892 resultados para Low bandgap materials
Resumo:
Although cementation is a widely recognized solidification/ stabilization process for immobilisation of Intermediate Level Radioactive Waste (ILRW), the low resistance to hyperalkaline pore waters compromises the effectiveness of the process when Portland Cement (PC) is employed. Moreover the manufacture of PC is responsible for significant CO2 emissions. In this context, low pH cements are environmentally more suitable and have emerged as a potential alternative for obtaining secure waste forms. This paper summarises the achievements on development of low-pH cements and the challenges of using these new materials for the ILRW immobilisation. The performance of waste forms is also discussed in terms of radionuclides release. Reactive magnesium oxide and magnesium phosphate cements are emphasised as they feature important advantages such as consumption of available constituents for controlling acid-base reactions, reduced permeability and higher density. Additionally, in order to identify new opportunities for study, the long-term modelling approach is also briefly discussed. Copyright © 2013 by ASME.
Resumo:
The third-order optical nonlinear refractive properties of InAs/GaAs quantum dots grown by molecular beam epitaxy have been measured using the reflection Z-scan technique at above-bandgap energy. The nonlinear refractive index and nonlinear absorption index of the InAs/GaAs quantum dots were determined for wavelengths from 740 to 777 nm. The measured results are compared with the nonlinear refractive response of several typical III-V group semiconductor materials. The corresponding mechanisms responsible for the large nonlinear response are discussed.
Resumo:
An efficient fabrication scheme of buried ridge waveguide devices is demonstrated by UV-light imprinting technique using organic-in organic hybrid sol-gel Zr-doped SiO2 materials. The refractive indices of a guiding layer and a cladding layer for the buried ridge waveguide structure are 1.537 and 1.492 measured at 1550 nm, respectively. The tested results show more circular mode profiles clue to existence of the cladding layer. A buried ridge single-mode waveguide operating at 1550 nm has a low propagation loss (0.088 dB/cm) and the 1 x 2 MMI power splitter exhibits uniform outputs, with a very low splitting loss of 0.029 dB at 1549 nm.
Resumo:
The traditional gate dielectric material Of SiO2 can not satisfy the need of the continuous downscaling of CMOS dimensions. High-K gate dielectric materials have attracted extensive research efforts recently and obtained great progress. In this paper, the developments of high-K gate materials were reviewed. Based on the author's background and research work in the area, the latest achievements of high-K gate dielectric materials on the recrystalization temperature, the low-K interface layer, and the dielectric breakdown and metal gate electrode were introduced in detail.
Resumo:
A new broadband filter, based on the high level bandgap in 1-D photonic crystals (PCs) of the form Si vertical bar air vertical bar Si vertical bar air vertical bar Si vertical bar air vertical bar Si vertical bar air vertical bar Si vertical bar air vertical bar Si is designed by the plane wave expansion method (PWEM) and the transfer matrix method (TMM) and fabricated by lithography. The optical response of this filter to normal-incident and oblique-incident light proves that utilizing the high-level bandgaps of PCs is an efficient method to lower the difficulties of fabricating PCs, increase the etching depth of semiconductor materials, and reduce the coupling loss at the interface between optical fibers and the PC device. (c) 2007 Society of Photo-Optical Instrumentation Engineers.
Resumo:
We have fabricated a set of samples of zincblende Mn-rich Mn(Ga)As clusters embedded in GaAs matrices by annealing (Ga,Mn)As films with different nominal Mn content at 650 degrees C. For the samples with Mn content no more than 4.5%, the Curie temperature reaches nearly 360 K. However, when Mn content is higher than 5.4%, the samples exhibit a spin-glass-like behavior. We suggest that these different magnetic properties are caused by the competing result of dipolar and Ruderman-Kittel-Kasuya-Yosida interaction among clusters. The low-temperature spin dynamic behavior, especially the relaxation effect, shows the extreme creeping effect which is reflected by the time constant tau of similar to 10(11) s at 10 K. We explain this phenomenon by the hierarchical model based on the mean-field approach. We also explain the memory effect by the relationship between the correlation function and the susceptibility.
Resumo:
Metal-semiconductor-metal (MSM) structures were fabricated by RF-plasma-assisted MBE using different buffer layer structures. One type of buffer structure consists of an AlN high-temperature buffer layer (HTBL) and a GaN intermediate temperature buffer layer (ITBL), another buffer structure consists of just a single A IN HTBL. Systematic measurements in the flicker noise and deep level transient Fourier spectroscopy (DLTFS) measurements were used to characterize the defect properties in the films. Both the noise and DLTFS measurements indicate improved properties for devices fabricated with the use of ITBL and is attributed to the relaxation of residue strain in the epitaxial layer during growth process. (C) 2003 Elsevier Ltd. All rights reserved.
Resumo:
1.5 mu m. n-type modulation-doping InGaAsP/InGaAsP strained multiple quantum wells grown by low pressure metalorganic chemistry vapor decomposition technology is reported for the first time in the world. N-type modulation-doped lasers exhibit much lower threshold current densities than conventional lasers with undoped barrier layers. The lowest threshold current density we obtained was 1052.5 A/cm(2) for 1000 mu m long lasers with seven quantum wells. The estimated threshold current density for an infinite cavity length was 94.72A/cm(2)/well, reduced by 23.3% compared with undoped barrier lasers. The n-type modulation doping effects on the lasing characteristics in 1.5 mu m devices have been demonstrated.
Resumo:
Microcrystalline silicon thin films at different growth stages were prepared by hot wire chemical vapor deposition. Atomic force microscopy has been applied to investigate the evolution of surface topography of these films. According to the fractal analysis I it was found that, the growth of Si film deposited on glass substrate is the zero-diffused stochastic deposition; while for the film on Si substrate, it is the finite diffused deposition on the initial growth stage, and transforms to the zero-diffused stochastic deposition when the film thickness reaches a certain value. The film thickness dependence of island density shows that a maximum of island density appears at the critical film thickness for both substrates. The data of Raman spectra approve that, on the glass substrate, the a-Si: H/mu c-Si:H transition is related to the critical film thickness. Different substrate materials directly affect the surface diffusion ability of radicals, resulting in the difference of growth modes on the earlier growth stage.
Resumo:
Using micro-photoluminescence technique, we observed a new photoluminescence peak about 0.348 eV above the bandgap of GaAs (E-0). By analyzing its optical characteristics, we assigned this peak to the nonequilibrium luminescence emission from the E-0 + Delta(0) bandgap in semi-insulated GaAs, which was further verified by Raman results. The observed polarization, excitation power dependence and temperature dependence of the photoluminescence spectra from the E-0 + Delta(0) energy level were very similar to those from the E-0 of GaAs. This mainly resulted from the common conduction band around Gamma(6) that was involved in the two optical transition processes, and indicated that the optical properties of bulk GaAs were mainly determined by the intrinsic properties of the conduction band. Our results demonstrated that the micro-photoluminescence technique is a powerful tool to investigate the high energy states above the fundamental bandgap in semiconductor materials.
Resumo:
In this paper, we analyze and compare electrical compensation and deep level defects in semi-insulating ( SI) materials prepared by Fe-doping and high temperature annealing of undoped InP. Influence of deep level defects in the SI-InP materials on the electrical compensation has been studied thermally stimulated current spectroscopy (TSC). Electrical property of the Fe-doped SI-InP is deteriorated due to involvement of a high concentration of deep level defects in the compensation. In contrast, the concentration of deep defects is very low in high temperature annealed undoped SI-InP in which Fe acceptors formed by diffusion act as the only compensation centre to pin the Fermi level, resulting in excellent electrical performance. A more comprehensive electrical compensation model of SI-InP has been given based on the research results.
Resumo:
Narrow stripe selective growth of oxide-free InGaAlAs/InGaAlAs multiple quantum wells (MQWs) has been successfully performed on patterned InP substrates by ultra-low pressure MOVPE. Flat and clear interfaces were obtained for the narrow stripe selectively grown MQWs under optimized growth conditions. These selectively grown MQWs were covered by specific InP layers, which can keep the MQWs from being oxidized during the fabrication of the devices. The characteristics of selectively grown MQWs were strongly dependent on the mask stripe width. In particular, a PL peak wavelength shift of 73 nm, a PL intensity of more than 57% and a PL FWHM of less than 102 meV were observed simultaneously with a small mask stripe width varying from 0 to 40 mu m. The results were explained by considering the migration effect from the masked region (MMR) and the lateral vapour diffusion effect (LVD).
Resumo:
The effects of In doped low-temperature (LT) AlGaN interlayer on the properties of GaN/Si(111) by MOCVD have been investigated. Using In doping LT-interlayer can decrease the stress sufficiently for avoiding crack formation in a thick (2.0 mu m) GaN layer. Significant improvement in the crystal and optical properties of GaN layer is also achieved. In doping is observed to reduce the stress in AlGaN interlayer measured by high-resolution X-ray diffraction (HRXRD). It can provide more compressive stress to counteract tensile stress and reduce crack density in subsequent GaN layer. Moreover, as a surfactant, indium is observed to cause an enhanced PL intensity and the narrowed linewidths of PL and XRD spectra for the LT-interlayer. Additionally, the crystal quality of GaN layer is found to be dependent on the growth parameters of underneath In-doped LT-AlGaN interlayer. The optimal parameters, such as TMIn flow rate, TMAl flow rates and thickness, are achieved to obtain nearly 2.0 mu m thick crack free GaN film with advanced optical and crystal properties. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
High quality InGaAsP/InGaAsP multiple quantum wells ( MQWs) have been selectively grown by ultra-low-pressure (22 mbar) metal-organic chemical vapor deposition. A large bandgap energy shift of 46 nm and photoluminescence with FWHM less than 30 meV were obtained with a rather small mask width variation (15-30 mu m). In order to study the uniformity of the MQWs grown in the selective area, novel tapered masks were employed, and the transition effect W the tapered region was also studied. The energy detuning of the tapered region was observed to be saturated at larger ratios of the mask width to the tapered region length.
Resumo:
Low temperature GaAs (LT-GaAs) was successfully grown at the temperature of 550 degrees C by metal organic vapor phase epitaxy on a semi-insular GaAs substrate. With such an absorber as well as an output coupler we obtain Q-switched mode-locked (QML) 1064 nm Nd:GdVO4 laser pumped by diode laser with high repetition rate, formed with a simple flat-flat cavity. The repetition rate of the Q-switched envelope increased from 100 to 660 kHz as the pump power increased from 2.28 to 7.29 W. The mode-locked pulses inside the Q-switched pulse envelope had a repetition rate of similar to 1.36 GHz. A maximum average output power of 953 mW was obtained. The dependence of the operational parameters on the pump power was also investigated experimentally. (C) 2005 Elsevier B.V. All rights reserved.