991 resultados para Aligned ZnO Nanorods
Resumo:
ZnO crystals were grown by CVT method in closed quartz tube under seeded condition. Carbon was used as a transport agent to enhance the chemical transport of ZnO in the growth process. ZnO single crystals were grown by using GaN/sapphire and GaN/Si wafer as seeds. The property and crystal quality of the ZnO single crystals was studied by photoluminescence spectroscopy and X-ray diffraction technique.
Resumo:
Valence-band type Auger lines in Al doped and undoped ZnO were comparatively studied with the corresponding core level x-ray photoelectron spectrography (XPS) spectra as references. Then the shift trend of energy levels in the valence band was that p and p-s-d states move upwards but e and p-d states downwards with increasing Al concentration. The decreased energy of the Zn 3d state is larger than the increased energy of the 0 2p state, indicating the lowering of total energy. This may indicate that Al doping could induce the enhancement of p-d coupling in ZnO, which originates from stronger Al-O hybridization. The shifts of these states and the mechanism were confirmed by valence band XPS spectra and 0 K-edge x-ray absorption spectrography (XAS) spectra. Finally, some previously reported phenomena are explained based on the Al doping induced enhancement of p-d coupling.
Resumo:
The electronic structure and optical properties of freestanding GaN wurtzite quantum wires are studied in the framework of six-band effective-mass envelope function theory. It is found that the electron states are either twofold or fourfold degenerate. There is a dark exciton effect when the radius R of GaN wurtzite quantum wires is in the range of [0.7, 10.9] nm. The linear polarization factors are calculated in three cases, the quantum confinement effect (finite long wire), the dielectric effect and both effects (infinitely long wire). It is found that the linear polarization factor of a finite long wire whose length is much less than the electromagnetic wavelength decreases as R increases, is very close to unity (0.979) at R = I nm, and changes from a positive value to a negative value around R = 4.1 nm. The linear polarization factor of the dielectric effect is 0.934, independent of radius, as long as the radius remains much less than the electromagnetic wavelength. The result for the two effects shows that the quantum confinement effect gives a correction to the dielectric effect result. It is found that the linear polarization factor of very long (treated approximately as infinitely long) quantum wires is in the range of [0.8, 1]. The linear polarization factors of the quantum confinement effect of CdSe wurtzite quantum wires are calculated for comparison. In the CdSe case, the linear polarization factor of R = I nm is 0.857, in agreement with the experimental results (Hu et al 2001 Science 292 2060). This value is much smaller than unity, unlike 0.979 in the GaN case, mainly due to the big spin-orbit splitting energy Delta(so) of CdSe material with wurtzite structure.
Resumo:
P-doped ZnO films were deposited on n-Si substrate by radio-frequency magnetron sputtering. Hall measurements revealed that the films annealed in situ at 750 degrees C in an oxygen ambient at a pressure of 1.3x10(-3)-3.9x10(-3) Pa showed p-type behavior with a hole concentration of 2.7x10(16)-2.2x10(17) cm(-3), a mobility of 4-13 cm(2)/V s, and a resistivity of 10.4-19.3 Omega cm. Films annealed at 750 degrees C in a vacuum or in oxygen ambient at higher pressures (5.2x10(-3) and 6.5x10(-3) Pa) showed n-type behavior. Additionally, the p-ZnO/n-Si heterojunction showed a diodelike I-V characteristic. Our results indicate that P-doped p-type ZnO films can be obtained by annealing in oxygen ambient at very low pressures. (c) 2006 American Institute of Physics.
Resumo:
Sb-doped and undoped ZnO thin films were deposited on Si (100) substrates by radio frequency (RF) magnetron sputtering. X-ray diffraction (XRD) and scanning electron microscopy (SEM) analyses revealed that all the films had polycrystalline wurtzite structure and c-axis preferred orientation. Room temperature Hall measurements showed that the as-grown films were n-type and conducting (rho similar to 1-10 Omega cm). Annealing in a nitrogen ambient at 400 degrees C for 1 h made both samples highly resistive (rho > 10(3) Omega cm). Increasing the annealing temperature up to 800 C, the resistivity of the ttndoped ZnO film decreased gradually, but it increased for the Sb-doped ZnO film. In the end, the Sb-doped ZnO film annealed at 800 C became semi-insulating with a resistivity of 10(4)Omega cm. In addition, the effects of annealing treatment and Sb-doping on the structural and electrical properties are discussed. (c) 2006 Elsevier B.V. All rights reserved.
Synthesis and temperature-dependent near-band-edge emission of chain-like Mg-doped ZnO nanoparticles
Resumo:
Chain-like Mg-doped ZnO nanoparticles were prepared using a wet chemical method combined with subsequent heat treatment. The blueshifted near-band-edge emission of the doped ZnO sample with respect to the undoped one was investigated by temperature-dependent photoluminescence. Based on the energy shift of the free-exciton transition, a band gap enlargement of similar to 83 meV was estimated, which seems to result in the equivalent shift of the bound-exciton transition. At 50 K, the transformation from the donor-acceptor-pair to free-to-acceptor emissions was observed for both the undoped and doped samples. The results show that Mg doping leads to the decrease of the acceptor binding energy. (c) 2006 American Institute of Physics.
Resumo:
The recombination property of nitrogen (N)-related acceptor-bound states in ZnO has been investigated by photoluminescence (PL), time-resolved PL, and selective PL. Several possible recombination processes were discussed by analyzing the relaxation and recombination properties under large Coulomb interaction. It is strongly suggested that bound exciton emission dominates the recombination process related to the N acceptor. The recombination lifetime is 750 ps and the binding energy is 67 meV for N-acceptor-bound exciton at low temperature. (c) 2006 American Institute of Physics.
Resumo:
The valence band structures of Al-N-codoped [ZnO:(Al, N)] and N-doped (ZnO:N) ZnO films were studied by normal and soft x-ray photoelectron spectroscopy. The valence-band maximum of ZnO:(Al, N) shifts up to Fermi energy level by about 300 meV compared with that of ZnO:N. Such a shift can be attributed to the existence of a kind of Al-N in ZnO:(Al, N), as supported by core level XPS spectra and comparison of modified Auger parameters. Al-N increased the relative quantity of Zn-N in ZnO:(Al, N), while N-N decreased that of Zn-N in ZnO:N. (c) 2006 American Institute of Physics.
Resumo:
High quality ZnO films have been successfully grown on a Si (100) substrate by metal organic chemical vapour deposition with a gamma-Al2O3 buffer. The crystal structure, surface morphology and optical properties of the ZnO films were characterized by x-ray diffraction, Raman spectroscopy, atomic force microscopy and photoluminescence (PL) spectroscopy. The propel-ties of the films with the Al2O3 buffer were improved in comparison with those of as-grown ZnO films. It is shown that the ZnO films with the gamma-Al2O3 buffer grown on Si (100) substrates have a highly-preferential c-axis (0002) orientation, a narrow (0002) peak, smooth surface morphology and better PL spectral properties. This demonstrates that the use of gamma-Al2O3/Si as a ZnO substrate is beneficial for reducing the residual stress for further growth of ZnO films, compared with the growth on bulk Si substrates.
Resumo:
Defects in ZnO films grown by radio-frequency reactive magnetron sputtering under variable ratios between oxygen and argon gas have been investigated by using the monoenergetic positron beam technique. The dominate intrinsic defects in these ZnO samples are O vacancies (V-O) and Zn interstitials (Zn-i) when the oxygen fraction in the O-2/Ar feed gas does not exceed 70% in the processing chamber. On the other hand, zinc vacancies are preponderant in the ZnO Elms fabricated in richer oxygen environment. The concentration of zinc vacancies increases with the increasing (2) fraction. For the oxygen fraction 85%, the number of zinc vacancies that could trap positrons will be smaller. It is speculated that some unknown defects could shield zinc vacancies. The concentration of zinc vacancies in the ZnO films varies with the oxygen fraction in the growth chamber, which is in agreement with the results of photoluminescence spectra.
Resumo:
The band structures of wurtzite ZnO are calculated using the empirical pseudopotential method (EPM). The 8 parameters of the Zn and O atom pesudopotential form factors with Schluter's formula are obtained. The effective mass parameters are extracted by using k.p Hamiltonian to fit the EPM results. The calculated band edge energies (E-g, E-A, E-B, and E-C) at Gamma point are in good agreement with experimental results. The ordering of ZnO at the top of valence band is found to be A(Gamma(7))-B(Gamma(9))-C(Gamma(7)) due to a negative spin-orbit (SO) splitting. Based on the band parameters obtained, the valence hole subbands of wurzite ZnO/MgxZn1-xO tensile-strained quantum wells (QWs) with different well widths and Mg compositions are calculated using 6-band k.p method. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
A new type of self-aligned spotsize converter (SSC) integrated 1.55 mum DFB lasers had been proposed in this article. The upper optical confinement layer and the butt-coupled tapered thickness waveguide were regrown simultaneously, which not only offered the separate optimization of the active region and the integrated SSC, but also reduced the difficulty of the butt-joint selective regrowth. The vertical and horizontal far field angles were 9degrees and 12degrees respectively, the 1- dB misalignment tolerance were both 3.6 and 3.4 mum. The directed coupling efficiency to tapered single mode fiber was 48%.
Resumo:
The growth pressure and mask width dependent thickness enhancement factors of selective-area MOCVD. grow th were investigated in this article. A, high enhancement of 5.8 was obtained at 130 mbar with the mask width of 70 mum. Mismatched InGaAsP (-0.5%) at the maskless region which could ensure the material at butt-joint region to be matched to InP was successively grown by controlling the composition and mismatch modulation in the selective-area growth. The upper optical confinement layer and the butt-coupled tapered thickness waveguide were regrown simultaneously in separated confined heterostructure 1.55 gm distributed feedback laser, which not only offered the separated optimization of the active region and the integrated spotsize converter, but also reduced the difficulty of the butt-joint selective regrowth. A narrow beam of 9degrees and 12degrees in the vertical and horizontal directions, a low threshold current of 6.5 mA was fabricated by using this technique. (C) 2003 Elsevier Science B.V. All rights reserved.
Resumo:
The Raman spectra of GaP nanorods grown in carbon nanotube templates have been reported. The red shifts of the TO and LO modes were observed due to phonon confinement effect in GaP nanorods. The measured red shifts range from 2 to 10cm(-1) depending on the size of the measured nanorods. It has been found that the polarization properties, which cannot be well explained by the selection rules of single nanorod, result from the direction disorder of nanorods in the measured area. The more the disorder is, the weaker the directionality of polarization properties is. The decrease of the Raman frequency of the TO and LO mode of the nanorods with the increasing power of the exciting laser suggests that the heating effect of the nanorods is far stronger than the bulk material. In addition, the saturation and then decrease of the Raman intensity with the increasing laser power indicate the rapid increase of the defects in the nanorods exposed to a strong exciting laser.
Resumo:
The effect of the growth temperature on the properties of InAlAs/AlGaAs quantum dots grown on GaAs(100) substrates is investigated. The optical efficiency and structural uniformity are improved by increasing the growth temperature from 530 to 560 degreesC. The improvements of InAlAs/AlGaAs quantum-dot characteristics could be explained by suppressing the incorporation of oxygen and the formation of group-III vacancies. Furthermore, edge-emitting laser diodes with six quantum-dot layers grown at 560 degreesC have been fabricated. Lasing occurs via the ground state at 725 nm, with a room-temperature threshold current density of 3.9 kA/cm(2), significantly better than previously reported values for this quantum-dot systems. (C) 2002 American Institute of Physics.