952 resultados para Phase formation
Resumo:
Measurements based on absorption, reflectance, or luminescence of molecular species or complex ions can be carried out directly on a solid support simultaneously to the retention of the analyte. The use of this strategy in flow-based systems is advantageous in view of the reproducible handling of solutions in retention and elution steps of the analyte. This approach can be exploited to increase sensitivity, minimize reagent consumption as well as waste generation, improve selectivity or for simultaneous determination based on selective retention or differences in sorption rates of the analytes. This review focuses on the main characteristics of direct solid-phase measurements in flow systems, including the discussion of advantages and limitations and practical guidelines to the successful implementation of this approach. Selected applications in diverse fields, such as pharmaceutical, food, and environmental analysis are discussed.
Resumo:
The formation of the Mn(III)/EDTA complex in a flow system with solenoid micro-pumps was exploited for fast manganese determination in freshwater. Manganese(II) was oxidized in a solid-phase reactor containing lead dioxide immobilized on polyester. Long pathlength spectrophotometry was exploited to increase sensitivity, aiming to reach the threshold limit established by environmental legislation. A linear response was observed from 25 to 1500 mu g L(-1), with a detection limit of 6 mu g L(-1) (99.7% confidence level). Sample throughput and coefficient of variation were 36 samples/h and 2.6% (n = 10), respectively. EDTA consumption and waste generation were estimated as 500 mu g and 3 mL per determination, respectively. The amount of Pb in the residue corresponds to 250 mu g per determination and a solid-phase reactor could be used for up to 1600 determinations. Adsorption in active charcoal avoided interferences caused by organic matter and the developed procedure was successfully applied for determination of manganese in freshwater samples. Results were in agreement with those attained by GFAAS at the 95% confidence level. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Here we present a system of coupled phase oscillators with nearest neighbors coupling, which we study for different boundary conditions. We concentrate at the transition to the total synchronization. We are able to develop exact solutions for the value of the coupling parameter when the system becomes completely synchronized, for the case of periodic boundary conditions as well as for a chain with fixed ends. We compare the results with those calculated numerically.
Resumo:
Drosophila pair-rule genes are expressed in striped patterns with a precise order of overlap between stripes of different genes. We investigated the role of Giant (Gt) in the regulation of even-skipped, hairy, runt, and fushi tarazu stripes formed in the vicinity of Gt expression domains. In gt null embryos, specific stripes of eve, h, run, and ftz are disrupted. With an ectopic expression system, we verified that stripes affected in the mutant are also repressed. Simultaneously hybridizing gt misxpressing embryos with two pair-rule gene probes, we were able to distinguish differences in the repression of pairs of stripes that overlap extensively. Together, our results showed Gt repression roles in the regulation of two groups of partially overlapping stripes and that Gt morphogen activity is part of the mechanism responsible for the differential positioning of these stripes borders. We discuss the possibility that other factors regulate Gt stripe targets as well. Developmental Dynamics 239:2989-2999, 2010. (C) 2010 Wiley-Liss, Inc.
Resumo:
The thick weathering profiles of humid tropical areas are an important, yet generally neglected, source of information on landscape evolution. Six complete profiles of the weathering mantle were sampled by drilling on the three stepped levels of the Campos do Jordao Plateau, on the NW flank of the Continental Rift of Southeastern Brazil. Mineralogical and micromorphological analyses of drill core samples, complemented by geochemical interpretations and by previous data on the upper saprolite, indicate continuity of a general lateritic trend during the entire process of mantle formation. Lateritization phases of different intensity were defined and considered to reflect adjustment to changes in environmental conditions created by the gradual uplift of the plateau to its present position. Older and more superficial materials related to intense lateritic weathering are characterized by allitization with direct formation of gibbsite from silicates, probably related to tropical climates existing immediately before the formation of the continental rift, during the Paleogene, and also before any significant increase in altitude. Monosialitization phase with general kaolinitization and restricted indirect formation of gibbsite from silicates could be associated to less aggressive climates that followed the Neogene (Miocene?) accentuation of uplift rates along the continental rift. The changes produced by uplift in the tropical climate eventually favored the development of a podzolization trend in soils above 1800m. (C) 2011 Elsevier BM. All rights reserved.
Resumo:
In the plasma kallikrein-kinin system, it has been shown that when plasma prekallikrein (PM) and high molecular weight kininogen (HK) assemble on endothelial cells, plasma kallikrein (huPK) becomes available to cleave HK, releasing bradykinin, a potent mediator of the inflammatory response. Because the formation of soluble glycosaminoglycans occurs concomitantly during the inflammatory processes, the effect of these polysaccharides on the interaction of HK on the cell surface or extracellular matrix (ECM) of two endothelial cell lines (ECV304 and RAEC) was investigated. In the presence of Zn(+2), HK binding to the surface or ECM of RAEC was abolished by heparin; reduced by heparan sulfate, keratan sulfate, chondroitin 4-sulfate or dermatan sulfate; and not affected by chondroitin 6-sulfate. By contrast, only heparin reduced HK binding to the ECV304 cell surface or ECM. Using heparin-correlated molecules such as low molecular weight dextran sulfate, low molecular weight heparin and N-desulfated heparin, we suggest that these effects were mainly dependent on the charge density and on the N-sulfated glucosamine present in heparin. Surprisingly, PM binding to cell- or ECM-bound-HK and PM activation was not modified by heparin. However, the hydrolysis of HK by huPK, releasing BK in the fluid phase, was augmented by this glycosaminoglycan in the presence of Zn(2+). Thus, a functional dichotomy exists in which soluble glycosaminoglycans may possibly either increase or decrease the formation of BK. In conclusion, glycosaminoglycans that accumulated in inflammatory fluids or used as a therapeutic drug (e.g., heparin) could act as pro- or anti-inflammatory mediators depending on different factors within the cell environment. (C) 2011 Elsevier Masson SAS. All rights reserved.
Resumo:
This study has as objective identifies the necessary competences to the physical education teachers of the basic education, in the teachers` of the public network of teaching of the Sao Paulo state perspective, licentiates and exits of the Physical Education School and Sport of the Sao Paulo University starting from 1995. It is a qualitative research, of nature no experimental, consisting of two studies (diagnostic and deepening). As instruments, questionnaire and semi-structured interview were used. It happened what the teachers judge importantly mobilize determined knowledges placed in a hierarchy or associated during the teaching practice, such as: knowledges pedagogic-educational, technical knowledges and cultural luggage, inserted in the current context and considering the cultural, social, political, economical and education transformations occurred along the history. There was shown up in this study the relevance of the formation continued for the teachers of Physical Education, who found her essential and basic added to the initial formation.
Resumo:
In this work, Ti(92)B(8) alloy was processed via rapid solidification (splat-cooling) and then heat-treated at 700 degrees C and 1000 degrees C. A careful microstructural characterization indicated that, after rapid solidification, a very fine two-phase microstructure was produced with no significant saturation of B in alpha/beta Ti. There was no indication of amorphous formation in the rapidly solidified splats. Both alpha Ti and TiB were observed in the microstructures of the splats after heat-treatment at 700 degrees C and 1000 degrees C, confirming the stability of the alpha Ti+TiB two-phase region in this temperature range. (C) 2008 Elsevier Inc. All rights reserved.
Resumo:
Yttria stabilized tetragonal zirconia (Y-TZP) ceramics were sintered by liquid phase sintering at low temperatures using bioglass as sintering additive. ZrO2-bioglass ceramics were prepared by mixing a ZrO2 stabilized with 3 Mol%Y2O3 and different amounts of bioglass based on 3CaO center dot P2O5-MgO-SiO2 system. Mixtures were compacted by uniaxial cold pressing and sintered in air, at 1200 and 1300 degrees C for 120 min. The influence of the bioglass content on the densification, tetragonal phase stability, bending strength, hardness and fracture toughness was investigated. The ceramics sintered at 1300 degrees C and prepared by addition of 3% of bioglass, exhibited the highest strength of 435 MPa, hardness of 1170 HV and fracture toughness of 6.3 MPa m(1/2). These results are related to the low monoclinic phase content, high relative density and the presence of the thermal residual stress generated between the ZrO2-matrix and bioglass grain boundary, contributing to the activation of the toughening mechanisms. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
Ti-rich Ti-Si-B alloys can be considered for structural applications at high temperatures (max. 700 degrees C), however, phase equilibria data is reported only for T = 1250 degrees C. Thus, in this work the phase stability of this system has been evaluated at 700 degrees C. In order to attain equilibrium conditions in shorter time, rapid solidified samples have been prepared and carefully characterized. The microstructural characterization of the produced materials were based on X-ray diffraction (XRD), scanning electron microscopy (SEM-BSE), high resolution transmission electron microscopy (HRTEM), High Temperature X-ray diffraction with Synchrotron radiation (XRDSR) and Differential Scanning Calorimetry (DSC). Amorphous and amorphous with embedded nanocrystals have been observed after rapid solidification from specific alloy compositions. The values of the crystallization temperature (Tx) of the alloys were in the 509-647 degrees C temperature range. After Differential Scanning Calorimetry and High Temperature X-ray Diffraction with Synchrotron radiation, the alloys showed crystalline and basically formed by two or three of the following phases: alpha Ti, Ti(6)Si(2)B; Ti(5)Si(3); Ti(3)Si and TiB. It has been shown the stability of the Ti(3)Si and Ti(6)Si(2)B phases at 700 degrees C and the proposition of an isothermal section at this temperature. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
High-purity niobium powder can be produced via the hydrogenation and dehydrogenation processes The present work aimed at the effect of temperature and cooling rate conditions on the niobium hydrogenation process using hydrogen gas The hydrogen contents of the materials were evaluated by weight change and chemical analysis X ray diffraction (XRD) was performed to identify and determine the lattice parameters of the formed hydride phases No hydrogenation took place under isothermal conditions only during cooling of the materials Significant hydrogenation occurred in the 500 C and 700 C experiments leading to the formation of a beta NbH(x) single phase material (C) 2010 Elsevier Ltd All rights reserved
Resumo:
In this work the Mn(5)Si(3) and Mn(5)SiB(2) phases were produced via arc melting and heat treatment at 1000 degrees C for 50 h under argon. A detailed microstructure characterization indicated the formation of single-phase Mn(5)Si(3) and near single-phase Mn(5)SiB(2) microstructures. The magnetic behavior of the Mn(5)Si(3) phase was investigated and the results are in agreement with previous data from the literature, which indicates the existence of two anti-ferromagnetic structures for temperatures below 98 K. The Mn(5)SiB(2) phase shows a ferromagnetic behavior presenting a saturation magnetization M(s) of about 5.35 x 10(5) A/m (0.67 T) at room temperature and an estimated Curie temperature between 470 and 490 K. In addition, AC susceptibility data indicates no evidence of any other magnetic ordering in 4-300 K temperature range. The magnetization values are smaller than that calculated using the magnetic moment from previous literature NMR results. This result suggests a probable ferrimagnetic arrangement of the Mn moments. (C) 2009 Elsevier B. V. All rights reserved.
Resumo:
Silicon nitride ceramics were sintered using Y(2)O(3)-Al(2)O(3) or E(2)O(3)-Al(2)O(3) (E(2)O(3) denotes a mixed oxide Of Y(2)O(3) and rare-earth oxides) as sintering additives. The intergranular phases formed after sintering was investigated using high-resolution X-ray diffraction (HRXRD). The use of synchrotron radiation enabled high angular resolution and a high signal to background ratio. Besides the appearance Of beta-Si(3)N(4) phase the intergranular phases Y(3)Al(5)O(12) (YAG) and Y(2)SiO(5) were identified in both samples. The refinement of the structural parameters by the Rietveld method indicated similar crystalline structure Of beta-Si(3)N(4) for both systems used as sintering additive. On the other hand, the intergranular phases Y(3)Al(5)O(12) and Y(2)SiO(5) shown a decrease of the lattice parameters, when E(2)O(3) was used as additive, indicating the formation of solid solutions of E(3)Al(5)O(12) and E(2)SiO(5), respectively. (C) 2007 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
Resumo:
BACKGROUND: The hydrolysis of hemicellulosic material can provide liquor with high xylose concentration (which can be used as a fermentation medium) and phenolic compounds (Phs), potentially immunostimulating compounds. However, these hydrolysates must be detoxified in order to remove the Phs that can act as inhibitors in bioconversions. RESULTS: Aqueous two-phase systems composed of thermoseparating copolymers were used for rice straw hydrolysate detoxification. The hydrolysis process was able to promote chemical breakdown of 85% of the total hemicellulose content, 14% of the cellulose, and 2% of the lignin. The hydrolysate obtained contained 19.7 g L-1 of xylose and several phenolic compounds, such as vanillin, vanillic acid, ferullic acid, etc. The phenolics extraction was studied as a function of copolymer molar mass (1100 g mol(-1), 2000 g mol(-1) and 2800 g mol(-1)), their percentages (from 5% to 50%) and Phs initial concentration. Phenolic compounds extraction of around 80% was obtained under the following conditions: 20% (w/w) and 35% (w/w) copolymer 1100 g mol-1, 35% (w/w) copolymer 2000 g mol(-1) and 35% (w/w) copolymer 2800 g mol(-1) at 25 degrees C. CONCLUSIONS: The results demonstrated the viability of this method for the removal of Phs from rice straw hydrolysate, which has potential uses in bioconversion processes. (c) 2007 Society of Chemical Industry.
Resumo:
In this work, SiC ceramics were liquid phase sintered (LPS), using AIN-Y(2)O(3) as additives, and oxidized at 1400 degrees C in air for up to 120 h. Oxidation was monitored by the weight gain of the samples as function of exposition time and temperature. A parabolic growth of the oxidation layer has been observed and the coefficient of the growth rate has been determined by relating the weight gain and the surface area. The effect of oxidation on strength has been determined by 4-point bending tests. Phase analysis by Xray diffraction and microstructural observation by scanning electron microscopy indicated the formation of a uniform and dense oxidation layer. The elimination of surface flaws and pores and the generation of compressive stresses in the surface resulted in a strength increase of the oxidized samples. (C) 2009 Published by Elsevier Ltd.