955 resultados para LAYER THICKNESS
Resumo:
A new structure of GaAs photocathode was introduced. The Be-doping concentration is variable in the new structure compared with the constant concentration of Be in the normal photocathode. Negative electron affinity GaAs photocathodes were fabricated by alternate input of Cs and O. The spectral response results measured by the on-line spectral response measurement system show that the integrated photosensitivity of the photocathodes with the new structure is enhanced by at least 50% as compared to those with the monolayer structure. Accordingly, two main factors leading to the enhanced photosensitivity of the photocathodes were discussed. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
The growth of InAs quantum dots on vicinal GaAs (100) Substrates was systematically studied using low-pressure metalorganic chemical vapor deposition (MOCVD). The dots showed a clear bimodal size distribution on vicinal substrates. The way of evolution of this bimodal size distribution was studied as a function of growth temperature, InAs layer thickness and InAs deposition rate. The optical properties of dots grown on vicinal substrates were also studied by photoluminescence (PL). It was found that, compared with dots on exact substrates, dots on vicinal substrates had better optical properties such as a narrower PL line width, a longer emission wavelength, and a larger PL intensity. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
The control of shape and spatial correlation of InAs-InAlAs-InP(001) nanostructure superlattices has been realized by changing the As overpressure during the molecular-beam epitaxy (MBE) growth of InAs layers. InAs quantum wires (QWRs) are obtained under higher As overpressure (1x10(-5) Torr), while elongated InAs quantum dots (QDs) are formed under lower As overpressure (5x10(-6) or 2.5x10(-6) Torr). Correspondingly, spatial correlation changes from vertical anti-correlation in QWR superlattices to vertical correlation in QD superlattices, which is well explained by the different alloy phase separation in InAlAs spacer layers triggered by the InAs nanostrcutures. It was observed that the alloy phase separation in QD superlattices could extend a long distance along the growth direction, indicating the vertical correlation of QD superlattices can be kept in a wide range of spacer layer thickness.
Resumo:
In order to understand the growth feature of GaN on GaAs (0 0 1) substrates grown by metalorganic chemical vapor deposition (MOCVD), the crystallinity of GaN buffer layers with different thicknesses was investigated by using double crystal X-ray diffraction (DCXRD) measurements. The XRD results showed that the buffer layers consist of predominantly hexagonal GaN (h-GaN) and its content increases with buffer layer thickness. The nominal GaN (111) reflections with chi at 54.74degrees can be detected easily, while (0 0 2) reflections are rather weak. The integrated intensity of reflections from (111) planes is 4-6 times that of (0 0 2) reflections. Possible explanations are presented. (C) 2003 Elsevier Science B.V. All rights reserved.
Resumo:
Ta is often used as a buffer layer in magnetic multilayers. In this study, Ta/Ni81Fe19/Ta multilayers were deposited by magnetron sputtering on sing-crystal Si with a 300-nm-thick SiO2 film. The composition and chemical states at the interface region of SiO2/Ta were studied using the X-ray photoelectron spectroscopy (XPS) and peak decomposition technique. The results show that there is an 'inter-mixing layer" at the SiO2/Ta interface due to a thermodynamically favorable reaction: 15 SiO2 + 37 Ta = 6 Ta2O5 + 5 Ta5Si3. Therefore, the Ta buffer layer thickness used to induce NiFe (111) texture increases.
Resumo:
Thermal processing of strained In0.2Ga0.8As/GaAs graded-index separate confinement heterostructure single quantum well laser diodes grown by molecular beam epitaxy is investigated. It is found that rapid thermal annealing can improve the 77K photoluminescence efficiency and electron emission from the active layer, due to the removal of nonradiative centers from the InGaAs/GaAs interface. Because of the interdiffusion of Al and Ga atoms, rapid thermal annealing increases simultaneously the density of DX centers in the AlGaAs graded layer. The current stressing experiments of postgrowth and annealed laser diodes are indicative of a corresponding increase in the concentration of DX centers, suggesting that DX centers may be responsible for the degradation of laser diode performance.
Resumo:
SiO2/Si/SiO2 nanometer double barriers (SSSNDB) with Si layers of twenty-seven different thicknesses in a range of 1-5 nm with an interval of 0.2 nm have been deposited on p-Si substrates using two-target alternative magnetron sputtering. Electroluminescence (EL) from the semitransparent Au film/SSSNDB/p-Si diodes and from a control diode without any Si layer have been observed under forward bias. Each EL spectrum of all these diodes can be fitted by two Gaussian bands with peak energies of 1.82 and 2.25 eV, and full widths at half maximum of 0.38 and 0.69 eV, respectively. It is found that the current, EL peak wavelength and intensities of the two Gaussian bands of the Au/SSSNDB/p-Si structure oscillate synchronously with increasing Si layer thickness with a period corresponding to half a de Broglie wavelength of the carriers. The experimental results strongly indicate that the EL originates mainly from two types of luminescence centres with energies of 1.82 and 2.25 eV in the SiO2 barriers, rather than from the nanometer Si well in the SSSNDB. The EL mechanism is discussed in detail.
Resumo:
We investigated properties of intraband absorption in In-x Ga1-xAs quantum dots (QDs) superlattice. Energy levels in conduction band in QDs were calculated for a cone-shaped quantum dot associated with coupling between QDs in the framework of the effective-mass envelope-function theory. Theoretical results demonstrated that energy levels in conduction band were greatly affected by the vertical coupling between quantum dots, which can be used to modify transition wavelength by adjusting the space layer thickness. Intraband transition is really sensitive to normal incidence and the absorption peak intensity is dependent on the polarization. A satisfying agreement is found between theoretical and experimental values. This result opens up prospects for the fabrication of QDs infrared detectors, which work at atmospheric windows.
Resumo:
Three n-p-n Si/SiGe/Si heterostructures with different layer thickness and doping concentration have been grown by a home-made gas source molecular-beam epitaxy (GSMBE) system using phosphine (PH3) and diborane (B2H6) as n-and p-type in situ doping sources, respectively. Heterojunction bipolar transistors (HBTs) have been fabricated using these structures and a current gain of 40 at 300 K and 62 at 77 K have been obtained. The influence of thickness and doping concentration of the deposited layers on the current gain of the HBTs is discussed. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
We show that part of the reflectance difference resonance near the E-0 energy of ZnSe is due to the anisotropic in-plane strain in the ZnSe thin films, as films grown on three distinctly different substrates, GaAs, GaP, and ZnS, all show the resonance at the same energy. Such anisotropic strain induced resonance is predicted and also observed near the E-1/E-1+Delta(1) energies in ZnSe grown on GaAs. The theory also predicts that there should be no resonance due to strain at, the E-0+Delta(0) energy, which is consistent with experiments. The strain anisotropy is rather independent of the ZnSe layer thickness, or whether the film is strain relaxed. For ZnSe films with large lattice mismatch with substrates, the resonance at the E-1/E-1+Delta(1) energies is absent, very likely due to the poor crystalline quality of the 20 nm or so surface layer. (C) 2000 American Vacuum Society. [S0734-211X(00)05604-3].
Resumo:
An X-ray diffraction method, estimating the strain relaxation in an ultrathin layer, has been discussed by using kinematic and dynamical X-ray diffraction (XRD) theory. The characteristic parameter Delta Omega, used as the criterion of the strain relaxation in ultrathin layers, is deduced theoretically. It reveals that Delta Omega should be independent of the layer thickness in a coherently strained layer. By this method, we characterized our ultrathin GaNxAs1-x samples with N contents up to 5%. XRD measurements show that our GaNxAs1-x layers are coherently strained on GaAs even for such a large amount of N. Furthermore, a series of GaNxAs1-x samples with same N contents but different layer thicknesses were also characterized. It was found that the critical thickness (L-c) of GaNAs in the GaAs/GaNAs/GaAs structures determined by XRD measurement was 10 times smaller than the theoretical predictions based on the Matthews and Blakeslee model. This result was also confirmed by in situ observation of reflection high-energy electron diffraction (RHEED) and photoluminescence (PL) measurements. RHEED observation showed that the growth mode of GaNAs layer changed from 2D- to 3D-mode as the layer thickness exceeded L-c. PL measurements showed that the optical properties of GaNAs layers deteriorated rapidly as the layer thickness exceeded L-c. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
We demonstrate that the carrier capture and relaxation processes in InAs/GaAs quantum dots can be detected by a simple degenerate pump-probe technique. We have observed a rising process in the transient reflectivity, following the initial fast relaxation in a GaAs matrix, and assigned this rising process to the carrier capture from the GaAs barriers to the InAs layers. The assignment was modeled using the Kramers-Kronig relations. The capture time was found to depend strongly on the InAs layer thickness as well as on the excitation density and photon energy. (C) 2000 Elsevier Science Ltd. All rights reserved.
Resumo:
After capping InAs islands with a thin enough GaAs layer, growth interruption has been introduced. Ejected energy of self-organized InAs/GaAs quantum dots has been successfully tuned in a controlled manner by changing the thickness of GaAs capping layer and the time of growth interruption and InAs layer thickness. The photoluminescence (PL) spectra showing the shift of the peak position reveals the tuning of the electronic states of the QD system. Enhanced uniformity of Quantum dots is observed judging from the decrease of full width at half maximum of FL. Injection InAs/GaAs quantum dot lasers have been fabricated and performed on various frequencies. (C) 2000 Published by Elsevier Science B.V. All rights reserved.
Resumo:
Using a newly-developed population mixing technique we have studied the exciton dynamics in self-organized InAs/GaAs quantum dots (QDs). It is found that the exciton lifetime in self-organized InAs/GaAs QDs is around 1 ns, almost independent of InAs layer thickness. The temperature dependence of the exciton lifetime varies from sample to sample, but no obvious experimental evidence was found that the lifetime is related to the delta-function of density of states in QDs. We have also found that the population mixing technique can be used to directly reveal the band-filling effect in the excited states of the QDs.
Resumo:
Periodicity fluctuations of layer thickness and composition in a superlattice not only decrease the intensity, they also broaden the width of the satellite peaks in the x-ray diffraction pattern. In this letter, we develop a method that is dependent on the width of satellite peaks to assess periodicity fluctuations of a superlattice quickly. A linear relation of the magnitude of fluctuations, peak width and peak order has been derived from x-ray diffraction kinematical theory. By means of this method, periodicity fluctuations in strained (GaNAs)(1)(GaAs)(m) superlattices grown on GaAs substrates by molecular beam epitaxy have been studied. Distinct satellite peaks indicate that the superlattices are of high quality. The N composition of 0.25 and its fluctuation of 20% in a strained GaNxAs1-x monolayer are obtained from simulations of the measured diffraction pattern. The x-ray simulations and in situ observation results of reflection high-energy electron diffraction are in good agreement. (C) 1999 American Institute of Physics. [S0003-6951(99)00828-1].