Resumo:
Electrically active deep levels related to nickel in silicon are studied under different diffusion conditions, quenching modes, and annealing conditions. The main nickel-related level is at Ev+0.32 eV. Levels at Ev+0.15 and Ev+0.54 eV are not related to nickel while those at Ev+0.50 and Ev+0.28 eV may be nickel related. Their concentrations depend on the quenching mode. There is no nickel-related level in the upper half of the band gap. The complicated annealing behavior of the main nickel-related level is explained on the basis of the formation and dissociation of a nickel-vacany complex. Journal of Applied Physics is copyrighted by The American Institute of Physics.
Resumo:
Electrical properties of deep defects induced in n-silicon by -particles of about 10 MeV energy at a dose of 1014 and 1015 cm-2 are studied by DLTS. The levels at Ec -0.18 eV, Ec -0.26 eV, and Ec -0.48 eV are identified as A center, V2 (=/-) and V2 (-/0) on the basis of activation energy, electron capture cross section, and annealing behavior. Two other irradiation related levels at Ec -0.28 eV and Ec -0.51 eV could not be related to any known center.
Resumo:
Silicon has demonstrated great potential as anode materials for next-generation high-energy density rechargeable lithium ion batteries. However, its poor mechanical integrity needs to be improved to achieve the required cycling stability. Nano-structured silicon has been used to prevent the mechanical failure caused by large volume expansion of silicon. Unfortunately, pristine silicon nanostructures still suffer from quick capacity decay due to several reasons, such as formation of solid electrolyte interphase, poor electrical contact and agglomeration of nanostructures. Recently, increasing attention has been paid to exploring the possibilities of hybridization with carbonaceous nanostructures to solve these problems. In this review, the recent advances in the design of carbon-silicon nanohybrid anodes and existing challenges for the development of high-performance lithium battery anodes are briefly discussed.
Resumo:
Aluminum-silicon alloy pins were slid against steel disks under nominally dry condition at a speed of 0.6 m s-1. Each pin was slid at a constant load for 5 min, the load being increased in suitable steps from 2 to 65 N. The results show the wear to increase almost monotonically with load, to be sensitive to the presence of silicon in the alloy, and to be insensitive to actual silicon content. The monotonic nature of wear rate-load characteristic suggests that one dominant wear mechanism prevails over the load range studied. Morphological studies of the pin surface and the debris support this contention and point to delamination as being the dominant mode of wear.
Resumo:
There has been a lot of effort to make Silicon optically active. In this work we examine two methods of generating nanocrystals of Silicon from bulk fragments. This approach of ours allows us to play with the shape of the nanocrystals and therefore the degeneracy of the conduction band minimum. We go on to examine whether similar sized particles with different shapes have the same physical properties, and finally whether Silicon may be rendered optically active by this route. While we do find that similar sized particles with different shapes may have different band gaps, this route of modifying the degeneracy of the conduction band minimum makes nano Si slightly optically active.
Resumo:
The apparent thermal activation energy of 0.56 eV and the electron thermal capture cross section of 2.0 × 10-16 cm2 are measured for the gold related acceptor level in p+ nn+ silicon diodes by isothermal current transient and DLTS techniques. Using the emission and capture rate data and a degeneracy ratio of 2, the energy separation of the trap level from the conduction band is calculated and found to have the same temperature dependence as the band gap indicating that the acceptor level is pinned with respect to the valence band a t Ev + 0.637 eV.
Resumo:
Silicon tetrahalides, SiX4 (X=F, Cl, Br) and the fluorosilicates of sodium and potassium react with phosphorus pentoxide above 300°C. The tetrahalides give rise to the corresponding phosphoryl halides and silica, while the fluorosilicates form the corresponding metal fluorophosphates and silicon tetrafluoride. The reaction of the fluorosilicates of sodium and potassium with sulphur trioxide occurs at room temperature to give rise to the corresponding metal fluorosulphates and silicon tetrafluoride.
Resumo:
Few-layer graphene films were grown by chemical vapor deposition and transferred onto n-type crystalline silicon wafers to fabricate graphene/n-silicon Schottky barrier solar cells. In order to increase the power conversion efficiency of such cells the graphene films were doped with nitric acid vapor and an antireflection treatment was implemented to reduce the sunlight reflection on the top of the device. The doping process increased the work function of the graphene film and had a beneficial effect on its conductivity. The deposition of a double antireflection coating led to an external quantum efficiency up to 90% across the visible and near infrared region, the highest ever reported for this type of devices. The combined effect of graphene doping and antireflection treatment allowed to reach a power conversion efficiency of 8.5% exceeding the pristine (undoped and uncoated) device performance by a factor of 4. The optical properties of the antireflection coating were found to be not affected by the exposure to nitric acid vapor and to remain stable over time.
Resumo:
Molybdenum trioxide (MoO3) has been deposited onto single-crystal p-type silicon by neutralized ion-beam sputter techniques. The results indicate that the diode behavior is a function of oxygen partial pressure during the reactive sputtering. Film thickness, deposition rate, index of refraction, resistivity, and integrated transmission have been measured under AM1 illumination. It appears that thin films of MoO3 could serve as an n-type transparent semiconductor for photovoltaic applications. Applied Physics Letters is copyrighted by The American Institute of Physics.
Resumo:
A mathematical model for doped-oxide-source diffusion is proposed. In this model the concept of segregation of impurity at the silicon-silicon dioxide is used and also a constant of “rate limitation” is introduced through a chemical reaction at the interface.
Role of silicon in resisting subsurface plastic deformation in tribology of aluminium-silicon alloys
Resumo:
Silicon particles standing proud on aluminium-silicon alloy surfaces provide protection in tribology. Permanent sinking of such particles into the matrix under load can be deleterious. The mechanical response of the alloy to nano-indentation of single silicon particles embedded in the matrix is explored. A nominal critical pressure required to plastically deform the matrix to permanently embed the particle is determined experimentally. Within a framework suggested by two-dimensional models of plastic response to indentation, a probable correlation is established between the normal mean pressure required to cause permanent sinking of silicon particles and a factor which relates the relevant particle dimensions.
Resumo:
Silicon batteries have attracted much attention in recent years due to their high theoretical capacity, although a rapid capacity fade is normally observed, attributed mainly to volume expansion during lithiation. Here, we report for the first time successful synthesis of Si/void/SiO2/void/C nanostructures. The synthesis strategy only involves selective etching of SiO2 in Si/SiO2/C structures with hydrofluoric acid solution. Compared with reported results, such novel structures include a hard SiO2-coated layer, a conductive carbon-coated layer, and two internal void spaces. In the structures, the carbon can enhance conductivity, the SiO2 layer has mechanically strong qualities, and the two internal void spaces can confine and accommodate volume expansion of silicon during lithiation. Therefore, these specially designed dual yolk-shell structures exhibit a stable and high capacity of 956 mA h g−1 after 430 cycles with capacity retention of 83%, while the capacity of Si/C core-shell structures rapidly decreases in the first ten cycles under the same experimental conditions. The novel dual yolk-shell structures developed for Si can also be extended to other battery materials that undergo large volume changes.