913 resultados para Luminescence spectroscopy


Relevância:

60.00% 60.00%

Publicador:

Resumo:

This is a work involving fundamental studies of chemistry where the synthesis and structural characterization, as well as a possible future application of these new compounds as luminescent sensors or sunscreen agents, complexes with 4,4 diaminostilbene-2,2-disulfonic (DSD) and trivalent lanthanide ions La3+, Nd3+, Eu3+, Gd3+ and Yb3+, were synthesized in the ratio of 3 mmol: 1 mmol (DSD: lanthanides). The complexes obtained with these ions were present in powder form and were characterized by complexometric titration with EDTA CHN Elemental analysis, molecular absorption spectroscopy in the ultraviolet region, the absorption spectroscopy in the infrared, thermal analysis (TG / DTG), Nuclear Magnetic Resonance - NMR 1H and Luminescence Spectroscopy. The complexometric titration and CHN analysis, confirmed the TG / DTG which suggest that these complexes have the following general chemical formulas: [La2(C14H12S2O6N2)2(H2O)2Cl2].7H2O,[Nd2(C14H12S2O6N2)2(H2O)2Cl2].6H2O,[Eu2(C14 H12S2O6N2)2(H2O)2Cl2].7H2O,[Gd2(C14H12S2O6N2)2(H2O)2Cl2].4H2O e [Yb2(C14H12S2O6N2)2(H2O)2].6H2O. The disappearance of the bands in the infrared spectrum at 2921 cm-1 and 2623 cm-1 and the displacement of the bands in the spectra of the amine complex indicate that the lanthanide ion is coordinated to the oxygen atoms and the sulfonate groups of the nitrogens amines, suggesting the formation of the dimer. The disappearance of the signal and the displacement signal SO3H amines in the 1H NMR spectrum of this complex are also indicative coordination and dimer formation. The Thermogravimetry indicates that the DSD is thermally stable in the range of 40º to 385°C and their complexes with lanthanide ions exhibit weight loss between 4 and 5 stages. The Uv-visible spectra indicated that the DSD and complexes exhibit cis isomers. The analysis of luminescence indicates that the complexes do not exhibit emission in the region of the lanthanides but an intense emission part of the binder. This is related to the triplet states of the ligand, which are in the lowest energy state emitting lanthanide ions, and also the formation of the dimer that suppress the luminescence of ion Eu3+. The formation of dimer was also confirmed by calculating the europium complex structure using the model Hamiltonian PM6 and Sparkle

Relevância:

60.00% 60.00%

Publicador:

Resumo:

This paper provides a review on the latest advances and applications of the luminescence spectroscopy for the development of pharmaceuticals analyses methods, basically based on the photo- and chemiluminescence. The different forms of the drugs determination on pharmaceuticals through the fluorescence and chemiluminescence are discussed. The analyses include the drugs native fluorescence (liquid and solid-phases); the fluorescence from the oxidizing or reducing forms of the drug; the fluorescence from the chemical derivatization and their photochemistry and hydrolysis reactions. The quenching of luminescence and chemiluminescence generation for the pharmaceutical quantification are also shown. Finally, the trends and future perspectives of the luminescence spectroscopy in the field of the pharmaceutical research are discussed.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

These films were obtained by dip coating. Parameters like dislocation velocity; number of deposits, suspension concentration, and number of deposits followed or not by heat treatment between each deposit and calcination temperature were evaluated for establishing the best homogeneity. The obtained films were characterized in terms of their morphology, optical quality and photoluminescence by scanning electron microscopy (SEM), UV-vis absorption spectrophotometry and luminescence spectroscopy, respectively. The morphologic and luminescent characteristics showed dip coating as good laboratory technique for development of thin films for optical applications.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The ZnO luminescent properties are strongly influenced by the preparation method and they are principally related to electronic and crystalline structures. This work reports about the correlation among luminescence properties of ZnO, obtained from zinc hydroxycarbonate, and crystalline lattice defects, microstrain, as function of thermal treatment. The crystallite size increase and the qualitative microstrain, obtained by Williamson-Hall plots, decrease as function of temperature. The evolution of electronic defects is analyzed by luminescence spectroscopy based on energy of the electronic transitions. From excitation spectrum, it is verified two bands around 377 nm and 405 nm attributed to the transitions between valence-conduction bands and valence band to interstitial zinc level, respectively. The emission spectra of sample treated at 600 degreesC shows large band at 670 nm. However, the green emission around 530 nm is observed for samples treated at 900 degreesC. The intensities of excitation and emission bands are associated with the increase of the electronic defects that depend on the strain lattice decrease. The lowest strain lattice results on the best green luminescent properties of zinc oxide. (C) 2001 Elsevier B.V. Ltd. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Pure yttrium oxide or mixed with europium oxide (3 at%) were treated in supercritical isopropanolic suspension at 500degreesC for 20 It and filling degree of 50%. Products were supercritically dried and characterized by scanning electron microscopy (SEM), X-ray powder diffraction (XRD), infrared spectroscopy (IR) and luminescence spectroscopy (LS). Particle shape is irregular with an equivalent diameter of ca. 5 mum. Cubic crystalline phase is mainly obtained and hydroxide ion in low concentration is detected by IR vibrational spectrum. Europium in this concentration does not extensively change such observed characteristics from the pure yttrium oxide. Luminescence spectra show that the doped product is a mixture of the two oxides added by oxyhydroxide impurities. Nevertheless, this precursor sample, after being heated at 900degreesC during 1 h, has all characteristics, especially luminescent ones, of the P22 commercial phosphor. (C) 2003 Elsevier B.V. (USA). All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Erbium-activated silica-based planar waveguides were prepared by three different technological routes: RF-sputtering, sol-gel and ion exchange. Various parameters of preparation were varied in order to optimize the waveguides for operation in the NIR region. Particular attention was devoted to the minimization of the losses and the increase of the luminescence efficiency of the metastable I-4(13/2) state of the Er3+ ion. Waveguide properties were determined by m-line spectroscopy and loss measurements. Waveguide Raman and luminescence spectroscopy were used to obtain information about the structure of the prepared films and about the dynamical processes related to the luminescence of the Er3+ ions.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

This work reports on the luminescence spectroscopy sensitivity in the determination of the phase purity in gadolinium compounds using Eu3+ as a probe. Cubic Gd2O3 and hexagonal Gd2O2S doped with Eu3+ spherical fine particles were obtained from doped gadolinium basic carbonates with morphological control and were also characterized by IR and XRD. Doped samples present Eu3+ characteristic transitions, with specific energy positions related to each phase. Emission and excitation spectra patterns were established for oxide and oxysulfide compounds, then oxysulfate and oxide impurities generated during oxysulfide preparation were monitored. From emission spectra some experimental intensity parameters were also calculated. All spectroscopic results reflect the presence or not of impurities in all compounds. (C) 2001 Elsevier B.V. Ltd. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

This work reports on the preparation of Gd2O3, cubic system, with spherical particles, narrow size distribution, whether or not doped with 1-5 at.% of Eu3+ and the influence of Eu3+ concentration on optical and morphological properties. Average diameter and size distribution particle analyses were performed for all samples from SEM results. Doped samples were also investigated by luminescence spectroscopy and emission kinetic measurements. All oxide samples present a particle average diameter distribution range from 110 to 150 nm and a decrease of particle average diameter with the presence of Eu3+. The particle size decrease is almost the same for all samples with different doping ion concentration. Therefore, the presence of doping ion may be inhibiting particle growth after the nucleation process. From spectroscopic studies, the doping ion distribution in the surface of oxide samples can be considered homogeneous because concentration quenching is not observed, as well as a significant difference among the calculated lifetime for each sample. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

In this work particles of ZnO of size range 33-56 Angstrom were prepared by a sol-gel method. The effect of reaction time on the particle size of ZnO or ZnO:Ce was investigated by transmission electron microscopy measurements, UV-vis absorption and luminescence spectroscopy. A linear increase of the mean particle size is observed as a function of reaction time. The cerium-doped particles are bigger than the pure ZnO ones obtained at the same reaction time. A shift to lower energy at the maximum of the bands is observed in all absorption, emission and excitation spectra as a function of particle growth. From the absorption spectra the optical energy gap values (Eg) for these particles were determined. In the quantum size regime, Eg was found to decrease with particle growth.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The effect of doping by europium triflate on the nanoscopic structure of organic-inorganic hybrid formed by a siliceous network containing pendant amine-terminated propyl chains, called aminosils, was investigated by Small-Angle X-ray Scattering (SAXS). It appears that the composites exhibit a two-level structure. The first level consists of well-condensed cubic-like siloxane octamers, with a radius of gyration around 2 angstrom. The second level is formed by the aggregation of these siloxane nanodomains to form larger structures, in which the nanodomains are spatially correlated and separated by the organic pendant chains. Europium doping inhibits the aggregation between siloxane octamers, leading to a less compact second-level structure. This can be explained by the Eu3+ stop coordination close to the external surface of the siloxane nanodomains, as detected by luminescence spectroscopy.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The synthesis and spectroscopic characterization of yttrium diphenylphosphinates doped with europium are reported. The purity of all samples was confirmed by carbon and hydrogen micro analysis, thermal analysis, IR vibrational spectroscopy, and X-ray diffraction. Luminescence spectra indicated the presence of two or more symmetry centers. The dynamic luminescence measurements suggested that one symmetry site presented an inversion center, while the others had lower symmetry. The average quantum yield of Eu3+ emission in the yttrium, matrices was 60%. (c) 2005 Elsevier B.V. All rights reserved.