The effect of film orientation on piezoelectric and ferroelectric properties of bismuth layered compounds deposited on platinum coated silicon substrates was investigated. Piezo-force microscopy was used to probe the local piezoelectric properties of Bi(4)Ti(3)O(12), CaBi(4)Ti(4)O(15) and SrBi(4)Ti(4)O(15) films. Our measurements on individual grains clearly reveal that the local piezoelectric properties are determined by the polarization state of the grain. A piezoelectric coefficient of 65 pm/V was attained after poling in a grain with a polar axis very close to the normal direction. The piezoelectric coefficient and the remanent polarization were larger for a-b axes oriented than for c-axis-oriented films. (c) 2007 Elsevier B.V All rights reserved.
Resumo:
A detector system that can measure X-ray intensity in the mammographic range of 22 to 36 kVp (equivalent photon energies ofthe beam between 11 and 15 keV) is presented. It consists of a lithium mobate detector and a high-sensitivity current-to-voltage converter.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Thin films of potassium niobate were deposited on (100) Si substrates by the polymeric precursor method (Pechini method). Annealing in static air was performed at 600degrees C for 20 h. The obtained films were characterized by X-ray diffraction and atomic force microscopy (AFM). Electrical characterization of the films pointed to ferroelectricity via hysteresis loop. The dielectric constant, dissipation factor and resistance were measured in frequency region from 10 Hz to 10 MHz. At 1 MHz, the dielectric constant was 158 and the dissipation factor was 0.11. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Ultasonic spray pyrolysis (SP) has been investigated for the production of the barium strontium titanate (BST) powders from the polymeric precursors. The processing parameters, such as flux of aerosol and temperature profile inside the furnace, were optimized to obtain single phase BST. The powders were characterized by the methods of X-ray diffraction analysis, SEM, EDS and TEM. The obtained powders were submicronic, consisting of spherical, polycrystalline particles, with internal nanocrystalline structure. Crystallite size of 10 nut, calculated using Rietveld refinement, is in a good agreement with results of HRTEM. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Lanthanum-modified bismuth titanate, Bi4-xLaxTi3O12 (BLT), with x ranging from 0 to 0.75 was grown on Pt/Ti/SiO2/Si substrates using a polymeric precursor solution and spin-coating method. The dielectric constant of highly doped bismuth titanate was equal to 148 while dielectric losses remained low (tan delta = 0.0018), and the films showed well-saturated polarization-electric field curves (2P(r) = 40.6 muC/cm(2) and V-c = 0.99 V). The leakage current densities improve for the lanthanum-doped system. For five-layered BLT films with x = 0.75, a charge storage density of 35 fC/mum(2) and a thickness of 320 nm were found. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)