Hydrated bacterial cellulose (BC) membranes obtained from cultures of Acetobacter xylinum were used in the preparation of silver nanoparticles containing cellulose membranes. In situ preparation of Ag nanoparticles was achieved from the hydrolytic decomposition of silver triethanolamine (TEA) complexes. Scanning electron microscopy (SEM) images and X-ray diffraction (XRD) patterns both lead to the observation of spherical metallic silver particles with mean diameter of 8 nm well adsorbed onto the BC fibriles. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Foram preparados os ditizonatos de Hg (I), Ag (I) e Bi (III). Termogravimetria (TG), termogravimetria derivada (DTG), calorimetria exploratória diferencial (DSC), difratometria de raios X pelo método do pó e análise elementar foram usados para caracterizar e para estudar a estabilidade térmica e a decomposição térmica da ditizona e destes ditizonatos.
Resumo:
Electrical resistivity measurements and scanning electron microscopy was used to study the dissolution of silver on Cu-Ag and Cu-Al-Ag alloys. The results seem to indicate that the dissolution temperature is affected by the addition of aluminium.
Resumo:
The use of internal standardization for simultaneous atomic absorption spectrometry (SIMAAS) was investigated for Cd and Pb determination in whole blood. The comparison of thermochemical and physicochemical parameters allowed the selection of Ag, Bi, and Tl as internal standard candidates. Correlation graphs, plotted from the normalized absorbance signals (n = 20) of internal standard (axis y) versus analyte ( axis x), precision and accuracy were used to select Ag as the most appropriate internal standard. Blood samples were diluted (1 + 9) with 0.11% (m/v) Triton X-100 + 1.1% (v/v) HNO3 + 0.28% (m/v) NH4H2PO4 + 10 mug L-1 Ag+. Pyrolysis and atomization temperatures for the optimized heating program were 550 and 1700 degreesC, respectively. Characteristic masses based on integrated absorbance were 1.68 +/- 0.01 pg for Cd and 30.3 +/- 0.1 pg for Pb. The detection limits (DL) were 0.095 +/- 0.001 mug L-1 and 0.86 +/- 0.01 mug L-1 for Cd and Pb, respectively. The mean RSD for all determinations was the same for Cd (13 +/- 9%) with or without Ag as internal standard ( IS). on the other hand, the use of Ag as IS improved the RSD for Pb from 3.6 +/- 4.0% to 2.2 +/- 2.0%. An effective contribution of the internal standard Ag was verified in the recoveries of spiked samples (0.5 mug L-1 Cd2+ and 5.0 mug L-1 Pb2+). The mean recoveries were 81 +/- 8% and 91 +/- 4% for Cd, and 80 +/- 11% and 93 +/- 6% for Pb without and with IS correction, respectively. This is the first application of IS for a simultaneous determination by SIMAAS.
Resumo:
The speciose Brazilian Elateridae fauna is characterized by high karyotypic diversity, including one species (Chalcolepidius zonatus Eschscholtz, 1829) with the lowest diploid number within any Coleoptera order. Cytogenetic analysis of Conoderus dimidiatus Germar, 1839, C. scalaris (Germar, 1824,) C. ternarius Germar, 1839, and C. stigmosus Germar, 1839 by standard and differential staining was performed with the aim of establishing mechanisms of karyotypic differentiation in these species. Conoderus dimidiatus, C. scalaris, and C. ternarius have diploid numbers of 2n(male) = 17 and 2n(female) = 18, and a X0/XX sex determination system, similar to that encountered in the majority of Conoderini species. The karyotype of C. stigmosus was characterized by a diploid number of 2n=16 and a neoXY/neoXX sex determination system that was highly differentiated from other species of the genus. Some features of the mitotic and meiotic chromosomes suggest an autosome/ancestral X chromosome fusion as the cause of the neoXY system origin in C. stigmosus. C-banding and silver impregnation techniques showed that the four Conoderus species possess similar chromosomal characteristics to those registered in most Polyphaga species, including pericentromeric C band and autosomal NORs. Triple staining techniques including CMA(3)/DA/DAPI also provided useful information for differentiating these Conoderus species. These techniques revealed unique GC-rich heterochromatin associated with NORs in C. scalaris and C. stigmosus and CMA(3)-heteromorphism in C. scalaris and C. ternarius.
Resumo:
Nucleoli are the sites of biosynthesis of ribosomal precursors. In this work the nucleolar activity at interphase and the meiotic cells of the testis in five species of triatomines were analysed by means of silver staining. Several nucleolar blocks in the polyploid nuclei of testicular tubules were observed, whereas only one nucleolar body could be seen in the spermatogonial nuclei of all five species. A single nucleolar body was evident in the 'confused stage' of Triatoma brasiliensis, T. delpontei, T. lecticularia and T. rubrovaria, while T. sordida presented two nucleolar dots. The existence of small, silver-stained dots in some metaphase I chromosomes of T. brasiliensis and T. sordida is reported. The number of nucleolar dots present in spermatids of each species varied within and among species. It is suggested that in addition to providing information on rRNA biosynthesis, studies of nucleolar organizing activity can also be important sources of data on differentiation patterns and species development.
Resumo:
Monofilamentary tapes (150 pm thickness) were prepared by swaging and rolling silver tubes containing the Bi:2212 ceramic (granulation below 20 mum) and the silver powder (about 0.8 mum). The study has been made, among other samples, on tapes with nominal proportions of 0, 10 and 20 wt.% of silver. The samples were characterized by SEM, and by electrical measurements under varying applied magnetic field. The measurements of J(c) showed that the addition of 10 wt.% silver powder is very beneficent to this property, doubling the obtained values at 60 K, while the 20 wt.% tape presented very low J(c). The tape with no silver content showed to have a J(c) as high as 2.2 x 10(5) A/cm(2), at 4.2 K, zero applied magnetic field. (C) 2004 Elsevier B.V. All rights reserved.