A folding nonblocking 4 X 4 optical matrix switch in simplified-tree architecture was designed and fabricated on a silicon-on-insulator wafer. To compress chip size, switch elements (SEs) were connected by total internal reflection mirrors instead of conventional S-bends. For obtaining smooth interfaces, potassium hydroxide (KOH) anisotropic chemical etching of silicon was employed. The device has a compact size of 20 X 3.2 mm(2) and a fast response of 8 +/- 1 mu s. Power consumption of 2 x 2 SE and excess loss per mirror were 145 mW and -1.1 dB, respectively. (c) 2005 Society of Photo-Optical Instrumentation Engineers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A folding rearrangeable nonblocking 4 x 4 optical matrix switch was designed and fabricated on silicon-on-insulator wafer. To compress chip size, switch elements (SEs) were interconnected by total internal reflection (TIR) mirrors instead of conventional S-bends. For obtaining smooth interfaces, potassium hydroxide anisotropic chemical etching of silicon was utilized to make the matrix switch for the first time. The device has a compact size of 20 x 1.6 mm(2) and a fast response of 7.5 mu s. The power consumption of each 2 x 2 SE and the average excess loss per mirror were 145 mW and -1.1 dB, respectively. Low path dependence of +/- 0.7 dB in total excess loss was obtained because of the symmetry of propagation paths in this novel matrix switch.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An optimal concentration of the etching solution for deep etching of silicon, including 3% tetramethyl ammonium hydroxide and 0.3% (NH4)(2)S2O8, was achieved in this paper. For this etching solution, the etching rates of silicon and silicon dioxide were about 1.1 mu m(.)min(-1) and 0.5 nm(.)min(-1), respectively. The etching ratio between (100) and (111) planes was about 34:1, and the etched surface was very smooth.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A low power consumption 2 x 2 thermo-optic switch with fast response was fabricated on silicon-on-insulator by anisotropy chemical etching. Blocking trenches were etched on both sides of the phase-shifting arms to shorten device length and reduce power consumption. Thin top cladding layer was grown to reduce power consumption and switching time. The device showed good characteristics, including a low switching power of 145 mW and a fast switching speed of 8 +/- 1 mus, respectively. Two-dimensional finite element method was applied to simulate temperature field in the phase-shifting arm instead of conventional one-dimensional method. According to the simulated result, a new two-dimensional index distribution of phase-shifting arm was determined. Consequently finite-difference beam propagation method was employed to simulate the light propagation in the switch, and calculate the power consumption as well as the switching speed. The experimental results were in good agreement with the theoretical estimations. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A compact optical switch matrix was designed, in which light circuits were folded by total internal reflective (TIR) mirrors. Two key elements, 2 x 2 switch and TIR mirror, have been fabricated on silicon-on-insulator wafer by anisotropy chemical etching. The 2 x 2 switch showed very low power consumption of 140 mW and a very high speed of 8 +/- 1 mus. An improved design for the TIR mirror was developed, and the fabricated mirror with smooth and vertical reflective facet showed low excess loss of 0.7 +/- 0.3 dB at 1.55 mum.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The three-dimensional morphology of In(Ga)As nanostructures embedded in a GaAs matrix is investigated by combining atomic force microscopy and removal of the GaAs cap layer by selective wet etching. This method is used to investigate how the morphology of In(Ga)As quantum dots changes upon GaAs capping and subsequent in situ etching with AsBr3. A wave function calculation based on the experimentally determined morphologies suggests that quantum dots transform into quantum rings during in situ etching. (c) 2007 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Inductively coupled plasma (ICP) etching of InP in Cl-2/BCl3 gas mixtures is studied in order to achieve low-damage and high-anisotropy etching of two-dimensional InP/InGaAsP photonic crystal. The etching mechanisms are discussed and the effect of plasma heating on wafer during etching is analyzed. It is shown that the balance between the undercut originating from plasma heating and the redeposition of sputtering on the side-wall is crucial for highly anisotropic etching, and the balance point moves toward lower bias when the ICP power is increased. High aspect-ratio etching at the DC bias of 203 V is obtained. Eventually, photonic crystal structure with nearly 90 degrees side-wall is achieved at low DC bias after optimization of the gas mixture.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We demonstrate a technique based on wet chemical etching that enables quick and accurate evaluation of edge- and screw/mixed-type threading dislocations (TDs) in GaN. Large and small etch pits are formed by phosphoric acid on the etched surfaces. The large etch pits are attributed to screw/mixed TDs and the small ones to edge TDs, according to their locations on the surface and Burgers vectors of TDs. Additionally, the origin of small etch pits is confirmed by a transmission electron microscopy. The difference in the size of etch pits is discussed in view of their origin and merging. Overetching at elevated temperatures or for a long time may result in merging of individual etch pits and underestimating of the density of TDs. Wet chemical etching has also been proved efficient in revealing the distribution of TDs in epitaxial lateral overgrowth GaN.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The crystallographic tilt of the lateral epitaxial overgrown (LEO) GaN on sapphire Substrate with SiNx mask is investiaated by double crystal X-ray diffraction. Two wing peaks beside the GaN 0002 peak can be observed for the as-grown LEO GaN. During the selective etching of SiNx mask, each wing peak splits into two peaks, one of which disappears as the mask is removed, while the other remains unchanged. This indicates that the crystallographic tilt of the overgrown region is caused not only by the plastic deformation resulted from the bending of threading dislocations, but by the non-uniformity elastic deformation related with the GaN, SiNx interfacial forces. The widths of these two peaks are also studied in this paper. (C) 2002 Elsevier Science B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Self-assembled Ge islands were grown on Si(100) substrate by Si2H6-Ge molecular beam epitaxy. After being subjected to chemical etching, it is found that the photoluminescence from the etched Ge islands became more intense and shifted to the higher-energy side compared to that of the as-deposited Ge islands. This behaviour was explained by the effect of chemical etching on the morphology of the Ge islands. Our results demonstrate that chemical etching can be a way to change the luminescence property of the as-deposited islands.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper the resonant wavelength of a long period fiber grating (LPG) is tuned toward longer wavelength by etching the fiber, For LP04 and LP05 cladding modes', the tuning ranges of 23 and 81 nm are achieved, respectively. Also the dependence of the resonant wavelength on the cladding radius of LPG is theoretically simulated. (C) 2001 Elsevier Science B,V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Self-assembled Ge islands were grown on Si (1 0 0) substrate by Si2H6-Ge molecular beam epitaxy. Subjected to a chemical etching, it is found that the size and shape (i.e. ratio of height to base width) of Ge islands change with etching time. In addition, the photoluminescence from the etched Ge islands shifted to the higher energy side compared to that of the as-deposited Ge islands. Our results demonstrated that chemical etching can be a way to change the size and shape of the as-deposited islands as well as their luminescence property. (C) 2001 Elsevier Science B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We measured the depth profiling of photoluminescence (PL) in cubic GaN films. The depth-resolved PL of normal grown GaN layers showed that the near-band-edge luminescence intensities of both cubic and wurtzite domains remained constant only until an etching depth of up to 2.7 mu m, but their ratio remained unchanged at all etching depths. Moreover, when a thin In0.1Ga0.9N layer was sandwiched between two GaN layers, the content of the wurtzite domains increased, and its distribution showed a dependence on thickness. As the reactive ion etching depth increased, the PL intensity ratio of cubic GaN to wurtzite domains increased. Based on the distribution, the strain relaxation, instead of the instability of cubic GaN at high temperature, was attributed to the origin of wurtzite domains. (C) 2000 Elsevier Science S.A. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An effective approach to enhance the light output power of InGaN/GaN light emitting diodes (LED) was proposed using pyramidal patterned sapphire substrates (PSS). The sapphire substrates were patterned by a selective chemical wet etching technique. GaN-based LEDs were fabricated on patterned sapphire substrates through metal organic chemical deposition (MOCVD). The LEDs fabricated on patterned sapphire substrates exhibit excellent device performance compared to the conventional LEDs fabricated on planar sapphire substrates in the case of the same growth and device fabricating conditions. The light output power of the LEDs fabricated on patterned sapphire substrates was about 37% higher than that of LEDs on planar sapphire substrates at an injection current of 20 mA. The significant enhancement is attributable to the improvement of the quality of GaN-based epilayers and improvement of the light extraction efficiency by patterned sapphire substrates.