953 resultados para Single crystals


Relevância:

60.00% 60.00%

Publicador:

Resumo:

用浮区法生长得到了宽禁带半导体材料β-Ga2O3单晶,对其吸收光谱、荧光光谱进行了分析。解释了禁带部分展宽的原因。并研究了Sn^4+和Ti^4+的掺杂对其紫外吸收边影响。β-Ga2O3单晶的荧光谱不仅观察到了3个特征峰:紫外光(395nm)、蓝光(471nm)、绿光(559nm),还观察到了在277和297nm的紫外光和692nm的红光荧光发射。

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Sapphire crystals, 140 mm in diameter and 90 turn in height, have been grown by temperature gradient techniques (TGT). The growth direction of the boule was fixed by means of Lane X-ray diffraction. A prominent 204 nm absorption band in TGT-Al2O3. which does not appear in single crystals grown by Czochralski method has been studied. Analysis further substantiates the F-center model of this band. Two relatively weaker bands absorbing at 232 nm and 254 nm were ascribed to F+ centers. F-type centers concentration was determined using Smakula's equation. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

采用提拉法生长了Yb^3+掺杂量分别为5.4at%,16.3at%,27.1at%,53.6at%和100at%的Yb:Y3Al5O12晶体.系统地表征和分析了Yb^3+掺杂量对晶体吸收光谱和荧光光谱的影响.随着Yb^3+掺杂量的增加,各峰值吸收系数呈线性增加的趋势.应用Smakula公式计算了各吸收峰对应的振荡强度,并分析了Yb^3+掺杂量对振荡强度的影响.当Yb^3+掺杂量增加到27.1at%时观察到了荧光猝灭现象;当Yb^3+掺杂量增加到53.6at%时,荧光光谱的线形发生了很大的变化。

Relevância:

60.00% 60.00%

Publicador:

Resumo:

用提拉法生长了掺铬、钕的钆镓石榴石(Cr^4+,Nd^3+:GGG)自调Q激光品体。报道了室温下的吸收光谱和荧光光谱特性。分析了Cr离子浓度对光谱性质的影响。比较了Cr^4+:GGG,Nd^3+:GGG和(Cr^4+,Nd^3+):GGG晶体吸收光谱的关系。测量了(Cr^4+,Nd^3+):GGG晶体和Nd^3+:GGG晶体的荧光寿命,它们分别是33μs和250μs。实验表明,(Cr^4+,Nd^3+):GGG晶体是一种非常有潜力的自调Q激光晶体,可以实现大功率激光器的小型化和全固态化。

Relevância:

60.00% 60.00%

Publicador:

Resumo:

采用快速提拉法生长出了透明、完整的γ-LIAlO2晶体,但是晶体的高熔点和易挥发性限制了γ-LiAlO2晶体质量.采用气相传输平衡法(vapor transport equilibration technique,VTE)工艺对晶体改性,半高宽(FWHM)值从116.9arcsec降至44.2arcsec,继续升高VTE处理温度至1300℃,FWHM值反而升高至55.2arcsec.快速提拉法生长出来晶体,[100]方向和[001]方向的热膨胀系数分别为17.2398×10^-6/K,10.7664×10

Relevância:

60.00% 60.00%

Publicador:

Resumo:

It was first reported the spectral properties of a low-temperature sintered transparent Yb: Y2-2x La-2x O-3 laser ceramics. Yb: Y2-2x La-2x O-3 laser ceramics have broad absorption band and large absorption cross- section of 4.0 x 10(-20) cm(2) at wavelengths 977nm of the highest absorption peak. Its fluorescence lifetime is 1.1 ms, and the emission cross-sections are 1.0 x 10(-20) cm(2) and 0.7 x 10(-20) cm(2) at wavelengths 1033nm and 1077nm, respectively. All the optical properties are similar to those of single crystals.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

本试验测试了Er^3+掺杂钨酸铅晶体(PbWO4:Er^3+)的吸收光谱,依据J-O理论,首次计算报道了光谱项特征:J-O强度参数、量子荧光效率、荧光分支比等,Ω2=3.75×10^-20cm^2,Ω4=0.67×10^-20cm^2,Ω6=0.41×10^-20cm^2。计算证实,PWO:Er^3+中几乎有80%的激发能量非辐射跃迁转移致^4I13/2能级,^4I13/2的计算寿命是5200μs,J-O计算显示,在PWO中产生^4I13/2→^4I15/2和发射1.53μm.有高的几率。讨论了不同浓度E

Relevância:

60.00% 60.00%

Publicador:

Resumo:

采用提拉法生长Y3Al5O12(YAG)晶体和Yb3+掺杂原子数分数分别为5%, 10%, 15%, 20%, 25%, 50%和100%的Yb∶Y3Al5O12(Yb∶YAG)晶体。系统表征和分析了Yb3+掺杂浓度对拉曼光谱的影响。随着Yb3+掺杂浓度的增加,晶体的振动模式没有明显的变化,晶体结构没有改变;在370 cm-1和785 cm-1附近,振动吸收峰的半峰全宽逐渐增大。分析得出,Yb3+掺杂浓度对晶体的晶格、对称性、荧光寿命均有影响,从而可能影响到晶体的光谱和激光性能。

Relevância:

60.00% 60.00%

Publicador:

Resumo:

应用中频感应提拉法生长出掺杂浓度为10 at.-%的Yb:YAG与Yb:YAP晶体,对比了室温下两种晶体的吸收和发射光谱特性。结果表明,Yb:YAG晶体比Yb:YAP晶体有更好的激光性能和低的阈值;同时对比发现,Yb:YAP晶体的吸收截面是Yb:YAG晶体的2.16倍,它容易实现LD泵;由于Yb:YAP晶体的各向异性,它有轴向效应明显,它可以产生偏振激光。

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The electronic structures and absorption spectra for the perfect PbMoO4 crystal and the crystal containing lead vacancy V-Pb(2-) with lattice structure optimized are calculated using density functional theory code CASTEP. The calculated absorption spectra of the PbMoO4 crystal containing V-Pb(2-) exhibit three absorption bands peaking at 2.0 eV (620 nm), 3.0 eV (413 run) and 3.3 eV (375 nm), which are in good agreement with experimental values. The theory predicts that the 390 nm, 430 nm and 580 run absorption bands are related to the existence of V-Pb(2-) in the PbMoO4 crystal.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Mg0.4Al2.4O4 single crystals with good optical quality were successfully grown by the Czochralski method. The transmission spectrum indicated that the absorption edge of the crystal was at 220nm, while no apparent absorption peaks were found. The X-ray diffraction and DSC curve analysis showed that Mg0.4Al2.4O4 crystal was stable at room temperature. While after annealing in the air and hydrogen atmosphere at about 1200 degrees C,Mg0.4Al2.4O4 decomposed into Al2O3 and (MgO)(0.4)(Al2O3)(x) (0.4 < x < 1.2). The reaction mainly occurred on the crystal surface, barely inside. (C) 2008 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

In nickel-based superalloys, substitutional solute species have a strong impact on in service mechanical properties as well as on oxidation and corrosion resistances. In alloy 718, recent studies carried out by tensile tests highlighted the fact that refractory solute species are able to interact strongly with mobile dislocations during plastic deformation, generating dynamic strain ageing, and, in wide ranges of tests temperatures and strain rates, Portevin-Le Chatelier effect. The precise nature of the substitutional element responsible for such a dynamic interaction is still subject to debate. We addressed this question by means of mechanical spectroscopy studies of alloy 718 and various related alloys corresponding to monitored changes in the chemical composition. Only a single internal friction relaxation peak has been observed for all the studied alloys. By analyzing the damping behavior of these alloys at different imposed solicitation frequencies by sweeping a large temperatures range, the activation energies of the relaxation process and the type of mechanism involved have been determined. The process is a "Zener relaxation" in the alloys, i.e. a substitutional atoms dipole reorientation under applied stress. The results tend to prove that Niobium is not involved in the relaxation process whereas Molybdenum content seems to play an important role in the relaxation intensity.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Atualmente grande parte dos resíduos descartados rotineiramente no Brasil é composta por material plástico como, por exemplo, o polietileno de alta densidade (PEAD), o qual é muito comum no lixo doméstico. Nesta Dissertação, embalagens de PEAD pós-consumo foram coletadas e moídas. Após processamento em extrusora, o material definido como PEAD reciclado (mistura de embalagens brancas, marfins e incolores) foi injetado e as propriedades mecânicas foram avaliadas e comparadas com uma amostra de PEAD comercial (HD7600U). A análise térmica através da calorimetria exploratória diferencial (DSC), em conjunto com a análise estatística dos resultados experimentais, também foi conduzida. Em relação à resistência à tração, a diferença entre as amostras de PEAD reciclado e PEAD comercial foram tão pouco expressivas que, dentro das condições experimentais adotadas, se pode afirmar que o material reciclado é equivalente ao comercial.Por sua vez, os modelos cinéticos aplicados na análise térmica revelaram quea amostra de PEAD comercial demonstra um processo de nucleação e crescimento dos cristais mais homogêneo e simples, embora a energia de ativação seja consideravelmente maior do que o das demais amostras de PEAD.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Analyses of crack growth under cyclic loading conditions are discussed where plastic flow arises from the motion of large numbers of discrete dislocations and the fracture properties are embedded in a cohesive surface constitutive relation. The formulation is the same as used to analyse crack growth under monotonic loading conditions, differing only in the remote loading being a cyclic function of time. Fatigue, i.e. crack growth in cyclic loading at a driving force for which the crack would have arrested under monotonic loading, emerges in the simulations as a consequence of the evolution of internal stresses associated with the irreversibility of the dislocation motion. A fatigue threshold, Paris law behaviour, striations, the accelerated growth of short cracks and the scaling with material properties are outcomes of the calculations. Results for single crystals and polycrystals will be discussed.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Bulk, polycrystalline MgB2 samples containing 2.5 wt.% multi-walled carbon nanotubes (CNTs) have been prepared by conventional solid state reaction at 800 °C. The effect of Mg precursor powders composed of two different particle sizes on the critical current density (Jc) of the as-sintered samples has been investigated. An enhancement of Jc at high field has been observed in MgB2 samples containing CNTs prepared with fine Mg powders, whereas the values of Jc in the sample prepared using the coarser Mg powders was slightly decreased. These results contrast significantly with measurements on pure, undoped, MgB2 samples prepared from the same Mg precursor powders. They suggest that carbon substitution into the MgB2 lattice, which accounts for increased flux pinning, and therefore Jc, is more effective in precursor Mg powders with a larger surface area. Rather surprisingly, the so-called fishtail effect, observed typically in MgB2 single crystals and in the (RE)BCO family of high temperature superconductors (HTSs), was observed in both sets of CNT-containing polycrystalline samples as a result of lattice defects associated with C substitution. Significantly, analytical fits to the data for each sample suggest that the same flux pinning mechanism accounts for the fishtail effect in polycrystalline MgB2 and (RE)BCO. © 2013 Elsevier B.V. All rights reserved.