905 resultados para Size effects
Resumo:
ZnO thin films were prepared by pulsed laser deposition (PLD) on glass substrates with growth temperature from room temperature (RT) to 500 degrees C. The effects of substrate temperature on the structural and optical properties of ZnO films have been investigated by X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission spectra, and RT photoluminescence (PL) measurements. The results showed that crystalline and (0 0 2)-oriented ZnO films were obtained at all substrate temperatures. As the substrate temperature increased from RT to 500 degrees C, the ratio of grain size in height direction to that in the lateral direction gradually decreased. The same grain size in two directions was obtained at 200 degrees C, and the size was smallest in all samples, which may result in maximum E, and E-0 of the films. UV emission was observed only in the films grown at 200 degrees C, which is probably because the stoichiometry of ZnO films was improved at a suitable substrate temperature. It was suggested that the UV emission might be related to the stoichiometry in the ZnO film rather than the grain size of the thin film. (c) 2007 Elsevier Ltd. All rights reserved.
Resumo:
To investigate the effect of radiation damage on the stability and the compressive stress of cubic boron nitride (c-BN) thin films, c-BN films with various crystalline qualities prepared by dual beam ion assisted deposition were irradiated at room temperature with 300 keV Ar+ ions over a large fluence range up to 2 x 10(16) cm(-2). Fourier transform infrared spectroscopy (FTIR) data were taken before and after each irradiation step. The results show that the c-BN films with high crystallinity are significantly more resistant against medium-energy bombardment than those of lower crystalline quality. However, even for pure c-BN films without any sp(2)-bonded BN, there is a mechanism present, which causes the transformation from pure c-BN to h-BN or to an amorphous BN phase. Additional high resolution transmission electron microscopy (HRTEM) results support the conclusion from the FTIR data. For c-BN films with thickness smaller than the projected range of the bombarding Ar ions, complete stress relaxation was found for ion fluences approaching 4 x 10(15) cm(-2). This relaxation is accompanied, however, by a significant increase of the width of c-BN FTIR TO-line. This observation points to a build-up of disorder and/or a decreasing average grain size due to the bombardment. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
InGaN/GaN quantum dots were grown on the sapphire (0 0 0 1) substrate in a metalorganic chemical vapor deposition system. The morphologies of QDs deposited on different modified underlayer (GaN) surfaces, including naturally as grown, Ga-mediated, In-mediated, and air-passivated ones, were investigated by atomic force microscopy (AFM). Photo luminescence (PL) method is used to evaluate optical properties. It is shown that InGaN QDs can form directly on the natural GaN layer. However, both the size and distribution show obvious inhomogeneities. Such a heavy fluctuation in size leads to double peaks for QDs with short growth time, and broad peaks for QDs with long growth time in their low-temperature PL spectra. QDs grown on the Ga-mediated GaN underlayer tends to coalesce. Distinct transform takes place from 3D to 2D growth on the In-mediated ones, and thus the formation of QDs is prohibited. Those results clarify Ga and In's surfactant behavior. When the GaN underlayer is passivated in the air, and together with an additional low-temperature-grown seeding layer, however, the island growth mode is enhanced. Subsequently, grown InGaN QDs are characterized by a relatively high density and an improved Gaussian-like distribution in size. Short surface diffusion length at low growth temperature accounts for that result. It is concluded that reduced temperature favors QD's 3D growth and surface passivation can provide another promising way to obtain high-density QDs that especially suits MOCVD system. (c) 2004 Elsevier Ltd. All rights reserved.
Resumo:
The authors report the effects of rapid thermal annealing (RTA) on the emission properties of highly uniform self-assembled InAs quantum dots (QDs) emitting at 1.3 mu m grown on GaAs substrate by metal organic chemical vapor deposition. Postgrowth RTA experiments were performed under N-2 flow at temperatures ranging from 600 to 900 degrees C for 30 s using GaAs proximity capping. Surprisingly, in spite of the capping, large blueshifts in the emission peak (up to about 380 meV at 850 degrees C) were observed (even at low annealing temperatures) along with enhanced integrated photoluminescence (PL) intensities. Moreover, pronounced peak broadenings occurred at low annealing temperatures (< 700 degrees C), indicating that RTA does not always cause peak narrowing, as is typically observed with traditional QDs with large inhomogeneous PL linewidths. The mechanism behind the large peak blueshift was studied and found to be attributed to the as-grown QDs with large size, which cause a larger dot-barrier interface and greater strain in and near the QD regions, thereby greatly promoting Ga-In intermixing across the interface during RTA. The results reported here demonstrate that it is possible to significantly shift the emission peak of the QDs by RTA without any additional procedures, even at lower annealing temperatures. (c) 2007 American Institute of Physics.
Resumo:
The effects of growth temperature on the bimodal size distribution of InAs quantum dots on vicinal GaAs(100) substrates grown by metal organic chemical vapor deposition are studied. An abnormal trend of the bimodal size evolution on temperature is observed. With the increase of the growth temperature, while the density of the large dots decreases continually, that of the small dots first grows larger when temperature was below 520 degrees C, and then exhibits a sudden decrease at 535 degrees C. The trend is explained by taking into account the presence of multiatomic steps on the substrates. Photoluminescence (PL) studies show that quantum dots on vicinal substrates have a narrower PL linewidth, a longer emission wavelength, and a larger PL intensity than those of the dots with exact substrates. (c) 2006 American Institute of Physics.
Resumo:
The Hamiltonian of wurtzite quantum rods with an ellipsoidal boundary under electric field is given after a coordinate transformation. The electronic structure and optical properties are studied in the framework of the effective-mass envelope-function theory. The quantum-confined Stark effect is illustrated by studying the change of the electronic structures under electric field. The transition probabilities between the electron and hole states decrease sharply with the increase of the electric field. The polarization factor increases with the increase of the electric field. Effects of the electric field and the shape of the rods on the exciton effect are also investigated. The exciton binding energy decreases with the increase of both the electric field and the aspect ratio. In the end, considering the exciton binding energy, we calculated the band gap variation of size- and shape-controlled colloidal CdSe quantum rods, which is in good agreement with experimental results.
Resumo:
The influence of reactor pressure on GaN nucleation layer (NL) and the quality of subsequent GaN on sapphire is studied. The layers were grown by low-pressure metalorganic chemical vapor deposition (MOCVD) on c-plane sapphire substrates and investigated by in situ laser reflectometry, atomic force microscope, scanning electron microscope, X-ray diffraction and photoluminescence. With the increase of reactor pressure prior to high-temperature GaN growth, the size of GaN nuclei formed after annealing decreases, the spacing between nucleation sites increases and the coalescence of GaN nuclei is deferred. The optical and crystalline qualities of GaN epilayer were improved when NLs were deposited at high pressure. The elongated lateral overgrowth of GaN islands is responsible for the quality improvement. (C) 2003 Elsevier Science B.V. All rights reserved.
Resumo:
The structure and optical properties of In(Ga)As with the introduction of InGaAlAs or InAlAs seed dot layers are investigated. The area density and size homogeneity of the upper InGaAs dots are efficiently improved by the introduction of a buried layer of high-density dots. Our explanation for the realization of high density and size homogeneity dots is presented. When the GaAs spacer layer is too thin to cover the seed dots, the upper dots exhibit some optical properties like those of a quantum well. By analyzing the growth dynamics, we refer to this kind of dot as an empty-core dot. (C) 2003 American Institute of Physics.
Resumo:
Post-growth rapid thermal annealing has been performed with In(Ga)As quantum dots (QDs) at different strain statuses. It is confirmed that the strain-enhanced interdiffusion decreases the inhomogeneous size distribution. The preferential lateral interdiffusion of QDs during annealing was observed. we attribute it to the naturally anisotropic strain distribution in/around the dots and the saturation of strain difference between the base boundary and the top of the dots. There exist strain-enhanced mechanism and vacancy diffusion enhanced mechanism during the annealing. As to which one dominates the QD interdiffusion depends on the thickness of capping layer and the annealing temperature. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
The effect of growth interruption on the InAs deposition and its subsequent growth as self-assembled island structures, in particular the material transport process of the InAs layers has been investigated by photoluminescence and transmission electron microscopy measurements. InAs material in structures with only coherent islands transfers from the wetting layer to the formed islands and the growth interruption causes a red shift of PL peak energy. On the other hand, the PL peak shifts to higher energy in structures containing simultaneously coherent and noncoherent islands with dislocations. In this case, the noncoherent islands capture InAs material from the surrounding wetting layer as well as coherent islands, which casues a reduction in the size of these islands. The variations in the PL intensity and line width are also discussed. (C) 1998 Elsevier Science B.V. All rights reserved.
Resumo:
The effect of electric field on the electronic structure of a spherical quantum dot is studied in the framework of the effective-mass envelope-function theory. The dependence of the energy of electron states and hole states on the applied electric field and on the quantum dot size is investigated; the mixing of heavy holes and light holes is taken into account. The selection rule for the optical transition between the conduction band and valence band states is obtained. The exciton binding energies are calculated as functions of the quantum dot radius and the strength of the electric field. (C) 1998 American Institute of Physics.
Resumo:
Post-growth annealing was carried out on ZnO thin films grown by metal-organic chemical vapor deposition (MOCVD). The grain size of ZnO thin film increases monotonically with annealing temperature. The ZnO thin films were preferential to c-axis oriented after annealing as confirmed by Xray diffraction (XRD) measurements. Fourier transformation infrared transmission measurements showed that ZnO films grown at low temperature contains CO2 molecules after post-growth annealing. A two-step reaction process has been proposed to explain the formation mechanism of CO2, which indicates the possible chemical reaction processes during the metal-organic chemical vapor deposition of ZnO films.
Resumo:
The boundary condition at the solid surface is one of the important problems for the microfluidics. In this paper we study the effects of the channel sizes on the boundary conditions (BC), using the hybrid computation scheme adjoining the molecular dynamics (MD) simulations and the continuum fluid mechanics. We could reproduce the three types of boundary conditions (slip, no-slip and locking) over the multiscale channel sizes. The slip lengths are found to be mainly dependent on the interfacial parameters with the fixed apparent shear rate. The channel size has little effects on the slip lengths if the size is above a critical value within a couple of tens of molecular diameters. We explore the liquid particle distributions nearest the solid walls and found that the slip boundary condition always corresponds to the uniform liquid particle distributions parallel to the solid walls, while the no-slip or locking boundary conditions correspond to the ordered liquid structures close to the solid walls. The slip, no-slip and locking interfacial parameters yield the positive, zero and negative slip lengths respectively. The three types of boundary conditions existing in "microscale" still occur in "macroscale". However, the slip lengths weakly dependent on the channel sizes yield the real shear rates and the slip velocity relative to the solid wall traveling speed approaching those with the no-slip boundary condition when the channel size is larger than thousands of liquid molecular diameters for all of the three types of interfacial parameters, leading to the quasi-no-slip boundary conditions.
Resumo:
High quality ZnO films are successfully grown on Si(100) substrates by metal-organic chemical vapor deposition at 300℃. The effects of the thickness of the ZnO films on crystal structure, surface morphology,and optical properties are investigated using X-ray diffraction, scanning probe microscopy,and photoluminescence spectra, respectively. It is shown that the ZnO films grown on Si substrates have a highly-preferential C-axis orientation,but it is difficult to obtain the better structural and optical properties of the ZnO films with the increasing of thickness. It is maybe due to that the grain size and the growth model are changed in the growth process.
Resumo:
A third-order weighted essentially nonoscillatory and non-free-parameter difference scheme magnetohydrodynamic solver has been established to investigate the mechanisms of magnetohydrodynamics controlling separation induced by an oblique shock wave impinging on a flat plate. The effects of magnetohydrodynamic interaction-zone location on the separation point, reattachment point, separation-bubble size, and boundary-layer velocity profiles are analyzed. The results show that there exists a best location for the magnetohydrodynamic zone to be applied, where the separation point is delayed the farthest, and the separation bubble is decreased up to about 50% in size compared to the case without magnetohydrodynamic control, which demonstrated the promising of magnetohydrodynamics suppressing the separation induced by shock-wave/boundary-layer interactions.