Among the wide variety of materials employed in the manufacture of shoes, thermoplastic polyurethanes (TPUs) are one of the most widely used. Given its widespread use, and associated waste management problems, the development of more biodegradable and evironmentally compatible solutions is needed. In this work, a polyester-based TPU used in the footwear industry for outsoles production was modified by compounding with lignin, starch and cellulose at content of 4% (w/w). The biodegradability was evaluated by using agar plate tests with the fungi Aspergillus niger ATCC16404, the Gram-negative bacteria Pseudomonas aeruginosa ATCC9027 and an association of both (consortium), and soil tests at 37 °C and 58 °C. The obtained results evidenced a positive effect of the tested biobased additives, the most favourable results being registered with lignin. These results were corroborated by the structural modifications observed by FTIR analysis. Additionally, mechanical tests prove the suitability of using the lignin modified TPUs for footwear outsoles production.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conservators have long been aware of the problems associated with the preservation of rubber objects due to inherent instability that can be attributed, in part, to the presence of additives. Inorganic additives, such as fillers, accelerators, stabilizers, and special ingredients are necessary in manufacturing to alter the properties of natural rubber. These materials all have different interactions with the rubber, and each other, and differing effects on the ageing process. To date, the most effective and accepted methods to preserve rubber are cold, dark storage of objects, or the use of low oxygen environments. While these methods are effective, they greatly limit access. The application of coatings to the surface of rubber objects can slow deterioration and greatly increase the ability of an institution to handle and display rubber objects. While numerous coatings for preventive and interventive treatment have been tested, none have been so successful to warrant routine use. The first section of this research highlighted the relationship between the inclusion of certain additives in natural rubber objects and the accelerated or slowed down overall degradation. In the second part of this research, the acrylic varnishes Golden Polymer Varnish with UVLS, Lascaux Acrylic Transparent Varnish-UV, Sennelier Matte Lacquer with UV Protection, and Liquitex Soluvar Varnish containing ultraviolet light absorbers or stabilizers were tested as a preventative coating for rubber. Through testing the visual and physical properties of the samples, as well as compound analysis the results of this research suggest that acrylic varnishes do provide protection, each to varying degrees. The results also provided insight into the behavior of rubber and these varnishes with continuing light exposure.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The ionic liquid (IL) 1-butyl-3-methylimidazolium chloride was used as a drying control chemical additive in the synthesis of silica sol-gel materials with and without methanol as a co-solvent. The resulting gels were characterized by using thermogravimetric analysis, differential scanning calorimetry, infrared spectroscopy and water sorption kinetics. Calcined gels were analyzed using scanning electron microscopy and nitrogen adsorption isotherms for surface area and pore volume determination. Non-calcined gels were monolithic and showed general cloudiness with lesser degrees observed at higher IL volumes. Calcinations resulted in the formation of powders with increased available surface area as the amount of IL volume was increased. This is consistent with an increase in respective pore volume but a general decrease in average pore size. The resulting materials exhibited conventional structural microdomains, in contrast to periodicity reported when other ionic liquids were used as templates.

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Endocrine-disrupting chemicals (EDCs) are capable of interfering with normal hormone homeostasis by acting on several targets and through a wide variety of mechanisms. Unwanted exposure to EDCs can lead to a wide spectrum of adverse health effects, especially when exposure is during critical windows of development. Feed and food are considered to be among the main routes of inadvertent exposure to EDCs, so there is an important need for efficient detection of EDCs in these matrices.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conversion of biomass for production of liquid fuels can help in reducing the greenhouse gas (GHG) emissions which are predominantly generated by combustion of fossil fuels. Adding oxymethylene ethers (OMEs) in conventional diesel fuel has the potential to reduce soot formation during the combustion in a diesel engine. OMEs are downstream products of syngas, which can be generated by the gasification of biomass. In this research, a thermodynamic analysis has been conducted through development of data intensive process models of all the unit operations involved in production of OMEs from biomass. Based on the developed model, the key process parameters affecting the OMEs production including equivalence ratio, H2/CO ratio, and extra water flow rate were identified. This was followed by development of an optimal process design for high OMEs production. It was found that for a fluidized bed gasifier with heat capacity of 28 MW, the conditions for highest OMEs production are at an air amount of 317 tonne/day, at H2/CO ratio of 2.1, and without extra water injection. At this level, the total OMEs production is 55 tonne/day (13 tonne/day OME3 and 9 tonne/day OME4). This model would further be used in a techno-economic assessment study of the whole biomass conversion chain to determine the most attractive pathways.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The search for ideal biomaterials is still on-going for tissue regeneration. In this study, blends of Poly ε-caprolactone (PCL) with Poly l-lactic acid (PLLA), Nalidixic Acid (NA) and Polyethylene glycol (PEG) were prepared. Mechanical and thermal properties of the blends were investigated by tensile and flexural analysis, DSC, TGA, WXRD, MFI, BET, SEM and hot stage optical microscopy. Results showed that the loading of PLLA caused a significant decrease in tensile strength and almost total eradication of the elongation at break of PCL matrix, especially after PEG and NA addition. Increased stiffness was also noted with additional NA, PEG and PLLA, resulting in an increase in the flexural modulus of the blends.
Isothermal degradation indicated that bulk PCL, PLLA and the blends were thermally stable at 200°C for the duration of 2h making extrusion of the blends at this temperature viable. Morphological study showed that increasing the PLLA content and addition of the very low viscosity PEG and powder NA decreased the Melt Flow Indexer and increased the viscosity.
At the higher temperature the PLLA begins to soften and eventually melts allowing for increased flow and, coupling this with, the natural increase in MFI caused by temperature is enhanced further. The PEG and NA addition increased dramatically the pore volume which is important for cell growth and flow transport of nutrients and metabolic waste.