to the introduction of the hydrophobic CF3 groups. The sulfonated copolyimides that incorporated with 1,8-naphthalimide (I-x) exhibited better hydrolytic and oxidative stabilities than those with 1,4,5,8-naphthalimide. Copolymer I-50 membrane endured for more than 83 h in Fenton's reagent at room temperature. The mechanical properties of I-50 membrane kept almost unchanged after immersing membrane in boiling water for 196 h. The proton conductivities of copolymer films increased with increasing IEC and temperature, reaching values above 6.8 x 10(-1) S/cm at 80 degrees C.
Resumo:
A novel dissolving process for chitin and chitosan has been developed by using the ionic liquid 1-butyl-3-methyl-imidazolium chloride ([Bmim]Cl) as a solvent, and a novel application of chitin and chitosan as substitutes for amino-functionalized synthetic polymers for capturing and releasing CO2 has also been exploited based on this processing strategy.
Resumo:
Covalent surface functionalization of carbon nanotubes with polypeptides is promising for possible medical applications. This work presents a graft-from approach to perform the polypeptide modification of multiwalled carbon nanotubes (MWTNs). The raw MWNTs are first amine-functionalized. The amine-functionalized MWNTs are then used as the initiator to initiate the ring-opening polymerization of gamma-benzyl-L-glutamate N-carboxyanhydride (BLG- NCA), to results in the polypeptide-grafted MWNTs. FT-IR, XPS, and TGA data demonstrate that the functionalization is successful. The TEM images of the products show that the thickness of the polypeptide shell of the PBLG-MWNT is about 4.5-22 nm. Using the facile route developed here, carbon nanotubes functionalized with other types of polypeptides can be easily fabricated using the corresponding NCAs.
Resumo:
Sulfonated poly(p-phenylene)s (SPPs) containing sulfonic acid groups in their side chains had been directly synthesized by Ni(0) catalytic coupling of sodium 3-(2,5-dichlorobenzoyl)benzenesulfonate and 2,5-dichlorobenzophenone. The synthesized copolymers possessed high molecular weights revealed by their high viscosity, and the formation of tough and flexible membranes by casting from DMAc solution. The copolymers exhibited excellent oxidative stability and mechanical properties due to their fully aromatic structure extending through the backbone and pendent groups. Transmission electron microscopic (TEM) analysis revealed that these side-chain type SPP membranes have a microphase-separated structure composed of hydrophilic side-chain domains and hydrophobic polyphenylene main chain domains. The proton conductivities of copolymer membranes increased with the increase of IEC and temperature, reaching values above 3.4 x 10(-1) S/cm at 120 degrees C, which are almost 2-3 times higher than that of Nafion 117 at the same measurement conditions. Consequently, these materials proved to be promising as proton exchange membranes.