989 resultados para LASER MATERIALS
Resumo:
The effects of laser phototherapy on the release of growth factors by human gingival fibroblasts were studied in vitro. Cells from a primary culture were irradiated twice (6 h interval), with continuous diode laser [gallium-aluminum-arsenium (GaAlAs), 780 nm, or indium-gallium-aluminum-phosphide (InGaAlP),_660 nm] in punctual and contact mode, 40 mW, spot size 0.042 cm(2), 3 J/cm(2) and 5 J/cm(2) (3 s and 5 s, respectively). Positive [10% fetal bovine serum (FBS)] and negative (1%FBS) controls were not irradiated. Production of keratinocyte growth factor (KGF) and basic fibroblast growth factor (bFGF) was quantified by enzyme-linked immunosorbent assay (ELISA). The data were statistically compared by analysis of variance (ANOVA) followed by Tukey`s test (P a parts per thousand currency signaEuro parts per thousand 0.05). The characterization of the cell line indicated a mesenchymal nature. KGF release was similar in all groups, while that of bFGF was significantly greater (1.49-times) in groups treated with infra-red laser. It was concluded that increased production of bFGF could be one of the mechanisms by which infra-red laser stimulates wound healing.
Resumo:
Y2O3 is a c-type rare earth oxide with a fluorite-related structure. This material has been used to refractory because of its high thermal stability and excellent resistance to hydration. In this study, the effective index was suggested in order to improve the electrolytic properties of Y2O3-based oxide. (CexY1-x)(2)O3+delta (x = 0.25 and 0.3) and [LaaSrbCe0.25Y(1-a-b)](2)O3+delta (a = 0.05, 0.1 and 0.15, b = 0, 0.006 and 0.0125) were prepared as the examples with intermediate and high index, respectively. The specimens with high index value such as (La0.15Ce0.25Y0.60)(2)O-3.25 and (La0.1Sr0.0125Ce0.25Y0.6375)(2)O-3.24 consisted of two phases such as c-type and fluorite, although (Ce0.25Y0.75)(2)O-3.25 with intermediate index value had a single phase of c-type rare earth oxide. Microanalysis indicates that a grain in the (La0.1Sr0.0125Ce0.25Y0.6375)(2)O-3.23(7) sintered body consists of c-type and fluorite phases. An interface between c-type and fluorite phases is coherent in a grain. This suggests that this effective index guides the crystal structure in the specimen to fluorite and the examined composition introduces the interface between c-type and fluorite in the microstructure. The electrochemical properties of specimens including Y2O3 were characterized on the basis of the suggested index. The electrical conductivity of Y2O3-based materials increased with an increase of the index. The apparent activation energy of Y2O3-based materials decreased with increasing index. The ionic transport number of oxygen of the specimens was improved by enhancement of the index, confirming validity of the index. The oxide ionic conductive region of (La0.1Sr0.0125Ce0.25Y0.(6375))(2)O-3.23(7) with high effective index extended up to P-O2 = 10(-18) atm at 800 degreesC, although the specimens with low or intermediate index showed p- or n-type semi-conduction in the same P-O2 region at 800 and 1000 degreesC. These results suggest that the interface between c-type and fluorite phases also contributes to improve the electrolytic properties in the grain. It is concluded that the improvement of electrolytic properties in Y2O3-based materials is attributable to the microstructure with interface between two phases in a grain and the fluorite structure guided by the suggested index. (C) 2001 Published by Elsevier Science B.V.
Resumo:
Purpose: To test the strength to failure and fracture mode of three indirect composite materials directly applied onto Ti-6Al-4V implant abutments vs cemented standard porcelain-fused-to-metal (PFM) crowns. Materials and Methods: Sixty-four locking taper abutments were randomly allocated to four groups and were cleaned in ethanol in an ultrasonic bath for 5 min. After drying under ambient conditions, the abutments were grit blasted and a custom 4-cusp molar crown mold was utilized to produce identical crowns (n = 16 per group) of Tescera (Bisco), Ceramage (Shofu), and Diamond Crown (DRM) according to the manufacturer`s instructions. The porcelain-fused-to-metal crowns were fabricated by conventional means involving the construction and a wax pattern and casting of a metallic coping followed by sintering of increasing layers of porcelain. All crowns were loaded to failure by an indenter placed at one of the cusp tips at a 1 mm/min rate. Subsequently, fracture analysis was performed by means of stereomicroscopy and scanning electron microscopy. One-way ANOVA at 95% level of significance was utilized for statistical analysis. Results: The single load to failure (+/- SD) results were: Tescera (1130 +/- 239 N), Ceramage (1099 +/- 257 N), Diamond Crown (1155 +/- 284 N), and PFM (1081 +/- 243 N). Stereomicroscopy analysis showed two distinct failure modes, where the loaded cusp failed either with or without abutment/metallic coping exposure. SEM analysis of the fractures showed multiple crack propagation towards the cervical region of the crown below a region of plastic deformation at the indenter contact region. Conclusion: The three indirect composites and PFM systems fractured at loads higher than those typically associated with normal occlusal function. Although each material had a different composition and handling technique, no significant differences were found concerning their single load to fracture resistance among composite systems and PFM.
Resumo:
Ameloblastoma is a benign locally aggressive infiltrative odontogenic lesion. It is characterized by slow growth and painless swelling. The treatment for ameloblastoma varies from curettage to en bloc resection, and the reported recurrence rates after treatment are high; the safety margin of resection is important to avoid recurrence. Advances in technology brought about great benefits in dentistry; a new generation of computed tomography scanners and 3-dimensional images enhance the surgical planning and management of maxillofacial tumors. The development of new prototyping systems provides accurate 3D biomodels on which surgery can be simulated, especially in cases of ameloblastoma, in which the safety margin is important for treatment success. A case of mandibular follicular ameloblastoma is reported where a 3D biomodel was used before and during surgery.
Resumo:
Objectives: The aim of this study was to assess the influence of irradiation distance and the use of cooling in the Er:YAG laser efficacy in preventing enamel demineralization. Methods: 84 enamel blocks were randomly assigned to seven groups (n = 12): G1: control group - no treatment, G2-G7: experimental groups treated with Er:YAG laser (80 mJ/2 Hz) at different irradiation distances with or without cooling: G2: 4 mm/2 mL; G3: 4 mm/no cooling; G4: 8 mm/2 mL; G5: 8 mm/no cooling; G6: 16 mm/2 mL; G7: 16 mm/no cooling. The samples were submitted to an in vitro pH cycles for 14 days. Next, the specimens were sectioned in sections of 80-100 mu m in thickness and the demineralization patterns of prepared slices were assessed using a polarized light microscope. Three samples from each group were analyzed with scanning electronic microscopy. Analysis of variance and the Fisher test were performed for the statistical analysis of the data obtained from the caries-lesion-depth measurements (CLDM) (alpha = 5%). Results: The control group (CLDM = 0.67 mm) was statistically different from group 2 (CLDM = 0.42 mm), which presented a smaller lesion depth, and group 6 (0.91 mm), which presented a greater lesion depth. The results of groups 3 (CLDM = 0.74 mm), 4 (CLDM = 0.70 mm), 5 (CLDM = 0.67 mm) and 7 (CLDM = 0.89 mm) presented statistical similarity. The scanning electronic microscopy analysis showed ablation areas in the samples from groups 4, 5, 6 and 7, and a slightly demineralized area in group 2. Conclusions: It was possible to conclude that Er:YAG laser was efficient in preventing enamel demineralization at a 4-mm irradiation distance using cooling. (C) 2010 Elsevier Ltd. All rights reserved.
Effect of erbium:yttrium-aluminum-garnet laser energies on superficial and deep dentin microhardness
Resumo:
This study evaluated the microhardness of superficial and deep dentin irradiated with different erbium:yttrium-aluminum-garnet (Er:YAG) laser energies. Seventy-two molars were bisected and randomly assigned to two groups (superficial dentin or deep dentin) and into six subgroups (160 mJ, 200 mJ, 260 mJ, 300 mJ, 360 mJ, and control). After irradiation, the cavities were longitudinally bisected. Microhardness was measured at six points (20 A mu m, 40 A mu m, 60 A mu m, 80 A mu m, 100 A mu m, and 200 A mu m) under the cavity floor. Data were submitted to analysis of variance (ANOVA) and Fisher`s tests (alpha = 0.05). Superficial dentin presented higher microhardness than deep dentin; energy of 160 mJ resulted in the highest microhardness and 360 mJ the lowest one. Values at all points were different, exhibiting increasing microhardness throughout; superficial dentin microhardness was the highest at 20 A mu m with 160 mJ energy; for deep dentin, microhardness after irradiation at 160 mJ and 200 mJ was similar to that of the control. The lowest energy increased superficial dentin microhardness at the closest extent under the cavity; deep dentin microhardness was not altered by energies of 160 mJ and 200 mJ.
Resumo:
The purpose of this study was to evaluate the effect of diode laser (GaAlAs - 780 nm) on pain to palpation and electromyographic (EMG) activity of the masseter and anterior temporalis muscles. The laser was applied on the temporalis and masseter muscles twice a week (four weeks). Forty-eight (48) patients with myofascial pain were randomly assigned between actual and placebo treatments and between the energetic doses of 25 J/cm(2) and 60 J/cm(2), and were evaluated using VAS before, immediately after the final application, and 30 days after the laser treatment. Surface electromyography was performed with maximum dental clenching before and after laser therapy. The results show there were no significant statistical differences in the EMG activity between the groups before and after laser treatment. With regard to the pain at palpation, although both groups presented a significant difference in the symptoms before and after the treatment, only the active doses showed statistically significant reductions in pain level in all the regions of the palpated muscles. However, there was no significant statistical difference between groups (experimental and placebo). In conclusion, low level laser did not promote any changes in EMG activity. The treatment did, however, lessen the pain symptoms in the experimental groups.
Resumo:
Background: There are no reported studies comparing different parameter settings of the CO(2) laser and irradiation direction considering their effect on the morphology of radicular dentine surface. Purpose: To evaluate the alterations of radicular dentine (cervical, middle, and apical thirds) irradiated with CO(2) laser at different potencies and irradiation directions. Study Design: Roots of 35 canines were prepared and randomly distributed according to the laser potency: GI: no laser treatment (control) (n = 5); GII, 2 W (n = 10); GIII: 4 W (n = 10); GIV: 6 W (n = 10). Each group (excepting GI) was divided in two subgroups according to the irradiation distance (n = 5): (A) parallel and (B) perpendicular to the root canal walls. The roots were splited longitudinally and analyzed by scanning electron microscopy in a qualiquatitative way. The scores were submitted to Kruskal-Wallis and Dunn`s tests. Results: No significant statistical differences were observed among root canal thirds (P > 0.05). The specimens irradiated with 2 W were statistically different (P < 0.05) from those irradiated with 4 and 6 W, which were statistically similar between themselves (P > 0.05). With 2, 4, and 6 W at in parallel irradiation and 2 W in perpendicular direction, the surface showed a fissured aspect. With 4 W in perpendicular direction and 6 W in parallel and perpendicular direction, surface was modified by laser action and exhibited fused areas. Conclusions: The intensity of the effects is dependent on the laser-irradiation dosimetries. Alterations were more intense when higher parameters were used. Microsc. Res. Tech. 72:737-743, 2009. (C) 2009 Wiley-Liss, Inc.
Resumo:
The Epiphany (TM) Sealer is a new dual-curing resin-based sealer and has been introduced as an alternative to gutta-percha and traditional root canal sealers. The canal filling is claimed to create a seal with the dentinal tubules within the root canal system producing a `monoblock` effect between the sealer and dentinal tubules. Therefore, considering the possibility to incorporate the others adhesive systems, it is important to study the bond strength of the resulting cement. Forty-eight root mandibular canines were sectioned 8-mm below CEJ. The dentine discs were prepared using a tapered diamond bur and irrigated with 1% NaOCl and 17% EDTA. Previous the application Epiphany (TM) Sealer, the Epiphany (TM) Primer, AdheSE, and One Up Bond F were applied to the root canal walls. The LED and QTH (Quartz Tungsten Halogen) were used to photo-activation during 45 s with power density of 400 and 720 mW/cm(2), respectively. The specimens were performed on a universal testing machine at a cross-head speed of 1 mm/min until bond failure occurred. The force was recorded and the debonding values were used to calculate Push-out bond strength. The analysis of variance (ANOVA) and Tukey`s post-hoc tests showed significant statistical differences (P < 0.05) to Epiphany (TM) Sealer/Epiphany (TM) Primer/QTH and EpiphanyTM Sealer/AdheSE/QTH, which had the highest mean values of bond strength. The efficiency of resin-based filling materials are dependent the type of light curing unit used including the power density, the polymerization characteristics of these resin-based filling materials, depending on the primer/adhesive used.
Resumo:
Background: The topographical features of intraradicular dentine pretreated with sodium hypochlorite (NaOCl) or ethylenediamine tetraacetic acid (EDTA) followed by diode laser irradiation have not yet been determined. Purpose: To evaluate the alterations of dentine irradiated with 980-nm diode laser at different parameters after the surface treatment with NaOCl and EDTA. Study design: Roots of 60 canines were biomechanically prepared and irrigated with NaOCl or EDTA. Groups were divided according to the laser parameters: 1.5 W/CW; 1.5 W/100 Hz; 3.0 W/CW; 3.0 W/100 Hz and no irradiation (control). The roots were splited longitudinally and analyzed by scanning electron microscopy (SEM) in a quali-quatitative way. The scores were submitted to two-way Kruskal-Wallis and Dunn`s tests. Results: The statistical analysis demonstrated that the specimens treated only with NaOCl or EDTA (control groups) were statistically different (P < 0.05) from the laser-irradiated specimens, regardless of the parameter setting. The specimens treated with NaOCl showed a laser-modified surface with smear layer, fissures, and no visible tubules. Those treated with EDTA and irradiated by laser presented absence of smear layer, tubules partially exposed and melting areas. Conclusions: The tested parameters of 980-nm diode laser promoted similar alterations on dentine morphology, dependent to the type of surface pretreatment. Microsc. Res. Tech. 72:22-27, 2009. (C) 2008 Wiley-Liss, Inc.
Resumo:
P>Aim To evaluate by 3D profilometry and scanning electron microscopy (SEM), the marginal adaptation of mineral trioxide aggregate (MTA) and Sealer 26 placed in root-end cavities with direct vision or under an optical microscope. Methodology The root ends of 52 root filled canine teeth were filled with MTA or Sealer 26 under direct vision or optical microscope (n = 13). In each group, eight specimens were analysed by profilometry for measurement of the area and depth of gaps. In the other five specimens, gap area was measured using SEM to verify marginal adaptation and surface characteristic. Data were analysed by parametric (anova and Tukey) and non-parametric (Kruskal-Wallis and Dunn) tests. Results The assessment of the adaptation of both materials to dentine was not influenced by the mode of visualization, which was confirmed by both profilometry and SEM observations. The voids measured with profilometry for Sealer 26 under direct vision were significantly wider and deeper than those for MTA under direct vision (P < 0.05). In SEM, significantly larger gap areas were observed with Sealer 26 (P < 0.05). Conclusion Root-end cavities filled with MTA had smaller gaps and better marginal adaptation than Sealer 26.
Resumo:
The purpose of this study was to evaluate the analgesic effect of Low Intensity Laser Therapy (LILT) and its influence on masticatory efficiency in patients with temporomandibular dysfunction (TMD). This study was performed using a random, placebo-controlled, and double-blind research design. Fourteen patients were selected and divided into two groups (active and placebo). Infrared laser (780 nm, 70 mw, 60s, 105J/cm(2)) was applied precisely and continuously into five points of the temporomandibular joint (TMJ) area: lateral point (LP), superior point (SP), anterior point (AP), posterior point (PP), and posterior-inferior point (PIP) of the condylar position. This was performed twice per week, for a total of eight sessions, To ensure a double-blind study, two identical probes supplied by the manufacturer were used: one for the active laser and one for the inactive placebo laser. They were marked with different letters (A and B) by a clinician who did not perform the applications. A Visual Analogue Scale (VAS) and a colorimetric capsule method were employed. Data were obtained three times: before treatment (Ev1), shortly after the eighth session (Ev2), and 30 days after the first application (Ev3). Statistical tests revealed significant differences at one percent (1%) likelihood, which implies that superiority of the active group offered considerable TMJ pain improvement. Both groups presented similar masticatory behavior, and no statistical differences were found. With regard to the evaluation session, Ev2 presented the lowest symptoms and highest masticatory efficiency throughout therapy. Therefore, low intensity laser application is effective in reducing TMD symptoms, and has influence over masticatory efficiency [Ev2 (0.2423) and Ev3 (0.2043), observed in the interaction Evaluations x Probes for effective dosage].
Resumo:
Aim To evaluate the bond strength of AH Plus and Epiphany sealers to human root canal dentine irradiated with a 980 nm diode laser at different power and frequency parameters, using the push-out test. Methodology Sixty canine roots were sectioned below the cementoenamel junction to provide 4-mm-thick dentine discs that had their root canals prepared with a tapered bur and irrigated with sodium hypochlorite, ethylenediaminetetraacetic acid and distilled water. The specimens were assigned to five groups (n = 12): one control (no laser) and four experimental groups that were submitted to 980 nm diode laser irradiation at different power (1.5 and 3.0 W) and frequency (continuous wave and 100 Hz) parameters. Half of specimens in each group had their canals filled with AH Plus sealer and half with Epiphany. The push-out test was performed and data (MPa) were analysed statistically by ANOVA and Tukey`s test (P < 0.05). The specimens were split longitudinally and examined under SEM to assess the failure modes after sealer displacement. Results The specimens irradiated with the diode laser and filled with AH Plus had significantly higher bond strength values (8.69 +/- 2.44) than those irradiated and filled with Epiphany (3.28 +/- 1.58) and the nonirradiated controls (3.86 +/- 0.60). The specimens filled with Epiphany did not differ significantly to each other or to the control (1.75 +/- 0.69). There was a predominance of adhesive failures at Epiphany-dentine interface (77%) and mixed failures at AH Plus-dentine interface (67%). Conclusions The 980 nm diode laser irradiation of root canal dentine increased the bond strength of AH Plus sealer, but did not affect the adhesion of Epiphany sealer.
Resumo:
Objectives: To evaluate the bonding interface in experimentally weakened roots reinforced with adhesive restorative materials and quartz fibre posts, varying the light-exposure time of the composite resin used for root reinforcement. Methods: Twelve extracted human maxillary incisors teeth were used. The crowns were removed and the roots were endodontically treated. After post space preparation, the roots were assigned to four groups. The thickness of the root dentine was reduced and adhesively restored with composite resin light-activated through a translucent fibre post for either 40 s (group 1), 80 s (group 2) or 120 s (group 3). In the case of control (group 4), the roots were not weakened. One day after post cementation, the specimens were sectioned transversally in three slices and processed for scanning electron microscopic analysis to observe bonding interface formation, quality of the hybrid layer and density of resin tags using a four-step scale method. Results: Formation of a hybrid layer and resin tags were evident in all groups. There was no statistically (p > 0.05) significant difference between the regions analysed in each group (Friedman test) and between groups in each section depth (Kruskal-Wallis test). Furthermore, comparison of the flared/reinforced groups showed that the different time;; used for composite resin cure did not affect the results significantly (Kruskal-Wallis test, p = 0.2139). Conclusions: Different light-exposure times used for composite resin polymerisation during root canal reinforcement did not affect significantly the formation and quality of the dentine/adhesive/composite resin bonding interface. (C) 2008 Elsevier Ltd. All rights reserved.