Solvothermal method to obtain europium-doped yttrium oxide


Autoria(s): Davolos, Marian Rosaly; Feliciano, S.; Pires, Ana Maria; Marques, RFC; Jafelicci, M.
Contribuinte(s)

Universidade Estadual Paulista (UNESP)

Data(s)

20/05/2014

20/05/2014

15/02/2003

Resumo

Pure yttrium oxide or mixed with europium oxide (3 at%) were treated in supercritical isopropanolic suspension at 500degreesC for 20 It and filling degree of 50%. Products were supercritically dried and characterized by scanning electron microscopy (SEM), X-ray powder diffraction (XRD), infrared spectroscopy (IR) and luminescence spectroscopy (LS). Particle shape is irregular with an equivalent diameter of ca. 5 mum. Cubic crystalline phase is mainly obtained and hydroxide ion in low concentration is detected by IR vibrational spectrum. Europium in this concentration does not extensively change such observed characteristics from the pure yttrium oxide. Luminescence spectra show that the doped product is a mixture of the two oxides added by oxyhydroxide impurities. Nevertheless, this precursor sample, after being heated at 900degreesC during 1 h, has all characteristics, especially luminescent ones, of the P22 commercial phosphor. (C) 2003 Elsevier B.V. (USA). All rights reserved.

Formato

268-272

Identificador

http://dx.doi.org/10.1016/S0022-4596(02)00174-3

Journal of Solid State Chemistry. San Diego: Academic Press Inc. Elsevier B.V., v. 171, n. 1-2, p. 268-272, 2003.

0022-4596

http://hdl.handle.net/11449/35214

10.1016/S0022-4596(02)00174-3

WOS:000183207400042

Idioma(s)

eng

Publicador

Elsevier B.V.

Relação

Journal of Solid State Chemistry

Direitos

closedAccess

Palavras-Chave #Y2O3 : Eu #solvothermal #isopropanol #luminescence
Tipo

info:eu-repo/semantics/article