861 resultados para odour and taste properties
Resumo:
We have utilized infra-red and optical absorption measurements, grazing incidence X-ray diffraction (GIXRD) and extended X-ray absorption fine structure (EXAFS) measurements to investigate the influence of hydrogenation on the optical and structural properties of GaAs thin films prepared by rf-magnetron sputtering. Hydrogenation induces distinct changes in the optical properties, namely shifts in the absorption edges and reduction of the Urbach energy. Such modifications are correlated to a reduction in structural disorder as determined by EXAFS and the increase of crystallinity determined by GIXRD. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
This work describes the preparation and characterization of composite materials obtained by the combination of natural rubber (NR) and carbon black (CB) in different percentages, aiming to improve their mechanical properties, processability, and electrical conductivity, aiming future applications as transducer in pressure sensors. The composites NR/CB were characterized through optical microscopy (OM), DC conductivity, thermal analysis using differential scanning calorimetry (DSC), dynamic mechanical thermal analysis (DMA), thermogravimetry (TGA), and stress-strain test. The electrical conductivity varied between 10(-9) and 10 S m(-1), depending on the percentage of CB in the composite. Furthermore, a linear (and reversible) dependence of the conductivity on the applied pressure between 0 and 1.6 MPa was observed for the sample with containing 80 wt % of NR and 20% of CB. (C) 2007 Wiley Periodicals, Inc.
Resumo:
Sorption isotherms of lemon juice (LE) powders with and without additives-18% maltodextrin (MA) or 18% gum Arabic (GA) were determined at 20-50 degrees C. Addition of additives was shown to affect the isotherms in such a way that, at the same water activity, samples LE + GA and LE + MA presented lower equilibrium moisture content and were not so affected by varying temperature. The net isosteric heats of sorption of juice powders with additives were higher (less negative) than those of lemon juice powders, suggesting that there are more active polar sites in the product without addition of GA or MA. In general, the quality properties decreased with the addition of maltodextrin and gum arabic and it was obtained similar values for LE + GA and LE + MA.
Resumo:
Pristine, W and Mn 1% doped Ba(0.6)Sr(0.4)TiO(3) epitaxial thin films grown on the LaAlO(3) substrate were deposited by pulsed laser deposition (PLD). Dielectric and ferroelectric properties were determined by the capacitance measurements and X-ray diffraction was used to determine both residual elastic strains and defect-related inhomogeneous strains-by analyzing diffraction line shifts and line broadening, respectively. We found that both elastic and inhomogeneous strains are affected by doping. This strain correlates with the change in Curie-Weiss temperature and can qualitatively explain changes in dielectric loss. To explain the experimental findings, we model the dielectric and ferroelectric properties of interest in the framework of the Landau-Ginzburg-Devonshire thermodynamic theory. As expected, an, elastic-strain contribution due to the epilayer-substrate misfit has an important influence on the free-energy. However, additional terms that correspond to the defect-related inhomogeneous strain had to be introduced to fully explain the measurements.
Resumo:
PLZT ceramics belong to one of the very important groups of functional materials that make a basis for the production of a large range of electronic devices. The microstructure and properties of ceramics depend on the powder preparation and thermal processing conditions. Various techniques have been used to obtain chemically homogeneous and fine starting powders. PLZT powders have been prepared by two different production routes: by a modified Pechini method, using a polymeric precursor method (PMM) and by a partial oxalate method. A two-step sintering process, including a hot pressing, was carried out at 1100 and 1200degreesC Distinct phases obtained during the sintering process have been investigated by SEM and EDS techniques and dielectric properties such as permittivity and dielectric loss were measured in a frequency range from 1 to 20 kHz.. A significant difference in microstructure and dielectric properties, depending on powder origin and sintering procedure, has been noticed.
Resumo:
In the present work, methylcellulose produced from sugar cane bagasse was characterized by FTIR, WAXD, DTA and TGA techniques. Two samples were synthesized: methylcellulose A and rnethylcellulose B. The only difference in the process was the addition of fresh reactants during the preparation of methylcellulose B. The ratio between the absorption intensities of the C-H stretching band at around 2900 cm(-1) and C-H stretching at around 3400 cm(-1) for methylcellulose B is higher than for methylcellulose A, indicating that methylcellulose B showed an increase in the degree of substitution (DS). Methylcellulose A presents a more heterogeneous structure, which is similar to the original cellulose as seen through FTIR and DTA. Methylcellulose B showed thermal properties similar to commercial methylcellulose. The modification of rnethylcellulose preparation method allows the production of a material with higher DS, crystallinity and thermal stability in relation to the original cellulose and to methylcellulose A. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
Undoped and indium-doped Zinc oxide (ZnO) solid films were deposited by the pyrosol process at 450 degrees C on glass substrates From solutions where In/Zn ratio was 2, 5, and 10 at.%. Electrical measurements performed at room temperature show that the addition of indium changes the resistance of the films. The resistivities of doped films are less than non-doped ZnO films by one to two orders of magnitude depending on the dopant concentration in the solution. Preferential orientation of the films with the c-axis perpendicular to the substrate was detected by X-ray diffraction and polarized extended X-ray absorption fine structures measurements at the Zn K edge. This orientation depends on the indium concentration in the starting solution. The most textured films were obtained for solutions where In/Zn ratio was 2 and 5 at.%. When In/Zn = 10 at.%, the films had a nearly random orientation of crystallites. Evidence of the incorporation of indium in the ZnO lattice was obtained from extended X-ray absorption fine structures at the In and Zn K edges. The structural analysis of the least resistive film (Zn/In = 5 at.%) shows that In substitutes Zn in the wurtzite structure. (C) 2000 Elsevier B.V. B.V. All rights reserved.
Resumo:
The effect of La2O3 addition on the densification and electrical properties of the (0.9895 - x) SnO2 + 0.01 CoO + 0.0005 Nb2O5 + x La2O5 system, where x = 0.0005 or 0.00075, was considered in this study. The samples were sintered at 1300 degreesC for 2 and 4 h and a single SnO2 phase was identified by X-ray diffraction. Microstructure analysis by scanning electron microscopy showed that the affect of La2O3 addition is to decrease the SnO2 grain size. J versus E curves indicated that the system exhibits a varistor behavior and the effect of La2O3 is to increase both the non-linear coefficient (alpha) and the breakdown voltage (E-2). Considering the Schottky thermionic emission model the potential height and the width were estimated. The addition of small amounts of La2O3 to the basic system increases the potential barrier height and decreases both grain size and potential barrier width. (C) 2001 Kluwer Academic Publishers.
Resumo:
Structural and electrical properties of ZnO varistors were investigated as a function of spinel composition. Six varistor mixtures differing only in chemical composition of spinel, were prepared by mixing separately synthesized constituent phases (DSCP method). Compositions of constituent phases in sintered samples were investigated by changes of lattice parameters of the phases, as well as by EDS analysis of the constituent phases. It was found that compositions of ZnO, intergranular and spinel phases were partially changed during sintering due to redistribution of additives, that was controlled by starting spinel composition and its stability. Electrical characterization showed significant difference in electrical properties of investigated varistors: nonlinearity coefficients ranging from 22 to 55 and leakage currents differing by the order of magnitude. Activation energies of conduction were obtained from ac impedance spectroscopy measurements. Calculated values of activation energies were in the range 0.61-1.0 eV confirming difference in defect structure of ZnO grain boundaries in varistors containing different spinel phases. (C) 2001 Elsevier B.V. Ltd and Techna S.r.l. All rights reserved.
Resumo:
Ferroelectric Pb1-xCaxTiO3 (x = 0.24) thin films were formed on a Pt/Ti/SiO2/Si substrate by the polymeric precursor method using the dip-coating technique for their deposition. Characterization of the films bq X-ray diffraction showed a perovskite single phase with a tetragonal structure after annealing at 700 degreesC. Atomic force microscopy (AFM) analyses showed that the film had a smooth and crack-free surface with low surface roughness. In addition, the PCT thin film had a granular structure with an 80 nm grain size. The thickness of the films observed by the scanning electron microscopy (SEM) is 550 nm and there is a good adhesion between the film and substrate. For the electrical measurements metal-ferroelectric-metal of the type capacitors were obtained, where the thin films showed good dielectric and ferroelectric properties. The dielectric constant and dissipation factor at 1 kHz and measured at room temperature were found to be 457 and 0.03. respectively. The remanent polarization and coercive field for the: deposited films were P-r = 17 muC/cm(2) and E-c = 75 kV/cm, respectively. Moreover. The 550-nm-thick film showed a current density in the order of 10(-8) A/cm(2) at the applied voltage of 2 V. The high values of the thin film's dielectric properties are attributed to its excellent microstructural quality and the chemical homogeneity obtained by the polymeric precursor method. (C) 2001 Elsevier science Ltd. All rights reserved.
Resumo:
Making heterolayered perovskite materials constitutes an approach for the creation of better dielectric and ferroelectric properties. In the experiment reported here, heterolayered PZT40/PZT60 films were grown on Pt/Ti/SiO2/Si (100) by a chemical solution deposition. The dielectric constant of the heterolayered thin film was significantly enhanced compared with that of pure PZT40 and PZT60 thin films. A dielectric constant of 701 at 100 kHz was observed for a stacking periodicity of six layers having a total thickness of 150 nm. The heterolayered film exhibited greater remanent polarization than PZT60 and PZT40 films. The values of remanent polarization were 7.9, 18.5, and 31 muC/cm(2), respectively, for pure PZT60, PZT40, and heterolayered thin films, suggesting that the superior dielectric and ferroelectric properties of the heterolayered thin film resulted from a cooperative interaction between the ferroelectric phases made from alternating tetragonal and rhombohedral phases of PZT, simulating the morphotropic phase boundary of this system. (C) 2004 American Institute of Physics.
Resumo:
A recent and innovative method to include Ti into the columbite precursor has permitted to synthesize 0.9PMN-0.1PT powders with high homogeneity. The present work describes this methodology, named modified columbite method, showing that the reaction between MN(T)and PbO at 800 degrees C for 2 h results in perovskite single-phase. The crystal structure alterations in the columbite and perovskite phases obtained by this methodology and the effects of potassium doping were investigated by the Rietveld method. Changes in the powder morphology, density and weight loss during the sintering process were also studied. Conclusively, potassium does not affect significantly the perovskite amount, but reduces the particle and grain sizes. This dopant also changes the relaxor behavior of 0.9PMN-0.1 PT ceramic, reducing the dielectric loss and enhancing the diffuseness of the phase transition. (C) 2005 Published by Elsevier Ltd and Techna Gronp S.r.l.
Resumo:
Stingrays of the family Potamotrygonidae are widespread throughout river systems of South America that drain into the Atlantic Ocean. Some species are endemic to the most extreme freshwater environment of the Brazil and cause frequent accidents to humans. The envenomation causes immediate, local, and intense pain, soft tissue edema, and a variable extent of bleeding. The present study was carried out in order to describe the principal biological and some biochemical properties of the Brazilian Potamotrygon fish venoms (Potamotrygon cf. scobina and P. gr. orbignyi). Both stingray venoms induced significant edematogenic and nociceptive responses in mice. Edematogenic and nociceptive responses were reduced when the venom was incubated at 37 or 56 degrees C. The results showed striking augments of leukocytes rolling and adherent cells to the endothelium of cremaster mice induced by both venoms. The data also presented that injection of both venoms induced necrosis, low level of proteolytic activity, without inducing haemorrhage. But when the venoms of both stingray species were injected together with their mucus secretion, the necrotizing activity was more vigorous. The present study provided in vivo evidence of toxic effects for P. cf. scobina and P. gr. orbignyi venoms. (c) 2006 Elsevier Ltd. All fights reserved.
Resumo:
BaxSr1-xTiO3 (x = 0.6) (BST) thin films were successfully prepared on a Pt(111)/TiO2/SiO2/Si(100) substrate by spin coating, using the polymeric precursor method. BST films with a perovskite single phase were obtained after heat treatment at 700 degrees C. The multilayer BST thin films had a granular structure will a grain size of approximately 60 nm. A 480-nm-thick film was obtained by carrying out five cycles of the spin-coating/heating process. Scanning electron microscopy and atomic force microscopy analyses showed that the thin films had a smooth, dense, crack-free surface with low surface roughness (3.6 nm). At room temperature and at a frequency of 100 kHz, the dielectric constant and the dissipation factor were, respectively, 748 and 0.042. The high dielectric constant value was due to the high microstructural quality and chemical homogeneity of the thin films obtained by the polymeric precursor method.
Resumo:
Barium strontium titanate (Ba0.8Sr0.2TiO3) thin films have been prepared on Pt/Ti/SiO2/Si substrates using a soft solution processing. X-ray diffraction and also micro-Raman spectroscopy showed that the Ba0.8Sr0.2TiO3 thin films exhibited a tetragonal structure at room temperature. The presence of Raman active modes was clearly shown at the 299 and 725 cm(-1) peaks. The tetragonal-to-cubic phase transition in the Ba0.8Sr0.2TiO3 thin films is broadened, and suppressed at about 35 degreesC, with a maximum dielectric constant of 948 (100 kHz). Electrical measurements for the prepared Ba0.8Sr0.2TiO3 thin films showed a remnant polarization (P-r) of 6.5 muC/cm(2), a coercive field (E-c) of 41 kV/cm, and good insulating properties. The dispersion of the refractive index is interpreted in terms of a single electronic oscillator at 6.97 eV. The direct band gap energy (E-g) and the refractive index (n) are estimated to be 3.3 eV and n = 2.27-2.10, respectively. (C) 2002 American Institute of Physics.