We demonstrate vertically aligned epitaxial GaAs nanowires of excellent crystallographic quality and optimal shape, grown by Au nanoparticle-catalyzed metalorganic chemical vapor deposition. This is achieved by a two-temperature growth procedure, consisting of a brief initial high-temperature growth step followed by prolonged growth at a lower temperature. The initial high-temperature step is essential for obtaining straight, vertically aligned epitaxial nanowires on the (111)B GaAs substrate. The lower temperature employed for subsequent growth imparts superior nanowire morphology and crystallographic quality by minimizing radial growth and eliminating twinning defects. Photoluminescence measurements confirm the excellent optical quality of these two-temperature grown nanowires. Two mechanisms are proposed to explain the success of this two-temperature growth process, one involving Au nanoparticle-GaAs interface conditions and the other involving melting-solidification temperature hysteresis of the Au-Ga nanoparticle alloy.
Resumo:
The defect evolution and its correlation with electrical properties of GaN films grown by metalorganic chemical vapor deposition are investigated. It is found that the dislocation density decreases gradually during the growth process, and the dislocation reduction rate in the island coalescence process is especially rapid. The changes in electron mobility of GaN with the increase of growth time are mainly dependent on the dislocations acting as scattering centers. Furthermore, the variation of carrier concentration in GaN may be related with the point defects and their clusters. The quality of GaN could be improved by suitably increasing the film thickness. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
The in situ optical reflectivity measurements are employed to monitor the GaN epilayer growth process above low-temperature AlN buffer layer on c-plane sapphire substrate by metalorganic chemical vapor deposition. It is found that the lateral growth of GaN islands and their coalescence is promoted in the initial growth stage if the AlN buffer layer is treated with a long annealing time and has an optimal thickness: As confirmed by atomic force microscopy observations, the quality of GaN epilayers is closely dependent on the surface morphology of AlN buffer layer, especially the grain size and nuclei density after the annealing treatment. (C) 2004 American Institute of Physics.
Resumo:
ZnO crystals were grown by CVT method in closed quartz tube under seeded condition. Carbon was used as a transport agent to enhance the chemical transport of ZnO in the growth process. ZnO single crystals were grown by using GaN/sapphire and GaN/Si wafer as seeds. The property and crystal quality of the ZnO single crystals was studied by photoluminescence spectroscopy and X-ray diffraction technique.
Resumo:
The Al composition of metalorganic chemical vapor deposition (MOCVD)-grown AlGaN alloy layers is found to be greatly influenced by the parasitic reaction between ammonia (NH3) and trimethylaluminum (TMAI). The growth process of AlN is carefully investigated by monitoring the in situ optical reflection. The abnormal dependencies of growth rate on growth temperature, reactor pressure, and flux of NH3 are observed and can be well explained by the effect of parasitic reaction. The increase of growth rate with increasing flux of TMAI is found to depend on the growth temperature and reactor pressure due to the presence of parasitic effect. A relatively low growth temperature and a reduced reactor pressure are suggested for the effective decrease of parasitic reaction during the MOCVD growth of AlN and probably lead to a more effective incorporation of Al into the AlGaN layers. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
The reduction of residual strain in cubic GaN growth by inserting a thermoannealing process is investigated. It is found that the epilayer with smaller tensile strain is subject to a wider optimal "growth window." Based on this process, we obtain the high-quality GaN film of pure cubic phase with the thickness of 4 mum by metalorganic chemical vapor deposition. The photoluminescence spectrum at room temperature shows the thick GaN layer has a near-band emission peak with a full width at half maximum of 42 meV which confirms its high crystal quality, further supported by the x-ray (002) diffraction measurement. A simplified model is demonstrated to interpret this strain effect on the growth process. (C) 2003 American Institute of Physics.
Resumo:
The growth morphologies of metalorganic chemical vapor deposition (MOCVD) grown GaN layer on Si(111) substrate were studied using atomic force microscopy and transmission electron microscopy. It was found that the growth process of GaN/Si(111) consisted of two cycles of island growth and coalescence. These two cycles process differs markedly from that of one cycle process reported. The stress of evolving GaN layers on Si(111) was characterized by measuring the lattice constant c of GaN using X-ray diffraction (XRD) technique. It was proposed that the large tensile stress within the film during growth initiated this second island growth cycle, and the interaction between the GaN islands with high orientational fluctuation on the buffer layer induced this large tensile growth stress when coalescence occurred. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
GaN epilayers on sapphire substrate grown by metalorganic vapor-phase epitaxy (MOVPE) in a horizontal-type low-pressure two-channel reactor were investigated. Samples were characterized by X-ray diffraction (XRD), Raman scattering, atomic force microscopy (AFM) and photoluminescence (PL) measurements. The influence of the temperature changes between low temperature (LT) deposited GaN buffer and high temperature (WT) grown GaN epilayer on crystal quality of epilayer was extensively studied. The effect of in situ thermal annealing during the growth on improving the GaN layer crystal quality was demonstrated and the possible mechanism involved in such a growth process was discussed. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
SiC was grown on Si (100) substrates oriented and off-oriented by 2-5 degrees towards [011] with simultaneous supply of C2H4 and S2H6 at 1050 degrees C. SiC formed during removal of oxide could be removed at 1150 degrees C. Twinned growth occurred on both oriented and off-oriented substrates during carbonization, but fewer twins formed on the off-oriented substrate than that on the oriented substrate. In SiC growth process, twinned growth continued on the off-oriented substrate whereas twinned growth stopped and single crystal SiC with double-domain (2 x 1) superstructure formed on the oriented substrate. SiC single crystal could grow on a carbonized twinned buffer layer. Obvious SiC LO and TO phonon modes were observed with Raman spectroscopy in the epilayer grown on the oriented substrate. The surface of the epilayer grown on the oriented substrate was smooth, while there was a high density of islands on the epilayer grown on the off-oriented substrate. The film grown on the oriented substrate is superior than that grown on the off-oriented substrate. (C) 1999 Elsevier Science B.V. All rights reserved.
Resumo:
The growth rate of GaN buffer layers on sapphire grown by metalorganic vapor-phase epitaxy (MOVPE) in an atmospheric pressure, two-channel reactor was studied. The growth rate, as measured using laser reflectance, was found to be dependent on growth temperature, molar flow rate of the sources tin this case, trimethylgallium and ammonia) and the input configuration of sources into the reactor. A model of the GaN buffer layer growth process by MOVPE is proposed to interpret the experimental evidence. (C) 1998 Elsevier Science B.V. All rights reserved.
Resumo:
High-quality InGaAs/InAlAs/InP high-electron-mobility transistor (HEMT) structures with lattice-matched or pseudomorphic channels have been grown by molecular-beam epitaxy (MBE). The purpose of this work is to enhance the channel conductivity by changing the epitaxial structure and growth process. With the use of pseudomorphic step quantum-well channel, the highest channel conductivity is achieved at x = 0.7, the corresponding electron mobilities are as high as 12300 (300 K) and 61000 cm(2)/V.s (77 K) with two-dimensional electron gas (2DEG) density of 3.3 x 10(12) cm(-2). These structures are comprehensively characterized by Hall measurements, photoluminescence, double crystal X-ray diffraction and transmission electron microscopy. Strong room-temperature luminescence is observed, demonstrating the high optical quality of the samples. We also show that decreasing the In composition in the InyAl1-yAs spacer is very effective to increase the 2DEG density of PHEMT structures. (C) 1998 Published by Elsevier Science B.V. All rights reserved.
Resumo:
ZnO crystals were grown by CVT method in closed quartz tube under seeded condition. Carbon was used as a transport agent to enhance the chemical transport of ZnO in the growth process. ZnO single crystals were grown by using GaN/sapphire and GaN/Si wafer as seeds. The property and crystal quality of the ZnO single crystals was studied by photoluminescence spectroscopy and X-ray diffraction technique.
Resumo:
Physical vapor transport studies of GeSe(x)Te1 - x (x = 0.1, 0.2, 0.3, and 0.4) solid solutions demonstrated, that individual, large single crystals of these materials can be grown in closed ampoules. A compositional analysis of the grown crystals revealed, that the mass transport (crystal growth) process under steady-state conditions is pseudo-congruent and controlled by diffusion processes in the source material. From these experiments, the degree of non-stoichiometry (Ge-vacancy concentrations) of GeSe(x)Te1 - x single crystals could be estimated. The effects of the cubic to rhombohedral phase transformation during cooling on the microstructure and morphology of the grown mixed crystals are observed. This work provides the basis for subsequent defect studies and electrical measurements on these crystals.
Resumo:
The nucleation and growth kinetics of CdS nanocrystals in a two-phase synthesis system have been investigated. It was found that the nucleation process is quite lengthy and overlapped with the growth process; nevertheless, as formed nanocrystals show extremely narrow size distribution owing to the unique heterogeneous reacting environment and Ostwald ripening growth. The nucleation and growth kinetics of the nanocrystals were also influenced strongly by the monomer concentration, capping agent concentration, and solvent polarity. It was also found that a high monomer concentration, a low capping agent concentration, and low solvent polarity lead to a higher maximum nucleus concentration and nanocrystal concentration, while high polarity solvents are favorable for the formation of nanocrystals with narrower size distribution and higher photoluminescence quantum yield.
Resumo:
La0.5Ba0.5MnO3 products with novel flowerlike, microcube, and nanocube structures were successfully synthesized by a simple hydrothermal route by controlling the alkalinity of the reaction solutions. The synthesized products were systematically studied by X-ray powder diffraction, field-emission scanning electron microscopy, transmission electron microscopy, and energy dispersive X-ray spectroscopy. The results showed that the formation of the flowerlike structures with a layer assembly experienced a nucleation-aggregation-crystallization growth process, while the cubic structures experienced a nucleation-crystallization growth process due to the effect of different alkalinity in the reaction solutions. The higher alkalinity also led to a decrease in the size in the cubic structures. Suitable temperature and pressure were demonstrated to be crucial to the formation of the flowerlike structures by carrying out further control experiments. The measurement of the magnetic properties of three samples obtained at different alkaline conditions indicated that the size of the La0.5Ba0.5MnO3 products had an obvious influence on their properties; however, the dependence of the properties upon the morphology of the La0.5Ba0.5MnO3 products was minor.