907 resultados para Metallurgical Engineer
Resumo:
Although titanium and Ti-6Al-4V alloy have been widely used as dental materials, possible undesirable effects such as cytotoxic reactions and neurological disorder due to metal release led to the development of more corrosion resistant and V and Al free titanium alloys, containing Nb, Zr, Mo and Ta atoxic elements. Fluoride containing products used in the prevention of plaque formation and dental caries can affect the stability of the passive oxide films formed on the Ti alloys. In this work, the corrosion behaviour of the new Ti-23Ta alloy has been evaluated in artificial saliva of different pH and fluoride concentration using electrochemical impedance spectroscopy. Electrochemical impedance spectroscopy study showed that the oxide film formed on the alloy in artificial saliva consists of an inner compact film and an outer porous layer. The corrosion resistance of Ti-23Ta alloy which is reduced by increasing F concentration or decreasing pH is related to the resistance of the inner compact layer. The presence of fluoride and low pH of the saliva enhance the porosity of the oxide film and its dissolution.
Resumo:
The thermal expansion anisotropy of the V(5)Si(3) and T(2)-phase of the V-Si-B system were determined by high-temperature X-ray diffraction from 298 to 1273 K. Alloys with nominal compositions V(62.5)Si(37.5) (V5Si3 phase) and V(63)Si(12)B(25) (T(2)-phase) were prepared from high-purity materials through arc-melting followed by heat-treatment at 1873 K by 24 h, under argon atmosphere. The V(5)Si(3) phase exhibits thermal expansion anisotropy equals to 1.3, with thermal expansion coefficients along the a and c-axis equal to 9.3 x 10(-6) K(-1) and 11.7 x 10(-6) K(-1), respectively. Similarly, the thermal expansion anisotropy value of the T(2)-phase is 0.9 with thermal expansion coefficients equal to 8.8 x 10(-6) K(-1) and 8.3 x 10(-6) K(-1) along the, a and c-axis respectively. Compared to other isostructural silicides of the 5:3 type and the Ti(5)Si(3) phase, the V(5)Si(3) phase presents lower thermal expansion anisotropy. The T(2)-phase present in the V-Si-B system exhibits low thermal expansion anisotropy, as the T(2)-phase of the Mo-Si-B, Nb-Si-B and W-Si-B systems. (C) 2009 Elsevier Ltd. All rights reserved.
Resumo:
Ti-6Al-4V alloy has been widely used in restorative surgery due to its high corrosion resistance and biocompatibility. Nevertheless, some studies showed that V and Al release in the organism might induce cytotoxic effects and neurological disorders, which led to the development of V-free alloys and both V- and Al-free alloys containing Nb, Zr, Ta, or Mo. Among these alloys, Ti-13Nb-13Zr alloy is promising due to its better biomechanical compatibility than Ti-6Al-4V. In this work, the corrosion behavior of Ti, Ti-6Al-4V, and Ti-xNb-13Zr alloys (x=5, 13, and 20) was evaluated in Ringer`s solution (pH 7.5) at 37 degrees C through open-circuit potential measurements, potentiodynamic polarization, and electrochemical impedance spectroscopy. Spontaneous passivity was observed for all materials in this medium. Low corrosion current densities (in the order of 10(-7) A/cm(2)) and high impedance values (in the order of 10(5) Omega cm(2) at low frequencies) indicated their high corrosion resistance. EIS results showed that the passivating films were constituted of an outer porous layer (very low resistance) and an inner compact layer (high resistance), the latter providing the corrosion resistance of the materials. There was evidence that the Ti-xNb-13Zr alloys were more corrosion resistant than both Ti and Ti-6Al-4V in Ringer`s solution.
Resumo:
Results of the surface modification of Ti-16Si-4B powder alloy by nitrogen ion implantation are presented, together with the experimental description of the preparation of that powder by high-energy ball milling and hot pressing. The phase structure, chemical composition and morphology of sample surfaces were observed by utilizing X-ray diffractometer (XRD), atomic force microscope (AFM) and scanning electron microscopy (SEM). A tribological characterization was carried out with a ball-on-disc tribometer and an SEM. Friction coefficient is compared with the one obtained for Ti-6Al-4V alloy and the wear scars characterized by SEM/EDS (energy dispersive spectroscopy). The concentration profile of the detected elements have been investigated using Auger electron spectroscopy (AES) depth profiling. Our results show that a shallow implanted layer of oxygen and nitrogen ions were obtained at the Ti-16Si -4B alloy surface, sufficient to modify slightly its tribological properties. Crown Copyright (C) 2011 Published by Elsevier Ltd. All rights reserved.
Resumo:
Hot tensile and creep tests were carried out on Kanthal A1 alloy in the temperature range from 600 to 800 degrees C. Each of these sets of data were analyzed separately according to their own methodologies, but an attempt was made to find a correlation between them. A new criterion proposed for converting hot tensile data to creep data, makes possible the analysis of the two kinds of results according to usual creep relations like: Norton, Monkman-Grant, Larson-Miller and others. The remarkable compatibility verified between both sets of data by this procedure strongly suggests that hot tensile data can be converted to creep data and vice-versa for Kanthal A1 alloy, as verified previously for other metallic materials.
Resumo:
In this work, SiC ceramics were liquid phase sintered (LPS), using AIN-Y(2)O(3) as additives, and oxidized at 1400 degrees C in air for up to 120 h. Oxidation was monitored by the weight gain of the samples as function of exposition time and temperature. A parabolic growth of the oxidation layer has been observed and the coefficient of the growth rate has been determined by relating the weight gain and the surface area. The effect of oxidation on strength has been determined by 4-point bending tests. Phase analysis by Xray diffraction and microstructural observation by scanning electron microscopy indicated the formation of a uniform and dense oxidation layer. The elimination of surface flaws and pores and the generation of compressive stresses in the surface resulted in a strength increase of the oxidized samples. (C) 2009 Published by Elsevier Ltd.
Resumo:
The crystallisation behaviour for alloys in the Al-rich corner in the Al-La-Ni system is reported in this paper Alloys were selected based on the topological instability criterion (lambda criterion) calculated from the alloy composition and metallic radii of the alloying elements and aluminum Amorphous ribbons were produced by melt-spinning and the crystallisation reactions were analysed by X-ray diffraction and calorimetry The results showed that increasing the values of lambda from 0.072 to 0.16 resulted in the following changes in the crystallisation behaviour, as predicted by the lambda criterion (a) nanocrystallisation of alpha-Al for the alloy composition corresponding to lambda = 0 072 and (b) detection of the glass transition temperature, T(g), for the alloys with composition close to lambda approximate to 0.1 line. For compositions corresponding to both ends of the lambda approximate to 0 1 line (near the binaries lines) T(g) could be detected only in the ""intermediary"" central region, and the alloy we produced in this region was considered the best glass former for the Al-rich corner Also, except for the alloys with the highest NI content, crystallisation proceeded by two distinct exothermic peaks which are typical of nanocrystallisation transformation. These behaviours are discussed in terms of compositional (lambda parameter) and topological aspects to account for cluster formation in the amorphous phase. Crown Copyright (C) 2009 Published by Elsevier B V All rights reserved
Resumo:
The design of supplementary damping controllers to mitigate the effects of electromechanical oscillations in power systems is a highly complex and time-consuming process, which requires a significant amount of knowledge from the part of the designer. In this study, the authors propose an automatic technique that takes the burden of tuning the controller parameters away from the power engineer and places it on the computer. Unlike other approaches that do the same based on robust control theories or evolutionary computing techniques, our proposed procedure uses an optimisation algorithm that works over a formulation of the classical tuning problem in terms of bilinear matrix inequalities. Using this formulation, it is possible to apply linear matrix inequality solvers to find a solution to the tuning problem via an iterative process, with the advantage that these solvers are widely available and have well-known convergence properties. The proposed algorithm is applied to tune the parameters of supplementary controllers for thyristor controlled series capacitors placed in the New England/New York benchmark test system, aiming at the improvement of the damping factor of inter-area modes, under several different operating conditions. The results of the linear analysis are validated by non-linear simulation and demonstrate the effectiveness of the proposed procedure.
Resumo:
A unidirectional fiber composite is considered here, the fibers of which are empty cylindrical holes periodically distributed in a transversely isotropic piezoelectric matrix, The empty-fiber cross-section is circular and the periodicity is the same in two directions at an angle pi/2 or pi/3. Closed-form formulae for all electromechanical effective properties of these 3-1 longitudinally periodic porous piezoelectric materials are presented. The derivation of such expressions is based on the asymptotic homogenization method as a limit of the effective properties of two-phase transversely isotropic parallel fiber-reinforced composites when the fibers properties tend to zero. The plane effective coefficients satisfy the corresponding Schulgasser-Benveniste-Dvorak universal type of relations, A new relation among the antiplane effective constants from the solutions of two antiplane strains and potential local problems is found. This relation is valid for arbitrary shapes of the empty-fiber cross-sections. Based on such a relation, and using recent numerical results for isotropic conductive composites, the antiplane effective properties are computed for different geometrical shapes of the empty-fiber cross-section. Comparisons with other analytical and numerical theories are presented. (c) 2008 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
In this paper results of tests on 32 concrete-filled steel tubular columns under axial load are reported. The test parameters were the concrete compressive strength, the column slenderness (L/D) and the wall thickness (t). The test results were compared with predictions from the codes NBR 8800:2008 and EN 1994-1-1:2004 (EC4). The columns were 3, 5, 7 and 10 length to diameter ratios (L/D) and were tested with 30MPa, 60MPa, 80MPa and 100MPa concrete compressive strengths. The results of ultimate strength predicted by codes showed good agreement with experimental results. The results of NBR 8800 code were the most conservative and the EC4 showed the best results, in mean, but it was not conservative for usual concrete-filled short columns.
Resumo:
The use of mechanical shear connectors, mainly headed stud bolts, is the most common way to achieve steel-concrete composite action. The encasement of the steel beam in the depth slab results in increase of strength and stiffness, reducing the total height of the floor. In this investigation, three partially encased composite beams were tested under flexural conditions and the main objective was to investigate some alternative positions for the headed studs. To provide longitudinal shear resistance between the I-shaped beam and the concrete, two positions of the,studs were investigated: vertically welded on the bottom flange and horizontally welded on the faces of the web. The experimental results have shown that the headed studs are effective to provide the composite action and increase the bending strength. Furthermore, the headed studs welded vertically on the bottom flange proved to be the most reliable position.
Resumo:
The transport of liquid and gaseous pollutants through porous geological media depends on the physical and chemical characteristics of the unconsolidated material, rocks and water associated with the characteristics of the pollutants. Of these characteristics, the sorption aspect is of fundamental importance and is a function of the mineral proportions, pH, Eh and void aspects encountered in the porous media. In the Sao Carlos region, located in the eastern-central part of the 9 ate of Sao Paulo, Brazil, there are basically two types of unconsolidated materials: the first is a residual from sandstones cemented with fines and the secondarily composed of claystones, siltstones and conglomerates from the Cretaceous Period that constitute the Itaqueri Formation; the second is a sandy sediment of the Tertiary Period. These geological conditions are found in areas where chemical products are disposed of characterized as either diffuse or point pollutions sources. Because of this situation, a study was developed to evaluate the sorption aspects of some inorganic cations that are frequently found in these sources, in varied concentrations. Taken into consideration were their physical/chemical properties, such as: specific weight, grain size, mineralogy, cationic exchange capacity, pH, hydraulic conductivity. Batch tests were run using solutions of KCl, ZnCl(2) and CuCl center dot H(2)O at three different pH values, and then with a combined solution (KCl + ZnCl(2) + CuCl center dot H(2)O), also at three different pH values.
Resumo:
The internal stresses and crystallographic texture in alpha-Al(2)O(3) scales grown on iron aluminides at 1100 degrees C were determined in situ using synchrotron X-ray diffraction. In the first hour of oxidation, alpha-Al(2)O(3) was formed by direct nucleation and by conversion from transition oxides (either theta-Al(2)O(3) or a mixed Fe-Al oxide). A sharp texture develops connected with the direct nucleation of alpha-Al(2)O(3), in contrast to the weaker texture observed in alpha-Al(2)O(3) originated by previous transformations, which also yielded tensile stresses in early oxidation stages. (C) 2011 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
This work evaluates the glass formation of selected alloys based on the Ti-Zr-Fe-Co system, assuming the synergy of two distinct criteria: minimum topological instability and average electronegativity plots. Combining the minimum topological instability and the average electronegativity values result in a plot in which the most probable good glass former compositions are identified Ti-Zr rich alloys with Fe and Co additions were produced, compared against the final plot, and the best glass forming alloy composition was found to be very close the theoretically predicted ones on the Ti-Zr rich side, for both Ti-Zr-Fe and Ti-Zr-Co systems. (C) 2009 Elsevier B V All rights reserved
Resumo:
Alloys of Al-Sn and Al-Si are widely used in tribological applications such as cylinder liners and journal bearings. Studies of the influence of the as-cast microstructures of these alloys on the final mechanical properties and wear resistance can be very useful for planning solidification conditions in order to permit a desired level of final properties to be achieved. The aim of the present study was to contribute to a better understanding about the relationship between the scale of the dendritic network and the corresponding mechanical properties and wear behavior. The Al-Sn (15 and 20 wt pct Sn) and Al-Si (3 and 5 wt pct Si) alloys were directionally solidified under unsteady-state heat flow conditions in water-cooled molds in order to permit samples with a wide range of dendritic spacings to be obtained. These samples were subjected to tensile and wear tests, and experimental quantitative expressions correlating the ultimate tensile strength (UTS), yield tensile strength, elongation, and wear volume to the primary dendritic arm spacing (DAS) have been determined. The wear resistance was shown to be significantly affected by the scale of primary dendrite arm spacing. For Al-Si alloys, the refinement of the dendritic array improved the wear resistance, while for the Al-Sn alloys, an opposite effect was observed, i.e., the increase in primary dendrite arm spacing improved the wear resistance. The effect of inverse segregation, which is observed for Al-Sn alloys, on the wear resistance is also discussed.